The economic use of chemical admixtures depends on supply chains. Therefore, in most regions ins sub-Saharan Africa (SSA), the use of admixtures is not common practice. This amplifies the unfavorable framework for concrete construction such as fragmentary supply chains, high local cement prices, and unfavorable construction site facilities in this region significantly. The use of superplasticizer (SP) and stabilizing agents (STA) can enhance the concrete technology in SSA, since they can disassociate the concrete quality from external boundary influences. After providing a general overview of the peculiarities of the SSA boundary framework, economic concepts are provided, how existing material solutions can be significantly improved by the use of SPs and STAs based on locally available materials such as lignosulphonates and cassava starch. Finally a three step optimization process is described that helps developing flowable concrete based on materials that can be accessed in most locations in SSA.
Control chart systems are used in quality management systems to keep production processes stable. In concrete production they are often applied for the control of the compressive strength. The most efficient control chart systems are cumulated sums (cusum), which help to observe deviations from a targeted value. Unlike alternative observation chart systems that focus on process data evaluation, cusum observations react very rapidly on systematic process changes in processes. Therefore, the cusum method is particularly suitable if immediate counteractions have to be taken, like in the case of fresh concrete properties of self-compacting concrete (SCC), which can have severe influences on the durability and mechanical strength of concrete. The rheology of SCC can be affected by an enormous variety of influencing factors, from raw material properties to handling or environmental temperature. The present study shows that regardless of the material based influencing parameter for a rheology change, a steady slump flow can be achieved only by adding supplementary superplasticizer in case of loss of flow and adding stabilising agent (ST) in case of increased flow if the respective V-mask indicates a systematic change. A reference SCC was artificially manipulated in order to achieve realistic experimental data for flowability and flowability changes due to changes in the raw material properties. The results point out that productions with applied cusum methods were capable of keeping the target slump flow deviation within approximately 1% only, while productions without applied cusum method deviated up to 14% and more from the target.
Today polycarboxylate ether based superplasticizer (PCE) is commonly used in concrete technology when high flow properties and water reduction are specified. The ionic strength of the polymers’ backbones determines the adsorption behaviour of polymers on clinker and early hydration products. The amount of required polymers for specified flow properties and the performance over the time of casting is thus determined by the molecular structure of the superplasticizer. The time depending consumption of polycarboxylate ether polymers strongly affects the reaction of aluminates and sulphate ions as well as the hydration process in general. Hence, the choice of polymers for particular flow properties greatly affects the very early properties of cementitious materials such as setting, heat evolution and autogenous deformations.
In order to better understand how PCEs influence the early properties, mixes from cement, limestone filler, viscosity modifying agent and water were varied with a high and a low charge density superplasticizer in differing amounts. Results are presented from measurements with an automatic Vicat device, an isothermal heat flow calorimeter, and shrinkage cones. Tests were conducted at 5, 20, and 30 °C.
It is shown that in presence of PCE the final set correlates well with the inflexion point of the heat flow curve, which emphasises the interrelation between C-S-H formation and setting. No such clear correlation can be found for the initial set, which is attributed to the fact that the initial set is rather a rheological than a structural phenomenon, so that other effects overlap with C-S-H formation. The results demonstrate that for a given polymer concentration low charge density polymers yield earlier setting than high charge polymers. However, this influence is overridden by the influence of the total amount of polymers in a cementitious system. Since PCE is typically added according to rheological specifications, and low charge PCE typically requires higher amounts of polymers than high charge PCE for comparable flow performance, low charge PCE retards setting more than high charge PCE.
The paper furthermore points out that there is no significant influence of the polymer type or amount on the early deformations. Since type and amount strongly affect the hydration, it is demonstrated that early setting causes higher strain after the final set. It is hence concluded that higher PCE solid contents reduce the risk of early cracks that occur at time of setting, when a solid structure has already been formed but without resistance against cracks yet.
Control chart systems are commonly used in quality management systems to keep production processes stable. The most efficient control chart systems are cumulated sums (cusum), which look at the deviations from a target value. Cusum charts react more rapidly on systematic changes in processes than other charts such as Shewhart charts, which look at the process values. The cusum method is often applied for compressive strength but it is particularly suitable if counteractions be taken immediately, like in the case of fresh concrete properties.
The present study shows that regardless of the manipulation, a steady slump flow can be achieved only by adding supplementary superplasticizer in case of loss of flow and adding stabilising agent (ST) in case of increased flow if the V-mask indicates a systematic change. A reference SCC was artificially manipulated in order to achieve either increased or reduced flowability. Arithmetic mean values and standard deviations were determined experimentally without and after taking counteractions. These parameters were used for case studies of steady SCC productions based on normally distributed random values. For the indication of a systematic change, a standard V-mask was used.
The results point out that productions with applied cusum methods were capable of keeping the slump flow deviation from the target in the order of magnitude of about 1% despite drastic manipulations, while productions without applied cusum method deviated up to 14% and more from the target slump flow value.
