Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (51)
- Vortrag (31)
- Forschungsdatensatz (23)
- Posterpräsentation (12)
- Beitrag zu einem Sammelband (4)
- Beitrag zu einem Tagungsband (4)
- Buchkapitel (1)
- Sonstiges (1)
- Forschungsbericht (1)
Schlagworte
- SEM (128) (entfernen)
Organisationseinheit der BAM
- 6 Materialchemie (56)
- 6.1 Oberflächen- und Dünnschichtanalyse (52)
- 5 Werkstofftechnik (10)
- 5.1 Mikrostruktur Design und Degradation (9)
- 1 Analytische Chemie; Referenzmaterialien (4)
- 6.6 Physik und chemische Analytik der Polymere (4)
- 1.6 Anorganische Referenzmaterialien (2)
- 1.8 Umweltanalytik (2)
- 3 Gefahrgutumschließungen; Energiespeicher (2)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (2)
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (31)
Lithium-ion batteries (LIBs) are one technology to overcome the challenges of climate and energy crisis. They are widely used in electric vehicles, consumer electronics, or as storage for renewable energy sources. However, despite innovations in batteries' components like cathode and anode materials, separators, and electrolytes, the aging mechanism related to metallic aluminum current collector degradation causes a significant drop in their performance and prevents the durable use of LIBs. Glow-discharge optical emission spectroscopy (GD-OES) is a powerful method for depth-profiling of batteries' electrode materials. This work investigates aging-induced aluminum deposition on commercial lithium cobalt oxide (LCO) batteries' cathodes. The results illustrate the depth-resolved elemental distribution from the cathode surface to the current collector. An accumulation of aluminum is found on the cathode surface by GD-OES, consistent with results from energy-dispersive X-ray spectroscopy (EDX) combined with focused ion beam (FIB) cutting. In comparison to FIB-EDX, GD-OES allows a fast and manageable depth-profiling. Results from different positions on an aged cathode indicate an inhomogeneous aluminum film growth on the surface. The conclusions from these experiments can lead to a better understanding of the degradation of the aluminum current collector, thus leading to higher lifetimes of LIBs.
Investigation of degradation of the aluminum current collector in lithium-ion batteries by GD-OES
(2022)
Lithium-ion batteries (LIBs) are one technology to overcome the challenges of climate and energy crisis. They are widely used in electric vehicles, consumer electronics, or as storage for renewable energy sources. However, despite innovations in batteries' components like cathode and anode materials, separators, and electrolytes, the aging mechanism related to metallic aluminum current collector degradation causes a significant drop in their performance and prevents the durable use of LIBs. Glow-discharge optical emission spectroscopy (GD-OES) is a powerful method for depth-profiling of batteries' electrode materials. This work investigates aging-induced aluminum deposition on commercial lithium cobalt oxide (LCO) batteries' cathodes. The results illustrate the depth-resolved elemental distribution from the cathode surface to the current collector. An accumulation of aluminum is found on the cathode surface by GD-OES, consistent with results from energy-dispersive X-ray spectroscopy (EDX) combined with focused ion beam (FIB) cutting. In comparison to FIB-EDX, GD-OES allows a fast and manageable depth-profiling. Results from different positions on an aged cathode indicate an inhomogeneous aluminum film growth on the surface. The conclusions from these experiments can lead to a better understanding of the degradation of the aluminum current collector, thus leading to higher lifetimes of LIBs.
We have studied the anisotropic milling of Cu with respect to the milling rate and the milling topography, as well. The background is twofold: i) anisotropic milling has to be taken into account during the preparation of TEM specimens and in the manufacturing of micro parts from crystalline materials, and ii) the orientation depending milling behaviour can be used to generate topographies with specific properties with respect to, for example, adsorption, wear, and corrosion.
In this chapter sample preparation, image acquisition, and nanoparticle size and shape characterization methods using the scanning electron microscope (SEM) in reflective and transmitted working modes are described. These help in obtaining reliable, highly repeatable results. The best solutions vary case-by-case and depend on the raw (powdered or suspension) nanoparticle material, the required measurement uncertainty and on the performance of the SEM.
