Filtern
Erscheinungsjahr
- 2015 (19) (entfernen)
Dokumenttyp
- Vortrag (9)
- Beitrag zu einem Tagungsband (7)
- Zeitschriftenartikel (3)
Schlagworte
- Corrosion (7)
- Carbon steel (2)
- Crevice corrosion (2)
- Geothermal (2)
- Geothermal energy (2)
- Inorganic acids (2)
- Lahendong (2)
- Localized corrosion (2)
- Organic acids (2)
- Sibayak (2)
Eingeladener Vortrag
- nein (9)
Condensates from the gas stream in simulated CO2 transport pipelines have been identified during the experiments in the laboratory. Because of their acidic origin the corrosion resistance of pipeline steels used for CCS (carbon capture and storage) technology might be limited. Over the last years it has become clear that the amount of water and acid building constituents in the CO2 stream has to be controlled very well. In this work, condensates formed in experiments using gaseous CO2 containing high amounts of water, NO2 and SO2 were analyzed, replicated, and used for extensive electrochemical experiments. These highly acidic condensates were enriched with CO2 and then applied to characteristic steels planned to use in the CCS transport chain. Even high alloy steels are susceptible to localized corrosion under these conditions. The results implicate that condensation of aggressive acid droplets has to be avoided or the locations where condensation takes place have to be controlled extensively.
In order to provide basic information on corrosion resistance to the designers and users of geothermal plants different metallic materials including duplex and austenitic stainless steels as well as a nickel alloy have been evaluated in artificial geothermal fluids simulating the conditions in some locations with geothermal potential in Germany as well as two sites in Indonesia. By electrochemical and long-term exposure tests at 100 °C and 150 °C the suitability of low alloyed steel UNS G41300, stainless steels UNS S31603 UNS S31803, UNS S32760, super austenitic steel UNS N08031 and nickel based alloy UNS N06059 was investigated in these geothermal fluids, using critical potentials and corrosion rates. In high-saline environments the crevice corrosion turned out to be the determining mechanism. The nickel based alloy shows excellent corrosion resistance against pitting corrosion. Excluding its high cost, it is very good to be used in the construction of geothermal facilities having highly saline brines. Stainless and duplex steels exhibit a limited corrosion resistance concerning pitting and crevice corrosion. Therefore they are not suitable for highly saline brines. The super austenite UNS N08031 showed a temperature depending behavior. In non-saline environments the low-alloyed steel UNS G41300 (beside of the higher alloyed materials) could be employed as a constructional material for the geothermal power plant, as long as a sufficient wall thickness of the material is considered.
Within the last years the use of feasible alternative energy sources has risen and is going to replace fossil resources more and more. Nevertheless, service conditions in solar facilities are due to the chemical composition of heat transmission media and temperatures, in many cases, extreme in terms of corrosion. Since the construction of power plants shall be economical with maximum life service, materials selection based on preliminary material qualification is essential to guarantee a secure and reliable operation of those facilities.
The materials selection depends on the operation temperature of a power plant on the chemical composition of the transmission fluid used. In high corrosive environments Ni-based alloys are often used as an all-round solution for the construction of corrosion resistant parts, because of their good corrosion properties. However, there might be limits for their use regarding their corrosion behavior, with which this contribution deals.
Experiences from the electrochemical characterization of materials in aqueous solutions are transferred to molten salts, providing a good addition to common exposure tests at temperatures from 450 0C to 600 0C.
By means of electrochemical measurements and exposure tests the suitability of high alloyed materials in molten nitrate salt (60 % NaNO3/40 % KNO3) can be characterized. The method was verified on different Ni-based alloys (UNS N08810, UNS N06600) and Titanium (UNS R50250).
In the literature there are not much data available to describe the corrosion behavior of titanium, nickel alloys and special stainless steels in acids at high temperature, in particular above the boiling point. Therefore, a laboratory testing program was performed with two titanium alloys (UNS R50400 and UNS R53400) to obtain corrosion data in formic acid, acetic acid, phosphoric acid, polyphosphoric acid, p-toluene sulfonic acid and lactic acid at 200 °C. Results were compared to previously published ones obtained on UNS N08031, UNS N06059 and UNS N10665.
From the results it can be concluded that titanium does not always show better corrosion resistance than Ni-based alloys.
UNS N06059 was the best choice for formic and acetic acids at temperatures of 200 °C. Both Ti-alloys are resistant in acetic acid. Some slight differences were observed for formic acid, where UNS R50400 is only resistant up to a 20 % solution and UNS R53400 in concentrated acid too. The phosphoric acid is extremely corrosive and none of the investigated materials was resistant. In the diluted acid (5 %) only UNS R53400 is resistant, whereas in 1 % solution all investigated materials performed satisfactory. UNS N10665 and UNS N06059 showed the best behavior in polyphosphoric acid. In 30 % concentrated p-toluene sulfonic acid at 200 °C all alloys tested were unsuitable. In very diluted acid (0.1 %) both Ti-alloys and the other three alloys behaved well. In lactic acid at 180 °C increased corrosion underneath deposits was detected; the best performance was observed for UNS N06059 and UNS R50400.
The corrosion behavior of carbon Steel and different high-alloyed metals including duplex and austenitic stainless steels as well as a nickel alloy have been evaluated in artificial geothermal fluids simulating the conditions in some locations with geothermal potential in Germany, as well as two sites in Indonesia.
