Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (24)
- Beitrag zu einem Tagungsband (4)
- Sonstiges (1)
Sprache
- Englisch (29) (entfernen)
Schlagworte
- Computed tomography (5)
- Neutron tomography (4)
- Tomography (4)
- Neutron imaging (3)
- Neutron radiography (3)
- Darkfield imaging (2)
- Hydrogen diffusion (2)
- Hydrogen embrittlement (2)
- Iterative reconstruction (2)
- Magnetic domains (2)
Organisationseinheit der BAM
Paper des Monats
- ja (1)
X-ray compton tomography
(2014)
The potentials of incoherent X-ray Scattering (Compton) tomography are investigated. Imaging materials of very different density or atomic number at once is a perpetual challenge for X-ray tomography or radiography, in general. In a basic laboratory set-up for simultaneous perpendicular Compton Scattering and direct beam attenuation tomographic scans are conducted by single channel photon counting. This results in asymmetric distortions of the projection profiles of the scattering CT-data set. ln a first approach corrections of Compton scattering data by taking advantage of rotational symmetry yield tomograms without major geometric artefacts.
A cylindrical sample composed of PE, PA, PVC, glass and wood demonstrates similar Compton contrast for all the substances, while the conventional absorption tomogram only reveals the two high order materials.
Compärison to neutron tomography reveals astonishing similarities except for the glass component (without hydrogen). Therefore, Compton CT bears the potential to replace neutron tomography, which requires much more efforts.
The potentials of incoherent X-ray scattering (Compton) computed tomography (CT) are investigated. The imaging of materials of very different atomic number or density at once is generally a perpetual challenge for X-ray tomography or radiography. In a basic laboratory set-up for simultaneous perpendicular Compton scattering and direct beam attenuation tomography are conducted by single channel photon counting line scans. This results in asymmetric distortions of the projection profiles of the scattering CT data set. In a first approach, corrections of Compton scattering data by taking advantage of rotational symmetry yield tomograms without major geometric artefacts. A cylindrical sample composed of PE, PA, PVC, glass and wood demonstrates similar Compton contrast for all the substances, while the conventional absorption tomogram only reveals the two high order materials. Comparison to neutron tomography
reveals astonishing similarities except for the glass component (without hydrogen). Therefore, Compton CT offers the potential to replace neutron tomography, which requires much more efforts.
Rechargeable sodium–oxygen batteries (NaOBs) are receiving extensive research interests because of their advantages such as ultrahigh energy density and cost efficiency. However, the severe failure of Na metal anodes has impeded the commercial development of NaOBs. Herein, combining in situ synchrotron X-ray computed tomography (SXCT) and other complementary characterizations, a novel electro-chemo-mechanical failure mechanism of sodium metal anode in NaOBs is elucidated. It is visually showcased that the Na metal anodes involve a three-stage decay evolution of a porous Na reactive interphase layer (NRIL): from the initially dot-shaped voids evolved into the spindle-shaped voids and the eventually-developed ruptured cracks. The initiation of this three-stage evolution begins with chemical-resting and is exacerbated by further electrochemical cycling. From corrosion science and fracture mechanics, theoretical simulations suggest that the evolution of porous NRIL is driven by the concentrated stress at crack tips. The findings illustrate the importance of preventing electro-chemo-mechanical degradation of Na anodes in practically
rechargeable NaOBs.
We present a synchrotron X-ray tomographic study on the morphology of carbon fiber-based gas diffusion layer (GDL) material under compression. A dedicated compression device is used to provide well-defined compression conditions. A flat compression punch is employed to study the fiber geometry at different degrees of compression. Transport relevant geometrical parameters such as porosity, pore size and tortuosity distributions are calculated. The geometric properties notably change upon compression which has direct impact on transport conditions for gas and fluid flow. The availability of broad 3D paths, which are most important for the transport of liquid water from the catalyst layer through the GDL, is markedly reduced after compression. In a second experiment, we study the influence of the channel-land-pattern of the flow-field on shape and microstructure of the GDL. A flow-field compression punch is employed to reproduce the inhomogeneous compression conditions found during fuel cell assembly. While homogenously compressed underneath the land the GDL is much less and inhomogeneously compressed under the channel. The GDL material extends far into the channel volume where it can considerably influence gas and fluid flow. Loose fiber endings penetrate deeply into the channel and form obstacles for the discharge of liquid water droplets.
This paper gives a brief overview on3D imaging of magnetic domains with shearing grating neutron tomography. We investigated the three-dimensional distribution of magnetic domain walls in the bulk of a wedge-shaped FeSi single crystal. The width of the magnetic domains wasanalyzed at different locations within the crystal. Magnetic domains close to the tip of the wedge are much smaller than in the bulk. Furthermore, the three-dimensional shape of individual domains wasinvestigated. We discuss prospects and limitations of the applied measurement technique.
