Filtern
Dokumenttyp
- Zeitschriftenartikel (12)
- Beitrag zu einem Tagungsband (5)
- Vortrag (4)
- Forschungsbericht (2)
- Buchkapitel (1)
- Posterpräsentation (1)
Schlagworte
- Brandschutz (13)
- Feuerwiderstand (8)
- Brandversuche (7)
- Reaktive Brandschutzsysteme (7)
- Stahl (7)
- Steel (6)
- Intumescent coating (5)
- Reaktives Brandschutzsystem (5)
- Reactive fire protection system (4)
- Brandversuch (3)
Organisationseinheit der BAM
- 7.3 Brandingenieurwesen (25) (entfernen)
Eingeladener Vortrag
- nein (4)
Intumescent fire protection coatings are used to improve the fire resistance of steel members. Due to slender cross-sections typically used for tension members, high demands are placed on the effectiveness and reliability of the intumescent coatings. This paper describes real-scale fire tests of intumescent coatings applied to steel tension members with circular solid and hollow sections. First, the current regulations for the application of intumescent coatings on steel tension members are discussed. After that, a comparison between the foaming behaviour and failure mechanisms of intumescent coatings applied to steel tension members with different cross-sections and loading conditions is given. Next, the experimental setup and procedure of the performed fire tests are presented. In addition, the influences of various parameters on the performance of the intumescent coating are analysed, including the geometry of the steel profile, dry film thickness of the intumescent coating, load utilisation level as well as the orientation of the member. Based on the theoretical considerations and results of the fire tests, it is evidenced that mechanically loaded fire tests are essential to assess accurately the contribution of intumescent fire protection coatings to the fire resistance of steel tension members with circular solid sections.
Intumescent coatings are commonly used in civil engineering to improve the fire resistance of steel constructions. Especially in the case of tension bars, where mostly circular or rectangular solid sections are used, intumescent coatings offer an efficient measure to improve the fire resistance taking advantage of profile-following application and low coating thickness requirements. Thus, the architectural appearance of slender profiles can be preserved. The paper describes real-scale mechanically loaded and unloaded fire tests of circular and rectangular solid steel tension bars with intumescent coating. The aim of these tests is to investigate the influence of the different profile types as well as different bar orientations on the performance of intumescent coatings. The results are used to specify a normative test and assessment procedure to be implemented in a new European standard for determining the contribution of intumescent coatings to the fire resistance of circular or rectangular bars used as tension members.
Reaktive Brandschutzsysteme
(2022)
Die Erkenntnisse zu reaktiven Brandschutzsystemen (RBS) werden kontinuierlich erweitert, was sich in der Entwicklung neuer Produkte und der Ausweitung des durch technische Regelungen abgedeckten Anwendungsbereichs äußert. Der vorliegende Beitrag konzentriert sich auf die Verwendung von RBS auf Stahlkonstruktionen. Neben einer umfassenden Darstellung der aktuellen nationalen und europäischen Regelungen zu RBS, werden technologische Besonderheiten und deren Einfluss auf den Regelungsinhalt im Beitrag thematisiert. Dabei werden neben sich abzeichnenden Neuerungen auch die entsprechenden wissenschaftlich-technologischen Grundlagen dargelegt. Ferner wird die Frage nach der Bewertung der Dauerhaftigkeit von RBS für deutlich über 10 Jahre hinausgehende Zeiträume, und den sich damit einstellenden Feuerwiderstand der Konstruktion behandelt. Der Beitrag schließt mit einer Darstellung zur aktuellen Forschung. Daraus abgeleitet wird ein Ausblick auf zukünftige Forschungsthemen.
Reaktive Brandschutzsysteme finden im baulichen Brandschutz Anwendung zur Erhöhung des Feuerwiderstands von Stahlkonstruktionen. Neben den Anforderungen an die Feuerwiderstandsdauer können damit auch Ansprüche an die Ästhetik erfüllt werden. Die profilfolgende Applikation und die geringen Trockenschichtdicken der Produkte ermöglichen es, das filigrane Erscheinungsbild von Stahlkonstruktionen aufrechtzuerhalten. Neben der thermischen Schutzwirkung muss auch die Dauerhaftigkeit der Brandschutzbeschichtung sichergestellt werden. Die Bewertungsmethoden, die auf europäischer Ebene durch das EAD 350402-00-1106 zur Verfügung stehen, zielen auf eine Nutzungsdauer von zehn Jahren ab. Prüfverfahren für einen darüber hinausgehenden Zeitraum sind nicht beschrieben. In diesem Beitrag werden experimentelle Untersuchungen zum Einfluss der Bewitterung auf das Expansionsverhalten, zur thermischen Schutzwirkung und zu den während des Aufschäumens im Brandfall stattfindenden Reaktionen vorgestellt. Die Versuche wurden an einem wasserbasierten und einem epoxidharzbasierten reaktiven Brandschutzsystem durchgeführt. Die Ergebnisse wurden im Rahmen des IGF-Forschungsvorhabens 20470 N erzielt.
