Alkali-silica reaction (ASR) is a chemical reaction within concrete which can lead over time to cracking and spalling. Due to the complexity of the problem, it still causes damage to concrete constructions worldwide.
The publication aims to illustrate the interdisciplinary research of the German Federal Institute for Materials Research and Testing (BAM) within the last 20 years, considering all aspects of ASR topics from the macro to the micro level. First, methods for characterization and assessment of ASR risks and reaction products used at BAM are explained and classified in the international context. Subsequently the added value of the research approach by combining different, preferably nondestructive, methods across all scales is explained using specific examples from a variety of research projects. Aspects covered range from the development of new test-setups to assess aggregate reactivity, to analysis of microstructure and reaction products using microscopical, spectroscopical and X-ray methods, to the development of a testing methodology for existing concrete pavements including in-depth analysis of the visual damage indicator and the de-icing salt input using innovative testing techniques. Finally, research regarding a novel avoidance strategy that makes use of internal hydrophobization of the concrete mix is presented.
To prevent future alkali-aggregate reaction (AAR) damage, which has occurred frequently in the Germanhighway network in recent years, a new regulation has been drafted. This regulation severely limits the use of alkali-sensitive aggregates by requiring that their suitability be verified by certified inspectors using newly developed AAR concrete tests that involve the external supply of alkali. This has led to a significant limitation in the number of aggregates usable for concrete pavements. A novel AAR avoidance strategy is now being pursued, which aims to enable the use of borderline alkali-sensitive aggregates through the application of an internal water-repellent treatment. The addition of water repellents during concrete production should significantly reduce the ingress of water and external de-icing salts into the concrete pavement, thus reducing the potential for AAR damage.
This paper presents the results of laboratory tests to assess the suitability of this new AAR prevention strategy. Representative, highly AAR-susceptible road paving concrete made with an alkali- sensitive greywacke and various water repellents were used as the basis for these experiments. The tests for concrete suitability included determining the conventional fresh and hardened concrete properties as well as concrete prism tests with external alkaline supply. Building on these results, laser-induced breakdown spectroscopy (LIBS) analyses of de-icing-salt intrusion as well as microscopic examinations for verification of the AAR characteristics were carried out.
The results of the AAR concrete tests with external alkaline supply support the conclusion that, when hydrophobic agents containing a suitable active ingredient are used, the AAR damage process in road paving concrete can be sufficiently prevented.
To prevent future alkali-aggregate reaction (AAR) damage, which has occurred frequently in the German highway network in recent years, a new regulation has been drafted. This regulation severely limits the use of alkali-sensitive aggregates by requiring that their suitability be verified by certified inspectors using newly developed AAR concrete tests that involve the external supply of alkali. This has led to a significant limitation in the number of aggregates usable for concrete pavements. A novel AAR avoidance strategy is now being pursued, which aims to enable the use of borderline alkali-sensitive aggregates through the application of an internal water-repellent treatment. The addition of water repellents during concrete production should significantly reduce the ingress of water and external de-icing salts into the concrete pavement, thus reducing the potential for AAR damage. This paper presents the results of laboratory tests to assess the suitability of this new AAR prevention strategy. Representative, highly AAR-susceptible road paving concrete made with an alkali-sensitive greywacke and various water repellents were used as the basis for these experiments. The tests for concrete suitability included determining the conventional fresh and hardened concrete properties as well as concrete prism tests with external alkaline supply. Building on these results, laser-induced breakdown spectroscopy (LIBS) analyses of de-icing-salt intrusion as well as microscopic examinations for verification of the AAR characteristics were carried out. The results of the AAR concrete tests with external alkaline supply support the conclusion that, when hydrophobic agents containing a suitable active ingredient are used, the AAR damage process in road paving concrete can be sufficiently prevented.
To prevent future alkali-aggregate reaction (AAR) damage, which has occurred frequently in the German highway network in recent years, a new regulation has been drafted. This regulation severely limits the use of alkali-sensitive aggregates by requiring that their suitability be verified by certified inspectors using newly developed AAR concrete tests that involve the external supply of alkali. This has led to a significant limitation in the number of aggregates usable for concrete pavements. A novel AAR avoidance strategy is now being pursued, which aims to enable the use of borderline alkali-sensitive aggregates through the application of an internal water-repellent treatment. The addition of water repellents during concrete production should significantly reduce the ingress of water and external de-icing salts into the concrete pavement, thus reducing the potential for AAR damage.
This paper presents the results of laboratory tests to assess the suitability of this new AAR prevention strategy. Representative, highly AAR-susceptible road paving concrete made with an alkali-sensitive greywacke and various water repellents were used as the basis for these experiments. The tests for concrete suitability included determining the conventional fresh and hardened concrete properties as well as concrete prism tests with external alkaline supply. Building on these results, laser-induced breakdown spectroscopy (LIBS) analyses of de-icing-salt intrusion as well as microscopic examinations for verification of the AAR characteristics were carried out.
The results of the AAR concrete tests with external alkaline supply support the conclusion that, when hydrophobic agents containing a suitable active ingredient are used, the AAR damage process in road paving concrete can be sufficiently prevented.
NMR is becoming increasingly popular for the investigation of building materials as it is a non-invasive technology that does not require any sample preparation nor causes damage to the material. Depending on the specific application it can offer insights into properties like porosity and spatial saturation degree as well as pore structure. Moreover it enables the determination of moisture transport properties and the (re-)distribution of internal moisture into different reservoirs or chemical phases upon damage and curing. However, as yet most investigations were carried out using devices originally either designed for geophysical applications or the analysis of rather homogeneous small scale (< 10 mL) samples. This paper describes the capabilities of an NMR tomograph, which has been specifically optimized for the investigation of larger, heterogeneous building material samples (diameters of up to 72 mm, length of up to 700 mm) with a high flexibility due to interchangeable coils allowing for a high SNR and short echo times (50 - 80 m s).
Utilisation of alkali-sensitive aggregates for concrete pavements by internal hydrophobisation
(2021)
In order to avoid the increased ASR damage to concrete pavements in the German motorway network in the future, the ARS 04/2013 introduced mandatory suitability tests to exclude alkali-sensitive aggregates in new construction measures. This resulted in a significant reduction of suitable aggregates. Against this background, borderline alkali-sensitive aggregates are to be made usable by adding an internal water repellent agent during concrete casting. The ASR avoidance strategy is based on the significant reduction of the penetration of water and de-icing salt solution into the concrete pavement. Laboratory tests show that, with a suitable active ingredient, the ASR damage process can be significantly reduced with internal hydrophobisation. The disadvantage is that this is associated with a deterioration of the mechanical properties and the resistance to freeze-thaw with de-icing salt. The aim of the ongoing research is to reduce these disadvantages through targeted modification of the hydrophobising agent and air-entraining agent.