Magnetic domains have been the subject of much scientific investigation since their theoretical existence was first postulated by P.-E. Weiss over a century ago. Up to now, the three-dimensional (3D) domain structure of bulk magnets has never been observed owing to the lack of appropriate experimental methods. Domain analysis in bulk matter thus remains one of the most challenging tasks in research on magnetic materials. All current domain observation methods are limited to studying surface domains or thin magnetic films. As the properties of magnetic materials are strongly affected by their domain structure, the development of a technique capable of investigating the shape, size and distribution of individual domains in three dimensions is of great importance. Here, we show that the novel technique of Talbot-Lau neutron tomography with inverted geometry enables direct imaging of the 3D network of magnetic domains within the bulk of FeSi crystals.
We investigated hydrogen embrittlement and blistering in electrochemically hydrogen-charged technical iron samples at room temperature. Hydrogen-stimulated cracks and blisters and the corresponding hydrogen distributions were observed by neutron tomography. Cold neutrons were provided by the research reactor BER II to picture the sample with a spatial resolution in the reconstructed three-dimensional model of ~25 µm. We made the unique observation that cracks were filled with molecular hydrogen and that cracks were surrounded by a 50 µm wide zone with a high hydrogen concentration. The zone contains up to ten times more hydrogen than the bulk material. The hydrogen enriched zone can be ascribed to a region of increased local defect density. Hydrogen also accumulated at the sample surface having the highest concentration at blistered areas. The surfaces of the brittle fractured cracks showed micropores visualized by scanning electron microscopy. The micropores were located at grain boundaries and were surrounded by stress fields detected by electron backscattered diffraction. The cracks clearly originated from the micropores.
The neutron imaging instrument CONRAD was operated as a part of the user program of the research reactor BER‐II at Helmholtz‐Zentrum Berlin (HZB) from 2005 to 2020. The Instrument was designed to use the neutron flux from the cold source of the reactor, transported by a curved neutron guide. The pure cold neutron spectrum provided a great advantage in the use of different neutron optical components such as focusing lenses and guides, solid‐state polarizers, Monochromators and phase gratings. The flexible setup of the instrument allowed for implementation of new methods including wavelength‐selective, dark‐field, phase‐contrast and imaging with polarized neutrons. In summary, these developments helped to attract a large number of scientists and industrial customers, who were introduced to neutron imaging and subsequently contributed to the Expansion of the neutron imaging community.
Rechargeable alkali metal−CO2 batteries, which combine high theoretical energy density and environmentally friendly CO2 fixation ability, have attracted worldwide attention. Unfortunately, their electrochemical performances are usually inferior for practical applications. Aiming to reveal the underlying causes, a combinatorial usage of advanced nondestructive and postmortem characterization tools is used to intensively study the failure mechanisms of Li/Na−CO2 batteries. It is found that a porous interphase layer is formed between the separator and the Li/Na anode during the overvoltage rising and battery performance decaying process. A series of control experiments are designed to identify the underlying mechanisms dictating the observed morphological evolution of Li/Na anodes, and it is found that the CO2 synergist facilitates Li/Na chemical corrosion, the process of which is further promoted by the unwanted galvanic corrosion and the electrochemical cycling conditions. A detailed compositional analysis reveals that the as-formed interphase layers under different conditions are similar in species, with the main differences being their inconsistent quantity. Theoretical calculation results not only suggest an inherent intermolecular affinity between the CO2 and the electrolyte solvent but also provide the most thermodynamically favored CO2 reaction pathways. Based on these results, important implications for the further development of rechargeable alkali metal−CO2 batteries are discussed. The current discoveries not only fundamentally enrich our knowledge of the failure mechanisms of rechargeable alkali metal−CO2 batteries but also provide mechanistic directions for protecting metal anodes to build high-reversible alkali metal−CO2 batteries.
Understanding the complicated interplay of the continuously evolving electrode materials in their inherent 3D states during the battery operating condition is of great importance for advancing rechargeable battery research.
In this regard, the synchrotron X-ray tomography technique, which enables non-destructive, multi-scale, and 3D imaging of a variety of electrode components before/during/after battery operation, becomes an essential tool to deepen this understanding. The past few years have witnessed an increasingly growing interest in applying this technique in battery research. Hence, it is time to not only summarize the already obtained battery-related Knowledge by using this technique, but also to present a fundamental elucidation of this technique to boost future studies in battery research. To this end, this review firstly introduces the fundamental principles and experimental Setups of the synchrotron X-ray tomography technique. After that, a user guide to ist application in battery research and examples of its applications in Research of various types of batteries are presented. The current review ends with a discussion of the future opportunities of this technique for next-generation rechargeable batteries research. It is expected that this review can enhance the reader’s understanding of the synchrotron X-ray tomography technique and stimulate new ideas and opportunities in battery research.