Complex special inspection of an old masonry arch bridge according to the Guideline on Inspection and Condition Assessment of Railway Bridges and numerical analysis of the structure are presented. The guideline summarises recommendations for the step-by-step investigation of railway bridges applying enhanced methods developed during the EU-funded project Sustainable Bridges. For the investigation of the arch barrel, the ballast parameters and the inner structure of the backfill behind the arch barrel a number of various advanced non-destructive and minor-destructive testing methods were applied. Deformation of the structure during load tests was measured using three independent measuring systems: laser vibrometer, LVDT and microwave radar. Results of calculations performed with 2D and 3D models based on FEM are compared with the field load tests. Sensitivity of the ultimate load of the structure to investigated parameters is studied in FE model. Some general conclusions according to methods of testing and modelling of masonry arch bridges are presented and discussed.
Single-pulse tests of the catastrophic optical damage (COD) are performed for three batches of diode lasers with different gain-regions. The tests involve in situ inspection of front, rear, and side of the devices by a thermocamera. Devices with an Al-containing gain-region show COD at the front facet, as expected for strong facet heating via surface recombination and reabsorption of laser light. In contrast, Al-free devices with low surface recombination rates tend to fail at the rear facet, pointing to a different heating scenario. The high carrier density at the rear facet favors heating and COD via Auger recombination processes.
The findings indicate that rolling contact fatigue with consecutive head checks develops preferentially in rail sections that have experienced operational work-hardening. Such hardening can be identified by instruments measuring the increased hardness values with respect to the base material. Eddy current testing was initially introduced with the aim to detect head checks and determine their damage depth. Because the material texture influences eddy current flow in the test objects very strongly, variations in hardness can easily be visualised using this method. Thus, in principle, it is possible to predict places where head checks will emerge later. This knowledge may be very helpful in improving our understanding of head check emergence under real conditions. This knowledge may also help in developing new and effective precautionary maintenance strategies.
In this work, the applicability of a new 3D micro X-ray fluorescence (3D Micro-XRF) laboratory spectrometer for the investigation of historical glass objects is demonstrated. The non-destructiveness of the technique and the possibility to measure three-dimensionally resolved fluorescence renders this technique into a suitable tool for the analysis of cultural heritage objects. Although absorption and resolution effects complicate qualitative analysis of the data, layered structures can be distinguished from homogeneous samples without the need for full quantification. Different manufacturing techniques were studied in this work with the help of hand-made reference samples. With the gained knowledge it could be shown for the investigated historical glass object, that black enamel as a stained glass contour colour was used in a cold painting. The object was not fired after the application of the black enamel, but instead the adhesion of the paint was solely provided through organic binding agents and the backing with metal foils. Thus, for the manufacturing of the object, a mixture of cold painting technique with a stained glass color was used. Quantitative measurements with a 3D Micro-XRF setup at the Berlin synchrotron BESSY II confirm the assumptions drawn on the basis of the qualitative investigation with the 3D Micro-XRF spectrometer with X-ray tube excitation.
Moisture ingress is one of major damaging factors for masonry buildings. As the complex resistivity (CR) is sensitive to textural properties as well as to the pore fluid chemistry of wet porous media, its non-destructive application can provide helpful information for conservators. In a comprehensive laboratory study it has been shown that CR might even be able to distinguish between salt content and saturation degree in only one measurement. The combined use of electrical and electromagnetic measurement techniques in two field-scale flooding experiments has shown some unexpected differences. Possible reasons are discussed and it is shown that bringing together the information of both methods leads to a clearer picture.