Within the framework of an AiF (The German Federation of Industrial Research Associations) project, investigations were conducted into the solidification behaviour of various high-alloy austenitic steels in laser and laser-GMA hybrid welding. For comparison purposes, reference was made to pure gas metalarc welding tests. It was possible to raise the welding speeds in hybrid welding compared with the individual gas metal-arc (GMA) and laser welding processes. The central subjects of the investigations were the type of solidification and the connected hot cracking behaviour during welding. In this respect, particular attention was paid not only to the kinetic effects during solidification which may be caused by the high solidification rates in laser and hybrid welding but also to their consequences.
Die aktuelle Normung bezüglich mikroskopischer Untersuchungen von Schweißverbindungen und die Zulässigkeit von Mikrorissen sowie deren Definition ist nicht eindeutig. Nach der Darstellung derzeit gültiger Normen im Bereich der Bewertung von Schweißnähten, Qualifizierung von Schweißverfahren und Ausführung von Schweißverbindungen, wird auf Grundlage aktueller Schweißversuche an hochfesten vergüteten Feinkornbaustählen die Problematik von Mikrorissen diskutiert. Offene Punkte und Fragen bzw. Verbesserungsmöglichkeiten werden aufgezeigt und zur Diskussion gestellt. Schließlich wird auf die Klärung des Einflusses von Mikrorissen auf die mechanisch- technologischen Werkstoffkennwerte der Schweißverbindung unter statischer sowie zyklischer Beanspruchung hingewiesen. ---------------------------------------------------------------------------------------------------------------------------------------------------------------
Neither the latest standardisation with regard to microscopic investigations on welded joints nor the permissibility of microcracks and their definition are unambiguous. According to the representation of currently applicable standards in the fields of the assessment of welds, the qualification of welding processes and the execution of welded joints, the problems associated with microcracks are discussed on the basis of the latest welding tests on high-strength quenched-and-tempered fine-grained structural steels. Not only outstanding points and questions but also improvement possibilities are indicated and opened for discussion. Finally, attention is drawn to the clarification of the influence of microcracks on the mechanical- technological material parameters of the welded joint subjected to both static and cyclic stresses.
The new multi-element alloying concept of systems with defined entropy (HEA — high-entropy alloy or MEA — medium-entropy alloy) is increasing in material research interest. Improved properties or combinations of properties are shown by several systems. Thus, the resulting microstructures and production of HEA/MEA as well as properties have been primarily investigated so far. Furthermore, processing is a key issue to transfer HEA/MEA systems to real components. Since welding is the most important joining process for metals, it is crucial to investigate the influence of welding to guarantee component integrity. Since most HEA are made of expensive alloying elements such as Co or Ni, they will not be used entirely as structural materials. Thus, it can be advantageous to weld conventional alloys such as austenitic stainless steels with the HEA and MEA to produce components that are both application-oriented and economically viable. Therefore, in this paper, first results of dissimilar metal welding, by tungsten inert gas (TIG) and friction stir welding (FSW), of a CoCrFeMnNi HEA as well as a CoCrNi MEA with a conventional AISI 304 austenitic stainless steel are presented. The focus is on the microstructure formation due to the two welding processes. The results of TIG welding show a dendritic microstructure, whereas in FSW both materials are stirred but still coexist.
Microcrack formation during gas metal arc welding of high-strength fine-grained structural steel
(2014)
The recent development of high-performance-modified spray arc processes in gas metal arc welding due to modern digital control technology and inverter power sources enables a focused spray arc, which results in higher penetration depths and welding speed. However, microcracks occurred in the weld metal while approaching the process limits of the modified spray arc, represented by a 20-mm double layer DV-groove butt-weld. These cracks were detected in structural steel exhibiting a yield strength level of up to 960 MPa and are neither dependent on the used weld power source nor a consequence of the modified spray arc process itself. The metallographic and fractographic investigations of the rather exceptional fracture surface lead to the classification of the microcracks as hot cracks. The effects of certain welding parameters on the crack probability are clarified using a statistical design of experiment. However, these microcracks do not impact the design specification for toughness in the Charpy V-notch test (absorbed energy at -40 °C for the present material is 30 J).