The suitability of low alloyed Steel UNS G41300, stainless steels UNS S31603 UNS S31803, UNS S32760 and super austenitic Steel UNSN08031 in these geothermal waters, investigated by electrochemical measurements and exposure tests, is limited. The nickel based alloy UNS N06059 shows excellent corrosion resistance against pitting corrosion. Excluding its high cost, it is a very good alternative to be used in the construction of geothermal facilities having highly sahne brines. Stainless and duplex steels exhibit a limited corrosion resistance concerning pitting and crevice corrosion.
Besides the higher alloyed materials, also the low-alloyed Steel UNS G41300 could be employed as a constructional material for the geothermal power plant in non-saline environments with moderate pH, as long as the wall thickness of the material vs. corrosion rate is taken into account.
Among all of the existing electric power generation facilities, corrosion is considered to be the most severe on geothermal power plants. The focus of this research was set to evaluate the suitability of carbon steel API Q125 as a construction material on the geothermal sites Sibayak and Lahendong, Indonesia. The investigations were performed in the artificial geothermal brines under stagnant conditions by means of short-term electrochemical methods (Tafel extrapolation) and long-term exposure tests (up to 6 months). Furthermore, the influence of different parameters on the steels performance (temperature 70 °C, 100 °C and 175 °C, salinity 20 mg/L and 1,500 mg/L chlorides, pH 2 and 4) was assessed as well to ensure a “safer operating window” of a power plant.
The results showed carbon steel API Q125 could be suitable for application in stagnant geothermal brines up to temperatures of 175 °C and a chloride concentration of 1,500 mg/L. Its applicability is limited in highly acidic environments (pH 2).
In the literature there are not much data available to describe the corrosion behavior of titanium, nickel alloys and special stainless steels in acids at high temperature, in particular above the boiling point. Therefore, a laboratory testing program was performed with two titanium alloys (grade 2 - UNS R50400 and grade 12 - UNS R53400) to obtain corrosion data in formic acid, acetic acid, phosphoric acid, polyphosphoric acid, p-toluene sulfonic acid and lactic acid at 200 °C. Results were compared to previously published ones obtained on alloy 31 (UNS N08031), alloy 59 (UNS N06059) and B-2 (UNS N10665).
From the results it can be concluded that titanium does not always Show better corrosion resistance than Ni-based alloys,
Alloy 59 was the best choice for formic and acetic acids at temperatures of 200°C. Both Ti-alloys are resistant in acetic acid. Some slight differences were observed for formic acid, where Ti grade 2 is only resistant up to a 20 % solution and grade 12 in concentrated acid too. The phosphoric acid is extremely corrosive and none of the investigated materials was resistant. In the diluted acid (5 %) only Ti grade 12 is resistant, whereas in 1 % solution all investigated materials withstand. Alloy B-2 and alloy 59 showed the best behavior in polyphosphoric acid. In 30 % concentrated p-toluene sulfonic acid at 200 °C all alloys tested were unsuitable. In very diluted acid (0.1 %) both Ti-alloys and the other three alloys behaved well. In lactic acid at 180 °C increased corrosion underneath deposits was detected; the best performance was observed for alloy 59 and Ti grade 2.
In the last years, geothermal power has become a reliable and significant energy source. Because service conditions in geothermal facilities from deeply located aquifers are usually critical in terms of corrosion, materials selection is a very important issue. Preliminary evaluation of the material's suitability represents therefore a valuable strategy to ensure a secure and reliable operation of the facilities. In geothermal applications, the use of high-alloyed materials such as superaustenitic stainless steels, duplex stainless steels, and nickel-based alloys has been considered as a good alternative because of their remarkable corrosion resistance and appropriate mechanical properties. Nevertheless, the corrosion behavior of those metallic materials in geothermal fluids at service conditions has not been determined in many cases. In this work, laboratory tests including electrochemical investigations and exposure tests at 100 degrees C and 150 degrees C (1,500 kPa) showed the limits of suitability concerning localized corrosion of three different, corrosion-resistant alloys in the highly saline fluid of the North German Basin.
Kohlendioxid (C02), das z.B. aus dem Abgas von fossilgefeuerten Kraftwerken, Stahlwerken oder Zementwerken abgetrennt wird, enthält Verunreinigungen. Dies sind beispielsweise Wasserdampf, 02, S0X, NOx und H2S. Derartige Gasmischungen sind instabil und ihre Komponenten können zu weiteren Produkten reagieren. Wenn Wassermoleküle zur Verfügung stehen, können saure Lösungen kondensieren. Die Korrosion von Werkstoffen und Bauteilen in Kontakt mit den transportierten Gasmischungen wird an der BAM in Laborversuchen untersucht, Das wichtigste Ziel ist, sichere und bezahlbare Kombinationen von zugelassenen Konstruktionswerkstoffen und Grenzwerten für Verunreinigungen im C02-Strom vorzuschlagen. In den bisherigen Arbeiten hat sich herausgestellt, dass für eine verlässliche Aussage die Experimente möglichst realitätsnah durchgeführt werden sollten. Hierfür müssen die Parameter: hoher Druck (um 100 bar), Temperatur (um 60 °C), Strömungsverhältnisse (laminar oder turbulent) sowie mechanische Spannung kombiniert werden. Für diese Anforderungen wurden Prüfstände entwickelt und Experimente durchgeführt.
Geothermal sources are found to be the most aggressive natural environments for construction materials in terms of corrosion. This study was focused on investigating the suitability of stainless steel UNS S31603 in volcanic areas of geothermal sites Sibayak and Lahendong (Indonesia). Influence of different factors (temperatures up to 175 °C, chloride content up to 1500 mg/L and pH down to 2) was assessed to determine a 'safe operating window' of a power plant and assure the system integrity. Investigations were performed by means of electrochemical methods and long-term exposure tests.