The surface modification of single-crystalline silicon induced by single 130 femtosecond (fs) Ti:sapphire laser pulses (wavelength 800 nm) in air is investigated by means of micro Raman spectroscopy (?-RS), atomic force microscopy and scanning laser microscopy. Depending on the laser fluence, in some regions the studies indicate a thin amorphous top-layer as well as ablated and recrystallized zones. The single-pulse threshold fluences for melting, ablation and polycrystalline recrystallization are determined quantitatively. Several different topographical surface structures (rims and protrusions) are found. Their formation is discussed in the context of recent studies of the laser irradiation of silicon. In combination with a thin-film optical model, the thickness of the amorphous layer is determined by two independent and nondestructive optical methods to be in the order of several 10 nm.
We have studied plasma formation and relaxation dynamics along with the corresponding topography modifications in fused silica and sapphire induced by single femtosecond laser pulses (800 nm and 120 fs). These materials, representative of high bandgap amorphous and crystalline dielectrics, respectively, require nonlinear mechanisms to absorb the laser light. The study employed a femtosecond time-resolved microscopy technique that allows obtaining reflectivity and transmission images of the material surface at well-defined temporal delays after the arrival of the pump pulse which excites the dielectric material. The transient evolution of the free-electron plasma formed can be followed by combining the time-resolved optical data with a Drude model to estimate transient electron densities and skin depths. The temporal evolution of the optical properties is very similar in both materials within the first few hundred picoseconds, including the formation of a high reflectivity ring at about 7 ps. In contrast, at longer delays (100 ps20 ns) the behavior of both materials differs significantly, revealing a longer lasting ablation process in sapphire. Moreover, transient images of sapphire show a concentric ring pattern surrounding the ablation crater, which is not observed in fused silica. We attribute this phenomenon to optical diffraction at a transient elevation of the ejected molten material at the crater border. On the other hand, the final topography of the ablation crater is radically different for each material. While in fused silica a relatively smooth crater with two distinct regimes is observed, sapphire shows much steeper crater walls, surrounded by a weak depression along with cracks in the material surface. These differences are explained in terms of the most relevant thermal and mechanical properties of the material. Despite these differences the maximum crater depth is comparable in both material at the highest fluences used (16J/cm2). The evolution of the crater depth as a function of fluence can be described taking into account the individual bandgap of each material.
Ultrashort pulse laser microstructuring (pulse duration 130 fs, wavelength 800 nm, repetition rate 2 Hz) of titanium nitride (TiN) films on silicon substrates was performed in air using the direct focusing technique. The lateral and vertical precision of laser ablation was evaluated. The TiN ablation threshold changed with the number of pulses applied to the surface due to an incubation effect. An ablation depth per pulse below the penetration depth of light was observed. Columnar structures were formed in the silicon substrate after drilling through the TiN layer.
Ablation experiments with ultrashort laser pulses (pulse duration 150 fs, wavelength 800 nm) on polymers (PC, PMMA) relevant for biomedical technology have been performed in air. The lateral and vertical machining precision was evaluated by optical, atomic force and scanning electron microscopy. The ablation threshold reaches values in the range of 0.52.5 J/cm2 and depends significantly on the number of laser pulses applied to the same spot. The hole diameters are influenced by the laser fluence and the number of laser pulses. The relation between the ablation threshold and the number of laser pulses applied to the same spot is described in accordance with an incubation model.
A new approach is presented to quantify the so-called "heat affected zone" (HAZ) during
femtosecond laser pulse processing. Ablation of titanium nitride (TiN) thin films (~3 μm
thickness) by multiple femtosecond laser pulses (τ=130 fs, λ=800 nm) in air environment was
studied by means of two different surface analytical methods both being sensitive to chemical
alterations at the surface. Scanning Auger electron microscopy was applied for a visualization of the
spatial distribution of specific elements (Ti, O) within the laser-modified areas. The chemical state
of the irradiated surface was revealed by complementary x-ray photoelectron spectroscopy. Both
methods were used for a depth-profiling chemical analysis (tracking the elements Ti, N, O, and C)
using an Ar-ion beam for surface sputtering. In a narrow laser fluence range slightly below the
ablation threshold of TiN significant superficial oxidation can be observed leading to the formation
of substoichiometric TiO2-x. At fluences above the ablation threshold, an increased titanium
concentration is observed within the entire ablation craters. Following upon sputter removal the
elemental distribution into the depth of the nonablated material, the results allow an estimation of
the heat-affected zone for femtosecond laser ablation in air environment. According to our analyses,
the HAZ extends up to a few hundreds of nanometers into the nonablated material.
