Nickel‐free high‐nitrogen‐alloyed stainless steels like the P2000 (X13CrMnMoN18‐14‐3) were developed to enhance the strength and corrosion resistance of austenitic stainless steels like 304 and 316 while keeping the typical high ductility. The mechanical and corrosive properties of P2000 were investigated and compared with 304 and 316 to highlight the application opportunities of this new alloy. The microstructure of the solution‐annealed condition was characterised by electron backscatter diffraction and the mechanical properties were studied by uniaxial tensile tests, Charpy impact tests and hardness measurements. The passivation behaviour was analysed using the electrochemical potentiodynamic reactivation, whereas the pitting corrosion resistance was compared by pitting potentials and pitting temperatures. However, secondary thermal influences or suboptimal heat treatment can impair the corrosion resistance due to the precipitation of secondary phases and the resulting sensitisation. Thermodynamic calculations and artificial ageing treatment in the range of 500–900°C for up to 100 h were used to determine critical time–temperature parameters for sensitisation. The microstructure of the various aged states was evaluated by scanning electron microscopy and compared with the degrading corrosion resistance characterised by the KorroPad method.
This contribution will show that gel-type electrolytes influence protective layers on zinc coatings considerably less than typical bulk electrolytes. Different zinc coatings are investigated, their naturally formed protective layers are electrochemically characterized and corrosion relevant values are determined by using a gel pad based on polysaccharide. From the results it is evident that gel-type electrolytes represent a viable and promising field in corrosion research.
Limitations are encountered regarding the electrolyte when studying atmospheric corrosion reactions on materials that form protective layers on their surface or tend to passivate. For example, the reconstruction of a thin wet film, as well as the interpretation of electrochemical measurements in so-called bulk solutions (a "mass" of electrolyte), often proves to be difficult in view of corrosion behavior under atmospheric conditions. A new approach to this problem in corrosion research includes the use of gel-type electrolytes as an alternative to bulk electrolytes. Gel-type electrolytes form a thin wet film on the surface of the material, whereby the naturally formed protective layer is affected similar to atmospheric conditions and can be examined in an almost non-destructive way. Through electrochemical instrumentation specific values such as polarization resistances and corrosion currents can be determined providing information on kinetics of surface layer formation and stability of surface layers formed under the influence of a thin wet film. Thus, new test methods can be developed that supply a better understanding of corrosion processes in specific atmospheres.
In this article different zinc coatings and aluminium alloys were investigated, their naturally formed protective layers were electrochemically characterized and corrosion relevant values were determined by using a gel pad based on polysaccharide. Corrosion relevant values allowed the differentiation of various coating systems and could describe the current protective effect provided by the coating. It is shown that gel-type electrolytes influence protective layers and coatings considerably less than corresponding bulk electrolytes and that an atmospheric wet film is approached by these test conditions. From the results it is evident that gel-type electrolytes represent a viable and promising field in corrosion research.
In the presentation different zinc coatings are presented and investigated. Their naturally formed protective layers are electrochemically characterized and corrosion relevant values are determined by using a gel pad based on polysaccharide. The corrosion relevant values allow the differentiation of various zinc coating systems and can describe the current protective effect provided by the coating. It is shown that gel-type electrolytes influence protective layers and coatings considerably less than corresponding bulk electrolytes. From the results it is evident that gel-type electrolytes represent a viable and promising field in corrosion research.
. Hard coated steel components are used in a wide application range, mostly for protective, wear resistant and decorative purposes. Despite of these coatings being regarded as relatively dense, there is always a high risk of localized corrosion when a coated low alloyed steel component encounters a surrounding high humidity atmosphere or even an aqueous medium. An approach to enhance the corrosion properties is the addition of magnesium to physical vapor deposited hard coatings, like TiN. It has been found that there is a remarkable increase in corrosion resistance in dependence of magnesium content of the TiMgN coating and its surface properties. In this work the authors will explain the underlying corrosion protection mechanisms by means of electrochemical and analytical studies. The positive impact of magnesium in the coating relates on its preferred dissolution vs. steel. This causes the potential to shift to more negative direction with respect to the steel substrate and additionally leads to a temporarily passivation of the steel due to alkalization of the surrounding electrolyte by formation of magnesium hydroxide.
A new approach to the assessment of the corrosion behaviour of zinc coatings under atmospheric conditions can be achieved using gel-type electrolytes as an alternative to standard aqueous test electrolytes. Gel-type electrolytes allow minimally invasive corrosion investigations on zinc coatings. They also provide the possibility to carry out corrosion investigations onsite. By using gel-type electrolytes corrosion-relevant characteristic values such as corrosion currents and polarization resistances can be determined. These allow to describe the formation and the stability of the formed corrosion product layers under various climatic conditions. With this knowledge, a prediction of the zinc coating life cycle is possible. In this contribution, the value of gel-type electrolytes for corrosion research on zinc coatings is presented.
