Alloy 36 is an iron-based alloy with 36% nickel. It is used in applications in which dimensional stability is critical, such as molding tools for composite materials in aerospace and automotive applications. Moreover, increasingly complex structures and the optimisation of resource efficiency also require additive manufacturing steps for the production or repair of components. Additively manufactured components have a heterogeneous microstructure and anisotropic mechanical properties. In addition, the manufactured components require subsequent machining surface finishing due to the high requirements. Nickel iron alloys are difficult to machine. Additionally, inhomogeneous microstructure may lead to unstable cutting forces and conditions. Alloy modifications are made to the alloy 36. For this purpose, titanium, zirconium and niobium are added up to 1 % by mass each. Plasma-Transferred-Arc is used for the welding tests. The hardness profile is determined on the transverse section. The initial structure as well as the modifications have an austenitic structure. The microstructure of the modifications of Alloy 36 with 1% Ti and 1% Zr is not refined, instead the grain size increases.
Alloy 36 (1.3912), also known as “Invar”, is an alloy with 36% nickel. The alloy has a remarkably low thermal expansion coefficient in certain temperature ranges. Therefore, it is used in applications in which dimensional stability is critical, such as moulding tools for composite materials in aerospace and automotive applications. Moreover, increasingly complex structures and the optimisation of resource efficiency also require additive manufacturing steps for the production or repair of components. Additively manufactured components have a heterogeneous microstructure and anisotropic mechanical properties. In part I of this investigation, the initial alloy 36 is modified with the elements Ti, Zr and Hf up to a maximum of 0.33 wt.-%. The influence of the modification elements on the microstructure as well as on the hardness of the AM components is examined. Part II focusses on the effect of the alloy modifications on machinability as well as on the surface integrity of plasma-transferred-arc-welded (PTA) and finish milled invar components. The results show that PTA welding cause numerous finely distributed precipitates with high silicon content.
Co-Cr alloys are frequently used for highly stressed components, especially in turbine and plant construction, due to their high resistance to thermal and mechanical stress, as well as to corrosive and abrasive loads. Furthermore, they are classified as difficult-to-cut materials because of their high strength and toughness as well as their low thermal conductivity. However, for Co, an increased cost and supply risk can be observed in recent years. Therefore, additive manufacturing (AM) offers significant economic advantages due to higher material efficiency regarding repair, modification, and manufacturing of such components. Concerning inhomogeneity and anisotropy of the microstructure and properties as well as manufacturing-related stresses, a lot of knowledge is still necessary for the economic use of additive welding processes in SMEs. In addition, subsequent machining, particularly contour milling, is essential to generate the required complex contours and surfaces. Hence, additive and machining manufacturing processes need to be coordinated in a complementary way, especially due to additional challenges arising in milling of heterogeneous hard-to-cut microstructures. Recently, it has been shown that modern, hybrid cutting processes, such as ultrasonic-assisted milling (US), can improve the cutting situation. In this investigation, the Co-Cr initial alloy is additionally modified with Ti and Zr up to 1 wt.-% with the aim to enhance the homogeneity of the microstructure and, thus, the machinability. Hence the investigation includes finish milling tests of the AM components and the comparison of US and conventional machining. Both the modifications and the ultrasonic assistance exhibit a significant effect on the machining situation, e.g., US causes a higher surface integrity of the finish milled surfaces compared to conventional milling.
Due to increasing requirements relating to the efficiency of highly stressed components in turbine or plant construction, the use of cost-intensive, difficult to process materials is increasingly necessary today. In this context, cobalt-chromium alloys in particular are highly resistant to thermal and mechanical stress, as well as to corrosive and abrasive loads. Moreover, increasingly complex structures and the optimisation of resource efficiency also require additive manufacturing steps for the production or repair of components in many sectors. In order to realise a homogeneous and isotropic microstructure, alloy modifications are made to the alloy CoCr26Ni9Mo5W. For this purpose, hafnium and zirconium are added at 1 % and 0,33 % by mass each, as these elements are supposed to have a positive effect on the microstructure morphology. Plasma-Transferred-Arc is used for the welding tests. Wall structures are welded by multiple single-layer, overlapping welding beads on low-alloyed steel substrate (S355). The results show that the alloying elements hafnium and zirconium have a clear influence on the microstructure. Hardness measurements were also carried out. With each modification, the hardness is increased compared to the original material. The machining analyses show a reduction in cutting forces using ultrasonic assisted milling for high cutting speed and low feed rate.