Varying ambient temperatures in plants or on construction sites during casting of SCC can cause serious problems affecting the fresh concrete performances, such as rheological properties and setting time, with consequences for the hardened properties in the structure. By sensible choices of the components, the robustness of SCC mixtures against temperature variations can be improved. However, this aspect has not been the focus of intensive research yet. In this study the effects of varied ambient temperatures on the early performance of differently composed SCC mixtures are investigated, with emphasis on changes in rheology, early deformations, heat evolution and setting. Focus is placed on the study of the influence of the polycarboxylate ether molecule type as well as different viscositymodifying agents on the temperature robustness. Effects on the relevance for practical concrete applications are evaluated, which will provide a reliable framework of possible actions on the appropriate use of admixtures for SCC.
Numerical simulations of concrete castings are complex and time consuming. In order to decrease simulation time and to simplify simulation procedure, an innovative modelling approach, which treats reinforced sections in a formwork as porous media, was proposed. In the previous studies, this numerical model was proved suitable to simulate casting of model yield-stress fluids through reinforced elements. This article focuses on the experimental validation of the proposed model at the concrete scale. For this purpose, a large-scale laboratory casting of a highly reinforced beam is performed. The casting process is numerically simulated and the numerical results are compared to the experimental measurements.
Although concrete in general is a non-combustible material, the fire resistance of concrete structures depends, to a large extent, on the mechanical material behaviour. Fire tests have shown that SCC is often susceptible to explosive spalling due to fire exposure, in a similar manner to HPC. But there are hardly any studies available that report properties of specimens at high temperatures.
Stabilising admixtures are commonly used additives in repair mortars and grouts. Beyond this, such type of admixture is increasingly used in concrete and other cementitious materials. In particular when fresh mortar or concrete properties have to be adjusted reliably, stabilising agents can be beneficially used to improve workability and robustness of the mixture. The mode of operation of these admixtures varies, rather affecting either the liquid phase or the solid particles in the dispersion, both causing strong interactions with the mortar or concrete system, and significant changes in their rheological behaviour. Furthermore, these are strongly affected by the environmental temperature during the casting process. In the paper the effect of temperature on the performance of stabilising agents in cementitious systems is presented and how performance changes affect fresh and hardening mortar or concrete properties. Particular attention is placed on interactions between stabilising agents and superplasticizers. Results are discussed with special focus on self-compacting concrete.
Chemical admixtures like superplasticisers or stabilising agents are of ever increasing importance for modern concrete technology. They liberate the workability of concrete from its dependency on water content, and thus, open the gate towards innovative and future oriented concrete technologies such as self-compacting concrete.
Today, admixture addition has become common practice in concrete technology, but the understanding of their highly complex mode of operation is extremely difficult and demands for understanding of processes within the range between nanometres and centimetres.
Due to its complex time-dependent, multi-phase and multi-scale behaviour, flowable concrete systems are highly complicated and cannot be described comprehensively by simple models. It is therefore extremely challenging to identify the relevant parameters that predominantly control flow phenomena on different size scales, since these may occur on any scale between the nano scale (e.g. superplasticizer adsorption) and macro scale (e.g. grading of the aggregates). The present study discusses fundamental mechanisms at the interface between particle or hydrate surfaces and the fluid phase at a very early stage of concrete formation, and links these effects to macroscopic flow phenomena. Methods are discussed that appear promising interdisciplinary tools for enhancement of the understanding of the relevant interactions that are responsible for the macroscopic flow of flowable concrete.
The fresh behaviour of self-compacting concrete (SCC) at varying temperatures differs from that of normal vibrated concrete. This is because the rheology of SCC depends not only on degree of cement hydration, but also on the adsorption of superplasticizers – mostly polycarboxylate based polymers (PCE) -, which is affected by the time and hydration progress. Due to the variety of PCEs and mixture compositions for SCC a prediction of the rheology at varying temperatures is complicated. The charge densities of PCEs as well as the water to solid ratio in the paste are identified to be the main decisive parameters for robust fresh concrete properties.
Rheometric concrete investigations with different SCC mixture compositions and varied anionic charge densities of the PCE were conducted. SCC which is rich in powder components showed robust performance at low temperatures while SCC with low powder content was favourable at high temperatures. High charge density PCE pointed out to be very robust at low temperatures but at high temperatures it significantly reduced the flow retention. Low charge density PCE could not generate self-compacting properties at low temperatures but retained the flow performance over sufficiently long time. Based on considerations about particle interactions and adsorption mechanisms of PCEs, the relevant processes are explained and options for the development of robust mixture compositions for individual temperature ranges are itemised.
Over the course of the last decades, concrete construction has significantly changed from mass application towards sophisticated more innovative, future oriented, and performance based materials technology. Today concrete no longer consists of cement, water, and aggregates, but can be enhanced significantly by using supplementary additions and chemical admixtures. Advancements in admixtures eventually facilitated the development of new concrete types such as self-compacting concrete (SCC) and high performance concrete (HPC) by uncoupling the workability from the water-cement ratio (w/c).
While for traditional concrete types the major mixture parameter for the workability and strength were the w/c and the grading of the aggregates, for SCC and HPC the performance parameters are more complicated and the performance depends highly on the powder components. This makes the system more sophisticated and in parallel more prone to scatter during the production. The complexity and difficulty to predict the effects of changes in the process and mixture makes it very difficult to identify the right potentials for savings.