Paper des Monats
- ja (2)
Alkali-silica reaction (ASR) is a chemical reaction within concrete which can lead over time to cracking and spalling. Due to the complexity of the problem, it still causes damage to concrete constructions worldwide.
The publication aims to illustrate the interdisciplinary research of the German Federal Institute for Materials Research and Testing (BAM) within the last 20 years, considering all aspects of ASR topics from the macro to the micro level. First, methods for characterization and assessment of ASR risks and reaction products used at BAM are explained and classified in the international context. Subsequently the added value of the research approach by combining different, preferably nondestructive, methods across all scales is explained using specific examples from a variety of research projects. Aspects covered range from the development of new test-setups to assess aggregate reactivity, to analysis of microstructure and reaction products using microscopical, spectroscopical and X-ray methods, to the development of a testing methodology for existing concrete pavements including in-depth analysis of the visual damage indicator and the de-icing salt input using innovative testing techniques. Finally, research regarding a novel avoidance strategy that makes use of internal hydrophobization of the concrete mix is presented.
The most common method for determination of the carbonation depth is the sprayed application of indicator solutions, Phenolphthalein in particular. Since the aerosols of Phenolphthalein are suspected to be carcinogenic, efforts have been intensified to use alternative indicators for the determination of carbonation depth. The subject and aim of this research paper are to examine indicator solutions from Alizarin Yellow R, Thymol Blue and a Mixed Indicator. These indicator solutions are commercially available and are not suspected to be carcinogenic.
For the purpose of this research, samples previously stored under accelerated carbonation conditions (1% CO2) were examined by thermogravimetric analysis (TGA) and examination of the pH value. Additionally, the electrolytic back-titration for determination of total CO2 amount was carried out comparatively to TGA.
The thermal gravimetric analysis (TG) is a common method for the examination of the carbonation progress of cement-based materials. Unfortunately, the thermal properties of some components complicate the evaluation of TG results. Various hydrate phases, like ettringite (AFt), C-S-H and AFm decompose almost simultaneously in the temperature range up to 200 °C. Additionally, physical bound water is released in the same temperature range. In the temperature range between 450 °C and 600 °C the decomposition of calcium hydroxide and amorphous or weakly bound carbonates takes place simultaneously. Carbonates, like calcite, from limestone powder or other additives may be already contained in the noncarbonated sample material. For this research an attempt was made to minimise the influence of these effects. Therefore, differential curves from DTG-results of non-carbonated areas and areas with various states of carbonation of the same sample material were calculated and evaluated. Concretes based on three different types of cement were produced and stored under accelerated carbonation conditions (1 % CO2 in air). The required sample material was obtained by cutting slices from various depth of previously CO2-treated specimen and subsequent grinding. During the sample preparation, a special attention was paid that no additional carbonation processes took place. As reference method for the determination of the carbonation depth the sprayed application of phenolphthalein solution was carried out. Microscopic analysis where examined to confirm the assumptions made previously. Furthermore, the observed effect of encapsulation of calcium hydroxide by carbonates caused by the accelerated carbonation conditions was examined more closely.
Esta pesquisa avaliou o fenômeno de autocicatrização nas propriedades mecânicas e absorção capilar de concretos estruturais. Foram avaliados dois aditivos cristalizantes em pó, dosados de acordo com o teor recomendado pelos fabricantes. Aditivos cristalizantes aumentam a densidade do gel C-S-H e formam cristais insolúveis, bloqueando fissuras. Três traços de concreto foram produzidos: referência, aditivo-X com 0,8% e aditivo-Y com 2,0% em relação a massa do cimento. Aplicou-se 75% da carga de ruptura aos 3- e 14-dias para gerar microfissuras e comparar com a referência. Posteriormente, a autocicatrização foi avaliada aos 28- e 76-dias. A propriedade de resistência à compressão axial foi determinada aos 28-dias, revelando que os aditivos cristalizantes contribuíram para um aumento médio de 12% desta propriedade. A idade do carregamento dos concretos não apresentou um impacto significativo na resistência à compressão axial, mas apontou resultados significativos entre os tipos de aditivos estudados, conforme ANOVA. As propriedades de absorção de água por capilaridade foram avaliadas aos 28- e 76-dias, indicando uma redução de absorção de água média de 42% devido ao uso dos aditivos cristalizantes. Em conclusão, a incorporação dos aditivos cristalizantes contribuiu de maneira positiva para a autocicatrização dos concretos estudados, indicando uma recuperação parcial das microfissuras.
