The molecular dynamics of two addition type polynorbornenes, exo-PNBSiand PTCNSi1, bearing microporosity has been investigated by broadbanddielectric spectroscopy, fast scanning calorimetry, and neutron scattering. Bothpolymers have the same side groups but different backbones. Due to theirfavorable transport properties, these polymers have potential applications inseparation membranes for gases. It is established in literature that molecularfluctuations are important for the diffusion of small molecules through poly-mers. For exo-PNBSi, two dielectric processes are observed, which are assignedto Maxwell/Wagner/Sillars (MWS) process due to blocking of charge carriersat internal voids or pore walls. For PTCNSi1, one MWS-polarization process isfound. This points to a bimodal pore-size distribution for exo-PNBSi. A glasstransition for exo-PNBSi and for PTCNSi1 could be evidenced for the first timeusing fast scanning calorimetry. For Tgand the corresponding apparent activa-tion energy, higher values were found for PTCNSi1 compared to exo-PNBSi.For both polymers, the neutron scattering data reveal one relaxation process.This process is mainly assigned to methyl group rotation probably overlayedby carbon–carbon torsional fluctuations.
Superglassy polymers with a large fractional free volume have emerged as novel materials with a broad range of applications, especially in the field of membrane separations. Highly permeable addition-type substituted polynorbornenes with high thermal resistance and chemical stability are among the most promising materials. The major obstacle for extending the practical membrane application is their strong tendency to physical aging, leading to a partial decline in their superior transport performance over time. In the present study, broadband dielectric spectroscopy with complementary X-ray scattering techniques were employed to reveal changes in microporous structure, molecular mobility, and conductivity by systematic
comparison of two polynorbornenes with different numbers of trimethylsilyl side groups. Their response upon heating (aging) was compared in terms of structure, dynamics, and charge transport behavior. Furthermore, a detailed analysis of the observed
Maxwell−Wagner−Sillars polarization at internal interfaces provides unique information about the microporous structure in the
solid films. The knowledge obtained from the experiments will guide and unlock potential in synthesizing addition-type polynorbornenes with versatile properties.
Thermal and corrosion (in)stability of polyamide 6 studied by broadbend dielectric spectroscopy
(2015)
The thermal and corrosion (in)stability of polyamide 6 (PA6) is investigated by dielectric spectroscopy. The dielectric spectra can be decomposed into two local relaxation modes, two segmental modes and a high temperature conductivity/Maxwell-Wagner-Sillars process assigned to the blocking of charge carriers at interfaces between amorphous and crystalline phases of PA6. After thermal testing, the PA6 sample shows no changes in the dielectric spectra. However, after the corrosion test two main changes are observed: (1) A higher activation energy for the local β-relaxation process and (2) an increased intensity of the MWS/conductivity process which is shifted to lower temperatures. It is argued that the changes in the dielectric spectra are caused by remaining salt ions in the sample. A comparative study with non-polar polyethylene reveals that the incorporation of the salt ions during the corrosion test can be traced back to the polarity of PA6.
The influence of distinct carbon based nanofillers: expanded graphite (EG), conducting carbon black (CB), thermally reduced graphene oxide (TRGO) and multi-walled carbon nanotubes (CNT) on the thermal, dielectric, electrical and rheological properties of polybutylene terephthalate (PBT) was examined. The glass transition temperature (Tg) of PBT nanocomposites is independent of the filler type and content. The carbon particles act as nucleation agents and significantly affect the melting temperature (Tm), the crystallization temperature (Tc) and the degree of crystallinity of PBT composites. PBT composites with EG show insulating behaviour over the tested concentration range of 0.5 to 2 wt.-% and hardly changed rheological behaviour. CB, CNT and TRGO induce electrical conductivity to their particular PBT composites by forming a conducting particle network within the polymer matrix. CNT reached the percolation threshold at the lowest concentration (<0.5 wt.-%), followed by TRGO (<1 wt.-%) and CB (<2 wt.-%). With the formation of a particle network, the flow behaviour of composites with CB, CNT and TRGO is affected, i.e., a flow limit occurs and the melt viscosity increases. The degree of influence of the carbon nanofillers on the rheological properties of PBT composites follows the same order as for electrical conductivity. Electrical and rheological results suggest an influence attributed to the particle dispersion, which is proposed to follow the order of EG<< CB<TRGO<CNT.
