The mechanical properties of unstabilised earthen building materials are distinctively influenced by changes in material moisture content. However, this moisture-dependency often remains unconsidered in the calculation of the load-bearing capacity of earth constructions. This paper aims to derive a convenient way to sufficiently consider the impact of different material moisture contents on the mechanical properties of unstabilised earth masonry. Therefore, the influence of relative humidity and temperature on the strength and deformation characteristics of unstabilised earth blocks, earth mortar and earth masonry is evaluated by conducting compression tests under various climate conditions. The results show that the compressive strength and the modulus of elasticity are linearly correlated with the relative humidity, whereas changes in temperature at constant relative humidity have no significant influence. To account the distinct moisture-dependency, a general applicable modification factor for unstabilised earthen materials is provided, which enables the adjustment of the compressive strength and the modulus of elasticity in dependency of arbitrary hygroscopic material moisture contents.
Damage and strength reduction of a high performance concrete due to thermomechanical stresses
(2008)
The main aim of the research was the development of a first valid database for material parameters of earth block masonry (EBM) with particular regard to statistical characteristics. A solid database is needed for the determination of the materials partial safety factor. Therefore, compressive strength tests were carried out with two types of earth blocks and two types of prefabricated earth mortar.
The evaluation has shown that the mean variation of the compressive strength was remarkably less than expected, which indicates high quality standards of the components earth block and mortar with regard to industrial production. Using the reliability method, a partial safety factor for EBM subjected to compression was determined on the basis of these test results. The findings have shown that a common calculation method for EBM based on partial safety factors following the valid masonry construction standard is feasible.
Within the presented research project, experimental and numerical investigations were performed to develop a thin-shelled, modular, mobile element system made of a micro-reinforced ultra-high-performance ductile concrete (DUCON®). Material parameters were experimentally determined to adapt the material model within the numerical analysis applying the Drucker-Prager relationship. Afterwards, for validation of the numerical models, quasi-static and high-velocity impact tests were performed on plate-like structures. Finally, a suitable geometry of transportable barrier elements will be designed, which provides a maximum of resistance against impact by a minimum of weight and a maximum of mobility.
Within the presented research project, experimental and numerical investigations were performed to develop a thin-shelled, modular, mobile element system made of a micro-reinforced ultra-high-performance ductile concrete (DUCON®). Material parameters were experimentally determined to adapt the material model within the numerical analysis applying the Drucker-Prager relationship. Afterwards, for validation of the numerical models, quasi-static and high-velocity impact tests were performed on plate-like structures. Finally, a suitable geometry of transportable barrier elements will be designed, which provides a maximum of resistance against impact by a minimum of weight and a maximum of mobility.
Within the presented research project, experimental and numerical investigations were performed to develop a thin-shelled, modular, mobile element system made of a micro-reinforced ultra-high-performance ductile concrete (DUCON®). Material parameters were experimentally determined to adapt the material model within the numerical analysis applying the Drucker-Prager relationship. Afterwards, for validation of the numerical models, quasi-static and high-velocity impact tests were performed on plate-like structures. Finally, a suitable geometry of transportable barrier elements will be designed, which provides a maximum of resistance against impact by a minimum of weight and a maximum of mobility.
Aim of this study is to provide information about moisture dependent material behaviour of unstabilised loadbearing earth blocks and mortars. Compressive strength and Young’s modulus were investigated after conditioning in varying relative humidity reaching from 40 % up to 95 %. The material composition and physical properties were investigated to understand the influence of relative humidity onto the mechanical properties. A normalisation of strength and stiffness by the values obtained at 23 ◦C and 50 % relative humidity reveals a linear dependence of compressive strength and Young’s modulus that is regardless of the material composition.
Thus, it is possible to describe the influence of relative humidity onto the load-bearing behaviour of unstabilised earth masonry materials in a generally valid formulation.
The paper presented here deals with rheological and hardening properties during the setting reaction, and density and compressive strength after the final setting of a figuline composite consisting of Ca2KNa(PO4)2 and 2wt% medium gel strength gelatin. Compared to the composite with monomodal particle size distribution (d50=7.18µm; span=3.9) and its properties during and after setting reaction, the goal of this work is to increase the resulting product compressive strength by mixing different particle sizes in order to obtain bi- and trimodal distributions. For the bimodal powder mixtures the ratio in diameter (dcourse/dsmall) was chosen with 7/1 and volume ratio dcourse/dsmall was 70/30%. For the trimodal powder mixtures the ratio in diameter (dcourse/dmedium/dsmall) was chosen with 70/7/1 and volume ratio dcourse/dmedium/dsmall was set to 44/28/28%.After establishing an adequate crushing and sieving process the tap density and powder density of each fraction was determined. Subsequently, the different particle sizes were mixed and the densities and the Hausner ratio were determined again. The mixtures show an increase in both densities especially the tap density increased significantly. Rheological investigations show that the graphs of storage and loss moduli of the multimodal powder mixtures respectively are similar. The characteristic setting times show a slight decrease compared with the monomodal composite but not significantly different data. When comparing the resulting compressive strength of cylindrical samples, which were stored direct after reaching the initial setting time under physiological conditions, the studies illustrated in all cases for the multimodal mixtures a significant increase in compressive strength and a higher density.