Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (129) (entfernen)
Sprache
- Englisch (129)
Schlagworte
- Laser-induced periodic surface structures (LIPSS) (36)
- Femtosecond laser ablation (24)
- Femtosecond laser (16)
- Laser processing (12)
- Laser ablation (11)
- Silicon (10)
- Surface functionalization (9)
- Nanostructures (7)
- Friction (6)
- High-speed optical techniques (6)
Organisationseinheit der BAM
- 6 Materialchemie (52)
- 6.2 Material- und Oberflächentechnologien (52)
- 9 Komponentensicherheit (7)
- 9.5 Tribologie und Verschleißschutz (7)
- 6.7 Materialsynthese und Design (4)
- 4 Material und Umwelt (3)
- 4.1 Biologische Materialschädigung und Referenzorganismen (3)
- 6.1 Oberflächen- und Dünnschichtanalyse (2)
- 6.6 Physik und chemische Analytik der Polymere (2)
- 5 Werkstofftechnik (1)
Paper des Monats
- ja (1)
Ti:sapphire laser pulses of 130 fs and 800 nm were focused on 3.2-7m-thick TiN films by a 60-mm focal length lens in air. The morphology of the ablated areas generated by laser pulses at a fluence slightly above the ablation threshold was characterized in dependence on the pulse number by scanning electron microscopy (SEM) and atomic force microscopy (AFM). The cavity profiles, depths, diameters, and volumes were quantitatively evaluated by AFM. The polarization state of the laser light is discussed as a further parameter, in addition to fluence and pulse number, that influences and controls the ablation precision of these materials. It was observed that circularly polarized radiation enhances the average ablation rates and reduces the roughness in the cavities by a factor of 2-3 as compared to linearly polarized radiation of the same incident laser fluence. Special attention was paid to the interfacial region between the coating and substrate. Ultrashort-pulse laser drilling into the Si substrate revealed the generation of columnar features which even may surmount the original coating under laser conditions.
Some applications of polymer films require the microstructuring of partly uneven substrates. This cannot be achieved by conventional photolithography, usually performed with ultraviolet short-pulse lasers (excimer, fourth harmonic Nd:YAG). When processing thermally sensitive or undoped polymers with low optical absorption, the use of femtosecond laser pulses can improve the ablation precision, also reducing the heat-affected zone. Therefore, a Ti:sapphire laser system was employed to perform ablation experiments on polyimide (PI). The irradiated areas were evaluated by means of optical and scanning electron microscopy. Highly oriented ripple structures, which are related to the polarization state of the laser pulses, were observed in the cavities. The relationship between the ablation threshold fluence and the number of laser pulses applied to the same spot is described in accordance with an incubation model.
Laser ablation with femtosecond pulses (130 fs, wavelength 800 nm, repetition rate 2 Hz) was compared with nanosecond-pulse ablation (10 ns, wavelength 266 nm, repetition rate 2.5 Hz) of bariumalumoborosilicate glass in air using the direct focusing technique. Different ablation thresholds and heat-affected zones were observed. The lateral and vertical machining precision was evaluated. Single nanosecond laser pulses in the far UV resulted in a bubble or a circular hole in the centre of the illuminated spot, depending on the applied fluence. The ablation behaviour in the case of near-IR femtosecond pulses contrasted to this. Bubble formation was not detected. It needed repeated pulses at the same spot to modify the surface until material removal could be observed (incubation). Cavity dimensions of less than the beam diameter were achieved in this case.
Ultrashort pulse laser microstructuring (pulse duration 130 fs, wavelength 800 nm, repetition rate 2 Hz) of titanium nitride (TiN) films on silicon substrates was performed in air using the direct focusing technique. The lateral and vertical precision of laser ablation was evaluated. The TiN ablation threshold changed with the number of pulses applied to the surface due to an incubation effect. An ablation depth per pulse below the penetration depth of light was observed. Columnar structures were formed in the silicon substrate after drilling through the TiN layer.
