Filtern
Dokumenttyp
Referierte Publikation
- ja (15) (entfernen)
Schlagworte
- Brandschutz (6)
- Brandversuche (5)
- Reaktive Brandschutzsysteme (4)
- Stahl (4)
- Fire test (3)
- Concrete (2)
- Concrete filled tube (CFT) column (2)
- Feuerwiderstand (2)
- Fire resistance (2)
- Intumescent coating (2)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (15) (entfernen)
Paper des Monats
- ja (2)
Understanding the susceptibility to spalling of concrete members in case of fire is important to evaluate the residual load-bearing capacity. The investigations of the spalling phenomenon of a concrete mixture using real scale members are necessary but expensive to carry out. Reducing the specimen size leads to an increase of boundary effects that can result in a reduced spalling or absence of spalling. In this study, fire tests were carried out on unrestrained, single-sided exposed, cuboid shaped specimens (0.6 m x 0.6 m x 0.29 m) as well as unrestrained and steel ring restrained cylindrical specimens (Ø = 0.47 m, h = 0.29 m), which induce different boundary conditions. These fire tests were carried out on two ordinary concrete mixtures. The two mixtures differ only in the type of aggregates (quartz gravel and basalt grit) and were used to investigate the influence of the thermal expansion of the aggregate on the spalling behaviour of the concrete. The results show a significant increase of
the spalling depth due to the restrained thermal expansion achieved by the applied steel rings. Additionally, the type of aggregate has a direct influence on the spalling behaviour of a concrete mixture. The reduction of the boundary effects by the steel rings recreate the test conditions in the centre of a large concrete member. Thus, this type of specimen is suitable to determine the susceptibility to spalling of a material (screening-tests) as preliminary investigations to full scale fire tests.
Die Anwendung von Zuggliedern aus Carbon ist durch die außergewöhnlich gute Ermüdungs- sowie hohe Zugfestigkeit des Werkstoffs motiviert. Ferner ergibt sich gegenüber Stahl eine deutliche Reduzierung des Querschnitts. Perspektivisch sollen damit u. a. Stahlzugglieder im Netzwerkbogenbrückenbau ersetzt werden. Das Tragverhalten von Carbonzuggliedern im Brandfall ist jedoch bislang unbekannt. Daher wurden mittels Bauteilbrandversuchen die Versagensmechanismen untersucht sowie anhand gewonnener Versuchsdaten eine exemplarische Einschätzung zur Gleichwertigkeit gegenüber konventionellen Stahlzuggliedern vorgenommen. Der Beitrag beschreibt realmaßstäbliche Brandversuche an mechanisch belasteten Carbonzuggliedern, die im Rahmen des Verbundforschungsvorhabens NeZuCa durchgeführt wurden. Das Versuchsprogramm umfasste vier Carbonzugglieder mit kreisrunden Querschnitten in zwei verschiedenen Durchmessern, 36 mm und 51 mm. In Ermangelung eines präskriptiven Brandszenarios für den im Projekt vorgesehenen Anwendungsfall und aus Gründen der Vergleichbarkeit erfolgte die Brandbeanspruchung nach Einheitstemperaturzeitkurve (ETK). Neben den Längsverformungen der Zugglieder wurden auch die Bauteil und Brandraumtemperaturen aufgezeichnet.
Reaktive Brandschutzsysteme finden im baulichen Brandschutz Anwendung zur Erhöhung des Feuerwiderstands von Stahlkonstruktionen. Neben den Anforderungen an die Feuerwiderstandsdauer können damit auch Ansprüche an die Ästhetik erfüllt werden. Die profilfolgende Applikation und die geringen Trockenschichtdicken der Produkte ermöglichen es, das filigrane Erscheinungsbild von Stahlkonstruktionen aufrechtzuerhalten. Neben der thermischen Schutzwirkung muss auch die Dauerhaftigkeit der Brandschutzbeschichtung sichergestellt werden. Die Bewertungsmethoden, die auf europäischer Ebene durch das EAD 350402-00-1106 zur Verfügung stehen, zielen auf eine Nutzungsdauer von zehn Jahren ab. Prüfverfahren für einen darüber hinausgehenden Zeitraum sind nicht beschrieben. In diesem Beitrag werden experimentelle Untersuchungen zum Einfluss der Bewitterung auf das Expansionsverhalten, zur thermischen Schutzwirkung und zu den während des Aufschäumens im Brandfall stattfindenden Reaktionen vorgestellt. Die Versuche wurden an einem wasserbasierten und einem epoxidharzbasierten reaktiven Brandschutzsystem durchgeführt. Die Ergebnisse wurden im Rahmen des IGF-Forschungsvorhabens 20470 N erzielt.
