Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (51) (entfernen)
Schlagworte
- SEM (51) (entfernen)
Organisationseinheit der BAM
- 6 Materialchemie (9)
- 6.1 Oberflächen- und Dünnschichtanalyse (8)
- 5 Werkstofftechnik (6)
- 5.1 Mikrostruktur Design und Degradation (5)
- 1 Analytische Chemie; Referenzmaterialien (2)
- 1.8 Umweltanalytik (2)
- 5.6 Glas (2)
- 9 Komponentensicherheit (2)
- 9.0 Abteilungsleitung und andere (2)
- 1.9 Chemische und optische Sensorik (1)
Paper des Monats
- ja (1)
Electron microscopy investigation of the structure of a compact extruded from nanopowder of nickel
(2007)
Currently, corrosion rates (CR) and/or corrosion products (CP) obtained for methanogen-induced microbiologically influenced corrosion (Mi-MIC) on carbon steel are mainly analyzed from static-incubations. By using a multiport-flow-column, much higher CRs (0.72 mm/yr) were observed, indicating static-incubations are not suitable for determining the corrosive potential of Mi-MIC. With the combination of various analytical methods (ToF-SIMS/SEM-EDS/SEM-FIB) and contrary to previously published data, we observed that CPs contained phosphorus, oxygen, magnesium, calcium and iron but lacked carbon-related species (e.g. siderite). Overall, siderite nucleation is disrupted by methanogens, as they convert aqueous bicarbonate into carbon dioxide for methanogenesis resulting in increased localized corrosion.
Efficient water electrolysis requires electrode coatings with high catalytic activity. Platinum efficiently catalyzes the hydrogen evolution reaction in acidic environments, but is a rare and expensive metal. The activity achieved per metal atom can be increased if small Pt particles are dispersed onto electrically conductive, highly accessible and stable support materials.
However, the addition of Nafion, a typical binder material used in the manufacture of electrode coatings, can decrease catalytic activity by the blocking of pores and active surface sites. A new approach is reported for the direct synthesis of highly active Nafion-free Pt/C catalyst films consisting of small Pt nanoparticles supported in size-controlled mesopores of a conductive carbon film. The synthesis relies on the co-deposition of suitable Pt and C precursors in the presence of polymer micelles, which act as pore templates. Subsequent carbonization in an inert atmosphere produces porous catalyst films with controlled film thickness, pore size and particle size. The catalysts clearly outperform all Nafion-based Pt/C catalysts reported in the literature, particularly at high current densities.
Scanning electron microscopes are usually equipped with energy-dispersive X-ray detectors for electron probe microanalysis. This widespread analytical method allows investigators to determine the elemental composition of specimens with a spatial resolution of about 1 µm. However, owing to the electron-specimen interaction, the emitted spectra reveal, in addition to characteristic lines, also a high level of continuous bremsstrahlung background. As a result, elements with low concentrations cannot be identified. The minimum detection limit can be diminished by two orders of magnitude if the characteristic lines are excited as fluorescence by an additional x-ray source. In this case, the emergence of bremsstrahlung is considerably reduced. Combining a high-brilliance microfocus x-ray tube with efficient polycapillary optics enables one to realize an experimental arrangement for performing local fluorescence analysis at the same point where the electron beam hits the sample. The polycapillary optics under consideration focuses the emitted x-radiation onto focal spots between 30 and 100 µm in diameter. Count rates of several thousands cps have been achieved. Elemental maps have been obtained by means of the motorized specimen stage of the microscope. Copyright © 2005 John Wiley & Sons, Ltd.
Structure formation on the surface of indium phosphide irradiated by femtosecond laser pulses
(2005)
Laser-induced periodic surface structures (LIPSS; ripples) with different spatial characteristics have been observed after irradiation of single-crystalline indium phosphide (c-InP) with multiple linearly polarized femtosecond pulses (130 fs, 800 nm) in air. With an increasing number of pulses per spot, N, up to 100, a characteristic evolution of two different types of ripples has been observed, i.e., (i) the growth of a grating perpendicular to the polarization vector consisting of nearly wavelength-sized periodic lines and (ii), in a specific pulse number regime (N = 530), the additional formation of equally oriented ripples with a spatial period close to half of the laser wavelength. For pulse numbers higher than 50, the formation of micrometer-spaced grooves has been found, which are oriented perpendicular to the ripples. These topographical surface alterations are discussed in the frame of existing LIPSS theories.
Numerical simulation of component and assembly behaviour under different loading conditions is a main tool for safety design in automobile body shell mass production. Knowledge of local material behaviour is fundamental to such simulation tests. As a contribution to the verification of simulation results, the local deformation properties of spot-welded similar and dissimilar material joints in shear tension tests were investigated in this study for a TRIP steel (HCT690T) and a micro-alloyed steel (HX340LAD). For this reason, the local strain distribution was calculated by the digital image correlation technique (DIC). On the basis of the hardness values and microstructure of the spot welds, the differences in local strain between the selected material combinations are discussed. Additionally, the retained austenite content in the TRIP steel was analysed to explain the local strain values. Results obtained in this study regarding similar material welds suggest significant lower local strain values of the TRIP steel HCT690T compared to HX340LAD. One reason could be the decrease of retained austenite in the welded area. Furthermore, it has been ascertained that the local strain in dissimilar material welds decreases for each component compared with the corresponding similar material weld.