The influence of isothermal ageing on microstructure, sensitisation and pitting corrosion resistance of the lean duplex stainless steel (LDSS) X2CrNiN23-4 was investigated with various electrochemical methods. The aging at 600 °C (from 0.1 h up to 20 h) lead to the formation of precipitations at the ferrite-ferrite (α/α) and ferrite-austenite (α/γ) grain boundaries, inducing sensitisation due to chromium depletion. The degree of sensitisation was evaluated with the double loop electrochemical potentiokinetic reactivation method (DL-EPR) according to ASTM G108 and correlated with critical pitting potentials (Epit) as well as critical pitting temperature (CPT) measured in an electrolyte according to ASTM G48 using electrochemical noise. Up to an ageing time of 1 h, the sensitisation did rise significantly, stabilising at a nearly constant level with a slight drop at 20 h. This behaviour correlated perfectly with the potentiodynamically determined pitting potentials Epit and sensitisation. The CPT showed a higher sensitivity at short ageing times compared to the DL-EPR and Epit. Finally, the KorroPad method was applied to visualise the sensitisation induced reduction of pitting corrosion resistance. The “KorroPad” is an agar-based gel-electrolyte containing 0.1 mol/l sodium chloride (NaCl) and 0.1 mol/l potassium ferricyanide III (K3[Fe(CN)6]), invented at the Federal Institute of Materials Research and Testing in Berlin (Germany) to detect surfaces of stainless steel prone to pitting corrosion. The standard configuration of the KorroPad showed no differentiation for the various aging conditions. Increasing the concentration of both NaCl and potassium ferrocyanide III to 0.5 M shifts the detection limit of the KorroPad method to stainless steels with higher corrosion resistance, producing the same trends detected by standard electrochemical pitting corrosion values (Epit, CPT) and sensitisation (DL-EPR). By that, the KorroPad method was successfully adjusted to the lean-duplex stainless steel X2CrNiN23-4, enabling short-time testing to detect sensitization.
Hard coated steel components are used in a wide application range, mostly for protective, wear resistant and decorative purposes. Despite of these coatings being regarded as relatively dense, there is always a high risk of localized corrosion when a coated low alloyed steel component encounters a surrounding high humidity atmosphere or even an aqueous medium. An approach to enhance the corrosion properties is the addition of magnesium to physical vapor deposited hard coatings, like TiN. It has been found that there is a remarkable increase in corrosion resistance in dependence of magnesium content of the TiMgN coating and its surface properties. In this work the authors will explain the underlying corrosion protection mechanisms by means of electrochemical and analytical studies. The positive impact of magnesium in the coating relates on its preferred dissolution vs. steel. This causes the potential to shift to more negative direction with respect to the steel substrate and additionally leads to a temporarily passivation of the steel due to alkalization of the surrounding electrolyte by formation of magnesium hydroxide.
Hard and wear resistant coatings deposited by PVD techniques have been characterized for decades for their capabilities to protect steel substrates from corrosion. In the present work the effect of Mg incorporated into TiN coatings is described in terms of the corrosion behavior as well as the mechanical and structural properties.
TiN and TiMgN films with Mg contents between 10 and 35 at.% were deposited onto mirror polished 100Cr6 (1.3505) steel samples with 2.5 and 5 μm thickness by using DC magnetron sputtering. The corrosion protection capabilities of the coatings were characterized by neutral salt spray (NSS) test, considering the amounts and sizes of growth defects inherent in each coated sample as determined by a recently developed optical scan method (Large Area High Resolution mapping). The defect data were statistically analyzed for improved interpretation of NSS test results. Chosen growth defects were additionally analyzed by focused ion beam technique. Furthermore the coating composition and morphology, the hardness and the tribological behavior were characterized.
Polished steel samples coated with 2.5 μm TiMgN containing about 35 at.% Mg were in the plane free of corrosion after 24 h in a NSS test. TiMgN with 10 or 20 at.% Mg only provided a slightly improved corrosion protection in relation to pure TiN coatings, which was limited to certain types of growth defects. The highest Mg containing coatings exhibited a decreased hardness down to 1200 or 1800 HV depending on type of deposition (HV 1200: Ti- and Mg-target with rotating substrate holder, 1800: Mg-plugged Ti-target with static substrate holder), but also showed a strongly improved wear resistance against Al2O3 related to pure TiN. By analyzing the NSS test results it was found that the corrosion behavior of the coated samples did not only depend strongly on the Mg content, but also on the sample individual defect concentrations. Therefore this subject is extensively discussed.