Filtern
Dokumenttyp
Referierte Publikation
- nein (7)
Schlagworte
- Fatigue (4)
- High-strength concrete (4)
- Ultrasonic testing (4)
- Acoustic emission testing (2)
- Compressive Cyclic loading (2)
- Compressive cyclic loading (2)
- Ermüdung (2)
- Hochfester Beton (2)
- Non destructive testing (2)
- Non-destructive testing (2)
Organisationseinheit der BAM
Eingeladener Vortrag
- nein (2)
The worldwide spread of windfarms brings new challenges, especially for concrete structures as a part of towers, connecting joints and foundations of wind turbines. High-cyclic loadings in such structures lead to a high relevance of the subject of fatigue. A proper assessment of the fatigue strength of concrete demands therefore a basis of reliable experimental data and the development of standardized testing methods. This article presents first results of an ongoing research program of BAM (Bundesanstalt für Materialforschung und -prüfung) which is a part of a joint project (WinConFat) funded by the German Federal Ministry for Economic Affairs and Energy. The subproject investigates the effects of size and slenderness of the specimens on the fatigue behaviour of high strength concrete at different stress levels. Not only the fatigue strength, but also the fatigue process itself is monitored by means of several measurement methods. Strain measurements are used to calculate the load dependent elastic modulus in the fatigue hysteresis as indicators for fatigue development. Furthermore, the application of non-destructive methods like acoustic emission analysis and ultrasonic measurement in laboratory tests gives a deeper insight into damage processes under cyclic loading. The results shall be used to improve design rules for concrete members under fatigue load and to develop or improve non-destructive techniques for in-service structural health monitoring.
The worldwide spread of windfarms brings new challenges, especially for concrete structures as a part of towers, connecting joints and foundations of wind turbines. High-cyclic loadings in such structures lead to a high relevance of the subject of fatigue. A proper assessment of the fatigue strength of concrete demands therefore a basis of reliable experimental data and the development of standardized testing methods. This article presents first results of an ongoing research program of BAM (Bundesanstalt für Materialforschung und -prüfung) which is a part of a joint project (WinConFat) funded by the German Federal Ministry for Economic Affairs and Energy. The subproject investigates the effects of size and slenderness of the specimens on the fatigue behaviour of high strength concrete at different stress levels. Not only the fatigue strength, but also the fatigue process itself is monitored by means of several measurement methods. Strain measurements are used to calculate the load dependent elastic modulus in the fatigue hysteresis as indicators for fatigue development. Furthermore, the application of non-destructive methods like acoustic emission analysis and ultrasonic measurement in laboratory tests gives a deeper insight into damage processes under cyclic loading. The results shall be used to improve design rules for concrete members under fatigue load and to develop or improve non-destructive techniques for in-service structural health monitoring.
Severe mechanical fatigue conditions for worldwide proliferating windfarms are a Major challenge for high-performance concrete in towers, connecting joints and foundations of wind turbines. High-performance concrete offers potential for the application in offshore windfarms, not only regarding its good mechanical, but also chemical resistivity due to low diffusivity in the highly densified microstructure. For a more reliable fatigue assessment, monitoring based on nondestructive testing can be a valuable complement to design rules. Both approaches demand reliable experimental data, information about scalability and the development of standardized testing methods. This article presents results of an ongoing research program of BAM (Bundesanstalt für Materialforschung und -prüfung), which is a part of a joint national project (WinConFat) funded by the German Federal Ministry for Economic Affairs and Energy. The subproject implemented by BAM examines the fatigue behavior in dependence of size and slenderness for varying concrete strength at different stress levels. Besides fatigue strength, nondestructive testing is carried out additionally.
Methods used are strain measurement and ultrasonic testing. The change of strain, stiffness and ultrasonic pulse velocity in the fatigue process is discussed. Results disclose a deeper insight into the damage process under cyclic loading of high-performance concrete and contribute to improve nondestructive monitoring.
Severe mechanical fatigue conditions for worldwide proliferating windfarms are a Major challenge for high-performance concrete in towers, connecting joints and foundations of wind turbines. High-performance concrete offers potential for the application in offshore windfarms, not only regarding its good mechanical, but also chemical resistivity due to low diffusivity in the highly densified microstructure. For a more reliable fatigue assessment, monitoring based on nondestructive testing can be a valuable complement to design rules. Both approaches demand reliable experimental data, information about scalability and the development of standardized testing methods. This article presents results of an ongoing research program of BAM (Bundesanstalt für Materialforschung und -prüfung), which is a part of a joint national project (WinConFat) funded by the German Federal Ministry for Economic Affairs and Energy. The subproject implemented by BAM examines the fatigue behavior in dependence of size and slenderness for varying concrete strength at different stress levels. Besides fatigue strength, nondestructive testing is carried out additionally.
Methods used are strain measurement and ultrasonic testing. The change of strain, stiffness and ultrasonic pulse velocity in the fatigue process is discussed. Results disclose a deeper insight into the damage process under cyclic loading of high-performance concrete and contribute to improve nondestructive monitoring.