Ablation experiments with ultrashort laser pulses (pulse duration 150 fs, wavelength 800 nm) on polymers (PC, PMMA) relevant for biomedical technology have been performed in air. The lateral and vertical machining precision was evaluated by optical, atomic force and scanning electron microscopy. The ablation threshold reaches values in the range of 0.52.5 J/cm2 and depends significantly on the number of laser pulses applied to the same spot. The hole diameters are influenced by the laser fluence and the number of laser pulses. The relation between the ablation threshold and the number of laser pulses applied to the same spot is described in accordance with an incubation model.
Chemical, morphological and accumulation phenomena in ultrashort-pulse laser ablation of TiN in air
(2000)
Ultrashort-pulse laser ablation (F=130 fs, 5=800 nm, repetition rate 2-20 Hz) of titanium nitride was investigated for laser fluences between 0.3 and 4.5 J/cm2 using the direct focusing technique in air. The influence of the laser pulse number and the peak fluence was investigated by means of several surface analytical techniques (optical microscopy, dynamic friction atomic force microscopy, scanning Auger electron microscopy and small-spot electron spectroscopy for chemical analysis). The correlation of the results about optical, physical and chemical properties of the irradiated areas allows us to propose a simple oxidation model, which explains different observed phenomena associated with surface damage such as mound formation and crater widening and clarifies the incubation behavior reported earlier for this material.
Ablation of indium phosphide wafers in air was performed with low repetition rate ultrashort laser pulses (130 fs, 10 Hz) of 800 nm wavelength. The relationships between the dimensions of the craters and the ablation parameters were analyzed. The ablation threshold fluence depends on the number of pulses applied to the same spot. The single-pulse ablation threshold value was estimated to be fth(1)=0.16 J/cm2. The dependence of the threshold fluence on the number of laser pulses indicates an incubation effect. Morphological and chemical changes of the ablated regions were characterized by means of scanning electron microscopy and Auger electron spectroscopy.
Physical and chemical phenomena resulting from irradiation of silicon and indium phosphide with ultrashort laser pulses (~100fs) were investigated
with respect to the difference between single- and multiple-pulse treatment. In the single-pulse case, several processes were identified: modification,
recrystallization and ablation. All processes exhibit a distinct treshold behaviour. A two photon-absorption coefficient can be determined from a single
spatial ablation profile. Accumulation effects were observed for multi-pulse illumination. Different morphological features like bubbles, rippels and
microcolumns were found.
Multiple pulse investigations of 130-fs Ti:sapphire laser-induced damage of a high reflecting mirror consisting of alternating ?/4-layers of Ta2O5 and SiO2 and a single 500-nm Ta2O5 film were performed. In both cases, fused silica served as the substrate. For a fixed number of 1000 laser pulses per spot, a decrease in the damage threshold fluence of the mirror by a factor of two was observed by changing the repetition rate from 10 Hz to 1 kHz. A single 500-nm Ta2O5 film shows higher damage resistance compared to the mirror. The mirror and the Ta2O5 film samples were partially coated with a 300-nm-thick aluminium layer. The aluminium coating does not influence the damage threshold of the dielectrics underneath.
We investigated the initial modification and ablation of crystalline silicon with single and multiple Ti:sapphire laser pulses of 5 to 400 fs duration. In accordance with earlier established models, we found the phenomena amorphization, melting, re-crystallization, nucleated vaporization, and ablation to occur with increasing laser fluence down to the shortest pulse durations. We noticed new morphological features (bubbles) as well as familiar ones (ripples, columns). A nearly constant ablation threshold fluence on the order of 0.2 J/cm2 for all pulse durations and multiple-pulse irradiation was observed. For a duration of ,100 fs, significant incubation can be observed, whereas for 5 fs pulses, the ablation threshold does not depend on the pulse number within the experimental error. For micromachining of silicon, a pulse duration of less than 500 fs is not advantageous.