Nanocomposites based on poly(ʟ-lactide) (PLA) and organically modified MgAl Layered Double Hydroxides (MgAl-LDH) were prepared by melt blending and investigated by a combination of Differential Scanning Calorimetry (DSC), Small- and Wide-Angle X-ray Scattering (SAXS, WAXS), and dielectric spectroscopy (BDS). Scanning microfocus SAXS investigations show that the MgAl-LDH is homogeneously distributed in the matrix as stacks of 6 layers and/or partly exfoliated layers. DSC and WAXS show that the degree of crystallinity decreases linearly with the content of LDH. The extrapolation of the dependencies (DSC and WAXS) to zero estimates a limiting concentration of LDH CCri of ca. 21 wt% where the crystallization of PLA is completely suppressed by the nanofiller. The dielectric behavior of neat PLA show two relaxation regions, a β-relaxation at low temperatures related to localized fluctuations and the α-relaxation at higher temperatures due to the dynamic glass transition. The dielectric spectra of the nanocomposites show several additional relaxation processes compared to neat PLA which are discussed in detail. For the nanocomposites around 260 K (ƒ = 1 kHz) an additional process is observed which intensity increases with increasing concentration of LDH. This process is mainly attributed to the exchanged dodecylbenzene sulfonate (SDBS) molecules which are adsorbed at the LDH layers and form a mixed phase with the polymer close to the layers and stacks. An analysis of this process provides information about the molecular dynamics in the interfacial region between the LDH layers and the PLA matrix which reveal glassy dynamics in this region. In the temperature range around 310 K (ƒ = 1 kHz) a further process is observed. Its relaxation rate has an unusual saddle-like temperature dependence. It was assigned to rotational fluctuations of water molecules in a nanoporous environment provided by the LDH filler. Above the glass transition temperature a further process is observed at temperatures above. It is related to Maxwell/Wagner/Sillars polarization due to the blocking of charges at the nanofiller.
Polymer based nanocomposites by melt blending of synthesized ZnAl-Layered Double Hydroxide (ZnAl-LDH) and polypropylene (PP) were investigated by temperature modulated differential scanning calorimetry (TMDSC). The LDH was organically modified by using a surfactant, sodium dodecylbenzene sulfonate (SDBS) to increase the interlayer spacing of the LDH, so that polymer segments can intercalate the inter layer galleries. The glass transition temperature (Tg) and the thermal relaxation strength (Δcp) were determined. The Tg remains constant for concentration till 12 wt% of LDH and a slight reduction of 3 K might be observed for 16 wt% LDH but within the experimental error. The thermal relaxation strength decreases indicating reduction in the amount of mobile polymer segments from amorphous fraction. This finding is supported by the increase in the rigid amorphous fraction (RAF) which is attributed to the polymer molecules which are in close proximity to the crystals and the LDH sheets, as they hinder their mobility. This is analyzed in detail and related to the dielectric relaxation spectroscopy (BDS) results.
Organically modified ZnAl Layered Double Hydroxides (ZnAl-LDH) was synthesized and melt blended with polyethylene to obtain nanocomposites. The resulting morphology was investigated by a combination of Differential Scanning Calorimetry (DSC), Small and Wide-angle X-ray scattering (SAXS and WAXS) and dielectric relaxation spectroscopy (DRS). The arrangement (intercalation) of polyethylene chains between LDH stacks was investigated employing SAXS. The homogeneity of the nanocomposites and average number of stack size (4–6 layers) were determined using scanning microfocus SAXS (BESSY II). DSC and WAXS results show that the degree of crystallinity decreases linearly with the increasing content of LDH. The extrapolation of this dependence to zero estimates a limiting concentration of ca. 45% LDH where the crystallization of PE is completely suppressed by the nanofiller. The dielectric spectra of the nanocomposites show several relaxation processes which are discussed in detail. The intensity of the dynamic glass transition (β-relaxation) increases with the concentration of LDH. This is attributed to the increasing concentration of the exchanged anion sodium dodecylbenzene sulfonate (SDBS) which is adsorbed at the LDH layers. Therefore, a detailed analysis of the β-relaxation provides information about the structure and the molecular dynamics in the interfacial region between the LDH layers and the polyethylene matrix which is otherwise dielectrically invisible (low dipole moment).
Nanocomposites based on polypropylene (PP) and organically modified ZnAl layered double hydroxides (ZnAl-LDH) were prepared by melt blending and investigated by a combination of differential scanning calorimetry (DSC), small- and wide-angle X-ray scattering (SAXS and WAXS), and dielectric relaxation spectroscopy (DRS). An average number of stack size of LDH layers is calculated by analyzing the SAXS data which is close to that of pure organically modified ZnAl-LDH. Scanning microfocus SAXS investigations show that the ZnAl-LDH is homogeneously distributed in the PP matrix as stacks of 4–5 layers with an intercalated morphology. DSC and WAXS results show that the degree of crystallinity decreases linearly with the increasing content of LDH. The extrapolation of this dependence to zero estimates a limiting concentration of ca. 40% LDH where the crystallization of PP is completely suppressed by the nanofiller. The dielectric spectra of the nanocomposites show several relaxation processes which are discussed in detail. The intensity of the dynamic glass transition (β-relaxation) increases with the concentration of LDH. This is attributed to the increasing concentration of the exchanged anion dodecylbenzenesulfonate (SDBS) which is adsorbed at the LDH layers. Therefore, a detailed analysis of the β-relaxation provides information about the structure and the molecular dynamics in the interfacial region between the LDH layers and the polypropylene matrix which is otherwise dielectrically invisible (low dipole moment). As a main result, it is found that the glass transition temperature in this interfacial region is by 30 K lower than that of pure polypropylene. This is accompanied by a drastic change of the fragility parameter deduced from the relaxation map.