We have employed ptychographic coherent diffractive imaging to completely characterize the focal spot wavefield and wavefront aberrations of a high-resolution diffractive X-ray lens. The ptychographic data from a strongly scattering object was acquired using the radiation cone emanating from a coherently illuminated Fresnel zone plate at a photon energy of 6.2 keV. Reconstructed images of the object were retrieved with a spatial resolution of 8 nm by combining the difference-map phase retrieval algorithm with a non-linear optimization refinement. By numerically propagating the reconstructed illumination function, we have obtained the X-ray wavefield profile of the 23 nm round focus of the Fresnel zone plate (outermost zone width, Δr = 20 nm) as well as the X-ray wavefront at the exit pupil of the lens. The measurements of the wavefront aberrations were repeatable to within a root mean square error of 0.006 waves, and we demonstrate that they can be related to manufacturing aspects of the diffractive optical element and to errors on the incident X-ray wavefront introduced by the upstream beamline optics.
Silver nanoparticles (SNP) are among the most commercialized nanoparticles. Here, we show that peptide-coated SNP cause functional impairment of human macrophages. A dose-dependent inhibition of phagocytosis is observed after nanoparticle treatment, and pretreatment of cells with N-acetyl cysteine (NAC) can counteract the phagocytosis disturbances caused by SNP.
Using the surface-sensitive mode of time-of-flight secondary ion mass spectrometry, in combination with multivariate statistical methods, we studied the composition of cell membranes in human macrophages upon exposure to SNP with and without NAC preconditioning. This method revealed characteristic changes in the lipid pattern of the cellular membrane outer leaflet in those cells challenged by SNP. Statistical analyses resulted in 19 characteristic ions, which can be used to distinguish between NAC pretreated and untreated macrophages. The present study discusses the assignments of surface cell membrane phospholipids for the identified ions and the resulting changes in the phospholipid pattern of treated cells. We conclude that the adverse effects in human macrophages caused by SNP can be partially reversed through NAC administration. Some alterations, however, remained.
The size, surface charge and agglomeration state of nanoparticles under physiological conditions are fundamental parameters to be determined prior to their application in toxicological studies. Although silica-based materials are among the most promising candidates for biomedical applications, more systematic studies concerning the characterisation before performing toxicological studies are necessary. This interest is based on the necessity to elucidate the mechanisms affecting its toxicity. We present here TEM, SAXS and SMPS as a combination of methods allowing an accurate determination of single nanoparticle sizes. For the commercial material, Ludox TM50 single particle sizes around 30 nm were found in solution. DLS measurements of single particles are rather affected by polydispersity and particles concentration but this technique is useful to monitor their agglomeration state. Here, the influence of nanoparticle concentration, ionic strength (IS), pH and bath sonication on the agglomeration behaviour of silica particles in solution has been systematically investigated. Moreover, the colloidal stability of silica particles in the presence of BSA has been investigated showing a correlation between silica and protein concentrations and the formation of agglomerates. Finally, the colloidal stability of silica particles in standard cell culture medium has been tested, concluding the necessity of surface modification in order to preserve silica as primary particles in the presence of serum. The results presented here have major implications on toxicity investigations because silica agglomeration will change the probability and uptake mechanisms and thereby may affect toxicity.
The synthesis, characterization, self-assembly, and gel formation of poly(γ-benzyl-L-glutamate) (PBLG) in a molecular weight range from ca. 7,000–100,000 g/mol and with narrow molecular weight distribution are described. The PBLG is synthesized by the nickel-mediated ring-opening polymerization and is characterized by size-exclusion chromatography coupled with multiple-angle laser light scattering, NMR, and Fourier transform infrared spectroscopy. The self-assembly and thermoreversible gel formation in the helicogenic solvent toluene is investigated by transmission electron microscopy, atomic force microscopy, small-angle X-ray scattering, and synchrotron powder X-ray diffraction. At concentrations significantly below the minimum gelation concentration, spherical aggregates are observed. At higher concentrations, gels are formed, which show a 3D network structure composed of nanofibers. The proposed self-assembly mechanism is based on a distorted hexagonal packing of PBLG helices parallel to the axis of the nanofiber. The gel network forms due to branching and rejoining of bundles of PBLG nanofibers. The network exhibits uniform domains with a length of 200±42 nm composed of densely packed PBLG helices.