The ultrafast laser ablation of silicon has been investigated experimentally and theoretically. The theoretical description is based on molecular dynamics (MD) simulations combined with a microscopic electronic model. We determine the thresholds of melting and ablation for two different pulse durations =20 and 500 fs. Experiments have been performed using 100 Ti:Sap-phire laser pulses per spot in air environment. The ablation thresholds were determined for pulses with a duration of 25 and 400 fs, respectively. Good agreement is obtained between theory and experiment.
The surface modification of single-crystalline silicon induced by single 130 femtosecond (fs) Ti:sapphire laser pulses (wavelength 800 nm) in air is investigated by means of micro Raman spectroscopy (?-RS), atomic force microscopy and scanning laser microscopy. Depending on the laser fluence, in some regions the studies indicate a thin amorphous top-layer as well as ablated and recrystallized zones. The single-pulse threshold fluences for melting, ablation and polycrystalline recrystallization are determined quantitatively. Several different topographical surface structures (rims and protrusions) are found. Their formation is discussed in the context of recent studies of the laser irradiation of silicon. In combination with a thin-film optical model, the thickness of the amorphous layer is determined by two independent and nondestructive optical methods to be in the order of several 10 nm.
Laser ablation of single-crystalline indium phosphide (InP) was performed in air by means of linearly polarized Ti : sapphire femtosecond pulses (800 nm, 130 fs, 10 Hz). As a result of the irradiation with a variable number of laser pulses per spot (N /spl les/ 5), several morphological changes (crater formation, rim formation, ripple structures, and cones) were observed. These effects were explored using force modulation microscopy (FMM), a technique based on scanning force microscopy, allowing the simultaneous imaging of both topography and local stiffness at a high lateral resolution. The first laser pulse induces the formation of a protruding rim (height < 20 nm, width /spl ap/ 300 nm) bordering the ablated crater. A Fourier analysis of the multipulse generated topographies reveals the formation of wavelength-sized periodic ripples (modulation depth < 100 nm) with an orientation perpendicular to that of the electric field vector of the laser radiation. Besides these morphological alterations, material modifications were also observed in the irradiated regions by means of the FMM technique. Within the ablated craters, local stiffness variations were found revealing an inhomogeneous material composition/structure as a consequence of the femtosecond pulse laser treatment.
Structure formation on the surface of indium phosphide irradiated by femtosecond laser pulses
(2005)
Laser-induced periodic surface structures (LIPSS; ripples) with different spatial characteristics have been observed after irradiation of single-crystalline indium phosphide (c-InP) with multiple linearly polarized femtosecond pulses (130 fs, 800 nm) in air. With an increasing number of pulses per spot, N, up to 100, a characteristic evolution of two different types of ripples has been observed, i.e., (i) the growth of a grating perpendicular to the polarization vector consisting of nearly wavelength-sized periodic lines and (ii), in a specific pulse number regime (N = 530), the additional formation of equally oriented ripples with a spatial period close to half of the laser wavelength. For pulse numbers higher than 50, the formation of micrometer-spaced grooves has been found, which are oriented perpendicular to the ripples. These topographical surface alterations are discussed in the frame of existing LIPSS theories.
Femtosecond time-resolved microscopy has been used to analyze the structural transformation dynamics (melting, ablation, and solidification phenomena) induced by single intense 130 fs laser pulses in single-crystalline (100)-indium phosphide wafers in air on a time scale from ~100 fs up to 8 ns. In the ablative regime close to the ablation threshold, transient surface reflectivity patterns are observed by fs microscopy on a ps to ns time scale as a consequence of the complex spatial density structure of the ablating material (dynamic Newton fringes). At higher fluences, exceeding six times the ablation threshold, optical breakdown causes another, more violent ablation regime, which reduces the energy deposition depth along with the time of significant material removal. As a consequence, ablation lasts longer in a ring-shaped region around the region of optical breakdown. This leads to the formation of a crater profile with a central protrusion. In the melting regime below the ablation threshold, the melting dynamics of indium phosphide has been quantified and subsequent superficial amorphization has been observed upon solidification on the ns time scale leading to amorphous layer thicknesses of the order of a few tens of nanometers.
