Filtern
Dokumenttyp
- Zeitschriftenartikel (6)
- Beitrag zu einem Tagungsband (1)
- Vortrag (1)
- Posterpräsentation (1)
Sprache
- Englisch (9)
Schlagworte
- Fire behavior (9) (entfernen)
Organisationseinheit der BAM
Eingeladener Vortrag
- nein (1)
The addition of nanoparticles as reinforcing fillers in elastomers yields nanocomposites with unique property profiles, which opens the door for various new application fields. Major factors influencing the performance of nanocomposites are studied by varying the type and shape of nanoparticles and their dispersion in the natural rubber matrix. The industrial applicability of these nanocomposites is put into focus using two types of graphene and a nanoscale carbon black, all commercially available, and scalable processing techniques in the form of a highly filled masterbatch production via latex premixing by simple stirring or ultrasonically assisted dispersing with surfactant followed by conventional two-roll milling and hot pressing. Different processing and measurement methods reveal the potential for possible improvements: rheology, curing behavior, static and dynamic mechanical properties, swelling, and fire behavior. The aspect ratio of the nanoparticles and their interaction with the surrounding matrix prove to be crucial for the development of superior nanocomposites. An enhanced dispersing method enables the utilization of the improvement potential at low filler loadings (3 parts per hundred of rubber [phr]) and yields multifunctional rubber nanocomposites: two-dimensional layered particles (graphene) result in anisotropic material behavior with strong reinforcement in the in-plane direction (157% increase in the Young's modulus). The peak heat release rate in the cone calorimeter is reduced by 55% by incorporating 3 phr of few-layer graphene via an optimized dispersing process.
Simulation of the burning and dripping cables in fire using the particle finite element method
(2022)
The behavior of the cable jacket in fire characterized by the tendency to melt and drip constitutes a major source of fire hazard. The reason is that the melted material may convey the flame from one point to another, expanding fire and contributing to the fire load. In this article, the capability of a new computational strategy based on the particle finite element method for simulating a bench-scale cables burning test is analyzed. The use bench-scale test has been previously used to simulate the full-scale test described in EN 50399. As the air effect is neglected, a simple combustion model is included. The samples selected are two cables consisting of a copper core and differently flame retarded thermoplastic polyurethane sheets. The key modeling parameters were determined from different literature sources as well as experimentally. During the experiment, the specimen was burned under the test set-up condition recording the process and measuring the temperature evolution by means of three thermocouples. Next, the test was reproduced numerically and compared with a real fire test. The numerical results show that the particle finite element method can accurately predict the evolution of the temperature and the melting of the jacket.
Rigid polyurethane foams (RPUFs) exhibit short times to ignition as well as rapid flame spread and are therefore considered to be hazardous materials. This paper focuses on the fire phenomena of RPUFs, which were investigated through a multimethodological approach. Water-blown polyurethane (PUR) foams without flame retardants (FRs) as well as waterblown PUR foams containing triethyl phosphate as a gas phase-active FR were examined. The aim of this study is to clarify the influence of the FR on the fire phenomena during combustion of the foams. Additionally, materials’ densitieswere varied to range from 30 to 100 kg/m3. Thermophysical properties were studied bymeans of thermogravimetry; fire behavior and flammability were investigated via cone calorimeter and limiting Oxygen index, respectively. During the cone calorimeter test, the temperature development inside the burning specimens was monitored with thermocouples, and cross sections of quenched specimens were examined visually, giving insight into the morphological changes during combustion.
The present paper delivers a comprehensive study, illuminating phenomena occurring during foam combustion and the influence of a FR active in the gas phase. The superior fire performance of flameretarded PUR foams was found to be based on flame inhibition, and on increased char yield leading to a more effective protective layer. It was proven that in-depth absorption of radiation is a significant factor for estimation of time to ignition. Cross sections investigated with the electron scanning microscope exhibited a pyrolysis front with an intact foam structure underneath. The measurement of temperature development inside burning specimens implied a shift of burning behavior towards that of non-cellular materials with rising foam density.
This work investigates the fire phenomena of rigid polyurethane foams (RPUF) in detail. Rigid polyurethane foams (RPUF) are widely used in industry and daily life because of their outstanding mechanical and thermal insulating properties. In case of fire, cellular polymers like RPUF behave differently from bulk materials, the reason for this is their low thermal inertia. The aim of this study is to investigate the fire phenomena of RPUF in detail. Characterized by simultaneous physical and chemical processes which interact, depend, and compete with each other, the combustion of RPUF is a highly complex occurrence. Therefore it is necessary to study all aspects in detail. The fire phenomena that were examined are gasification, liquefaction, charring and structural integrity as well as collapse. The comprehensive understanding of the processes taking place during combustion is the foundation of customized development of successful flame retardant approaches. Advanced cone calorimeter investigations provide insight into the fire behavior under forced flaming conditions. Thermocouples in the inside of specimens give information about the temperature gradient and temperature of the pyrolysis zone during combustion. Changes in the morphology and thickness of the pyrolysis zone were examined using a hot-stage microscope, as well as SEM images of cross-sections of quenched foam specimens. Furthermore, fire phenomena were characterized using LOI and thermal analysis. By using a multimethodological approach and systematically varied sets of Polyurethane and Polyisocyanurate foams, new insights into the burning of RPUF were won. The detailed knowledge of fire phenomena is essential for future development of tailored flame retardant strategies for RPUF.