The hydration process of Portland cement in a cementitious system is crucial for development of the high-quality cementbased construction material. Complementary experiments of Xray diffraction analysis (XRD), scanning electron microscopy (SEM) and time-resolved laser fluorescence spectroscopy (TRLFS) using europium (Eu(III)) as an optical probe are used to analyse the hydration process of two cement systems in the absence and presence of different organic admixtures.
We Show that different analysed admixtures and the used sulphate carriers in each cement system have a significant influence on the hydration process, namely on the time-dependence in the formation of different hydrate phases of cement. Moreover, the effect of a particular admixture is related to the type of sulphate carrier used.
The quantitative information on the amounts of the crystalline cement paste components is accessible via XRD analysis. Distinctly different morphologies of ettringite and calcium-silicate-hydrates (C-S-H) determined by SEM allow visual conclusions about formation of these phases at particular ageing times. The TRLFS data provides information about the admixture influence on the course of the silicate reaction. The dip in the dependence of the luminescence decay times on the hydration time indicates the change in the structure of C-S-H in the early hydration period. Complementary information from XRD, SEM and TRLFS provides detailed information on distinct periods of the cement hydration process.
Sample preparation for analytical scanning electron microscopy using initial notch sectioning
(2021)
A novel method for broad ion beam based sample sectioning using the concept of initial notches is presented. An adapted sample geometry is utilized in order to create terraces with a well-define d step in erosion depth from the surface. The method consists of milling a notch into the surface, followed by glancing-angle ion beam erosion, which leads to preferential erosion at the notch due to increased local surface elevation. The process of terrace formation can be utilized in sample preparation for analytical scanning electron microscopy in order to get efficient access to the depth-dependent microstructure of a material. It is demonstrated that the method can be applied to both conducting and non-conducting specimens. Furthermore, experimental parameters influencing the preparation success are determined. Finally, as a proof-of-concept, an electron backscatter diffraction study on a surface crystallized diopside glass ceramic is performed, where the method is used to analyze orientation dependent crystal growth phenomena occurring during growth of surface crystals into the bulk.
The materials in oxyfuel power plant will be subjected to CO2– and SO2–rich gases on the fireside. The oxidation behaviour of two 9–12 % Cr steels T92 and VM12 was studied under dry oxyfuel environment in the temperature range of 580–650 °C for up to 1,000 h. The oxide structure and morphology were analyzed using various experimental techniques. A complex temperature dependence of oxidation rate is observed for both T92 and VM12 whereby the oxidation rate decreased with increasing temperature. This is attributed to increased Cr-enrichment in the inner scale with increasing temperature. T92 and VM12 alloys are also susceptible to carburization in an oxyfuel environment.
In order to bridge the gap between lab-scale and industrial-scale production of graphene it is necessary to develop processes, equipment and measurement procedures to control the material features. One of the crucial reasons of graphene’s limited commercialization is the lack of standard procedures to properly characterize and define the material chemical and structural properties down to the nanometer level. This leads to many issues regarding material synthesis repeatability, inappropriateness choice of measurands and measurement reproducibility which heavily affect the consistency of the material performance.
In our study, a comparative analysis is performed on two different series (G5 and G6) of industrial graphene powders, each series produced with four types of functionalization: raw graphene, oxygen-functionalized, nitrogen-functionalized and fluorine-functionalized. All the 8 sample variants were analyzed from a chemical and morphological point of view in the form of powders prepared as slightly pressed in metallic sample holders.
The results of the comparative chemical analyses XPS and EDS show a good agreement in the concentration values for all the elements present in the samples, despite the different analysis volumes addressed by the two techniques. For this reason, the samples can be considered homogeneous in both lateral and vertical direction.
A clear influence of the morphology on the composition is evident. Therefore, such correlative measurements of morphology and composition are necessary for a comprehensive characterization of industrial graphene flakes.
We report a surface analytical study of poly(methyl methacrylate) (PMMA) microparticles (beads) with a grafted shell of poly(acrylic acid) (PAA) with thicknesses up to 4 nm using scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS), time-of-flight secondary ion mass spectrometry (ToF-SIMS), and near-edge X-ray adsorption fine structure (NEXAFS) spectroscopy. These polymer microparticles were analyzed before and after reaction of the surface carboxyl (CO2H) groups with 2,2,2-trifluoroethylamine (TFEA) to gain a better understanding of methods with use of covalently bound probe molecules for surface group analysis. The results obtained with chemical derivatization XPS using TFEA are discussed in terms of surface quantification of reactive CO2H groups on these PAA-coated microparticles. A labeling yield of about 50% was found for TFEA-derivatized particles with amounts of surface-grafted CO2H groups of 99 µmol/g or more, which is consistent with predicted reaction yields for homogeneously dispersed PAA hydrogels.