Um Stahlbauteile im Brandfall vor einer zu schnellen Erwärmung zu schützen, wird häufig auf reaktive Brandschutzsysteme (RBS) zurückgegriffen. Die Produkte eigenen sich besonders aufgrund der profilfolgenden Applikationsmöglichkeit und der vergleichsweise geringen Beschichtungsdicken. Bei einer Brandbeanspruchung schäumt das RBS auf und bildet eine thermische Schutzschicht um das Stahlprofil aus. Dadurch wird die Erwärmung des Stahls verlangsamt und der temperaturbedingte Festigkeitsverlust verzögert, wodurch sich die Feuerwiderstandsdauer des Stahlbauteils verbessert. Aus Brandversuchen ist bekannt, dass die Leistungsfähigkeit von RBS auf Stahlprofilen mit gekrümmter Oberfläche meist schlechter ausfällt als bei vergleichbaren Bauteilen mit ebener Oberfläche. Zum Einfluss der Oberflächenkrümmung auf die thermische Schutzwirkung von RBS werden in dem folgenden Beitrag sowohl theoretische Hintergründe als auch die Ergebnisse aus Brandversuchen an kleinformatigen Probekörpern vorgestellt. Die systematischen Untersuchungen zeigen, dass mit zunehmender Oberflächenkrümmung die Leistungsfähigkeit des RBS tendenziell abnimmt. Bei der Beurteilung der thermischen Schutzwirkung eines RBS sollte die Oberflächenkrümmung eines Bauteils berücksichtigt werden. Die alleinige Fokussierung auf den Profilfaktor eines Stahlprofils ist im Allgemeinen nicht ausreichend. Die Untersuchungen bilden die Grundlage für die Entwicklung von Screening-Tests zur Beurteilung der Eignung von RBS für gekrümmte Oberflächen, wodurch eine Vorauswahl von Produkten für diesen Einsatzzweck ermöglicht wird.
Intumescent coatings are used in civil engineering to improve the fire resistance of steel constructions. Due to the thin coating thickness and the profile-following application, the architectural appearance of the steel structure can be preserved. EN 13381-8 provides regulations to determine the contribution to the fire resistance of intumescent coatings applied to steel beams and columns. The scope of this standard excludes tension members and steel members with solid sections. For products that have already been successfully tested and assessed on beams and columns, EN 13381-10 offers the possibility based on unloaded fire tests to extend the scope of application of intumescent coatings to tension bars with solid sections. This approach contradicts the national safety level in Germany, where mechanically loaded testing is mandatory. Therefore, a new part of the test standard series EN 13381 is currently developed to enable the application of intumescent coatings on steel tension bars with solid section based on mechanically loaded fire tests. BAM has already carried out numerous fire tests on loaded steel tension members with intumescent coatings. Currently, in the BAM research project FIRESTEMIC, the influence of the steel bar orientation and the profile type on the thermal performance of intumescent coatings are investigated. Both questions concerning the thermal protection ability of intumescent coatings were analysed based on three different test sets, which were carried out in the tension furnace (Fig. 1a). The fire exposure corresponds to the standard temperature-time curve according to EN 1363-1.
This paper summarises the main findings from the fire tests conducted in the FIRESTEMIC project. The results serve as an experimental background for the proposal of the new standard. Regarding the bar orientation, a new test setup was developed and proposed for the new standard. The two tested commercial water-based intumescent coatings with applied dry film thickness from 1.5 mm to 2.5 mm showed only a slight dependence on the bar orientation. In terms of the steel profile type, circular and rectangular solid sections with identical section factor and applied dry film thickness were tested. It was observed that the circular solid bars with diameter 30 mm heat up faster compared to the solid rectangular bars with dimension 30×30 mm (Fig. 1b). Also at larger steel bars, i.e. diameter 40 mm and dimension 40×40 mm, the same trend occurred. Thus, it is recommended for the new test standard to allow a transfer of the test results from circular to rectangular solid sections. In addition, the paper will describe and explain the test and assessment procedure proposed for the newly developed standard.
Der Beitrag stellt experimentelle Untersuchungen zum Feuerwiderstand von Carbonzuggliedern vor. Die Anwendung von Zuggliedern aus Carbon ist durch die außergewöhnlich gute Ermüdungs- sowie hohe Zugfestigkeit des Werkstoffs motiviert. Ferner ergibt sich gegenüber Stahl eine deutliche Reduzierung des Querschnitts. Perspektivisch sollen damit Stahlzugglieder im Netzwerkbogenbrückenbau ersetzt werden. Durch die Materialsubstitution werden Ressourcen nicht nur beim Zugglied selbst, sondern auch am Gesamttragwerk der Brücke eingespart. Da zum Tragverhalten von Carbonzuggliedern im Brandfall bislang keine Erkenntnisse vorliegen, sollen mit Hilfe von Bauteilbrandversuchen die Versagensmechanismen sowie die grundsätzliche Gleichwertigkeit gegenüber konventionellen Stahlhängern untersucht werden.