Multiple principal element alloys encompass the well-known high entropy alloys (HEA). The alloy system represents a new class of materials consisting of at least three alloying elements, each containing 5 to 35 at.%. Thus, this alloying concept differs fundamentally from conventional materials such as steel or nickel alloys. For this purpose, the alloying elements are specifically selected, the microstructures are adjusted in a single-phase and, in some cases, multi-phase manner. In particular, conflicting goals, such as the trade-off between strength and ductility in conventional steels, are overcome. However, in the last 20 years, the focus has been on material synthesis. With the increase in available material quantities, the focus is now on processing issues such as joining and welding processes. The weldability of HEAs has received very little attention so far. The experience with dissimilar metal welds is completely lacking but is essential for the application of these materials in combination with conventional materials. The present study presents comprehensive experimental results on the weldability of an equimolar CoCrFeMnNi-HEA in cold-rolled and heat-treated condition, which was joined by tungsten inert gas welding to an austenitic steel AISI 304. The mechanical properties of the dissimilar metal welds were characterized by cross-weld tensile samples, whereas the local deformation in the weld of the different welding zones was measured by digital image correlation. In accordance with the respective initial HEA condition (cold-rolled vs. heat-treated), the local strain behavior was divergent and influenced the global mechanical properties of both DMW types. Nonetheless, the experiments provided proof in principle of the weldability for dissimilar joints of the CoCrFeMnNi-HEA welded to conventional materials like austenitic stainless steels ensuring a corresponding capability for mechanical loading. This allows further considerations on the application of these innovative materials.
Für eine nachhaltige und ressourceneffiziente Fertigung von Windkraftanlagen ist der Einsatz moderner hochfester Feinkornbaustähle vielfach notwendig. Bei der Montage hochfester Stahlkonstruktionen kommt es trotz anforderungsgerechter schweißtechnischer Fertigung vereinzelt zur Detektion von unzulässigen Unregelmäßigkeiten im Schweißbereich. Derzeitige Normen und Verarbeitungsrichtlinien geben hierbei kaum Informationen zu adäquaten Reparaturkonzepten, insbesondere für hochfeste Stähle. Vor diesem Hintergrund werden an der Bundesanstalt für Materialforschung und -prüfung (BAM) bauteilrelevante Untersuchungen zu den schweißbedingten Beanspruchungen und Gefügeveränderungen bei der schweißtechnischen Reparatur durch lokales thermisches Ausfugen und erneutes Schweißen durchgeführt.
Hierzu werden einige wesentliche Ergebnisse an Beispielen des Ingenieurbaus, mit Blick auf die mechanisch-technologischen Eigenschaften und Eigenspannungen erörtert. In einem aktuellen Vorhaben (FOSTA P1311, IGF 20162N) sind darauf aufbauend die Einflüsse durch die Schrumpfbehinderung und Wärmeführung beim Reparaturschweißen hochfester Feinkornbaustähle (S500MLO, S960QL) sowie die Reparaturzyklenanzahl Fokus systematischer Untersuchungen. Mittels strukturmechanischer Berechnungen ließen sich hierzu selbstbeanspruchende Probenformen identifizieren, die unterschiedliche definierte Steifigkeitsverhältnisse von Reparaturschweißnähten realer Bauteile abbilden. Schweißnähte an diesen bauteilähnlichen Proben weisen signifikant erhöhte schweißbedingte Beanspruchungen mit zunehmenden (Biege-)Einspanngraden auf. Im Vergleich mit bisherigen Erkenntnissen wird gezeigt, dass eine sichere Reparatur solcher Schweißnähte nur mittels optimaler Reparaturkonzepte und Wärmeführung gelingt, um diesen hohen Beanspruchungen und auch den speziellen Gefügen hochfester Stähle Rechnung zu tragen.
Ziel der Untersuchungen ist es letztlich, Empfehlungen für beanspruchungs- und werkstoffgerechte Reparaturkonzepte gerade für KMU abzuleiten, um Schäden und zumeist teure Nacharbeiten zu vermeiden.