The formation of nearly wavelength-sized laser-induced periodic surface structures (LIPSSs) on single-crystalline silicon upon irradiation with single or multiple femtosecond-laser pulses (pulse duration τ=130 fs and central wavelength λ=800 nm) in air is studied experimentally and theoretically. In our theoretical approach, we model the LIPSS formation by combining the generally accepted first-principles theory of Sipe and co-workers with a Drude model in order to account for transient intrapulse changes in the optical properties of the material due to the excitation of a dense electron-hole plasma. Our results are capable to explain quantitatively the spatial periods of the LIPSSs being somewhat smaller than the laser wavelength, their orientation perpendicular to the laser beam polarization, and their characteristic fluence dependence. Moreover, evidence is presented that surface plasmon polaritons play a dominant role during the initial stage of near-wavelength-sized periodic surface structures in femtosecond-laser irradiated silicon, and it is demonstrated that these LIPSSs can be formed in silicon upon irradiation by single femtosecond-laser pulses.
Ablation of single-crystalline (100) indium phosphide wafer surfaces with single 10 fs Ti:sapphire laser pulses in air has been studied by means of complementary cross-sectional transmission electron microscopy, scanning force microscopy, and optical microscopy. A local protrusion of ~70 nm height is generated within the ablation craters for fluences exceeding 0.78 J/cm². This morphological feature has been studied in detail, revealing the material structure of the laser-affected zone and its spatial extent. The resolidified layer (60-200 nm thick) consists of polycrystalline grains (5-15 nm diameter) and is covered by an ~10 nm thick amorphous top layer. Interestingly, the sharp boundary of the solidified layer to the unaffected crystal underneath exhibits a Gaussian-like shape and does not follow the shape of the surface topography. Evidence is presented that the central crater protrusion is formed by near-surface optical breakdown, and that the absorption in the material transiently changes during the femtosecond-laser pulse.
The formation of nearly wavelength-sized laser-induced periodic surface structures (LIPSS) on
single-crystalline silicon upon irradiation with single (N = 1) and multiple (N ≤ 1000) linearly
polarized femtosecond (fs) laser pulses (pulse duration τ = 130 fs, central wavelength λ = 800 nm)
in air is studied experimentally. Scanning electron microscopy (SEM) and optical microscopy are
used for imaging of the ablated surface morphologies, both revealing LIPSS with periodicities close
to the laser wavelength and an orientation always perpendicular to the polarization of the fs-laser
beam. It is experimentally demonstrated that these LIPSS can be formed in silicon upon irradiation
by single fs-laser pulses—a result that is additionally supported by a recent theoretical model.
Two-dimensional Fourier transforms of the SEM images allow the detailed analysis of the
distribution of the spatial frequencies of the LIPSS and indicate, at a fixed peak fluence, a
monotonous decrease in their mean spatial period between ~770 nm (N = 1) and 560 nm (N
= 1000). The characteristic decrease in the LIPSS period is caused by a feedback-mechanism acting
upon excitation of surface plasmon polaritons at the rough silicon surface which is developing under
the action of multiple pulses into a periodically corrugated surface.
Femtosecond (fs) laser pulse ablation (pulse duration of 150 fs, wavelength of 775 nm, repetition rate of 1 kHz) of single-crystalline TeO2 surfaces was performed in air using the direct focusing technique. The lateral and vertical dimensions of laser ablated craters as well as the laser damage thresholds were evaluated for different pulse numbers applied to the same spot. The joint observation using optical microscopy, atomic force microscopy and scanning electron microscopy revealed the surface morphology of the ablated craters and also showed that the ablation threshold depends significantly on the number of laser pulses applied to the same spot due to incubation effects. The incubation effects change the absorption processes involved in fs-laser ablation of the transparent material from multiphoton absorption to a single-photon absorption. These results are discussed on the basis of recent models of the interaction of fs-laser pulses with dielectrics.