Der Beitrag beschreibt die Durchführung und die Ergebnisse von Brandversuchen an mechanisch belasteten Carbonzuggliedern. Die realmaßstäblichen Versuche werden am unikalen Zugbauteil-prüfofen der BAM im Mai 2022 durchgeführt. Das Versuchsprogramm umfasst vier Carbonzugglieder mit kreisrunden Querschnitten in zwei verschiedenen Durchmessern, ⌀36 mm und ⌀51 mm. Aus Gründen der Vergleichbarkeit erfolgt die Brandbeanspruchung nach Einheits-Temperaturzeitkurve (ETK). Während des Brandversuches wird die axiale Prüfkraft von 750 kN bzw. 1500 kN bis zum Eintreten des Probenversagens konstant gehalten. Zusätzlich werden die Längsverformung sowie die Bauteil- und Brandraumtemperaturen aufgezeichnet.
In einem Vorversuch an einem unbelasteten Bauteilabschnitt eines Carbonzuggliedes konnte das Brand- und Erwärmungsverhalten des Verbundmaterials untersucht werden. Dabei zeigten sich Makrorisse und eine Zersetzung der Kunststoffmatrix sowie eine hohe Temperaturbeständigkeit der Kohlenstofffasern. Durch das Fehlen der schützenden Matrix reagierten die Carbonfasern sensibel auf Querbeanspruchung. Dies führte zu einem Bruch und Ablösen der oberflächennahen Fasern.
Spannbeton-Hohlplatten (engl.: Hollow Core Slabs, HC-Platten) werden insbesondere aus wirtschaftlichen Gründen als Deckensysteme im Hochbau eingesetzt. Bei einem 2007 aufgetretenen Brandereignis in einem Parkhaus in Rotterdam kam es zu einer teilweisen Ablösung des unteren Plattenspiegels. Dies hatte eine europaweite Diskussion zur brandschutztechnischen Bewertung dieser Bauart zur Folge. Mittlerweile liegen eine Vielzahl von gutachterlichen Stellungnahmen, Literaturauswertungen und auch jüngeren Forschungsarbeiten zum Feuerwiderstand von Konstruktionen aus Spannbeton-Hohlplatten vor. In den Untersuchungen wurde unter anderem das Tragverhalten von HC-Platten bei starrer Auflagerung, insbesondere hinsichtlich der Querkrafttragfähigkeit, analysiert. Ein weiterer, bei der Prüfung und Bewertung von Spannbeton-Hohlplatten bisher kaum beachteter Aspekt ist die im Brandfall auftretende Behinderung der Querdehnung. In der Praxis kann für HC-Platten eine Querdehnungsbehinderung im Brandfall auftreten, wenn beispielsweise eine sehr steife Begrenzung des brandbeanspruchten Deckenbereichs vorliegt, z. B. durch Treppenhauskerne oder auch durch umgebende Deckenfelder bei lokaler Brandbeanspruchung. Um dieser Fragestellung nachzugehen, wurden an der BAM entsprechende experimentelle und numerische Untersuchungen an Deckenfeldern aus Spannbeton-Hohlplatten mit unterschiedlicher seitlicher Zwängung durchgeführt. Im Beitrag werden die im Realmaßstab durchgeführten Brandversuche ausführlich beschrieben und deren Ergebnisse und daraus abgeleiteten Erkenntnisse vorgestellt. Die an der BAM durchgeführten Untersuchungen haben gezeigt, dass bei einer Zunahme der seitlichen Zwängung die Horizontalrissbildung in den Plattenstegen zu- und die Längsrissbildung abnimmt. Trotz der ausgeprägten Horizontalrissbildung kam es in den Brandversuchen nicht zu- einer Ablösung des unteren Plattenspiegels. Ebenso zeigte sich kein negativer Einfluss der Horizontalrisse auf das Trag- und Verformungsverhalten der brandbeanspruchten Deckenkonstruktion. Die Ergebnisse aus den Brandversuchen stehen zukünftig zur Validierung numerischer Modelle zur Verfügung.
