Filtern
Erscheinungsjahr
- 2019 (56) (entfernen)
Dokumenttyp
- Vortrag (24)
- Zeitschriftenartikel (14)
- Beitrag zu einem Tagungsband (9)
- Posterpräsentation (5)
- Sonstiges (2)
- Buchkapitel (1)
- Forschungsbericht (1)
Sprache
- Englisch (56) (entfernen)
Schlagworte
- Corrosion (56) (entfernen)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (30)
- 7.6 Korrosion und Korrosionsschutz (29)
- 5 Werkstofftechnik (17)
- 5.1 Mikrostruktur Design und Degradation (16)
- 4 Material und Umwelt (14)
- 4.1 Biologische Materialschädigung und Referenzorganismen (12)
- 6 Materialchemie (5)
- 6.2 Material- und Oberflächentechnologien (5)
- 8 Zerstörungsfreie Prüfung (3)
- 4.2 Material-Mikrobiom Wechselwirkungen (2)
Eingeladener Vortrag
- nein (24)
Microbially influenced corrosion (MIC) of iron is usually attributed to sulfate-reducing microorganisms (SRM) which act upon the metal by the reactiveness of hydrogen sulfide, and by withdrawal of the available electrons in electrical contact with the metal. Methanogenic archaea can also cause MIC by directly withdrawing electrons from the iron surface for methanogenesis. However, the mechanistic details and kinetics of the overall process are poorly understood. Precipitation of siderite, a by-product of methanogenesis, (4Fe + 5HCO3 + 5H+ 4FeCO3 + CH4 + 3H2O) can lead to an insulating layer on the metal surface and lower the corrosion rate. Still, the extent of FeCO3 precipitation may be significantly influenced by environmental conditions such as pH and advective processes.
In Europe biodiesel gained from rapeseeds are considered as an alternative to common fossil fuels due to its environmental performance and its independence from import of raw materials. Biodiesel is also suitable to serve as blending component to heating oil. In that case, it must be considered that changes of fuel composition might cause material degradation.
The objective of this research was to investigate the resistance of metallic materials exposed to heating oil, heating oil blend B20 with 20 % biodiesel and pure biodiesel. Furthermore, the resistance of metals to eight-year aged B10 and six-year aged pure biodiesel was evaluated. Ageing of biodiesel forms acids and water which might propagate metal corrosion. The investigated metals (aluminium, unalloyed steel, austenitic CrNi-steel, copper, die cast zinc and brass) are commonly used for components in middle distillate facilities.
According to DIN 50905-4 the immersed metals were exposed in a climate chamber at 50°C for 4 weeks. The metallic materials were evaluated as resistant if the annual corrosion rate due to uniform corrosion remained under 0.1 mm/year and no localized corrosion in the form of pitting occurred.
The corrosion rates of the exposed materials stayed far below the limit of 0.1 mm/year for all tested fuels. An exception was die cast zinc ZP0410 in eight-year aged B10; a corrosion rate up to 0.3 mm/year due to uniform corrosion was measured. In no case localized corrosion occurred. Copper and brass caused discolouration of biodiesel from yellow to green.
In conclusion, the tested metallic materials were resistant in heating oil, heating oil blend B20 and pure biodiesel at 50 °C. Even the metals exposed to six-year aged biodiesel and eight-year aged B10 showed no uniform or localized corrosion; except for zinc, which was not resistant in eight-year aged B10.
Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids
(2019)
The susceptibility of AISI 304 stainless steel to crevice corrosion on the effect of contact with electrochemically active fluids was investigated using exposure and stepwise potentiostatic polarisation. Crevice materials made up of 304 SS and Polyether ether ketone (PEEK) forming two kinds of crevices including 304 SS-to-PEEK and 304 SS-to-304 SS were tested.
Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids
(2019)
The susceptibility of AISI 304 stainless steel to crevice corrosion on the effect of contact with electrochemically active fluids was investigated using exposure and stepwise potentiostatic polarisation. Crevice materials made up of 304 SS and Polyether ether ketone (PEEK) forming two kinds of crevices including 304 SS-to-PEEK and 304 SS-to-304 SS were tested.
Microbiologically influenced corrosion is a multidisciplinary research area. To develop successful mitigation strategies, expertise from the industry and research institutes are essential. In Department 4.1, we developed an innovative laboratory flow model (Hi-Tension) that allows effective monitoring of MIC under both standard and non-standard conditions. The flow model allows flexibility with material selection, flow rates, temperature and other environmental parameters changes. Furthermore, the flow model allows integration of electrochemical measurements using microsensors, providing a comprehensive view of corrosion at the biofilm level. Currently, initial results indicate corrosion in the flow model is significantly higher than that of standard laboratory set ups, i.e. static incubations, particularly for methane-producing microorganisms.
Microbial modelling of sulfate-reducing bacteria (SRB) and methanogenic archaea (ME) using iron
(2019)
Sulfate reducing bacteria (SRB) and methanogenic archaea (MA) are commonly found in the oil and gas environments. The formation of hydrogen sulfide (HS-) is particularly concerning for the petroleum industry due to its corrosiveness. However, the activities of SRB are limited to the concentration of sulfate present in the environment, whereas methanogens can utilize substrates such as H¬2 for methanogenesis. MA is commonly found in sulfate-free environments, such as deep sediments, and are known to form interspecies electron transfer relationships with SRB. Recently, SRB and MA capable of microbiologically influenced corrosion (MIC) by using elemental iron as a direct electron source (EMIC) have gained increased attention. On the iron surface, EMIC-SRB can outcompete EMIC-MA in the presence of sulfate, but this changes as sulfate depletes. The formation of FeS on the metal surface can be further utilized by MA for methanogenesis as it provides a conductive path. However, the possible kinetics involved of the overall process are currently unknown.
We obtained a co-culture of EMIC-SRB and EMIC-MA to investigate the growth rates and electrical potential changes under different environmental conditions, including changes in pH, temperature and salinity. Results indicate that under neutral conditions and using iron as the sole substrate, methane production (up to 5 mM) starts after sulfate was depleted. Electrochemical measurements will be conducted on the co-culture under different conditions to determine the changes in the electrical potential in correlation with the sulfate and methane concentration. Fluorescence and electron microscope images of the biofilm structure will be used to visualize cell distribution and morphology. This study embarks the first step of understanding the relationship between EMIC-SRB and EMIC-MA. Such knowledge is important for the field of microbial electrophysiology and can be further explored for industrial applications.