A new technique for investigation of interfacial dislocations in nickel-base superalloys by scanning electron microscopy is presented. At high temperatures the pressure of interfacial dislocations against the gamma/gamma'-interface causes grooves. This 'fingerprint of the dislocation network' is visualized by deep selective etching, which removes the gamma'-phase down to the gamma/gamma'-interface. Compared with transmission electron microscopy, the proposed method has important advantages: observation of large sample areas, no superposition of dislocations lying in different specimen depths, possibility of three-dimensional view of dislocation configurations, information about the dislocation mobility, reduced time for preparation and visualization. The method can be applied for multiphase materials where the interface is grooved by interfacial dislocations.
The impact of the microstructure of Fe-16Cr-0.2C on high-temperature oxidation – sulphidation in SO2
(2021)
This study elucidates the impact of the microstructure of Fe-16Cr-0.2C on oxide layer formation at 650 ◦C in Ar-0.5 % SO2. A cold-rolled and two heat-treated states of the alloy were exposed for up to 1000 h. The samples were characterised in detail from microstructural and chemical perspectives using scanning electron microscopy (SEM), X-ray diffraction (XRD) and time-of-flight secondary ion mass spectrometry (ToF-SIMS). The microstructural modification of the alloy by heat-treatment was advantageous. It was found that Cr-carbides support chromia formation and reduce sulphidation when their area fraction is low and diameter is small.
The hydrogen influence on the microstructure of the austenitic-ferritic Cr22-Ni5-Mo3 stainless steel was investigated. Cathodic hydrogen charging was performed electrochemically from aqueous solution of 0.1M H2SO4 with hydrogen entry promoter addition. The aim of this study was to reveal microstructural changes appearing during the hydrogen charging and particularly to clarify the occurrence of phase transformations induced by hydrogen. The specific changes in both phases of steel were observed. In the ferritic phase, strong increase of dislocation density was noticed. Longer time of hydrogen charging leaded also to the strips and twin plates formation in ferrite phase. In the austenitic phase, the generation of stacking faults, followed by the formation of α' martensite was remarked.
Considerations using silver nitrate as a reference for in vitro tests with silver nanoparticles
(2016)
Most in vitro tests regarding the cellular toxicology of nanoparticulate metals compare particle to associated metal ion exposure. However. it is also a fact. that for example silver ions are reduced by sugars or transformed to silver chloride by chloride salts which are abundant components of cell culture media. These reactions are likely to either complicate or even invalidate comparisons between effects of ions and particles. Here. we present a fast and quantitative method to determine particle formation and numbers in different cell culture media with non-destructive small-angle X-ray scattering (SAXS). Silver nitrate with a concentration of25 (.Jg Ag mL -I was dissolved for up to 24 h at 37 'C in Dulbeccos Modified Eagle Medium (DMEM) with and without 10% fetal bovine serum (FBS) and a solution ofO-glucose (4.5 (.Jg mL -1). respectively. Silver nanopartides were observed in all Solutions after 5 min. The cell culture media displayed a limited particle-growth. FBS showed an effect on the polydispersity of the generated particles but after 5 min the overall particle size was nearly equal in FBS and non FBS supplemented medium. Particles in D-glucose were precipitating after 10 min. Particulate silver concentration was between 3 and 4 (.Jg mL -1 in both cell culture media (CCM). These results should be taken into account when performing silver ion-toxicity experiments in relevant media.
The fluorine content of polymer particles labelled with 2,2,2-trifluoroethylamine was reliably quantified with overlapping sensitivity ranges by XPS and solid-state NMR. This provides a first step towards reference materials for the metrological traceability of surface group quantifications. The extension of this concept to fluorescence spectroscopy is illustrated.
More and more sub-micro and nano-materials shall be "quickly", but accurately characterized with respect to their morphology, shape, size or size distribution, but also to the chemical composition as well by means of an SEM/EDX (Scanning Electron Microscopy / X-Ray Energy Dispersive Spectrometry) system. This undertaking is becoming successful indeed if the transmission mode at low voltages such as those at a SEM, i. e. mostly up to 30 kV, and EDX, respectively is employed. The transmission mode at conventional SEM can e "activated" firstly by re-defining the specimen to be analyzed and preparing it as a thin specimen, which is quasi-transparent to electrons and by finding a way of collecting only the transmitted electrons for analysis. The first issue can be easily realized by using the conventional TEM grids (and the respective sample preparation); the second one becomes feasible either (i) by placing a socalled STEM semiconductor detector directly under the thin specimen or (ii) by using a Special transmission set-up, which enables to the conventional Everhart-Thornley detector to collect only transmitted electrons by blocking the direct collection of secondary electrons and guiding only the transmitted electrons onto it.