Die heute in der Anwendung befindlichen Bemessungskonzepte für Ermüdung von Beton stammen zum Teil noch aus den 1990er Jahren und sind speziell hinsichtlich hochfester Betone konservativ ausgelegt. Um die Vorteile von Türmen für Windkraftanlagen, vor allem auch aus hochfesten Betonen, im Zuge des geplanten Ausbaus der Windenergieversorgung in Deutschland wirtschaftlich nutzbar zu machen, müssen diese Bemessungskonzepte weiterentwickelt werden. Dafür sind umfangreiche Untersuchungen zur Ermittlung von Bruchlastwechselzahlen und zur Charakterisierung der Schädigungsentwicklung unter Ermüdungsbeanspruchung erforderlich. Allgemein anerkannte bzw. verbindliche Regelwerke oder Verfahren zur experimentellen Bestimmung der Ermüdungsfestigkeit (Bruchlastwechselzahlen) an Betonproben gibt es zurzeit aber nicht und die bisher durchgeführten Untersuchungen variieren in Parametern wie Probengeometrie, Probengröße und Prüffrequenz. Eine vergleichende Analyse der Ergebnisse der Studien und insbesondere die Übertragbarkeit auf bauteilrelevante Abmessungen ist auf dieser Grundlage nur sehr eingeschränkt möglich.
Derzeit ist die Instandhaltung von großen Betontragwerken wie Brücken oder Windenergieanlagen problemorientiert und von einem reaktiven Vorgehen geprägt. Das bedeutet, erst wenn sichtbare Schäden vorliegen, werden diese meist unter Beeinträchtigung des Betriebs instand gesetzt. Im Hinblick auf die Entwicklung von prädiktiven Instandhaltungsstrategien, deren Fokus in der langfristigen Bauwerksüberwachung und der Vorhersage von Schädigungsentwicklungen liegt, wurde die Anwendung von Ultraschallverfahren für die Identifizierung der Degradationsprozesse von Betontragwerken unter Ermüdungsbeanspruchung untersucht. Hierzu fanden Arbeiten im vom Bundesministerium für Wirtschaft und Klimaschutz (BMWK) geförderten Verbundprojekt WinConFat zum "Einfluss der Probengeometrie und -größe auf die Ermüdung von Beton" an der Bundesanstalt für Materialforschung und -prüfung (BAM) und zu den "Methoden zur Zustandsanalyse von Windenergieanlagen" am Institut für Massivbau (IfMa) der Leibniz Universität Hannover (LUH) statt, welches zudem vom Deutschen Beton- und Bautechnik Verein e.V. (Forschungsvorhaben DBV-311) gefördert wurde. Dabei wurden verschiedene Einflussfaktoren auf die Schädigungsentwicklung unter Ermüdungsbeanspruchung wie die Probekörpergröße, das Belastungsniveau und die Betonfestigkeit untersucht. Als Schädigungsindikator und Vergleichsparameter wurden die Ultraschallgeschwindigkeit und der dynamische E-Modul des Betons verwendet. Um das Potential der Schädigungserfassung im Beton mittels Ultraschallprüfung umfassender zu bewerten, wurden zusätzlich Versuche an Betonproben unter monoton steigender Belastung, Kriechversuche, Temperaturversuche und Untersuchungen an großformatigen Balken durchgeführt.
Die zunehmende Anwendung hochfesten Betons in ermüdungsbelasteten Bauwerken, herausfordernde Belastungsszenarien im Bereich von On- und Offshore Windenergieanlagen bezüglich sehr hoher Lastwechselzahlen sowie das gleichzeitige Streben nach energie- und ressourcenschonendem Bauen stellen die Bemessung von Beton gegen Ermüdung vor neue Aufgaben. Eine Vielzahl von Studien beschreibt bereits die Auswirkung von Einflussfaktoren wie Mischungszusammensetzung, Feuchte, Probekörpergröße oder Belastungsart auf die Ermüdungsfestigkeit und den Ermüdungsprozess. Aufgrund der unterschiedlichen Geometrien und Mischungen der in den verschiedenen Studien verwendeten Proben sind die Auswirkungen der Einflussfaktoren jedoch kaum miteinander vergleichbar. In dem vom Bundesministerium für Wirtschaft und Klimaschutz (BMWK) geförderten Verbundprojekt WinConFat wurden deshalb verschiedene Einflussfaktoren gezielt an Proben mit einheitlichen Mischungen untersucht. Das durch die Bundesanstalt für Materialforschung und -prüfung (BAM) bearbeitete Teilprojekt fokussierte sich auf den „Einfluss der Probengeometrie und -größe auf die Ermüdung von Beton“. Neben der Erhebung von Daten zur Ermüdungsfestigkeit wurde der Ermüdungsprozess mit zerstörungsfreien Prüf- und Messmethoden untersucht. Diese Prüfmethoden wurden auch hinsichtlich ihrer Anwendbarkeit zur Erfassung der ermüdungsbedingten Schädigungsentwicklung an Betonbauwerken im Rahmen von Monitoringkonzepten bewertet. Untersucht wurden die Ermüdungsfestigkeiten und der Ermüdungsprozess an Zylindern mit drei unterschiedlichen Betonmischungen sowie unterschiedlicher Größe und Schlankheit. Die Ergebnisse dieser Untersuchungen werden im Folgenden vorgestellt und diskutiert.