The use of duplex stainless steels (DSS) in energy related applications is well known. Nowadays, DSS steels become more favorable than austenitic steels due to the outstanding mechanical properties, the good corrosion resistance and the lower nickel content. However, the use of the duplex grade in acidic environments such as seawater often leads to severe degradation of the structural integrity of the steel by hydrogen-induced/assisted cracking (HAC) phenomena, which can eventually result in premature failure. Hydrogen assisted degradation and cracking of steels are active fields of research even though this topic is intensively studied for more than a century. A bottleneck is the analytical validation of the theoretical models proposed ion the literature at the sub-micron scale.
Industrial and the research communities see a need for an accurate analytical method by which it is possible to image the distribution of hydrogen in the microstructure of a steels or and other alloys. Among the very few available methods hydrogen imaging methods, Time-of-Flight secondary ion mass spectrometry (ToF-SIMS) has the principal capability for mapping of hydrogen in a steel’s microstructure. The combination of ToF-SIMS with multivariate data analysis (MVA), electron microscopy (SEM) and electron-backscattered diffraction (EBSD) is a powerful approach for providing chemical and structural information. The use of data fusion techniques has been shown recently to enhance the better understanding of the hydrogen induced degradation processes in in a DSS steel.
Coordination chemistry was applied to deposit pyridine-functionalized gold nanoparticles on silicon substrates. The particles were synthesized through the Brust/Schiffrin route with a subsequent ligand exchange reaction yielding well-defined particles of two different sizes. Multilayer deposition was carried out on a pyridine-terminated SAM, anchored on a hydroxyl-terminated silicon surface. Analogously, Hunter/Vögtle-type tetralactam macrocycle multilayers were deposited as well as mixed layers containing both either in an alternating sequence or as a macrocycle multilayer with a terminating nanoparticle layer. These composite layers were examined with respect to their ability to bind squaraine axles in the macrocycle cavities. The amount of guest bound is higher for the composite layer with alternating macrocycles and nanoparticles.
Several restoration projects of stained-glass windows have been performed in Poland since 2010.Chemical analysis of glass samples was performed with SEM/EDX on a FEI ESEM-XL 30, (EDX-EDAX) and with Micro-XRF (M4 Tornado, Bruker).The chemical composition of medieval glass samples and of glass samples of the 19th Century have been determined.
Signal optimization for transmission Kikuchi diffraction (TKD) measurements in the scanning electron microscope is investigated by a comparison of different sample holder designs. An optimized design is presented, which uses a metal shield to efficiently trap the electron beam after transmission through the sample. For comparison, a second holder configuration allows a significant number of the transmitted electrons to scatter back from the surface of the sample holder onto the diffraction camera screen. It is shown that the secondary interaction with the sample holder leads to a significant increase in the background level, as well as to additional noise in the final Kikuchi diffraction signal. The clean TKD signal of the optimized holder design with reduced background scattering makes it possible to use small signal changes in the range of 2% of the camera full dynamic range. As is shown by an analysis of the power spectrum, the signal-to-noise ratio in the processed Kikuchi diffraction patterns is improved by an order of magnitude. As a result, the optimized design allows an increase in pattern signal to noise ratio which may lead to increase in measurement speed and indexing reliability.
Characterization of organic aerogels as model materials for thermal conductivity measurements
(2008)
A scanning transmission x-ray microscopy (STXM) based methodology is introduced for determining the dimensions (shell thickness, core and total diameter) of core-shell nanoparticles which exhibit a strong x-ray absorption contrast and a sharp interface between core and shell material. A low radiation dosage during data acquisition and, therefore, less x-ray beam induced damage of the sample is achieved by recording STXM images only at two predetermined energies of maximum absorption contrast instead of recording a stack of images across the whole absorption edge. A model core-shell nanoparticle, polytetrafluoroethylene (PTFE) cores with polystyrene (PS) shell, investigated at the HERMES beamline is presented for demonstration. This STXM based methodology yields particle dimensions in good agreement with the scanning electron microscopy (SEM) results (deviation equal or less than 10%). Extension of this methodology to core-shell nanoparticles with inorganic core and organic shell will also be presented and the challenges encountered will be highlighted.
The early stages of corrosion of Fe-Cr-model alloys (2 and 9 % Cr) were investigated after exposure at 650 °C in0.5 % SO2containing gas by electron backscattered diffraction (EBSD) and transmission electron microscopy(TEM). The impact of the grain orientation of the base alloy on the orientation relations of the corrosion productsis presented. After 2 min–5 min exposure the formation of a multi-layered corrosion zone was discovered. Aclear orientation relationship between ferrite and the (Fe,Cr)3O4 spinel could be demonstrated. The obtainedresults show the importance of the grain orientation on oxidation resistance.