Steel tension rod systems consist of tension rods, fork connectors and associated intersection or connecting plates. They are used for truss systems, bracings or suspensions owing to slender design and increased economic efficiency. In case of fire, beside the tension rods themselves, the connection parts require appropriate fire protection. The use of intumescent fire protection coatings prevents a rapid heating of the steel and helps to ensure the load-carrying capacity of the structures. Because the connection components of the tension rod systems feature surface curvature as well as a complex geometry, high demand is placed on the intumescence and thermal protection effectiveness of the reactive fire protection coatings. Experimental studies were carried out to investigate the performance of intumescent coatings applied to the components of tension rod systems. The examined aspects include the foaming and cracking behaviour of the intumescent coatings, the influence of different dry film thicknesses (DFT), the heating rate of the steel connecting parts in comparison to the tension rods, as well as the mounting orientation of the tension rods together with their associated fork connectors. The results show that a decrease in the surface curvature and/or an increase in the mass concentration of the steel components lead to a lower heating rate of the steel. Moreover, the performance of the intumescent coating on tension rod systems is influenced by the mounting orientation of the steel components.
Steel tension rod systems consist of tension rods, fork connectors and associated intersection or connecting plates. They are used for truss systems, bracings or suspensions owing to slender design and increased economic efficiency. In case of fire, beside the tension rods themselves, the connection parts require appropriate fire protection. The use of intumescent fire protection coatings prevents a rapid heating of the steel and helps to ensure the load-carrying capacity of the structures. Because the connection components of the tension rod systems feature surface curvature as well as a complex geometry, high demand is placed on the intumescence and thermal protection effectiveness of the reactive fire protection coatings. Experimental studies were carried out to investigate the performance of intumescent coatings applied to the components of tension rod systems. The examined aspects include the foaming and cracking behaviour of the intumescent coatings, the influence of different dry film thicknesses (DFT), the heating rate of the steel connecting parts in comparison to the tension rods, as well as the mounting orientation of the tension rods together with their associated fork connectors. The results show that a decrease in the surface curvature and/or an increase in the mass concentration of the steel components lead to a lower heating rate of the steel. Moreover, the performance of the intumescent coating on tension rod systems is influenced by the mounting orientation of the steel components.
Reaktive Brandschutzsysteme können die Feuerwiderstandsdauer von Stahlbauteilen signifikant erhöhen. Im Brandfall schäumt das reaktive Brandschutzsystem auf und bildet um das Stahlbauteil eine thermische Schutzschicht aus. Dadurch wird die Erwärmung des Stahls verlangsamt und der temperaturbedingte Festigkeitsverlust verzögert. Reaktive Brandschutzsysteme werden überwiegend in drei Bereichen angewendet: Hochbau, Offshore bzw. maritimer Sektor sowie Tank- bzw. Behälterbau. Insbesondere bei Stahltanks und -behältern sind häufig einfach oder auch doppelt gekrümmte Bauteiloberflächen anzutreffen. Aufgrund des meist begrenzten seitlichen Expansionsvermögens von reaktiven Brandschutzsystemen kann es bei Bauteilen mit konvexer Oberflächenkrümmung zu einer Intensivierung der Rissbildung im Schaum kommen, wodurch sich häufig die thermische Schutzwirkung verschlechtert. Da zum Thema des Einflusses der Oberflächenkrümmung auf die Leistungsfähigkeit reaktiver Brandschutzsysteme bisher kaum Untersuchungen vorliegen, wurden exemplarisch zwei Tankböden mit zwei verschiedenen Trockenschichtdicken eines reaktiven Brandschutzsystems einer Brandprüfung unterzogen. Bei gleicher Trockenschichtdicke des reaktiven Brandschutzsystems zeigten die Tankböden eine wesentlich schnellere Erwärmung als ebene Stahlplatten mit vergleichbarem Profilfaktor. Die Brandprüfungen und die Ergebnisse zum Einfluss der Oberflächenkrümmung werden im Beitrag ausführlich vorgestellt und diskutiert.
Purpose – The purpose of this paper is to investigate the performance of intumescent coating on tension rod systems and their components. Steel tension rod systems consist of tension rods, fork end connectors and associated intersection or gusset plates. In case of fire, beside the tension rods themselves, the connection parts require appropriate fire protection. Intumescent fire protection coatings prevent a rapid heating of the steel and help secure the structural load-carrying capacity. Because the connection components of tension rod systems feature surface curvature and a complex geometry, high demand is placed on the intumescence and thermal protection performance of the coatings.
Design/methodology/approach – In this paper, experimental studies were carried out for steel tension rod systems with intumescent coating. The examined aspects include the foaming and cracking behaviour, the influence of different dry film thicknesses, the heating rate of the steel connecting parts in comparison to the tension rods, and the mounting orientation of the tension rods together with their fork end connectors.
Findings – The results show that a decrease in surface curvature and/or an increase inmass concentration of the steel components leads to a lower heating rate of the steel. Moreover, the performance of the intumescent coating on tension rod systems is influenced by themounting orientation of the steel components.
Originality/value – The findings based on fire tests contribute to a better understanding of the intumescent coating performance on connection components of tension rod systems. This subject has not been extensively studied yet.
