Agar gel pads have been used for electrochemical measurements for some time. For zinc in particular, a standard method for measuring the stability of the corrosion product layer is being established. The main interpretation factor is the corrosion product layer resistance RL, as it is easy to determine and interpret. A high corrosion product layer resistance indicates a high level of protection. However, it is not yet known how low the corrosion product layer resistance is for freshly produced zinc samples. As zinc is highly active, it reacts immediately with the environment to form a corrosion product layer, which affects the corrosion product layer resistance. The addition of zinc acetate to the agar gel pads prevents the formation of a surface layer and destroys existing ones.
This makes it possible to measure an almost corrosion product-free zinc surface. This is important in defining the range of corrosion product layer resistance for a protective surface.
Um zu klären, unter welchen Umständen eine potentielle Gefährdung von Spannstählen beim Kontakt mit verzinkten Bauteilen gegeben ist, wurden Laborversuche in alkalischen Lösungen und Beton sowie Zeitstandversuche an Spannbetonprobekörpern durchgeführt. Abstandsvariationen im Nahbereich haben nur einen geringen Einfluss auf die Polarisation des Stahls. Ein praxisrelevanter, unkritischer Abstand für den indirekten Kontakt, z. B. über die schlaffe Bewehrung, kann nicht definiert werden. Hinsichtlich des Flächenverhältnisses Stahl : Zink wurde ein signifikanter Einfluss festgestellt. Flächenverhältnisse über 10 : 1 führen nicht zu einer Polarisation in den Bereich der Wasserstoffentwicklung. Die Ergebnisse wurden durch Untersuchungen an realen Spannbetonfertigteilen verifiziert.
Zeitstandversuche unter Wasserstoffbeladung führten an zugelassenen Spannstählen nicht zu Brüchen während der Versuchszeit. Die anschließend ermittelten mechanischen Kennwerte zeigten keine signifikanten Änderungen. Ein indirekter Kontakt von Spannstählen zu verzinkten Einbauteilen ist deshalb als unkritisch zu bewerten. Der direkte Kontakt ist durch Einhaltung des in der DIN 1045-1 geforderten Mindestabstands von 2 cm sicher auszuschließen.
Determining a pore structure’s mechanical and chemical data on lime rendering exposed outdoors and including masonry in the laboratory, with regard to their behaviour on moisture transport and weathering was the objective. In search of clues for a dose-response relation - i.e. upon a connection between the emission rate of SO2 and NOx on one hand and the degree of damage to mainly plaster having a lime component on the other - it has been of interest to what extent their structural characteristics including pore space are modified and so consequently also physico-technical properties and chemical composition. For determining corresponding criteria, a widely diversified spectrum of test methods such as to obtain data concerning porosity and moisture transport, mechanical behaviour, and chemistry as well is available. A description of the manufacture of plate-shaped rendering specimens with lime putty, industrially hydrated lime and dolomitic hydrate (the last two also having a cement admixture) and also hydraulic lime as binding agents is included. First deposition velocity and absorption rate for SO2 were determined in laboratory tests on these materials in dry and moist states. After their exposure on outdoor racks at six locations in the Berlin region with differing SO2 atmospheric contents over at least 5 years, the samples of course show timedependent modifications of chemical and physical qualities which are especially reflected in the form of profiles of structure, strength and concentration, e.g. for sulphate. Local climatic differences, however, partly exert a greater influence on material than emissions. Similar investigations were performed on samples of comparable composition exposed 4 and 17 years. But the real surprise is furnished by the renderings’ behaviour depending upon orientation and upon height at a building. Since weathering behaviour and moisture Transport (absorption, storage, release) are directly interdependent, further criteria are necessary for a critical assessment of a plasters’ pore structure. Starting from sands, plasters were characterized. The structural parameters were lastly influenced by the respective contents of sand, binder and mixing water. These results and those gained from bricks naturally find their expression in masonry sections manufactured there from, and above all in their capillary and evaporative behaviours, and also when applying different test liquids. Summary and cited literature is given at the end of this report.
Validierung zerstörungsfreier Messmethoden zur zuverlässigen Erfassung von Bewehrungskorrosion
(2011)
Die Ergebnisse der Untersuchungen sind in ein Konzept zur Durchführung und Auswertung der Potentialfeld- und Polarisationsmessung eingegangen, um den Ingenieuren in der Praxis ein effizienten Werkzeug zur zerstörungsfreien Erfassung des Korrosionszustandes anzubieten. Das Ziel des Vorhabens wurde erreicht.
Der maßgebliche Korrosionsschutz von nicht rostendem Stahl in Beton basiert, anders als bei unlegiertem Betonstahl, auf der Ausbildung einer Chromoxidschicht. Die Chromoxidschicht ist in alkalischem und in carbonatisiertem Beton beständig, sodass nicht rostende Stähle in einem passiven Zustand vorliegen.
Die Initiierung von Lochkorrosionserscheinungen ist dagegen auch an nicht rostenden Stählen in Beton möglich. Der korrosionsauslösende Chloridgehalt ist neben dem Gehalt an Legierungselementen (insbesondere dem Chromgehalt) und der Oberflächenbeschaffenheit auch vom Konzentrationsverhältnis von OH“ zu CI“ im Elektrolyten abhängig. Daher ist prinzipiell zu erwarten, dass in karbonatisierten Betonen geringere Chloridgehalte Korrosion initiieren können als in Betonen mit höheren pH-Werten. Dies gilt in besonderem Maße für nicht rostende Betonstähle mit geringen Chromgehalten, wie z. B. Produkte aus dem Werkstoff 1.4003 (X2CrNi12) mit seiner im Vergleich zu den Standardausteniten geringen Beständigkeit. Um den kritischen korrosionsauslösenden Chloridgehalt am Beispiel eines am Markt verfügbaren ferritischen Chromstahls zu bestimmen, wurden an der Bundesanstalt für Materialforschung und -prüfung (BAM) umfangreiche Untersuchungen zu beschleunigten Korrosionsversuchen in alkalischen und karbonatisierten Mörteln durchgeführt. Mittels Laser-induced Breakdown Spectroscopy (LIBS) konnten die korrosionsauslösenden Chloridgehalte im Phasengrenzbereich Betonstahl-Mörtel ermittelt werden.
In maritimer Exposition können Zinkbauteile Nutzungsdauern von 50 Jahren erreichen. Dabei werden Expositionen mit Spritzwasserbelastung durch Meerwasser nicht betrachtet. Normative Betrachtungen und Korrosionsprognosen basierend auf Einjahreswerten liefern hier grundlegend falsche Ergbnisse, da sie eine signifikant höhere Belastung der Atmosphäre mit SO2 voraussetzen.
In maritimer Exposition können Zinkbauteile Nutzungsdauern von 50 Jahren erreichen. Dabei werden Expositionen mit Spritzwasserbelastung durch Meerwasser nicht betrachtet. Normative Betrachtungen und Korrosionsprognosen basierend auf Einjahreswerten liefern hier grundlegend falsche Ergbnisse, da sie eine signifikant höhere Belastung der Atmosphäre mit SO2 voraussetzen.
In maritimer Exposition können Zinkbauteile Nutzungsdauern von 50 Jahren erreichen. Dabei werden Expositionen mit Spritzwasserbelastung durch Meerwasser nicht betrachtet. Normative Betrachtungen und Korrosionsprognosen basierend auf Einjahreswerten liefern hier grundlegend falsche Ergebnisse, da sie eine signifikant höhere Belastung der Atmosphäre mit SO2 voraussetzen.