The local structure around Ni and La atoms in Al85Ni10La5 amorphous powder after ball milling was investigated by X-ray absorption spectroscopy. A continuous decrease in coordination number of Ni and La as a function of milling time was observed, while the nearest neighbour distance and the mean square atomic displacement did not change, pointing at the creation of free volume around the Ni and La atoms. These structural changes resemble those of a liquid upon temperature increase. The results are described by a shear band model in which the coordination numbers of Ni and La are different within and outside a shear band.
The relationship between fracture toughness and Yttria content in modern zirconia ceramics was revised. For that purpose, we evaluated here 10 modern Y2O3-stabilized zirconia (YSZ) materials currently used in biomedical applications, namely prosthetic and implant dentistry. The most relevant range between 2-5 mol% Y2O3 was addressed by selecting from conventional opaque 3 mol% YSZ up to more translucent compositions (4-5 mol% YSZs). A technical 2YSZ was used to extend the range of our evaluation. The bulk mol% Y2O3 concentration was measured by X-Ray Fluorescence Spectroscopy. Phase quantification by Rietveld refinement considered two tetragonal phases or an additional cubic phase. A first-account of the fracture toughness (KIc) of the pre-sintered blocks is given, which amounted to 0.4 – 0.7 MPa√m. In the fully-densified state, an inverse power-law behavior was obtained between KIc and bulk mol% Y2O3 content, whether using only our measurements or including literature data, challenging some established relationships. A linear relationship between KIc and the fraction of the transformable t-phase was established within the range of 30–70 vol%.