Material modelling and lifetime prediction of Ni-base gas turbine blades under TMF conditions
(2014)
Under cyclic thermomechanical loading conditions, various damage mechanisms such as strain accumulation, creep cavitation, ageing, fatigue surface cracking etc. may take place in the material of a gas turbine blade. Depending on the loading conditions, all these effects can contribute to reduce the lifetime of the component. Subject of the present work is the development of a material model to describe the mechanical effects mentioned above, as well as the development of a lifetime model able to discriminate the different damage mechanisms.