Intumescent coatings are commonly used in civil engineering to improve the fire resistance of steel constructions. Especially in the case of tension bars, where mostly circular or rectangular solid sections are used, intumescent coatings offer an efficient measure to improve the fire resistance taking advantage of profile-following application and low coating thickness requirements. Thus, the architectural appearance of slender profiles can be preserved. The paper describes real-scale mechanically loaded and unloaded fire tests of circular and rectangular solid steel tension bars with intumescent coating. The aim of these tests is to investigate the influence of the different profile types as well as different bar orientations on the performance of intumescent coatings. The results are used to specify a normative test and assessment procedure to be implemented in a new European standard for determining the contribution of intumescent coatings to the fire resistance of circular or rectangular bars used as tension members.
The size effect has its origin in fracture mechanics and describes the formation as well as propagation of cracks in brittle and solid materials in dependence of the specimen size. However, the size effect in concrete spalling describes the damage behaviour on a macroscopic scale for different sized specimens in case of fire. Concrete spalling is a very complex and yet not fully understood phenomenon. To reduce the effort of fire tests to analyse the spalling behaviour of concrete mixtures, this study investigates the susceptibility to spalling for six different concrete mixtures and three specimen sizes. The sizes were divided in full scale slabs (1.8 m x 1.2 m x 0.3 m), intermediate scale cuboids (0.6 m x 0.6 m x 0.3 m) and small scale cylinders (Ø0.15 m x 0.3 m). For this purpose, a novel test set-up was built to test six intermediate scale or twelve small scale specimens simultaneously to ensure a similar heating regime for every specimen. All specimens were fire exposed on one side and remained unrestrained. A size effect occurred for four of the six concrete mixtures. Compared to the full scale specimens the spalling was reduced significantly for all smaller specimen sizes. Additionally, spalling did not occur for the small scale specimens. The results show that the specimen size is an essential parameter to investigate the susceptibility to spalling of a concrete mixture. For future investigations the testing conditions must be adjusted for the intermediate scale specimens to recreate the conditions of the slabs.
Intumescent fire protection coatings are used to improve the fire resistance of steel members. Due to slender cross-sections typically used for tension members, high demands are placed on the effectiveness and reliability of the intumescent coatings. This paper describes real-scale fire tests of intumescent coatings applied to steel tension members with circular solid and hollow sections. First, the current regulations for the application of intumescent coatings on steel tension members are discussed. After that, a comparison between the foaming behaviour and failure mechanisms of intumescent coatings applied to steel tension members with different cross-sections and loading conditions is given. Next, the experimental setup and procedure of the performed fire tests are presented. In addition, the influences of various parameters on the performance of the intumescent coating are analysed, including the geometry of the steel profile, dry film thickness of the intumescent coating, load utilisation level as well as the orientation of the member. Based on the theoretical considerations and results of the fire tests, it is evidenced that mechanically loaded fire tests are essential to assess accurately the contribution of intumescent fire protection coatings to the fire resistance of steel tension members with circular solid sections.
Um Stahlbauteile im Brandfall vor einer zu schnellen Erwärmung zu schützen, wird häufig auf reaktive Brandschutzsysteme (RBS) zurückgegriffen. Die Produkte eigenen sich besonders aufgrund der profilfolgenden Applikationsmöglichkeit und der vergleichsweise geringen Beschichtungsdicken. Bei einer Brandbeanspruchung schäumt das RBS auf und bildet eine thermische Schutzschicht um das Stahlprofil aus. Dadurch wird die Erwärmung des Stahls verlangsamt und der temperaturbedingte Festigkeitsverlust verzögert, wodurch sich die Feuerwiderstandsdauer des Stahlbauteils verbessert. Aus Brandversuchen ist bekannt, dass die Leistungsfähigkeit von RBS auf Stahlprofilen mit gekrümmter Oberfläche meist schlechter ausfällt als bei vergleichbaren Bauteilen mit ebener Oberfläche. Zum Einfluss der Oberflächenkrümmung auf die thermische Schutzwirkung von RBS werden in dem folgenden Beitrag sowohl theoretische Hintergründe als auch die Ergebnisse aus Brandversuchen an kleinformatigen Probekörpern vorgestellt. Die systematischen Untersuchungen zeigen, dass mit zunehmender Oberflächenkrümmung die Leistungsfähigkeit des RBS tendenziell abnimmt. Bei der Beurteilung der thermischen Schutzwirkung eines RBS sollte die Oberflächenkrümmung eines Bauteils berücksichtigt werden. Die alleinige Fokussierung auf den Profilfaktor eines Stahlprofils ist im Allgemeinen nicht ausreichend. Die Untersuchungen bilden die Grundlage für die Entwicklung von Screening-Tests zur Beurteilung der Eignung von RBS für gekrümmte Oberflächen, wodurch eine Vorauswahl von Produkten für diesen Einsatzzweck ermöglicht wird.
