- Welding (12)
- Additive Fertigung (10)
- Eigenspannungen (9)
- Hochfester Stahl (9)
- Residual stress (9)
- LIBS (8)
- TIG welding (8)
- Ultraschallunterstütztes Fräsen (8)
- Wasserstoff (8)
- Mikrolegierungseinfluss (7)
Organisationseinheit der BAM
- 9.4 Integrität von Schweißverbindungen (88) (entfernen)
Eingeladener Vortrag
- nein (88) (entfernen)
This study gives an overview on the important field of joining processes for component fabrication in hydrogen technologies. The current main issues and future perspectives are highlighted for the different technological field of hydrogen generation, storage, transport and use. In addition, the emerging field of additive manufacturing is included. Some remarks are given for standardization and regulations.
Das DVS-Vorhaben 01.3211 „Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ ist ein Kooperationsprojekt der Bundesanstalt für Materialforschung und -prüfung (BAM) und dem Institut für Schweißtechnik und Trennende Fertigungsverfahren (ISAF) der Technischen Universität Clausthal. Das Übergeordnete Projektziel ist das Erlangen von Erkenntnissen für eine sichere und wirtschaftliche, kombinierte additive und abtragende Fertigung aus kostenintensiven Werkstoffen hochbelasteter Komponenten insbesondere für KMU. Dabei stehe die beiden Werkstoffe CoCr26Ni9Mo5W (2.4681) und FeNi36 (1.3912) im Fokus. Mittels Modifikation der Schweißzusätze sind homogen und isotrop ausgeprägte Werkstoffeigenschaften und eine Erhöhung der Prozessstabilität und Fertigungsfreiheitsgrade bei der additiven Fertigung erzielbar. Darüber hinaus wird der Einfluss nachfolgender abtragender Bearbeitungsschritte des ultraschallunterstützen und des konventionellen Fräsprozesses untersucht. Die mit dem Forschungsvorhaben verbundenen Nutzen für KMU sind die Stärkung der Innovationsfähigkeit und der Wirtschaftlichkeit sowie die Erhöhung der Wettbewerbsfähigkeit. In AP-3 wurden die Mikrostruktur der MSG-Schweißung der CoCr-Referenzlegierung untersucht. In AP-4 wurden Zerspanversuche an der MSG-Schweißung der CoCr-Referenzlegierung durchgeführt.
Die Wasserstoffinfrastruktur ist eine zentraler Bestandteil der erfolgreichen Umsetzung der wasserstoffbasierten Energiewende. Dabei bilden Ferngasleitungen quasi das "Rückgrat" der Transportinfrastruktur großer Gasmengen. Dabei müssen unter Umständen Reparaturen an den Pipelines durchgeführt werden. Dabei ist in der Erdgasinfrastruktur das Schweißen an in Betrieb befindlichen (d.h. von Gas durchflossenen) Pipelines Stand der Technik. Es ist jedoch vollkommen offen, inwieweit diese Technik auf die reine Wasserstoffpipelines übertragbar sind. Hierzu leistet das Projekt H2SuD wichtige Beiträge zur Aufklärung des Einfluss eines Reparaturschweißprozesses auf die Wasserstoffaufnahme und Degradation im Betrieb befindlicher H2 Gasleitungen.
Die schädigende Wirkung von Wasserstoff auf die mechanischen Eigenschaften von Stählen ist zwar bekannt, aber noch immer nicht ausreichend erforscht. Die schnelle und sichere Markteinführung von Wasserstofftechnologien macht es erforderlich, dieses Thema genauer zu untersuchen. Im Allgemeinen wird dies oft als Wasserstoffversprödung bezeichnet. Daher ist es wünschenswert, eine Prüfmethode zu entwickeln, die auf einfache Weise die Materialeigenschaften unter Wasserstoffatmosphäre ermitteln kann. Derzeit werden mechanische Prüfungen unter Wasserstoffatmosphäre in Autoklaven durchgeführt. Für diese Technik ist eine aufwendige Hardware erforderlich, daher sind die Prüfungen teuer und die Prüfkapazitäten nur in geringem Umfang verfügbar. Die hier vorgestellte Prüfmethode verspricht einen zukunftsweisenden Ansatz zur Reduzierung von Kosten und Bearbeitungszeiten durch die Verwendung von Hohlkörpern, d.h. die Probe selbst stellt den Autoklav dar.
It was found that there is a systematic dependence of the crack growth on the welding parameters as well as on the load. Decreasing welding speeds with simultaneously higher heat input promote crack formation with increasing strain rate.
Based on the results, a new crack criterion was finally selected which allows an extended assessment of the material behavior during the MVT-test. The threshold introduced can quantify the dependencies of the crack formation on the welding and testing parameters, which could not be comprehensively described with the conventional evaluation. In principle, the evaluation routine can also be transferred to other Varestraint or externally loaded hot cracking tests.
This presentation summarizes the latest research results of the influence of the post weld heat treatment (PWHT) rate and
the global mechanical stress conditions on the stress relief cracking (SRC) susceptibility of low-alloyed and creep-resistant CrMoV steel submerged arc weld joints. It was found that a certain effect of very low heating rates could be confirmed. In addition, the interlinking of SRC susceptibility increasing effects during the PWHT and the ex-post indentification in metallographic cross-section via microstructure characterization is very complex.
This presentation summarizes the latest results on the microalloying influence on the preciptitation behavior on the mechanical properties of welded high-strength steel with a design yield strength of 690 MPa and above. For that reason, Charpy tests were performed for the pure weld metal and different heat-affected zones. Thermodynamic phase field modeling showed the usefulness of calculations in Thermocalc to predict the preciptiation behavior and (finally) to conclude the mechanistic behavior of the welded joint.
High entropy alloys (HEA) are a new class of materials that have been investigated since the early 2000s and offer great potential to replace conventional alloys. However, since they sometimes have significant contents of expensive alloying elements such as Co or Ni, their use is only conceivable in highly stressed areas of components. For this purpose, the weldability with conventional alloys such as high-alloy austenitic steels must be investigated. In addition to the resulting microstructure, the mechanical properties are also fundamental for the usability of HEAs in DMWs. For this purpose, TIG welds of CoCrFeMnNi HEA (cold rolled and recrystallized state) with AISI 304 austenitic steel are investigated. These mechanical properties are analyzed in this work by means of tensile tests and local hardness measurement. The local strain behavior of the welded joints is also characterized by means of Digital Image Correlation (DIC). The results of the local hardness measurement show a clear influence of the initial condition of the HEA on the HAZ. Thus, the HEA in the cold-rolled condition shows a clear softening because of recrystallization processes in the HAZ. On the other hand, there is no influence on the hardness of the weld metal, which is approx. 200 HV0.1 in both cases. The tensile tests show a consistent failure of the weld in the weld metal. However, regardless of the HEA condition, strengths in the range of the recrystallized HEA (RM ~ 550–600 MPa) are achieved, although with significantly reduced fracture elongations.