Filtern
Erscheinungsjahr
- 2017 (14) (entfernen)
Dokumenttyp
Sprache
- Englisch (14)
Schlagworte
- Cermet (4)
- Hardness (3)
- Liquid phase sintering (3)
- Microstructure (3)
- Wear (3)
- Carbon (2)
- Friction (2)
- Graphite furnace (2)
- High-resolution continuum source absorption spectrometry (2)
- Molecular absorption (2)
Lanthanide-doped upconversion nanoparticles (UCNPs) are of great interest for biomedical applications. Currently, the applicability of UCNP bionanotechnology is hampered by the generally low luminescence intensity of UCNPs and inefficient energy Transfer from UCNPs to surface-bound chromophores used e.g. for photodynamic therapy or analyte sensing. In this work, we address the low-Efficiency issue by developing versatile core-Shell nanostructures, where high-concentration sensitizers and activators are confined in the core and Shell Region of representative hexagonal NaYF2:Yb,Er UCNPs. After Doping concentration optimization, the sensitizer-rich core is able to harvest/accumulate more excitation energy and generate almost one order of Magnitude higher luminescence intesity than conventional homogeneously doped nanostructures. At the same time, the activator Ions located in the Shell enable a ~6 times more efficient resonant energy Transfer from UCNPs to surface-bound acceptor dye molecules due to the short distance between donor-acceptor pairs. Our work provides new insights into the rational design of UCNPs and will greatly encrease the General applicability of upconversion nanotechnologies.
Under the Comité Consultatif pour la Quantité de Matière (CCQM), a key comparison, CCQM-K104, was coordinated by the National Institute of Metrology (NIM). The comparison was designed to demonstrate a laboratory's performance in determining the mass fraction of the main component in a complex high purity organic material. Nine NMIs or DIs participated in the comparison. Eight participants reported their results. An additional impurity was resolved from the avermectin B1a peak and was tentatively identified as an unknown impurity by NMIA (National Measurement Institute (Australia)). It was subsequently identified by NIM as a diastereoisomer of avermectin B1a at the C-26 position. Final reference value (KCRV) = 924.63 mg/g, with uncertainty (k=1) = 3.89 mg/g, and expanded uncertainty = 8.97 mg/g. The degrees of equivalence with the avermectin B1a KCRV for each participant were reported. The measurement results and degrees of equivalence should be indicative of the performance of a laboratory's measurement capability for the purity assignment of organic compounds of high structural complexity (relative molecular mass range of 500 Da -1000 Da and low polarity (-log KOW ≤ -2).
The current study reports on the influence of the Addition of 5–15 vol% VC or/and Mo2C carbide on the microstructure and mechanical properties of nickel bonded NbC cermets, which are compared to cobalt bonded NbC cermets. The NbC, Ni and secondary carbides powder mixtures were liquid phase sintered for 1 h at 1420 °C in vacuum. The fully densified cermets are composed of a cubic NbC grains matrix and an evenly distributed fcc Ni binder. NbC grain growth was significantly inhibited and a homogeneous NbC grain size distribution was obtained in the cermets with VC/Mo2C additions. The mechanical properties of the NbC-Ni matrix cermets are strongly dependent on the carbide and Ni binder content and are directly compared to their NbC-Co equivalents.
The liquid phase sintered NbC-12 vol% Ni cermet had a modest Vickers hardness (HV30) of 1077 ± 22 kg/mm2 and an indentation toughness of 9.1 ± 0.5 MPa·m1/2. With the addition of 10–15 vol% VC, the hardness increased to 1359 ± 15 kg/mm2, whereas the toughness increased to 11.3 ± 0.1 MPa·m1/2. Addition of 5 and 10 vol% Mo2C into a NbC-12 vol% Ni mixtures generated the same values in HV30 and KIC when compared to VC additions. A maximum flexural strength of 1899 ± 77 MPa was obtained in the cermet with 20 vol% Ni binder and 4 vol% VC+4 vol% Mo2C addition, exhibiting a high fracture toughness of 15.0 ± 0.5 MPa·m1/2, but associated with a loss in hardness due to the high Ni content. The dry sliding wear behaviour was established at room temperature and 400 °C from 0.1 to 10 m/s.
