Filtern
Dokumenttyp
- Zeitschriftenartikel (27)
- Posterpräsentation (6)
- Beitrag zu einem Tagungsband (3)
- Vortrag (3)
Schlagworte
- Additive manufacturing (12)
- Computed tomography (9)
- Laser powder bed fusion (4)
- Metal matrix composite (4)
- Neutron diffraction (4)
- Aluminum alloy (3)
- Metal Matrix Composite (3)
- Residual stress (3)
- Synchrotron X-ray diffraction (3)
- Ti-6Al-4V (3)
Organisationseinheit der BAM
Eingeladener Vortrag
- nein (3)
The performance of grating interferometers coming up now for Imaging interfaces within materials depends on the efficiency (visibility) of their main component, namely the phase grating. Therefore, experiments with monochromatic synchrotron radiation and corresponding simulations are carried out. The visibility of a Phase grating is optimized by different photon energies, varying detector to grating distances and continuous rotation of the phase grating about the grid lines. Such kind of rotation changes the projected grating shapes, and thereby the distribution profiles of phase shifts. This yields higher visibilities than derived from ideal rectangular shapes. By continuous grating rotation and variation of the propagation distance, we achieve 2D visibility maps. Such maps provide the visibility for a certain combination of grating orientation and detector position. Optimum visibilities occur at considerably smaller distances than in the standard setup.
Damage Analysis in Metal Matrix Composites by means of Synchrotron Radiation Computed Tomography
(2017)
The damage evolution after compression tests of two types of MMC, consisting of eutectic AlSi12CuMgNi alloy and reinforced with 15vol% of Al2O3 fibers and with 7vol% of Al2O3 fibers+15vol% of SiC particles was studied by synchrotron CT. Internal damage at different pre-strain conditions in eutectic Si, intermetallic phases and Al2O3 fibers was observed, as well as debonding of SiC particles.
Two metal matrix composites, both consisting of a near-eutectic cast AlSi12CuMgNi alloy, one reinforced with 15%vol. Al2O3 short fibers and the other with 7%vol. Al2O3 short fibers + 15%vol. SiC particles were studied. Distribution, orientation, and volume fraction of the different phases was determined by means of synchrotron computed tomography. The load partitioning between phases was investigated by in-situ neutron diffraction compression tests. The internal damage of the eutectic Si phase and Al2O3 fibers after ex-situ compression tests was directly observed in CT reconstructed volumes. Significant debonding between Al-matrix and SiC particles was found. Those observations allowed rationalizing the load transfer among the constituent phases of two different composites. Finally, based on the Maxwell scheme, a micro-mechanical model was utilized for the composite with one and two ceramic reinforcements. The model rationalizes the experimental data, and predicts the evolution of principal stresses in each phase.
Load partitioning between phases in a cast AlSi12CuMgNi alloy was investigated by in-situ compression test during neutron diffraction experiments. Computed tomography (CT) was used to determine volume fractions of eutectic Si and intermetallic (IM) phases, and to assess internal damage after ex-situ compression tests. The CT reconstructed volumes showed the interconnectivity of IM phases, which build a 3D network together with eutectic Si. Large stresses were found in IMs, revealing their significant role as a reinforcement for the alloy. An existing micromechanical model based on Maxwell scheme was extended to the present case, assuming the alloy as a three-phase composite (Al matrix, eutectic Si, IM phases). The model agrees well with the experimental data.
Moreover, it allows predicting the principal stresses in each phase, while experiments can only determine stress differences between the axial and radial sample directions. Finally, we showed that the addition of alloying elements not only allowed developing a 3D interconnected network, but also improved the strength of the Al matrix, and the ability of the alloy constituents to bear mechanical load.
Near eutectic cast Al–Si alloys are the basis of all Al-alloys used for pistons due to their high fluidity and relatively high strength-to-weight ratio. Their microstructure is characterized by the presence of eutectic-Si embedded in an age hardenable -Al matrix. During solution heat treatment, the eutectic Si network undergoes a process of gradual disintegration, reducing the load bearing capability and the strength of the alloy. The improvement of the high temperature strength is achieved by addition of transition elements such as Cu, Mg or Ni through the formation of stiff intermetallic (IM) phases.
In present study a near-eutectic AlSi12CuMgNi alloy produced by squeeze casting was investigated in as-cast condition. The in-situ neutron diffraction compression tests revealed the stress partitioning mechanism between phases of the alloy. Large stresses were found in IMs, showing their significant role as a reinforcement elements. After the failure of IM and Si phases the load is transferred back to the Al matrix, inducing further plastic deformation in it, yet without creating microcracking. The neutron diffraction experiments were coupled with assessment of internal damage after ex-situ compression tests by synchrotron radiation computed tomography. The quantitative analysis of CT data revealed that local tensile stresses in IM and Si phases induce microcracks with preferential orientation, parallel to the axis of applied load.
Altogether, present experimental data was used as an input for the developed micromechanical model based on Maxwell homogenization scheme. In contrast to the neutron diffraction experiment, which can only determine stress differences between the axial and radial sample directions, the model allows predicting the principal stresses in each phase of the alloy.
