Polydopamine (PDA) is a biological / biomimetic polymer which has spiked considerable interest in recent years. Its monomer is an important neurotransmitter and it is one of the strongest glues produced by biological organisms. Polydopamine is a candidate for several applications, mainly in the field of biology and medicine, but also - recently - for layer coatings with optical, electrical, and mechanical function.
In this work, we investigate PDA layers intended as reflectivity enhancers for mirror surfaces in X-ray astronomical observatories. It has previously been shown, that such X-ray telescopes can be improved by a coating of PDA in the thickness range of several nm. Accurate thickness determination is required to monitor and optimise the coating process. We use spectroscopic ellipsometry to determine first the dielectric function of the polydopamine layers using model coatings of sufficient thickness. This data is then used to accurately determine the layer thickness of much thinner PDA layers. This study resulted in data on the thickness and dielectric function of PDA layers that could lead to a better understanding of the correlation of layer thickness and layer properties depending on the process parameters.
Biopolymers are the building blocks of life. Their properties are exploited for material functionalization on the nanoscale in a flexible manner. An overview over current research activities in the field of sensing, nanostrcuturing, radiation damage measurements on DNA and proteins and microfluidics is given.
Basic paths towards fully green flame retarded kenaf fiber reinforced polylactic acid (K-PLA) biocomposites are compared. Multicomponent flame retardant Systems are investigated using an amount of 20 wt% such as Mg(OH)2 (MH), ammonium polyphosphate (APP) and expandable graphite (EG), and combinations with Silicon dioxide or layered silicate (LS) nanofillers. Adding Kenaf fibers and flame retardants increases the E modulus up to a factor 2, although no compatibilizer was used at all. Thus, in particular adding EG and MH decreases the strength at maximum elongation, and kenaf fibers, MH, and EG are crucial for reducing the elongation to break. The Oxygen index is improved by up to 33 vol% compared to 17 vol% for K-PLA. The HB classification of K-PLA in the UL 94 test is outperformed. All flame retarded biocomposites show somewhat lower thermal stability and increased amounts of residue. MH decreases the fire load significantly, and the greatest reduction in peak heat release rate is obtained for K-PLA/15MH/5LS. Synergistic effects are observed between EG and APP (ratio 2:1) in flammability and fire properties. Synergistic multicomponent systems containing EG and APP, or MH with adjuvants offer a promising route to green flame retarded natural fiber reinforced PLA biocomposites.
Copolyesters of glycolic acid combined with adipic acid and 1,4 butanediol were synthesized, their in vitro hydrolytic degradation was studied and correlated with their structure. The hydrolytic degradation of the copolyesters was directly related with the degree of crystallinity and the diameter of the crystallites. It was found that glycolate units disturb the ordering of the butylene adipate units, which results in a decrease of the crystallinity. By comparing the hydrolysis parameters of synthesized copolyesters with those of similar aliphatic copolyesters a hydrolysis mechanism was proposed. According to this mechanism, the degradation takes place not only by the loss of end units, but also through the removal of larger segments. MALDI-TOF MS data showed that the possibility of a copolyester macromolecule forming cyclic structures correlates with the arrangement of ester groups in the macromolecules and the structure of the linear segments.
Stabilising admixtures are commonly used additives in repair mortars and grouts. Beyond this, such type of admixture is increasingly used in concrete and other cementitious materials. In particular when fresh mortar or concrete properties have to be adjusted reliably, stabilising agents can be beneficially used to improve workability and robustness of the mixture. The mode of operation of these admixtures varies, rather affecting either the liquid phase or the solid particles in the dispersion, both causing strong interactions with the mortar or concrete system, and significant changes in their rheological behaviour. Furthermore, these are strongly affected by the environmental temperature during the casting process. In the paper the effect of temperature on the performance of stabilising agents in cementitious systems is presented and how performance changes affect fresh and hardening mortar or concrete properties. Particular attention is placed on interactions between stabilising agents and superplasticizers. Results are discussed with special focus on self-compacting concrete.