Nowadays there are intumescent coatings available for diverse applications. There is no established assessment of their protection performance besides the standard time-temperature curve, but natural fire scenarios often play an important role. A reliable straightforward performance-based assessment is presented. The effective thermal conductivity per thickness is calculated based on intermediate-scale fire tests. The optimum thermal insulation, the time to reach it, and the time until contingent failure of the coating are used for an assessment independent of the heating curve. The procedure was conducted on four different commercially intumescent coatings for steel construction, one solvent-based, one waterborne, one epoxy-based, and a bandage impregnated with a waterborne coating. The performance was studied under four different but similar shaped heating curves with different maximum temperatures (standard time-temperature curve, hydrocarbon curve and two self-designed curves with reduced temperature). The thermal protection performance is crucially affected by the residue morphology. Therefore, a comprehensive morphology analysis, including micro-computed tomography and scanning electron microscopy, was conducted on small-scale residues (7.5 x 7.5 cm2). Two different types of inner structures and the residue surface after different heat exposures were discussed in terms of their influence on thermal protection performance.
Im Stahlbau wird die feuerwiderstandserhöhende Wirkung reaktiver Brandschutzsysteme (RBS) bereits seit Jahrzehnten erfolgreich und mit stetig wachsender Nachfrage genutzt. Die Anwendung dieser Systeme wird durch Zulassungen geregelt. Die Ermittlung des Beitrages reaktiver Brandschutzsysteme zur Feuerwiderstandsdauer von Stahlbauteilen wird in der Regel mit Hilfe von mechanisch belasteten und unbelasteten Brandversuchen beurteilt. Ein entsprechendes Prüf- und Bewertungsverfahren war bisher für Träger und Stützen, jedoch nicht für Zugglieder vorhanden. Mehrjährige Forschungen, haben in Deutschland zur Entwicklung eines neuen Prüf- und Bewertungsverfahrens geführt, so dass der durch Zulassungen geregelte Anwendungsbereich reaktiver Brandschutzsysteme auf filigrane Stahlzugglieder, insbesondere mit Vollprofil, erweitert werden konnte. Der Beitrag beschreibt die Besonderheiten und Herausforderungen für den Einsatz von reaktiven Brandschutzsystemen auf filigranen Stahlzuggliedern, die wesentlichen Einflussparameter sowie die maßgebenden Versagensmechanismen. Ferner wird gezeigt, wie anhand von Brandversuchen, Materialuntersuchungen im Hochtemperaturbereich und numerischen Simulationen das neue Prüf- und Bewertungsverfahren entwickelt, validiert und angewendet wurde. Abschließend erfolgt ein Ausblick auf noch zu untersuchende Fragestellungen, z. B. hinsichtlich der Bauteilorientierung sowie zum Umgang mit den Anschlussbauteilen von Stahlzuggliedern.
Die Feuerwiderstandsdauer von ungeschützten Stahlbauteilen lässt sich durch den Einsatz reaktiver Brandschutzsysteme (RBS) signifikant erhöhen. Durch den profilfolgenden Auftrag der Brandschutzbeschichtung und die hierfür erforderlichen geringen Trockenschichtdicken, welche in der Regel nur wenige Millimeter betragen, können neben den brandschutztechnischen Anforderungen auch die an die Stahlkonstruktion gestellten gestalterischen Ansprüche erfüllt werden. Kommt es zu einem Brand, schäumt das reaktive Brandschutzsystem auf und bildet eine thermische Schutzschicht um das Stahlbauteil aus. Dadurch wird die Erwärmung des Stahls verlangsamt und der Festigkeitsverlust infolge Temperatur wird verzögert. Die Verwendung von reaktiven Brandschutzsystemen auf Stahlbauteilen wird durch Zulassungen geregelt. In Bezug auf den durch die Zulassung geregelten Anwendungsbereich von reaktiven Brandschutzsystemen auf zugbeanspruchten Stahlbauteilen haben sich in den vergangenen Jahren verschiedene Änderungen ergeben. Der nachfolgende Beitrag gibt hierzu einen aktuellen Überblick und beschreibt die Hintergründe, welche zu den neuen Regelungen geführt haben. Ferner erfolgt in diesem Zusammenhang ein Ausblick auf noch zu untersuchende Fragestellungen, welche bisher noch nicht durch die Regelungen in den Zulassungen abgedeckt werden. Bei den nachfolgenden Ausführungen handelt es sich um einen Auszug des Beitrages für die 18. EIPOS-Sachverständigentage Brandschutz.
