Amorphous carbon (a-C) multilayered films consisting of sequential layers rich in sp2 (A) and sp3 (B) content have been developed by magnetron sputtering. We study here the effect of thickness d of the A layer in developing stable thick films with controllable stress and elastic properties. In situ spectroscopic ellipsometry is used to calculate the thickness and the composition of the individual layers. The latter were compared with those obtained by depth profiling X-ray photoelectron spectroscopy, which also provides the different chemical bonding of the multilayers in depth. The stress and hardness of the deposited a-C films were found to be related to the thickness of the Aj layers and the relative ratio dAj/dB of thicknesses. The possible mechanisms for the stress control, stability and enhancement of elastic properties of multilayered a-C films are discussed.
A study on the bonding structure and mechanical properties of magnetron sputtered CNx thin films
(2001)
Carbon nitride (CNx) films have been deposited by reactive (RF) magnetron sputtering, in order to investigate the effect of the energetic ion bombardment during deposition (IBD), in terms of applied Vb, on their bonding structure. Fourier Transform IR Ellipsometry (FTIRE) and X-ray photoelectron spectroscopy (XPS) were used for the investigation of the films bonding structure, while their mechanical properties were evaluated by nanoindentation measurements. At films grown with low negative Vb, (low energy IBD) the N atoms are distributed homogeneously in substitutional sites in graphitic rings through both sp2 and sp3 bonds and in linear chains, through sp2 bonds. In contrast, the high negative Vb (high energy IBD) has been suggested to promote the non-homogeneous N distribution at localized regions in the films where the formation of sp3 C---N bonds is favored. This behavior was also evidenced by the C1s and N1s XPS peak components, assigned to the sp3 and sp2 carbonnitrogen bonds. Also, high energy IBD films revealed increased values of hardness and elasticity, while hardness values up to 45 GPa were measured at localized regions.