The surface modification of single-crystalline silicon induced by single 130 femtosecond (fs) Ti:sapphire laser pulses (wavelength 800 nm) in air is investigated by means of micro Raman spectroscopy (?-RS), atomic force microscopy and scanning laser microscopy. Depending on the laser fluence, in some regions the studies indicate a thin amorphous top-layer as well as ablated and recrystallized zones. The single-pulse threshold fluences for melting, ablation and polycrystalline recrystallization are determined quantitatively. Several different topographical surface structures (rims and protrusions) are found. Their formation is discussed in the context of recent studies of the laser irradiation of silicon. In combination with a thin-film optical model, the thickness of the amorphous layer is determined by two independent and nondestructive optical methods to be in the order of several 10 nm.
Ultrashort pulse laser microstructuring (pulse duration 130 fs, wavelength 800 nm, repetition rate 2 Hz) of titanium nitride (TiN) films on silicon substrates was performed in air using the direct focusing technique. The lateral and vertical precision of laser ablation was evaluated. The TiN ablation threshold changed with the number of pulses applied to the surface due to an incubation effect. An ablation depth per pulse below the penetration depth of light was observed. Columnar structures were formed in the silicon substrate after drilling through the TiN layer.
The formation of nearly wavelength-sized laser-induced periodic surface structures (LIPSSs) on single-crystalline silicon upon irradiation with single or multiple femtosecond-laser pulses (pulse duration τ=130 fs and central wavelength λ=800 nm) in air is studied experimentally and theoretically. In our theoretical approach, we model the LIPSS formation by combining the generally accepted first-principles theory of Sipe and co-workers with a Drude model in order to account for transient intrapulse changes in the optical properties of the material due to the excitation of a dense electron-hole plasma. Our results are capable to explain quantitatively the spatial periods of the LIPSSs being somewhat smaller than the laser wavelength, their orientation perpendicular to the laser beam polarization, and their characteristic fluence dependence. Moreover, evidence is presented that surface plasmon polaritons play a dominant role during the initial stage of near-wavelength-sized periodic surface structures in femtosecond-laser irradiated silicon, and it is demonstrated that these LIPSSs can be formed in silicon upon irradiation by single femtosecond-laser pulses.
XUV- and X-ray free-electron-lasers (FEL) combine short wavelength, ultrashort pulse duration, spatial coherence and high intensity. This unique combination of properties opens up new possibilities to study the dynamics of non-reversible phenomena with ultrafast temporal and nano- to atomic-scale spatial resolution. In this contribution we wish to present results of time-resolved experiments performed at the XUV-FEL FLASH (HASYLAB/Hamburg) aimed to investigate the nano-scale structural dynamics of laser-irradiated materials. Thin films and fabricated nano-structures, deposited on Si3N4-membranes, have been excited with ultrashort optical laser pulses. The dynamics of the non-reversible structural evolution of the irradiated samples during laser-induced melting and ablation has been studied in an optical pump - XUV-probe configuration by means of single-shot coherent scattering techniques (i.e. diffraction imaging [1]). In a first set of experiments we investigated the formation of laser induced periodic surface structures (LIPSS) on the surface of thin Si-films (thickness 100 nm). In a simplified view LIPPS are generated as a result of interference between the incident laser pulse and surface scattered waves which leads to a periodically modulated energy deposition. Time-resolved scattering using femtosecond XUV-pulses (with a wavelength of 13.5 nm and 7 nm) allowed us to directly follow LIPSS evolution on an ultrafast time-scale and with better than 40 nm spatial resolution. The observed scattering patterns show almost quantitative agreement with theoretical predictions [2] and reveal that the LIPSS start to form already during the 12 ps pump pulse. In the second set of measurements we studied picosecond and femtosecond laser induced ablation and disintegration of fabricated nano-structures. Correlations of coherent diffraction patterns measured at various time delays to the pattern of the undisturbed object show that order in the structure is progressively lost starting from short length scales. This structural rearrangement progresses at close to the speed of sound in the material. Under certain circumstances (e.g. adequate sampling) it became also possible to reconstruct real-space images of the object as it evolves over time [3]. The possibility of femtosecond single-shot imaging of ultrafast dynamic processes with nanoscale resolution provides yet more details of the physical processes involved. [1] H. N. Chapman et al. Nature Phys. 2, 839 (2006). [2] J. F. Young et al., Phys. Rev. B 27, 1155 (1983). [3] A. Barty et al. Nature Phot. 2, 415 (2008).
The formation of gratings on the surface of a silicon wafer by nanosecond laser irradiation through a phase mask using an ArF laser emitting at 193 nm is studied. The phase mask along with some focusing optics is capable to generate via interference a periodic intensity distribution, which can be used for surface patterning. The surface patterning strongly depends on the laser energy density and on the number of pulses, as revealed by atomic force microscopy (AFM). The results show that irradiation even with a single laser pulse produces periodic depth modulations on the surface. The spatial surface modulation is in the micrometer (1.7 µm) range while the depth modulation is in the nanometer regime (1–20 nm). With an increasing number of pulses (1–100), the depth modulation amplitude increases smoothly. Increasing the number of pulses further results in the progressive destruction of the grating, vanishing completely after ~5000 pulses. This evolution is also monitored in situ by measuring the intensity of the first order-diffracted probe beam and the behavior is in accordance with what is observed by AFM. Finally, we qualitatively explain the results invoking thermally induced effects in the melted Si: these physical processes involved are probably thermocapillary and/or Marangoni effects inducing material displacement as the surface melts.