The bond between polymer fibers and the surrounding cementitious matrix is essential for the development of concrete reinforcement. The single fiber pull-out test (SFPT) is the standard characterization technique for testing the bond strength. However, the different phases of debonding cannot be distinguished by the SFPT. This study investigates the debonding of different polymer fibers from the surrounding cementitious matrix with a modified SFPT and proposes methods to change the SFPT setup to generate more valuable information on the debonding mechanism. The SFPT was equipped with linear variable differential transformers (LVDT), digital image correlation (DIC) and acoustic emission (AE) analysis. The results demonstrate that the modified SFPT allows a better understanding of the different phases of debonding during fiber pull-out. Furthermore, bond strength values calculated by different methods reveal that the chemical bond of the investigated polymers is not different as reported by previous studies. Deformation measurements performed using LVDTs and DIC are suitable measuring techniques to characterize the debonding mechanism in SFPT. A correlation between recorded AE and debonding phases was not found.
Polymers that help tailoring rheological properties during the casting process have become inevitable constituents for all kinds of high-performance concrete technologies. Due to lacking industries, these typically crude-oil based admixtures are not readily available in many parts of the world, which limits the implementation of more sustainable high-performance construction technologies in these regions. Alternative polymers, which often demand for less processing, can be derived from local plant-based resources. The paper provides experimental data of flow tests of cement pastes with polysaccharides from Triumfetta pendrata A. Rich, acacia gum and cassava without and in the presence of polycarboxylate ether superplasticizer. The flow tests are amended by observations of the zeta potentials and the hydrodynamic diameters in the presence of and without calcium ions in the dispersion medium. The results show that in the presence of and without calcium ions all polysaccharides provide negative zeta potentials, yet, they affect flowability and thixotropy in different ways. Cassava starch, acacia gum, and the gum of Triumfetta pendrata A. Rich qualified well for robustness improvement, strong stiffening, and additive manufacturing, respectively. The reason for the different effects can be found in their average sizes and size distribution. Due to the promising results, a flow chart for local value chains is derived on the example of yet unused cassava wastes, which can be converted in parallel.
Structural design and application have always been linked to the compressive strength of concrete as the main relevant criterion. This was justifiable in the past, where concrete consisted of water, ordinary Portland cement and aggregates, but this concept is no longer relevant for modern and more sustainable cement and concrete.
Despite these new developments, existing standards, guidelines and academic curricula have not been much updated and are still used worldwide. There is a need to change this situation by proper education of the users.
This overview describes the challenges that arise at a user Level from the higher complexity of modern concrete, and defines needs and requirements for enhanced applicability of sustainable concrete concepts.
Furthermore, recommendations are given on how better concrete practice can be communicated to all the involved parties, from civil and design engineers to constructors and site-appliers on the construction site.
The aim of RILEM TC 247-DTA ‘Durability Testing of Alkali-Activated Materials’ is to identify and validate methodologies for testing the durability of alkali-activated concretes. To underpin the durability testing work of this committee, five alkali-activated concrete mixes were developed based on blast furnace slag, fly ash, and flash-calcined metakaolin. The concretes were designed with different intended performance levels, aiming to assess the capability of test methods to discriminate between concretes on this basis. A total of fifteen laboratories worldwide participated in this round robin test programme, where all concretes were produced with the same mix designs, from single-source aluminosilicate precursors and locally available aggregates. This paper reports the mix designs tested, and the compressive strength results obtained, including critical insight into reasons for the observed variability in strength within and between laboratories.
Application of electrochemical methods for studying steel corrosion in alkali-activated materials
(2023)
Alkali-activated materials (AAMs) are binders that can complement and partially substitute the current use of conventional cement. However, the present knowledge about how AAMs protect steel reinforcement in concrete elements is incomplete, and uncertainties exist regarding the application of electrochemical methods to investigate this issue. The present review by EFC WP11-Task Force ‘Corrosion of steel in alkali-activated materials’ demonstrates that important differences exist between AAMs and Portland cement, and between different classes of AAMs, which are mainly caused by differing pore solution compositions, and which affect the outcomes of electrochemical measurements. The high sulfide concentrations in blast furnace slag-based AAMs lead to distinct anodic polarisation curves, unusually low open circuit potentials, and low polarisation resistances, which might be incorrectly interpreted as indicating active corrosion of steel reinforcement. No systematic study of the influence of the steel–concrete interface on the susceptibility of steel to corrosion in AAMs is available. Less common electrochemical methods present an opportunity for future progress in the field.
NMR is becoming increasingly popular for the investigation of building materials as it is a non-invasive technology that does not require any sample preparation nor causes damage to the material. Depending on the specific application it can offer insights into properties like porosity and spatial saturation degree as well as pore structure. Moreover it enables the determination of moisture transport properties and the (re-)distribution of internal moisture into different reservoirs or chemical phases upon damage and curing. However, as yet most investigations were carried out using devices originally either designed for geophysical applications or the analysis of rather homogeneous small scale (< 10 mL) samples. This paper describes the capabilities of an NMR tomograph, which has been specifically optimized for the investigation of larger, heterogeneous building material samples (diameters of up to 72 mm, length of up to 700 mm) with a high flexibility due to interchangeable coils allowing for a high SNR and short echo times (50 - 80 m s).