Zur brandschutztechnischen Ertüchtigung von Stahlkonstruktionen werden reaktive Brandschutzsysteme aufgrund der geringen Beschichtungsdicken und der profilfolgenden Applikation in zunehmendem Maße eingesetzt. Da die für Zugstabsysteme eingesetzten Bauteile meist eine stark konvex gekrümmte Oberfläche aufweisen und der Anschlussbereich über eine vergleichsweise komplexe Geometrie verfügt, stellt dies besonders hohe Anforderungen an die Leistungsfähigkeit von reaktiven Brandschutzsystemen. Anhand von realmaßstäblichen Brandversuchen wurden das Aufschäumungs- und Rissverhalten, der Einfluss der Trockenschichtdicke, die Erwärmung der einzelnen Stahlbauteile sowie der Einfluss der Bauteilorientierung untersucht. Die Ergebnisse zeigen, dass eine Abnahme der Oberflächenkrümmung oder eine Erhöhung der Massenkonzentration der Stahlbauteile zu einer geringeren Aufheizrate des Stahls führt. Darüber hinaus ist festzustellen, dass die Leistungsfähigkeit des reaktiven Brandschutzsystems von der Bauteilorientierung der Zugstabsysteme beeinflusst wird. Die durchgeführten Brandversuche können zur Entwicklung geeigneter Prüfszenarien für die Beurteilung von reaktiven Brandschutzsystemen auf Zugstabsystemen und deren Anschlusskonstruktionen verwendet werden, wodurch eine Erweiterung des zulassungsbasierten Anwendungsbereichs ermöglicht wird.
Die Erkenntnisse zu reaktiven Brandschutzsystemen (RBS) werden kontinuierlich erweitert, was sich in der Entwicklung neuer Produkte und der Ausweitung des durch technische Regelungen abgedeckten Anwendungsbereichs äußert. Der hier vorliegende Beitrag konzentriert sich auf die Verwendung von RBS auf Stahlkonstruktionen. In den vergangenen zehn Jahren wurden, abgesichert durch neue Erkenntnisse aus der Forschung, die Anwendung auf Stahlzuggliedern mit offenem Profil präzisiert und im Rahmen allgemeiner bauaufsichtlicher Zulassungen (abZ) neu geregelt. Ferner wurde die Grundlage geschaffen, die Anwendung von RBS auf Zuggliedern mit kreisrundem Vollprofil zu bewerten und auf Basis der abZ zu ermöglichen.
Neben einer umfassenden Darstellung der aktuellen nationalen und europäischen Regelungen zu RBS, werden technologische Besonderheiten und deren Einfluss auf den Regelungsinhalt im Beitrag thematisiert.
In der jüngsten Vergangenheit stellt sich mit zunehmender Dringlichkeit die Frage nach der Bewertung der Dauerhaftigkeit von RBS für lange Zeiträume, wobei damit Nutzungsdauern weit jenseits der in den nationalen und europäischen Regelungen bereits etablierten 10 Jahre gemeint sind. In diesem Zusammenhang ist zu klären, wie der Feuerwiderstand von Konstruktionen zu bewerten ist, die bereits über lange Zeiträume mit RBS versehen sind. Nicht zuletzt stellt sich die Frage nach der Dauerhaftigkeit der Systeme selbst und adäquaten Prüfverfahren zu deren Beantwortung. Neue und bereits etablierte
Ansätze werden vorgestellt und diskutiert.
Der Beitrag schließt mit einer Darstellung der aktuellen Forschung. Neben den Forschungsaktivitäten zur Dauerhaftigkeit sind hier insbesondere Untersuchungen zur Anwendung und Bewertung von RBS auf Grundlage von Naturbränden und extremen Brandereignissen genannt. Neuste Untersuchungen befassen sich auch mit der Anwendung von RBS auf komplexen Geometrien wie auch auf anderen Substraten wie Beton, Aluminium und faserverstärkten Kunststoffen sowie hybriden Werkstoffen. Die hybriden Werkstoffe aus der Kombination von Metallen und Verbundwerkstoffen sind derzeit vorwiegend im Behälter-, Fahrzeug- und Flugzeugbau anzutreffen. Auch die bereits vor Jahrzehnten begonnenen Aktivitäten zur Entwicklung rechnerischer Verfahren zur Beurteilung der Wirkungsweise von RBS werden in der aktuellen Forschung fortgeführt und weiterentwickelt.
Ziel des Forschungsvorhabens ist es, ein standardisiertes Prüf- und Bewertungsverfahren zur Bestimmung des Beitrags reaktiver Brandschutzsysteme (RBS) zum Feuerwiderstand von Stahlzuggliedern zu erarbeiten und dieses in ein Entwurfsdokument für eine europäische Prüfnorm zu überführen. Hierzu wurden einerseits bereits vorhandene Erfahrungen und Erkenntnisse genutzt und andererseits mittels Brandversuchen neue Prüfdaten zur Beantwortung bisher offengebliebener Aspekte zum Einfluss der Bauteilorientierung und Profilart erzeugt und ausgewertet. Dadurch wird die prüftechnische Grundlage für eine sichere, zulassungsbasierte Anwendung von reaktiven Brandschutzsystemen auf zugbeanspruchten Stahlbauteilen gelegt und ein einheitliches Sicherheitsniveau etabliert.