Reconstructing the course of a fire and performing chemical analysis of ignitable liquids in fire debris is an important tool to conduct fire investigations in suspected arson cases. Here, a total of five fire tests has been performed to investigate the effect of fire accelerants on the fire development of a room fire and to prove the capability of analytical methods. Different experimental scenarios have been realized (no accelerant, accelerant applied at different positions, and different amounts of fire accelerant). Each test room was equipped with an identical set of living room furnishing. The location and amount of the fire accelerant applied löschen varied in four of five tests. One experiment was carried out without fire accelerant. Fire quantities such as mass loss (of the entire room), gas temperatures (at several locations in the room), and heat release were determined during the experiments, and chemical-analytical studies were carried out. A headspace solid phase micro extraction procedure, using gas chromatography–mass spectrometry, was used to analyze fire debris samples to potentially detect ignitable liquids. Beside the analysis of fire debris samples, swipe soot samples were analyzed and the detectability of the fire accelerant used was demonstrated. Results show that it is possible to provide evidence of ignitable liquids in soot samples collected from walls. This allows an additional sampling strategy at potential crime scenes, besides taking fire debris samples.
First developments of a new test to evaluate the fire behavior of photovoltaic modules on roofs
(2015)
A new test for photovoltaic (PV) modules exposed to an external fire source on roofs is proposed, and first results are presented. This is a simplification of the standards commonly in use for testing PV modules as roofing parts, roofing components or building components. Most of the tests required different fire scenarios and the use of burning brands such as wood cribs. In our study we proposed replacing wooden burning brands with a propane burner, the output of which is close to the one that can be observed in the burning of wooden cribs 500 g and 2 kg in size. The fire behavior was assessed by measuring smoke evolution, burning drips, flaming debris, and the time to burn-through of monocrystalline, polycrystalline and amorphous silicon panels. Two different configurations of the burner were tested, with the fire source on the top of the module or under the tilted module, respectively. The fire behavior of the modules was dependent on the burner output (16 to 46 kW), but also on the construction type of the panel (glass/glass or glass/plastic sheet) and on the position of the fire source (top or bottom). These preliminary tests for further development of the procedure yielded encouraging results for the evaluation of PV panels on roofs.
Nanotechnology is one of the key technologies of the 21st century. The exploitation of 'new' effects that arise from materials structured on the nano-scale has also been proposed successfully for flame retardancy of polymers since the end of the 90s. Of all of the approaches these include, at this time the use of nanocomposites offers the best potential for industrial application, also some other ideas are sketched, such as using electrospun nanofibers mats or layer-by-layer deposits as protection coatings, as well as sub-micrometer multilayer coatings as effective IR-mirrors. The general phenomena, inducing a flow limit in the pyrolysing melt and changing the fire residue, are identified in nanocomposites. Key experiments are performed such as quasi online investigation of the protection layer formation to understand what is going on in detail. The flame retardancy mechanisms are discussed and their impact on fire behaviour quantified. With the latter, the presentation pushes forward the state of the art. For instance, the heat shielding is experimentally quantified for a layered silicate epoxy resin nanocomposite proving that it is the only import mechanism controlling the reduction in peak heat release rate in the investigated system for different irradiations. The flame retardancy performance is assessed comprehensively illuminating not only the strengths but also the weak points of the concepts. Guidelines for materials development are deduced and discussed. Apart from inorganic fillers (layered silicate, boehmite, etc.) not only carbon nanoobjects such as multiwall carbon nanotubes, multilayer graphene and graphene are investigated, but also nanoparticles that are more reactive and harbor the potential for more beneficial interactions with the polymer matrix.
Layered silicate epoxy nanocomposites: formation of the inorganic-carbonaceous fire protection layer
(2011)
The layered silicate (LS) modification and processing parameters applied control the morphology of the LS/polymer composites. Here, increasing the surface area of the LS particles by using alternative drying processes increases dispersion towards a more typical nanocomposite morphology, which is a basic requirement for promising flame retardancy. Nevertheless, the morphology at room temperature does not act itself with respect to flame retardancy, but serves as a prerequisite for the formation of an efficient surface protection layer during pyrolysis. The formation of this residue layer was addressed experimentally for the actual pyrolysis region of a burning nanocomposite and thus our results are valid without any assumptions or compromises on the time period, dimension, surrounding atmosphere or temperature. The formation of the inorganic-carbonaceous residue is influenced by bubbling, migration, reorientation, agglomeration, ablation, and perhaps also delamination induced thermally and by decomposition, whereas true sintering of the inorganic particles was ruled out as an important mechanism. Multiple, quite different mechanisms are relevant during the formation of the residue, and the importance of each mechanism probably differs from one nanocomposite system to another. The main fire protection effect of the surface layer in polymer nanocomposites based on non-charring or nearly non-charring polymers is the increase in surface temperature, resulting in a substantial increase in reradiated heat flux (heat shielding).