Since additive manufacturing processes typically introduce heterogeneous microstructures and residual stresses, the applicability of parts produced in an as-built state is limited. Therefore, often different post-processing treatments are necessary to obtain the desired stress state and properties.
For additively manufactured Inconel 718, the recently developed standard ASTM F3301 provides guidance for the heat treatment of powder bed fusion specimens. Although this standard is based on standards developed for wrought Inconel 718, it does not include the direct aging variant. In this study, we characterized the microstructure and tensile behavior of Inconel 718 specimens produced by a laser powder bed fusion process. The specimens were heat-treated according to two different routines after stress relieving: a full heat treatment cycle versus a one-step aging process. Differences in the resulting texture and grain morphology were observed. Although these differences prevail, the ex-situ tensile behavior was broadly similar. Minor differences were observed in yield strength and work hardening rate for the direct aged specimen. In order to understand this behavior, investigations with in-situ tensile testing during synchrotron energy-dispersive X-ray diffraction measurements revealed differences in the load partitioning among different crystal directions. This was attributed to microstructural differences between the heat treatment variants. Further analysis emphasized that the various strengthening mechanisms are present to a different extent depending on the heat-treatment cycle applied. In addition, the elastic anisotropy expressed by the differences in the diffraction elastic constants displayed a dependence on the microstructure. Importantly, a precise knowledge of such constants is indispensable to reliably determine residual stresses in parts.
Laser powder bed fusion is used to create near net shape metal parts with a high degree of freedom in geometry design. When it comes to the production of safety critical components, a strict quality assurance is mandatory. An alternative to cost-intensive non-destructive testing of the produced parts is the utilization of in-situ process monitoring techniques. The formation of defects is linked to deviations of the local thermal history of the part from standard conditions. Therefore, one of the most promising monitoring techniques in additive manufacturing is thermography. In this study, features extracted from thermographic data are utilized to investigate the thermal history of cylindrical metal parts. The influence of process parameters, part geometry and scan strategy on the local heat distribution and on the resulting part porosity are presented. The suitability of the extracted features for in-situ process monitoring is discussed.
The present research focuses on the weldability of PBF-LB/M lattice structure parts of Inconel 718 by means of laser beam welding. The integration of complex and lightweight AM structures into assemblies employing conventional joining methods is challenging. During the welding process, dissipation of the laser heat input through thin-walled structures of these lightweight structures is strongly limited, resulting in heat accumulation, atypical cooling rates, and affecting weld geometry, quality of the joint and microstructure. PBF-LB/M parts have been manufactured in three characteristic build directions. They were all stress relieved, then a group of them were submitted to an additional solution annealing and the second group to a two-step aging treatment. Afterwards, these parts were welded to identical PBF-LB/M parts and to wrought ones in butt position. To gain insight into the welding temperature field and to explain segregation mechanisms, grain growth and asymmetries, thermocouples have been attached on the surface’s regions and struts nearby. Joining a lattice structure with a full material wrought sample results in clear asymmetric welds due to dissimilar heat dissipation on both sides of the seam. Selected pre-weld heat treatments have a crucial influence on the quality of the seam on the AM part.