Ablation of single-crystalline (100) indium phosphide wafer surfaces with single 10 fs Ti:sapphire laser pulses in air has been studied by means of complementary cross-sectional transmission electron microscopy, scanning force microscopy, and optical microscopy. A local protrusion of ~70 nm height is generated within the ablation craters for fluences exceeding 0.78 J/cm². This morphological feature has been studied in detail, revealing the material structure of the laser-affected zone and its spatial extent. The resolidified layer (60-200 nm thick) consists of polycrystalline grains (5-15 nm diameter) and is covered by an ~10 nm thick amorphous top layer. Interestingly, the sharp boundary of the solidified layer to the unaffected crystal underneath exhibits a Gaussian-like shape and does not follow the shape of the surface topography. Evidence is presented that the central crater protrusion is formed by near-surface optical breakdown, and that the absorption in the material transiently changes during the femtosecond-laser pulse.
Femtosecond (fs) laser pulse ablation (pulse duration of 150 fs, wavelength of 775 nm, repetition rate of 1 kHz) of single-crystalline TeO2 surfaces was performed in air using the direct focusing technique. The lateral and vertical dimensions of laser ablated craters as well as the laser damage thresholds were evaluated for different pulse numbers applied to the same spot. The joint observation using optical microscopy, atomic force microscopy and scanning electron microscopy revealed the surface morphology of the ablated craters and also showed that the ablation threshold depends significantly on the number of laser pulses applied to the same spot due to incubation effects. The incubation effects change the absorption processes involved in fs-laser ablation of the transparent material from multiphoton absorption to a single-photon absorption. These results are discussed on the basis of recent models of the interaction of fs-laser pulses with dielectrics.
The dynamics of the formation of laser-induced periodic surface structures (LIPSS) on fused silica upon irradiation with linearly polarized fs-laser pulses (50 fs pulse duration) is studied by cross-polarized two-color double-fs-pulse experiments. In order to analyze the relevance of temporally distributed energy deposition in the early stage of LIPSS formation, a Mach-Zehnder interferometer was used for generating multiple double-pulse sequences at two different wavelengths (400 and 800 nm). The inter-pulse delay between the individual cross-polarized pulses of each sequence was systematically varied in the sub-ps range and the resulting LIPSS morphologies were characterized by scanning electron microscopy. It is found that the polarization of the first laser pulse arriving to the surface determines the orientation and the periodicity of the LIPSS. These two-color experiments further confirm the importance of the ultrafast energy deposition to the silica surface for LIPSS formation, particularly by the first laser pulse of each sequence. The second laser pulse subsequently reinforces the previously seeded spatial LIPSS characteristics (period, orientation).
Ultrashort laser pulses with durations in the fs-to-ps range were used for large area surface processing of steel aimed at mimicking the morphology and extraordinary wetting behaviour of bark bugs (Aradidae) found in nature. The processing was performed by scanning the laser beam over the surface of polished flat sample surfaces. A systematic variation of the laser processing parameters (peak fluence and effective number of pulses per spot diameter) allowed the identification of different regimes associated with characteristic surface morphologies (laser-induced periodic surface structures, i.e., LIPSS, grooves, spikes, etc.). Moreover, different laser processing strategies, varying laser wavelength, pulse duration, angle of incidence, irradiation atmosphere, and repetition rates, allowed to achieve a range of morphologies that resemble specific structures found on bark bugs. For identifying the ideal combination of parameters for mimicking bug-like structures, the surfaces were inspected by scanning electron microscopy. In particular, tilted micrometre-sized spikes are the best match for the structure found on bark bugs. Complementary to the morphology study, the wetting behaviour of the surface structures for water and oil was examined in terms of philic/ phobic nature and fluid transport. These results point out a route towards reproducing complex surface structures inspired by nature and their functional response in technologically relevant materials.