Modeling of silicon surface topographies induced by single nanosecond laser pulse induced melt-flows
(2019)
Irradiation with a single nanosecond laser pulse in the melting regime can result in a characteristic change in the surface morphology of crystalline silicon. This has been verified experimentally in a variety of situations, where dimple-shaped surface topographies are produced. In this work, the dimple height, depth, and width are modeled following and extending in a more rigorous manner the approach of Wood and Giles [Phys. Rev. B 23, 2923–2942 (1981)] and that of Schwarz-Selinger and coworkers [Phys. Rev. B 64, 155323 (2001)], upon varying the laser irradiation parameters such as peak energy density, pulse duration, and wavelength. This is achieved with numerical simulations of one-dimensional heat flow as input to the analytical fluid-flow equations.
The formation of laser-induced periodic surface structures (LIPSS) in different materials (metals, semiconductors, and dielectrics) upon irradiation with linearly polarized fs-laser pulses (τ~30–150 fs, λ~800 nm) in air environment is studied experimentally and theoretically. In metals, predominantly low-spatial-frequency-LIPSS with periods close to the laser wavelength λ are observed perpendicular to the polarization. Under specific irradiation conditions, high-spatial-frequency-LIPSS with sub-100-nm spatial periods (~λ/10) can be generated. For semiconductors, the impact of transient changes of the optical properties to the LIPSS periods is analyzed theoretically and experimentally. In dielectrics, the importance of transient excitation stages in the LIPSS formation is demonstrated experimentally using (multiple) double-fs-laser-pulse irradiation sequences. A characteristic decrease of the LIPSS periods is observed for double-pulse delays of less than 2 ps.
The formation of nearly wavelength-sized laser-induced periodic surface structures (LIPSS) on
single-crystalline silicon upon irradiation with single (N = 1) and multiple (N ≤ 1000) linearly
polarized femtosecond (fs) laser pulses (pulse duration τ = 130 fs, central wavelength λ = 800 nm)
in air is studied experimentally. Scanning electron microscopy (SEM) and optical microscopy are
used for imaging of the ablated surface morphologies, both revealing LIPSS with periodicities close
to the laser wavelength and an orientation always perpendicular to the polarization of the fs-laser
beam. It is experimentally demonstrated that these LIPSS can be formed in silicon upon irradiation
by single fs-laser pulses—a result that is additionally supported by a recent theoretical model.
Two-dimensional Fourier transforms of the SEM images allow the detailed analysis of the
distribution of the spatial frequencies of the LIPSS and indicate, at a fixed peak fluence, a
monotonous decrease in their mean spatial period between ~770 nm (N = 1) and 560 nm (N
= 1000). The characteristic decrease in the LIPSS period is caused by a feedback-mechanism acting
upon excitation of surface plasmon polaritons at the rough silicon surface which is developing under
the action of multiple pulses into a periodically corrugated surface.
The formation of laser-induced periodic surface structures (LIPSS) upon irradiation of silicon wafer surfaces by linearly polarized Ti:sapphire femtosecond laser pulses (pulse duration 130 fs, central wavelength 800 nm) is studied experimentally and theoretically. In the experiments, so-called low-spatial frequency LIPSS (LSFL) were found with periods smaller than the laser wavelength and an orientation perpendicular to the polarization. The experimental results are analyzed by means of a new theoretical approach, which combines the widely accepted LIPSS theory of Sipe et al. with a Drude model, in order to account for transient (intra-pulse) changes of the optical properties of the irradiated materials. It is found that the LSFL formation is caused by the excitation of surface plasmon polaritons, SPPs, once the initially semiconducting material turns to a metallic state upon formation of a dense free-electron-plasma in the material and the subsequent interference between its electrical field with that of the incident laser beam resulting in a spatially modulated energy deposition at the surface. Moreover, the influence of the laser-excited carrier density and the role of the feedback upon the multi-pulse irradiation and its relation to the excitation of SPP in a grating-like surface structure is discussed.
The formation of laser-induced periodic surface structures (LIPSS) upon irradiation of semiconductors and dielectrics by linearly polarized high-intensity Ti:sapphire fs-laser pulses (τ ~100 fs, λ ~800 nm) is studied experimentally and theoretically. In the experiments, two different types of LIPSS exhibiting very different spatial periods are observed (socalled LSFL low spatial frequency LIPSS, and HSFL - high spatial frequency LIPSS), both having a different dependence on the incident laser fluence and pulse number per spot. The experimental results are analyzed by means of a new theoretical approach, which combines the generally accepted LIPSS theory of J. E. Sipe and co-workers [Phys. Rev. B 27, 1141-1154 (1983)] with a Drude model, in order to account for transient changes of the optical properties of the irradiated materials. The joint Sipe-Drude model is capable of explaining numerous aspects of fs-LIPSS formation, i.e., the orientation of the LIPSS, their fluence dependence as well as their spatial periods. The latter aspect is specifically demonstrated for silicon crystals, which show experimental LSFL periods Λ somewhat smaller than λ. This behaviour is caused by the excitation of surface plasmon polaritons, SPP, (once the initially semiconducting material turns to a metallic state upon formation of a dense free-electron-plasma in the material) and the subsequent interference between its electrical fields with that of the incident laser beam, resulting in a spatially modulated energy deposition at the surface.
Upon multi-pulse irradiation, a feedback mechanism, caused by the redshift of the resonance in a grating-assisted SPP excitation, is further reducing the LSFL spatial periods. The SPP-based mechanism of LSFL successfully explains the remarkably large range of LSFL periods between ~0.6 λ and λ.