A mono-component intumescent flame retardant named ethylenediamine-modified ammonium polyphosphate (MAPP) is used in polyethylene-octene elastomer (POE). Insight into the flame-retardant mechanisms of the MAPP is provided from a new perspective. The fire performance of POE/MAPP composites is investigated by oxygen index (OI) and vertical burning (UL-94) tests. POE Composite containing 35 wt% MAPP achieves a V-0 rating, and its OI is 29.3 vol%. The thermogravimetric Analysis (TGA) and Fourier transform infrared spectra (FTIR) confirm that the incorporation of ethylenediamine changes the thermal decomposition of APP, mainly resulting in the formation of char layer with a thermally stable structure. Cone calorimeter analysis revealed the flame-retardant modes of action of MAPP in POE under forced-flaming conditions. Quantitative analysis illustrates that both the residue due to charring and the fuel dilution/flame Inhibition resulting from the release of incombustible products/ phosphorus species decrease the total heat release (fire load) by 20e28%. The residue increases linearly with increasing MAPP content, whereas the reduction in effective heat of combustion levels off. Moreover, the flame-retardant effect resulting from the protective properties of the char is discovered to be the dominant mode of action (up to 85% reduction) with respect to the peak heat release rate, leading to the excellent flame retardancy of POE/MAPP.
The self-ignition of coal dust deposits and its subsequent smoldering combustion pose a high fire hazard to oxy-fuel power systems which burn fuels using pure oxygen for the sake of carbon capture and storage. The increasing risk of explosion in the gas-phase and self-ignition in the solid-phase for an oxygen enhanced combustion environment has not been well studied yet. In this work, the heterogeneous reactions of a bituminous coal dust are investigated by using a novel hot-basket apparatus with an emphasis on the roles of O2 and diluent gas in chemisorption and smoldering. Experiments show that increasing O2 mole fraction accelerates both self-ignition and the following smoldering combustion. On the other hand, the presence of CO2 increases the ignition temperature and reduces the maximum smoldering temperature. However, the promotion in the fire and explosion risk by elevating O2 mole fraction is substantially stronger than the retardation effected by presence of CO2. The emission-gas measurements show that the CO to CO2 ratio increases significantly after self-ignition, and CH4 counts for 1–8% of the total carbon emission. This research may help improve the understanding of heterogeneous coal combustion and the fire safety in oxy-fuel power systems.
For the purpose of finding suitable molecules applicable to sulfur determination and to compare their analytical sensitivity systematically, high-resolution overview molecular absorption spectra of sulfides of group 14 elements produced in a graphite furnace were investigated. To that end a modular simultaneous echelle spectrograph (MOSES) was used, which allows recording sub-ranges of spectra out of a total wavelength range from 190 nm to 735 nm. The combined overview spectra show a complex structure with many vibrational bands, each of them consisting of a multitude of sharp rotational lines. The absorption of rotational lines of SiS (282.910 nm), GeS (295.209 nm), SnS (271.578 nm), and PbS (335.085 nm) has been analyzed for optimizing the particular experimental conditions regarding to the sulfur determination. Using the commercial CS AAS instrument contrAA 600 under optimized conditions such as the temperature program, the modification of the platform with Zr and the use of chemical modifiers, the achieved characteristic masses for sulfur are 12 ng (CS), 15.7 ng (SiS), 9.4 ng (GeS), 20 ng (SnS), and 220 ng (PbS). The first four sulfides provide an analytical sensitivity with roughly the same level, but the GeS molecule seems to be the best one with respect to analytical sensitivity and flexibility in molecular formation control. The PbS molecule provides the lowest analytical sensitivity, and together with its low bond strength it is not recommended for sulfur determination.
Boron isotope amount ratios n(10B)/n(11B) have been determined by monitoring the absorption spectrum of boron monohydride (BH) in a graphite furnace using high-resolution continuum source molecular absorption spectrometry (HR-CS-MAS). Bands (0→0) and (1→1) for the electronic transition X1Σ+ → A1Π were evaluated around wavelengths 433.1 nm and 437.1 nm respectively. Clean and free of memory effect molecular spectra of BH were recorded. In order to eliminate the memory effect of boron, a combination of 2% (v/v) hydrogen gas in argon and 1% trifluoromethane in argon, an acid solution of calcium chloride and mannitol as chemical modifiers was used. Partial least square regression (PLS) for analysis of samples and reference materials were applied. For this, a spectral library with different isotopes ratios for PLS regression was built. Results obtained around the 433.1 nm and 437.1 nm spectral regions are metrologically compatible with those reported by mass spectrometric methods. Moreover, for the evaluated region of 437 nm, an accuracy of 0.15‰ is obtained as the average deviation from the isotope reference materials. Expanded uncertainties with a coverage factor of k = 2 range between 0.15 and 0.44‰. This accuracy and precision are compatible with those obtained by mass spectrometry for boron isotope ratio measurements.