Reaktive Brandschutzsysteme können die Feuerwiderstandsdauer von Stahlbauteilen signifikant erhöhen. Im Brandfall schäumt das reaktive Brandschutzsystem auf und bildet um das Stahlbauteil eine thermische Schutzschicht aus. Dadurch wird die Erwärmung des Stahls verlangsamt und der temperaturbedingte Festigkeitsverlust verzögert. Reaktive Brandschutzsysteme werden überwiegend in drei Bereichen angewendet: Hochbau, Offshore bzw. maritimer Sektor sowie Tank- bzw. Behälterbau. Insbesondere bei Stahltanks und -behältern sind häufig einfach oder auch doppelt gekrümmte Bauteiloberflächen anzutreffen. Aufgrund des meist begrenzten seitlichen Expansionsvermögens von reaktiven Brandschutzsystemen kann es bei Bauteilen mit konvexer Oberflächenkrümmung zu einer Intensivierung der Rissbildung im Schaum kommen, wodurch sich häufig die thermische Schutzwirkung verschlechtert. Da zum Thema des Einflusses der Oberflächenkrümmung auf die Leistungsfähigkeit reaktiver Brandschutzsysteme bisher kaum Untersuchungen vorliegen, wurden exemplarisch zwei Tankböden mit zwei verschiedenen Trockenschichtdicken eines reaktiven Brandschutzsystems einer Brandprüfung unterzogen. Bei gleicher Trockenschichtdicke des reaktiven Brandschutzsystems zeigten die Tankböden eine wesentlich schnellere Erwärmung als ebene Stahlplatten mit vergleichbarem Profilfaktor. Die Brandprüfungen und die Ergebnisse zum Einfluss der Oberflächenkrümmung werden im Beitrag ausführlich vorgestellt und diskutiert.
Nowadays there are intumescent coatings available for diverse applications. There is no established assessment of their protection performance besides the standard time-temperature curve, but natural fire scenarios often play an important role. A reliable straightforward performance-based assessment is presented. The effective thermal conductivity per thickness is calculated based on intermediate-scale fire tests. The optimum thermal insulation, the time to reach it, and the time until contingent failure of the coating are used for an assessment independent of the heating curve. The procedure was conducted on four different commercially intumescent coatings for steel construction, one solvent-based, one waterborne, one epoxy-based, and a bandage impregnated with a waterborne coating. The performance was studied under four different but similar shaped heating curves with different maximum temperatures (standard time-temperature curve, hydrocarbon curve and two self-designed curves with reduced temperature). The thermal protection performance is crucially affected by the residue morphology. Therefore, a comprehensive morphology analysis, including micro-computed tomography and scanning electron microscopy, was conducted on small-scale residues (7.5 x 7.5 cm2). Two different types of inner structures and the residue surface after different heat exposures were discussed in terms of their influence on thermal protection performance.
Zur brandschutztechnischen Ertüchtigung von Stahlkonstruktionen werden reaktive Brandschutzsysteme aufgrund der geringen Beschichtungsdicken und der profilfolgenden Applikation in zunehmendem Maße eingesetzt. Da die für Zugstabsysteme eingesetzten Bauteile meist eine stark konvex gekrümmte Oberfläche aufweisen und der Anschlussbereich über eine vergleichsweise komplexe Geometrie verfügt, stellt dies besonders hohe Anforderungen an die Leistungsfähigkeit von reaktiven Brandschutzsystemen. Anhand von realmaßstäblichen Brandversuchen wurden das Aufschäumungs- und Rissverhalten, der Einfluss der Trockenschichtdicke, die Erwärmung der einzelnen Stahlbauteile sowie der Einfluss der Bauteilorientierung untersucht. Die Ergebnisse zeigen, dass eine Abnahme der Oberflächenkrümmung oder eine Erhöhung der Massenkonzentration der Stahlbauteile zu einer geringeren Aufheizrate des Stahls führt. Darüber hinaus ist festzustellen, dass die Leistungsfähigkeit des reaktiven Brandschutzsystems von der Bauteilorientierung der Zugstabsysteme beeinflusst wird. Die durchgeführten Brandversuche können zur Entwicklung geeigneter Prüfszenarien für die Beurteilung von reaktiven Brandschutzsystemen auf Zugstabsystemen und deren Anschlusskonstruktionen verwendet werden, wodurch eine Erweiterung des zulassungsbasierten Anwendungsbereichs ermöglicht wird.