Filtern
Erscheinungsjahr
- 2019 (111) (entfernen)
Dokumenttyp
- Vortrag (111)
Referierte Publikation
- nein (111) (entfernen)
Schlagworte
- Additive Manufacturing (11)
- Welding (9)
- Wasserstoff (8)
- Additive Fertigung (7)
- Residual stress (7)
- Additive manufacturing (6)
- Hydrogen (6)
- Schweißen (6)
- Thermography (6)
- Hochfeste Feinkornbaustähle (5)
Organisationseinheit der BAM
- 9 Komponentensicherheit (111) (entfernen)
Eingeladener Vortrag
- nein (111) (entfernen)
Der Vortrag gibt einen Überblick über Arbeiten im Rahmen der Themenstellung "photonische Prozessketten" des SimCoLas Projekts. Es werden Ergebnisse zur Datendurchgängigkeit der Prozesskette Umformen/Laserstrahlschweißen sowie erste Ergebnisse zu numerischen Schweißstruktursimulationen zur Bewertung der Heissrisskritikalität eines tiefgezogenen Napfes beim Laserstrahlschweißen gegeben.
Laser beam welding of aluminum die casting is challenging. A large quantity of gases (in particular hydrogen) is absorbed by aluminum during the die-cast manufacturing process and is contained in the base material in solved or bound form. After re-melting by the laser, the gases are released and are present in the melt as pores. Many of these metallurgic pores remain in the weld seam as a result of the high solidification velocities. The natural (Archimedean) buoyancy is not sufficient to remove the pores from the weld pool leading to process instabilities and poor mechanical properties of the weld. Therefore, an electromagnetic (EM) system is used to apply an additional buoyancy component to the pores. The physical mechanism is based on the generation of Lorentz forces, whereby an electromagnetic pressure is introduced into the weld pool. The EM system exploits the difference in electrical conductivity between poorly conducting pores (inclusions) and the comparatively better conducting aluminum melt to increase the resulting buoyancy velocity of the pores. Within the present study, the electromagnetic supported degassing is investigated in dependence on the laser beam power, welding velocity and electromagnetic flux density. By means of a design of experiments a systematic variation of these parameters is carried out for partial penetration laser beam welding of 6 mm thick sheets of wrought aluminum alloy AlMg3 and die-cast aluminum alloy AlSi12(Fe) where the wrought alloy serves as a reference. The proportion of pores in the weld seams is determined using X-ray images, computed tomography (CT-) images and cross-section images. The results prove a significant reduction of the porosity up to 70 % for both materials as a function of the magnetic flux density
Im Vortrag werden Ergebnisse eines Forschungsvorhabens des DVS vorgestellt, in dem ein Verfahren zur Vermeidung von Schweißimperfektionen im Überlappbereich einer laserstrahlhybridgeschweißten Rundnaht entwickelt wird. Die Strategie der Prozessführung beim Schließen der Rundnaht sieht hervor, dass ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht wird. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl- sowie MSG-Schweißprozess realisiert. Es konnte gezeigt werden, dass eine Defokussierung des Laserstrahls von bis zu 40 mm über den Weg von max. 15 mm während der Bewegung des Schweißkopfes zu einer deutlich besseren Nahtausbildung im Überlappbereich führt. Es konnte eine günstige kelchförmige Schweißnahtform ohne eine Tendenz zur Rissbildung erzielt werden.
Localized laser surface treatments are able to produce tailor-made surface properties to fulfill requirements of a variety of technical applications. Especially micrometric surface topologies can be beneficial for optimizing tribological contact situations. Structures with lowered surface features are already utilized for bearings or cylinders of combustion engines. There are also other fields of application, where the potential of protruding surface features is known, e. g. for metal forming tools.
A promising approach for a tailored surface treatment working in the microsecond range is the localized dispersing of hard ceramic particles by pulsed laser radiation, the so-called laser implantation. This technique is able to produce micrometric surface structures and to improve simultaneously the wear resistance by creating metal matrix composites.
In this talk, the laser implantation technique is described and compared to the state of the art. The potential to adjust the geometry as well as the mechanical properties of laser implanted surfaces is demonstrated by means of microstructural and topographical investigations of different ceramic materials and steel substrates. Finally, results of research projects are presented aiming on the application of such structured surfaces. Their capability to change and optimize friction and wear are demonstrated for fully lubricated contacts, tools for hot sheet metal forming and tools for cold rolling of sheets for automotive applications.
Das Prozessmonitoring stellt einen wichtigen Baustein für eine Qualitätssicherung additiv gefertigter Bauteile dar, insbesondere bei kleinen Losgrößen. Der Vortrag zeigt einen Überblick aktueller Entwicklungen der BAM im Bereich des Prozessmonitorings für das Laserstrahlschmelzen (laser powder bed fusion) metallischer Werkstoffe. Durch Vergleich mit der Referenzmethode Computertomografie wird am Beispiel der thermografischen Verfahren gezeigt, wie relevante Defekte in Bauteilen detektiert werden können und Einsatzpotenziale sowie Limitierungen aufgezeigt.
Force-distance curves have been recorded on thin films of lubricants. The lubricants wet the AFM tip, which causes a capillary force. This force depends on the shape of the tip, as well as on physical properties like viscosity and surface tension, which have been determined additionally with other methods. This way, their influence on the shape of the curves could be analyzed.
At the Stakeholder meeting of the EMPIR project “Multifunctional ultrafast microprobes for on-the-machine measurements”, details about two measurement modes were presented. Force distance curves and contact resonance measurements are compared. The basic principles are explained and exemplary measurements concerning mechanical properties of polymers are shown.
High heat input leads to grain coarsening and softening in WM and HAZ; the tensile strength is reduced. Low heat input leads to inadmissible hardening in the WM; the impact strength is reduced.
The proposed t8/5-time of 3 s to 15 s could be achieved through the reduced welding velocity.
The concept of electromagnetic weld pool support system allowed single-pass welds in flat position without gravity drop-outs even for reduced welding speeds; in this way the heat input can be controlled.
The adaptation of the electromagnetic weld pool support system to laser and laser hybrid welding process can dramatically increase the potential field of application of these technologies for real industrial implementation.
Schwerpunkte:
Strategie zur Vermeidung von Schweißimperfektionen im Überlappbereich beilaserhybridgeschweißten Rundnähten für 9.5 mm dicke Rohre.
Anpassung der Laserleistung in Kombination mit der Defokussierung des
Laserstrahls sowie einer Endkraterfüllung am Ende der Schweißnaht führte zu einer besseren Nahtausbildung.
Herausrampung der Energie des Schweißprozesses, sodass ein Übergang von Durchschweißung zu einer Einschweißung mit gewünschter kelchförmiger Nahtgeometrie stattfand.
Einstellung eines Wärmestaus durch Defokussierung und Verschiebung des
Laserstrahls führt zu einem gut ausgebildeten Überlappbereich ohne Poren, Risse.
Schweißungen an Rohrabschnitten mit einer max. Wandstärke von 15 mm, bei gegebenenfalls weiteren Parameteranpassungen.