Here we characterize new metal-functionalized amphiphilic diblock copolymers, developed for both surface and solution molecular recognition applications. Polybutadiene-block-poly(ethylene oxide) copolymers functionalized with nitrilotriacetic acid and tris(nitrilotriacetic acid) were complexed with nickel(II) to obtain coordination sites for oligohistidine residues of model proteins. Mixtures of functionalized polymers with the respective non-functionalized block copolymers self-assemble in aqueous solution into vesicular structures with a controlled density of the metal end-groups on their surface. In solution, binding of His6-tagged green fluorescent protein (EGFP) and red fluorescent protein (RFP) to the vesicle surface was quantified by fluorescence correlation spectroscopy. Small-angle X-ray scattering indicates an increase of the membrane thickness by 2-3 nm upon protein binding. Block copolymer monolayers at the air-water interface and on solid support served as a model system to characterize the protein-decorated membranes by Brewster angle microscopy and AFM. High resolution AFM of solid-supported, hydrated monolayers indicates that the proteins form densely packed and partially ordered arrays with the cylindrically shaped EGFP molecules lying flat on the surface of the films.
Biomimetic synthesis of chiral erbium-doped silver/peptide/silica core-shell nanoparticles (ESPN)
(2011)
Peptide-modified silver nanoparticles have been coated with an erbium-doped silica layer using a method inspired by silica biomineralization. Electron microscopy and small-angle X-ray scattering confirm the presence of an Ag/peptide core and silica shell. The erbium is present as small Er2O3 particles in and on the silica shell. Raman, IR, UV-Vis, and circular dichroism spectroscopies show that the peptide is still present after shell formation and the nanoparticles conserve a chiral plasmon resonance. Magnetic measurements find a paramagnetic behavior. In vitro tests using a macrophage cell line model show that the resulting multicomponent nanoparticles have a low toxicity for macrophages, even on partial dissolution of the silica shell.
Ionic liquids (ILs) have attracted tremendous interest in the recent past for their potential in many chemical fields. The current report explores the effects of a set of ILs based on the 1-ethyl-3-methyl-imidazolium cation and different anions on the formation of gold nanoparticles. X-Ray diffraction finds face-centered cubic gold in all cases, but transmission electron microscopy (TEM) shows that there are distinct differences in particle formation and stabilization with the ethyl sulfate (ES), trifluoromethanesulfonate (TfO) and methanesulfonate (MS) anions. With the MS anion, nanoparticles with diameters between 5 and 7 nm form, which increasingly aggregate at higher reaction temperatures. With TfO, also small 5 to 7 nm particles form, but only at low temperatures. Above ca. 160 °C, large, ill-defined and aggregated particles form. With ES, polydisperse samples form at all temperatures except 160 °C. In this case the nanoparticles appear often surrounded by an IL film, which appears to stabilize individual, ca. 15 to 20 nm particles. Dynamic light scattering and UV/Vis spectroscopy further show that in suspension the particles are, much like seen in the TEM, more strongly aggregated with higher reaction temperatures. In summary, the results suggest that there are very specific IL-gold interactions that are responsible for the formation of gold particles with an IL-specific shape, size, and aggregation behavior.
Dispersions of Fe3C nanoparticles in several ionic liquids (ILs) have been investigated. The ILs are based on 1-ethyl-3-methylimidazolium [Emim] and 1-butyl-3-methylimidazolium [Bmim] cations. Anions are ethylsulfate [ES], methanesulfonate [MS], trifluoromethylsulfonate (triflate) [TfO], tetrafluoroborate [BF4], dicyanamide [N(CN)2], and thiocyanate [SCN]. Among the ILs studied, [Emim][SCN] and [Emim][N(CN)2] stand out because only in these ILs have stable and transparent nanoparticle dispersions been obtained. All other ILs lead to blackish, slightly turbid dispersions or to completely nontransparent suspensions, which often contain undispersed sediment. UV/vis spectroscopy, transmission electron microscopy, and X-ray scattering suggest that the reason for the stabilization of the Fe3C nanoparticles in [Emim][SCN] is the leaching of traces of iron from the particles (without affecting the crystal structure of the Fe3C particles). The resulting particle surface is thus carbon-rich, which presumably favors the stabilization of the particles. A similar explanation can be postulated for [Emim][N(CN)2], with the dicyanamide anion also being a good ligand for iron.