Detection of the electronic structure of iron-(III)-oxo oligomers forming in aqueous solutions
(2017)
The nature of the small iron-oxo oligomers in iron-(III) aqueous solutions has a determining effect on the chemical processes that govern the formation of nanoparticles in aqueous phase. Here we report on a liquid-Jet photoelectron-spectroscopy experiment for the investigation of the electronic structure of the occurring iron-oxo oligomers in FeCl3 aqueous solutions. The only iron species in the as-prepared 0.75 M solution are Fe3+ monomers. Addition of NaOH initiates Fe3+ hydrolysis which is followed by the formation of iron-oxo oligomers. At small enough NaOH concentrations, corresponding to approximately [OH]/[Fe] = 0.2–0.25 ratio, the iron oligomers can be stabilized for several hours without engaging in further aggregation. Here, we apply a combination of non-resonant as well as iron 2p and Oxygen 1s resonant photoelectron spectroscopy from a liquid microjet to detect the electronic structure of the occurring species. Specifically, the oxygen 1s partial electron yield X-ray absorption (PEY-XA) spectra are found to exhibit a peak well below the onset of liquid water and OH (aq) absorption. The iron 2p absorption gives rise to signal centered between the main absorption bands typical for aqueous Fe3+. Absorption bands in both PEY-XA spectra are found to correlate with an enhanced photoelectron Peak near 20 eV binding energy, which demonstrates the sensitivity of resonant photoelectron (RPE) spectroscopy to mixing between iron and ligand orbitals. These various signals from the iron-oxo oligomers exhibit Maximum intensity at [OH]/[Fe] = 0.25 ratio. For the same ratio, we observe changes in the pH as well as in complementary Raman spectra, which can be assigned to the Transition from monomeric to oligomeric species. At approximately [OH]/[Fe] = 0.3 we begin to observe particles larger than 1 nm in radius, detected by small-angle X-ray scattering.
Polynuclear aluminium species (Al13 keggin cluster) find application in different areas like water purification, contaminant transport, and as pilling clays with high specific surface areas, due to their strong binding ability to aggregates and high positive charge.
In the present contribution, we report on the in situ investigation of the Al13 sulfate synthesis by synchrotron wide-angle X-ray scattering (WAXS). Al13 cluster were crystallized by precipitating hydrolyzed aluminum solutions by the addition of sodium sulfate. The measurements were performed using a custom-made acoustic levitator as sample holder. The study provides information about the intermediates during the crystallization process. From the data, a mechanism was derived indicating the influence of the crystallization process.
Iron can form numerous oxides, hydroxides, and oxide−hydroxides. Despite their relevance, many of the transformation processes between these phases are still poorly understood. In particular the crystallization of quasi-amorphous hydroxides and oxide−hydroxides is difficult to assess, since typical diffraction and scattering methods provide only sampleaveraged information about the crystallized phases. We report a new approach for the investigation of the crystallization of oxide−hydroxides. The approach relies on model-type films that comprise a defined homogeneous nanostructure. The nanostructure allows quantitative linking of Information obtained by bulk-averaging diffraction techniques (XRD, SAXS) with locally resolved information, i.e., Domain sizes (SEM, TEM, LEEM) and phase composition (SAED). Using time-resolved imaging and diffraction we deduce mechanism and kinetics for the crystallization of ferrihydrite into hematite. Hematite forms via nucleation of hematite domains and subsequent Domain growth that terminates only upon complete transformation. A Johnson−Mehl−Avrami−Kolmogorov model describes the kinetics over a wide temperature range. The derived understanding enables the first synthesis of ferrihydrite films with ordered mesoporosity and quantitative control over the films’ hematite and ferrihydrite content.
The mechanochemical synthesis of the zinc N-(phosphonomethyl)glycinate Zn(O₃PCH₂NH₂CH₂CO₂) H₂O is presented. The structure was solved from powder X-ray diffraction (PXRD) data. In the three-dimensional pillared structure, the Zn atoms are coordinated tetrahedrally. In situ investigations of the reaction process with synchrotron PXRD and Raman spectroscopy reveal a two-step process including the formation of an intermediate.