X-ray refraction related interaction has received rising interest since about two decades in the field of imaging, beam shaping and analysis although being discovered a century ago. Due to refraction at interfaces in inhomogeneous media X-rays undergo natural focusing (or defocusing) of waves, revealing caustics. Such Kind of intensity patterns are well-known for visible light, but have been sparsely discussed for X-rays. The Variation of irradiation density may be predicted in case of known shapes. Analogously to light optics, the intensity distributions cover several orders of magnitude including complete extinction. The partly convergent (and divergent) caustic stripes originate from narrow zones of typical size of some 10−6 of the boundary curvature radius. For the deflection of plane wave synchrotron radiation (energy in the range of some keV to some ten keV) at rods and tubes of several μm diameter, we find good Agreement between experiments and modeling by ray tracing according to Snell’s law without additional diffraction contributions. Apart from Basic Research implications, caustics may influence the performance of irradiation technologies such as sterilization or molecular cross-linking.
The quality of components made by laser beam melting (LBM) additive manufacturing is naturally influenced by the quality of the powder bed. A packing density <1 and porosity inside the powder particles lead to intrinsic voids in the powder bed. Since the packing density is determined by the particle size and shape distribution, the determination of these properties is of significant interest to assess the printing process. In this work, the size and shape distribution, the amount of the particle’s intrinsic porosity, as well as the packing density of micrometric powder used for LBM, have been investigated by means of synchrotron X-ray computed tomography (CT). Two different powder batches were investigated: Ti–6Al–4V produced by plasma atomization and stainless steel 316L produced by gas atomization. Plasma atomization particles were observed to be more spherical in terms of the mean anisotropy compared to particles produced by gas atomization. The two kinds of particles were comparable in size according to the equivalent diameter. The packing density was lower (i.e., the powder bed contained more voids in between particles) for the Ti–6Al–4V particles. The comparison of the tomographic results with laser diffraction, as another particle size measurement technique, proved to be in agreement.
Im vergangenen Jahrzehnt sind gitterinterferometrische Röntgenabbildungen zunehmend in den Fokus des Interesses gerückt. Sie sind insbesondere dann Vorteil, wenn der in der Standardradiographie erreichbare Kontrast nicht genügt, schwach absorbierende Mikro- und Nanostrukturen abzubilden.
Auf Kosten mehrerer Aufnahmen gestattet die Talbot-Lau Gitterinterferometrie, die Beiträge aus Absorption, Refraktion und (refraktiver) Streuung zu trennen. Dazu werden die Störungen der Interferenzmuster von Phasengittern ausgewertet. Im Gegensatz zu einer Vielzahl anderer refraktionsbasierter Abbildungsmethoden kann diese Technik mit konventionellen Röntgenröhren (mit divergenter, polychromatischer Strahlung) angewendet werden. Damit ist die Technik geeignet, typische ZfP-Fragestellungen zu lösen.
Hier stellen wir Untersuchungen zur Effizienz von Phasengittern vor. Die Visibilität (d.h. die Höhe der Oszillation im Interferenzmuster) wird als Funktion verschiedener geometrischer Parameter verfolgt. Eine Rotation um die Achse parallel zu den Gitterstegen ändert die Form des Gitterprofils (d.h. die Verteilung der Phasenschiebungen). Die kontinuierliche Variation des Winkels und des Detektionsabstandes führt zur Identifikation von ausgezeichneten Kombinationen mit maximaler Visibilität, wobei die Abstände deutlich geringer sind als im Standardaufbau mit senkrechter Gitterbestrahlung.
Unsere Studie umfasst Simulationen für monochromatische Quelle und den Vergleich zu experimentellen Ergebnissen mit der Synchrotronstrahlung.
In der Literatur wurden die Vorteile der Talbot-Lau Interferometrie für die zerstörungsfreie Prüfung von Faserkompositen und Verbundwerkstoffen demonstriert. Hier werden als Beispiele Messungen an Aluminiumtitanat (Al2TiO5) Pulver gezeigt.
The most substantial innovations in radiographic imaging techniques of the last two decades aim at enhanced image contrast of weakly absorbing micro and nano structures by taking advantage of X-ray refraction effects occurring at outer and inner surfaces. The applications range from fibre reinforced plastics to biological tissues. These techniques comprise, among others, X-ray refraction topography, diffraction enhanced imaging, phase contrast imaging, Talbot-Lau grating interferometry, and refraction enhanced imaging. They all make use of selective beam deflections up to a few minutes of arc: the X-ray refraction effect. In contrast to diffraction, this type of interaction has a 100 % scattering cross section, as shown experimentally. Since X-ray refraction is very sensitive to the orientation of interfaces, it is additionally a tool to detect, e.g., fibre or pore orientation. If the detector resolution exceeds the size of (small) individual features, one detects the integral information (of inner surfaces) within the gauge volume. We describe the above-mentioned techniques, and show their experimental implementation in the lab and at a synchrotron source. We also show strategies for data processing and quantitative analysis.