Interpreting high-temperature corrosion induced by mixed-gas atmospheres is challenging due to the different contributions of oxidizing gases. Here, a comprehensive study on the combined oxidation/sulfidation using label molecules is presented. Fe-Cr model alloys with 2 wt% and 9 wt% Cr were isothermally exposed using a volumetric mixture of 0.5%S16O2/27%H218O and 0.5%S16O2/7%H218O at 650 ◦C for 5 h and then characterized by secondary ion mass spectroscopy (SIMS). Additionally, the reactions were followed in-situ utilizing energy dispersive X-ray diffraction. The study showed that both S16O2 and H218O contribute to the oxidation of the alloys but to different extents depending on the Cr-content.
In the present work, the influence of deuterium on the microstructure of a duplex stainless steel type EN 1.4462 has been characterized by Time-of-Flight Secondary Ion Mass Spectrometry (ToF-SIMS) supported by scanning electron microscopy (SEM), focused ion beam (FIB), electron back scattered diffraction(EBSD) and energy dispersive x-ray (EDX) investigations. Characterization has been carried out before and after electrochemical charging with deuterium which has been used as a tracer, due to its similar behavior to hydrogen in the steel microstructure. In a first approach, the distribution of the deuterium occurring at temperatures above 58 °C has been visualized. Further it turned out that sub-surface micro blisters are formed in the ferrite-austenite interface, followed by the formation of needle shaped plates and subsequent cracking at the ferrite surface. In the austenite phase, parallel cracking alongside twins and hexagonal close packed (martensitic) regions has been observed. In both phases and even in the apparent interface, cracking has been associated with high deuterium concentrations, as compared to the surrounding undamaged microstructure. Sub-surface blistering in the ferrite has to be attributed to the accumulation and recombination of deuterium at the ferrite-austenite interface underneath the respective ferrite grains and after fast diffusing through this phase. Generally, the present application of chemometric imaging and structural analyses allows characterization of hydrogen assisted degradation at a sub-micron lateral resolution.
Scanning Electron Microscopy (SEM) or Transmission Electron Microscopy (TEM) ? This is a question, nowadays discussed in EM labs of research and industry involved in the characterization and metrology of nanoparticles. The Scanning principle is adapted to TEM, the Transmission mode is adapted to Ultra High Resolution SEM. Can modern SEM replace TEM, reach atomic resolution even without Cs corrector or nm lateral resolution for X-ray Spectroscopy (EDX)?
Due to the development of a New Cold Field Emission (NCFE) electron source Hitachi SEMs SU9000 and SU8200 can deliver routinely sub-nm image resolution and EDX mappings at very high count rates and a lateral EDX resolution of a few nm. A TiO2 sample provided by BAM was analysed at 30 kV using low kV STEM – simultaneously with the Through-the-lens (TTL) SE detector, the Bright Field transmission and Dark Field transmission signals. By this method a pixel-precise information of the particle’s surface using SE, its chemical nature using DF-STEM and its crystalline structure using Bright Field signal is given in one 40sec scan. The advantage of this observation mode compared to Ultra Low Voltage imaging is outlined.
Scanning Electron Microscopy (SEM) or Transmission Electron Microscopy (TEM) ? This is a question, nowadays discussed in EM labs of research and industry involved in the characterization and metrology of nanoparticles. The Scanning principle is adapted to TEM, the Transmission mode is adapted to Ultra High Resolution SEM. Can modern SEM replace TEM, reach atomic resolution even without Cs corrector or nm lateral resolution for energydispersive X-ray spectroscopy (EDX)?
Due to the development of a New Cold Field Emission (NCFE) electron source Hitachi SEMs SU9000 and SU8200 can deliver routinely sub-nm image resolution and EDX mappings at very high count rates and a lateral EDX resolution of a few nm. A TiO2 sample provided by BAM was analysed at 30kV using low kV STEM – simultaneously with the Through-the-lens (TTL) SE detector, the Bright Field transmitted and Dark Field transmitted signals. By this method a pixel precise information of the particles surface using SE, its chemical nature using DF-STEM and its crystalline structure using Bright Field signal is given in one 40sec scan. The advantage of this observation mode compared to Ultra Low Voltage imaging is outlined.
Kalibrierung unterschiedlicher 3D-Messmethoden mit einem vielseitig einsetzbaren Kalibrierobjekt