Der im Rahmen des Forschungsprojektes entwickelte Normentwurf wurde mit den Fachexperten der zuständigen nationalen und europäischen Normungsgremien diskutiert und abgestimmt. Das erarbeitete Prüf- und Auswertungsverfahren basiert auf der Durchführung von Brandversuchen an mechanisch belasteten Stahlzuggliedern mit RBS. Ergänzend sind unbelastete Brandversuche zur Beurteilung des Einflusses der Bauteilorientierung sowie der Eignung bei Schwelbrandbeanspruchung möglich. Die im Projekt durchgeführten experimentellen Untersuchungen liefern die Grundlage für den im Normenentwurf vorgeschlagenen Prüfaufbau der mechanisch belasteten und unbelasteten Brandversuche. Ferner konnte durch die Untersuchungen gezeigt werden, dass sich unter bestimmten Voraussetzungen die Prüfergebnisse von Stahlzuggliedern mit Kreisvollprofil ohne zusätzliche Brandversuche auf entsprechende Zugglieder mit Rechteckvollprofil übertragen lassen. Darüber hinaus konnte belegt werden, dass die Leistungsfähigkeit eines RBS aufgrund unterschiedlicher Bauteilorientierungen abnehmen kann und daher zwingend beim Anwendungsbereich des RBS zu berücksichtigen ist. Hierzu wird ein Temperaturdifferenz-kriterium vorgeschlagen, bei dessen Einhaltung die Wirksamkeit des RBS bei von der horizontalen Referenzorientierung abweichenden Bauteilneigungen noch gleichwertig gegeben ist. Andernfalls bietet der Normenentwurf die Möglichkeit die reduzierte thermische Schutzwirkung des RBS im Assessment zu berücksichtigen.
Die Ergebnisse aus dem Forschungsvorhaben wurden bereits auf einem wissenschaftlichen Symposium vorgestellt sowie in einer referierten Fachzeitschrift publiziert. Ferner wurden die Informationen zum Forschungsprojekt und dem Normenentwurf im Rahmen eines Anwenderworkshops interessierten Kreisen zugänglich gemacht. Der im Projekt ausgearbeitete Normenentwurf wird dem zuständigen europäischen Normungsgremien, CEN/TC 127/WG 1, zur Verfügung gestellt und dort zur Abstimmung gestellt.
Die Anwendung von Zuggliedern aus Carbon ist durch die außergewöhnlich gute Ermüdungs- sowie hohe Zugfestigkeit des Werkstoffs motiviert. Ferner ergibt sich gegenüber Stahl eine deutliche Reduzierung des Querschnitts. Perspektivisch sollen damit u. a. Stahlzugglieder im Netzwerkbogenbrückenbau ersetzt werden. Das Tragverhalten von Carbonzuggliedern im Brandfall ist jedoch bislang unbekannt. Daher wurden mittels Bauteilbrandversuchen die Versagensmechanismen untersucht sowie anhand gewonnener Versuchsdaten eine exemplarische Einschätzung zur Gleichwertigkeit gegenüber konventionellen Stahlzuggliedern vorgenommen. Der Beitrag beschreibt realmaßstäbliche Brandversuche an mechanisch belasteten Carbonzuggliedern, die im Rahmen des Verbundforschungsvorhabens NeZuCa durchgeführt wurden. Das Versuchsprogramm umfasste vier Carbonzugglieder mit kreisrunden Querschnitten in zwei verschiedenen Durchmessern, 36 mm und 51 mm. In Ermangelung eines präskriptiven Brandszenarios für den im Projekt vorgesehenen Anwendungsfall und aus Gründen der Vergleichbarkeit erfolgte die Brandbeanspruchung nach Einheitstemperaturzeitkurve (ETK). Neben den Längsverformungen der Zugglieder wurden auch die Bauteil und Brandraumtemperaturen aufgezeichnet.
For intumescent coatings durability is an important aspect. Due to ageing, which is caused by climatic conditions, the thermal protection performance of intumescent coatings can be reduced during the working life. The national German and the European procedures to assess the durability of intumescent coatings presume a working life of 10 years. For a longer period, additional investigations are required. However, the European assessment procedure does not provide specific information how to prove a durability of more than 10 years. In addition to this formal reason, also from a scientifical position, it is necessary to investigate the degradation of intumescent coatings in detail to propose a corresponding test concept for a durability of more than 10 years.
