In this work, a series of 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide (DOPO) derivative salts containing phosphorus and nitrogen were synthesized, and their effects on mechanical properties, thermal stability and flame retardancy of flexible polyurethane foam (FPUF) were investigated. Studies have shown that the addition of DOPO derivatives will increase the tensile strength, compression set, and compression hardness of FPUF, but it will lead to a decrease in elongation at break. Thermogravimetric analysis showed that the initial decomposition temperature of FPUF containing DOPO derivatives was reduecd, but the char reside was significantly improved. A series of combustion tests indicated that the addition of DOPO derivative salts can improve the flame retardancy of FPUF, of which 10-hydroxy-9,10-dihydro-9-oxa-10 phosphaphenanthrene-10-oxide dicyandiamide salt (D-DICY) exhibited the best flame retardancy. When the load of D-DICY was 20 phr, the limiting oxygen index (LOI) of foam reached 24.5%, and the peak heat release rate and total heat release were decreased by 55.7% and 52.9%, respectively. Furthermore, based on the analysis of the gas phase combustion products and the char residue of the condensed phase, the possible flame retardant mechanism was proposed.
The impact fracture behavior of two common high-density polyethylene grades for container applications were intensively studied by the instrumented Charpy impact test after well-defined exposure to UV-irradiation. Individual stages of the impact event, such as crack initiation and crack propagation energy as well as maximum impact load, were investigated from the recorded load–deflection curves. UV-induced material property changes were further investigated by infrared spectroscopy, differential scanning calorimetry, and dynamic-mechanical analysis as well as density measurements. Based on the results of the Charpy impact test, three indicators were identified to describe the extend of photooxidation on high-density polyethylene: (a) a reduced Charpy impact strength—at least to half of its initial value for a distinctly brittle impact fracture, (b) a marked decrease in the crack propagation contribution to the impact strength, and (c) an increase of the brittle features of the fracture surface.
Aluminum tris (diethylphosphinate) (AlPi) is known to have an efficient flame-retardant effect when used in poly(butadiene terephthalates) (PBT). Additionally, better flame-retardant effects can be achieved through the partial substitution of AlPi by boehmite in multi-component systems, which have been shown to be an effective synergist due to cooling effects and residue formation. Although the potential of beneficial effects is generally well known, the influence of particle sizes and behavior in synergistic compositions are still unknown. Within this paper, it is shown that the synergistic effects in flammability measured by limiting oxygen index (LOI) can vary depending on the particle size distribution used in PBT. In conducting thermogravimetric analysis (TGA) measurements, it was observed that smaller boehmite particles result in slightly increased char yields, most probably due to increased reactivity of the metal oxides formed, and they react slightly earlier than larger boehmite particles. This leads to an earlier release of water into the system enhancing the hydrolysis of PBT. Supported by Fourier transformation infrared spectroscopy (FTIR), we propose that the later reactions of the larger boehmite particles decrease the portion of highly flammable tetrahydrofuran in the gas phase within early burning stages. Therefore, the LOI index increased by 4 vol.% when lager boehmite particles were used for the synergistic mixture.