The presentation summarises the existing knowledge about the degradation behaviour and ageing of intumescent coatings. Furthermore, the results of different approaches from a recently conducted research project are presented. Starting from a water-based and an epoxy-based guide formulation, in a first approach a degradation of the intumescent coating was carried out directly during the production process, i.e. by reducing the concentration of functionally relevant chemical components. In another approach, the duration of the short-term weathering tests was significantly extended, i.e. by multiple repetition of the artificial weathering. The thermal protection performance of the intumescent coating was assessed by fire tests and tests with electrical heating source. In addition, small-scale tests were carried out to determine the thermal material properties of the intumescent coating and thermo-analytical methods were applied to characterise the degradation. Derived from this knowledge, possibilities to test and assess a working life for a period of more than 10 years are proposed.
Im Rahmen des Forschungsprojektes IGF 20470N wurden Untersuchungen zum Alterungsverhalten von reaktiven Brandschutzsystemen (RBS) auf Stahlbauteilen durchgeführt. Mithilfe der Ergebnisse einer umfangreichen Literaturrecherche sowie experimentellen und numerischen Untersuchungen sollte ein Vorschlag für ein Prüfkonzept zum Nachweis einer Nutzungsdauer von RBS von mehr als 10 Jahren auf Basis von Kurzzeitversuchen abgeleitet werden. Dabei setzt die Bewertung des Alterungsverhaltens von RBS voraus, dass die Mechanismen der Alterung hinreichend bekannt sind.
Dafür wurden zunächst systematisch Daten von Kurz- und Langzeitversuchen von nationalen Zulassungsprüfungen der letzten Jahrzehnte ausgewertet. Anschließend wurden umfangreiche experimentelle Untersuchungen an einer wasserbasierten sowie einer epoxidharzbasierten Richtrezeptur durchgeführt. Da aus der Literatur bekannt ist, dass die Einflüsse der Bewitterung zu einer Veränderung der Konzentration der Bestandteile innerhalb der Beschichtung führen können, wurden Untersuchungen mit Mangelrezepturen durchgeführt, wobei systematisch einzelne Bestandteile reduziert wurden. Neben optischen Untersuchungen wurden thermoanalytische Verfahren (DSC-TG-, ATR-FTIR-, Elementar-, Farbanalyse) angewandt sowie Brandversuche an beschichteten Stahlplatten durchgeführt. Des Weiteren wurden die Richtrezepturen den beschleunigten Kurzzeitversuchen gemäß EAD 350402-00-1106 (2017) unterzogen, welche die Zulassung von Produkten auf europäischer Ebene regelt. Für die wasserbasierte Richtrezeptur wurden die Bewitterung für den feuchten Innenraum (Typ Z1) mehrfach wiederholt (1x, 3x, 6x). Für die epoxidharzbasierte Richtrezeptur entsprach die Bewitterung dem Zyklus für die Außenanwendung (Typ X). In Brandversuchen sowie thermoanalytischen und optischen Untersuchungen wurde das Alterungsverhalten sowie die thermische Schutzwirkung analysiert.
Anschließend wurden numerische Simulationen von Stahlbauteilen mit gealterten RBS durchgeführt und anhand der experimentellen Untersuchungen validiert. Mithilfe der numerischen Modelle kann eine Bewertung der thermischen Schutzwirkung von Stahlbauteilen mit gealterten RBS vorgenommen werden.
Mithilfe der gesammelten Erkenntnisse wurde ein Vorschlag für ein Prüfkonzept für den Nachweis einer Nutzungsdauer von mehr als 10 Jahren abgeleitet. Das Prüfkonzept besteht dabei aus einem Katalog von Möglichkeiten, die aktuellen Zulassungsprüfungen auf europäischer Ebene für eine Nutzungsdauer von 10 Jahren auf einen längeren Zeitraum zu erweitern.
Der Beitrag beschreibt die Entwicklung eines neuartigen in situ Nachweisverfahrens zur Beurteilung des Feuerwiderstandes von bestehenden Stahlkonstruktionen mit gealtertem reaktivem Brandschutzsystem (RBS). Derzeit ist ein solcher Nachweis ausschließlich anhand eines Bauteilbrandversuchs möglich. Hierzu muss ein Bauteil aus der Bestandskonstruktion entnommen und einer zerstörenden Brandprüfung unterzogen werden. In Zusammenhang mit der Dauerhaftigkeitsbewertung von RBS für Zeiträume von mehr als 10 Jahren besteht in der Praxis vermehrt der Bedarf an einem minimal invasiven Prüfverfahren, mit dessen Hilfe sich direkt am Bestandsbauwerk die tatsächlich vorhandene Leistungsfähigkeit des gealterten RBS überprüfen lässt. Durch einen erfolgreichen Funktionsnachweis wäre eine Weiternutzung der Bestandkonstruktion bei Aufrechterhaltung des bestehenden Sicherheitsniveaus möglich.