Filtern
Erscheinungsjahr
- 2023 (264) (entfernen)
Dokumenttyp
- Vortrag (147)
- Zeitschriftenartikel (55)
- Beitrag zu einem Tagungsband (42)
- Posterpräsentation (11)
- Forschungsdatensatz (3)
- Dissertation (2)
- Forschungsbericht (2)
- Tagungsband (Herausgeberschaft für den kompletten Band) (1)
- Sonstiges (1)
Schlagworte
- Additive manufacturing (23)
- Laser beam welding (21)
- Additive Fertigung (20)
- Hydrogen (15)
- Wasserstoff (15)
- Additive Manufacturing (14)
- Hochfester Stahl (14)
- Ultraschallunterstütztes Fräsen (14)
- Eigenspannungen (12)
- Oberflächenintegrität (12)
Organisationseinheit der BAM
- 9 Komponentensicherheit (264) (entfernen)
Paper des Monats
- ja (6)
Eingeladener Vortrag
- nein (147)
The main solidification parameters, namely the crystal axis, the growth rate, and the cross-sectional area of the columnar crystal control the primary microstructure and thus the final weld seam properties.
Limited understanding of solidification parameters due to complexities in experimental and theoretical weld pool boundary determination and
its mathematical description.
Application of local Lamé curves for efficient weld pool boundary reconstruction Derivation of general analytical solutions for the main solidification parameters of a two-dimensional columnar crystal growth during laser beam welding of thin steel sheets.
The Lamé curves approximation technique was successfully applied for the reconstruction of the rear part of the two-dimensional steady-state weld pool boundary. General analytical expressions for the main solidification parameters, namely the crystal axis, the growth rate and the cross-sectional area of the crystal were derived.
The derived expressions and herewith obtained results were verified and validated by comparing them to known theoretical solutions and experimental measurements. Dimensionless analysis of the influence of the size and shape of the rear weld pool boundary on the solidification parameters was provided.
The derived general solutions and the analysis provided allow for critical welding parameters to be estimated and adapted accordingly to improve the welding process.
A technique for calculating the main solidification parameters for a two-dimensional columnar crystal growth during complete penetration laser beam welding of thin steel sheets was developed. Given that the weld pool interface is described by Lamé curves (superellipses) within the horizontal plane of growth, general analytical solutions were derived for the geometry of the crystal axis and the corresponding growth rate and cross-sectional area of the crystal. A dimensionless analysis was performed to provide insights on the dependence of the solidification parameters on the shape and dimensions of the rear part of the weld pool boundary. The derived solutions were applied for the case of complete penetration laser beam keyhole welding of 2 mm thick 316L austenitic chromium-nickel steel sheets. It was shown that the reconstruction of the weld pool boundary with Lamé curves provides higher accuracy and flexibility compared to results obtained with elliptical functions. The validity of the proposed technique and the derived analytical solutions was backed up by a comparison of the obtained solutions to known analytical solutions and experimentally determined shapes and sizes of the crystals on the top surface of the sheet. The dimensions of the calculated crystal axis correlated well with the experimentally obtained results.
A three-dimensional numerical model was developed to accurately predict the steady-state weld pool shape in full penetration laser beam welding. The model accounts for the coupling between the heat transfer and the fluid dynamics by considering the effects of solid/liquid phase transition, thermo-capillary convection, natural convection, and phase-specific and temperature-dependent material properties up to the evaporation temperature. A fixed right circular cone was utilized as a keyhole geometry to consider the heat absorbed from the laser beam. The model was used to analyze the influence of the thermodynamic activity of solutes and turbulence on the weld pool shape. A mesh sensitivity analysis was performed on a hybrid mesh combining hexahedral and tetrahedral elements. For the case of full penetration laser beam welding of 8 mm thick unalloyed steel sheets, the dependence of the weld pool shape on the surface-active element sulfur was found to be negligible. The analysis of the results showed that a laminar formulation is sufficient for accurately predicting the weld pool shape since the turbulence has a minor impact on the flow dynamics in the weld pool. The validity of the numerical results was backed up by experimental measurements and observations, including weld pool length, local temperature history, and a range of metallographic crosssections.
Numerical study on the formation of a bulging region in partial penetration laser beam welding
(2023)
A transient three-dimensional thermo-fluid dynamics numerical model was developed to study the formation of a bulging region in partial penetration laser beam welding. The model accounts for the coupling between the fluid flow, the heat transfer, and the keyhole dynamics by considering the effects of multiple reflections and Fresnel absorption of the laser beam in the keyhole, the phase transitions during melting and evaporating, the thermo-capillary convection, the natural convection, and the phase-specific and temperature-dependent material properties up to the evaporation temperature. The validity of the model was backed up by experimentally obtained data, including the drilling time, the weld pool length, the local temperature history outside the weld pool, the process efficiency, and a range of metallographic crosssections.
The model was applied for the cases of partial penetration laser beam welding of 8 mm and 12 mm thick unalloyed steel sheets. The obtained experimental and numerical results reveal that the bulging region forms transiently depending on the penetration depth of the weld, showing a tendency to transition from a slight bulging to a fully developed bulging region between penetration depths of 6 mm and 9 mm, respectively.
The performance of titanium alloy (Ti6Al4V) surfaces was investigated in lubricated reciprocating sliding tribological tests (RSTT). Special emphasis was laid on the effect of surface nanostructures in area of contact on the respective friction and wear behaviour. These so-called laser-induced periodic surface structures (LIPSS, ripples) were produced on the titanium alloy surface upon scan processing in air by an ultrashort pulsed femtosecond (fs) laser. As lubricant served two types of base oils, a pure polyalcylene-glycol, and an SAE 0W30 oil containing only antioxidants and temperature stabilizers. Tribological tests were carried out on polished as well as LIPSS covered areas using both types of base oil. A test metrics was established, combining the additive 2-ethylhexyl-zincdithiophosphate (ZDDP) or the ionic liquid [P6,6,6,14] [DEHP] (98% purity) with the respective base oils. The test metrics also considered the orientation of motion with respect to the orientation of the structures formed on the surface. Results are presented which show that the interplay between LIPSS and the local chemistry formed by the respective additives is beneficial for the tribological behaviour of the titanium alloy. Certain combinations of base oil, additive and LIPSS reduced friction and wear significantly in the tribological contact.
The amount of absorbed energy in the keyhole as well as its spatial and temporal distribution is essential to model the laser beam welding process. The recoil pressure, which develops because of the evaporation process induced by the absorbed laser energy at the keyhole wall, is a key determining factor for the macroscopic flow of the molten metal in the weld pool during high-power laser beam welding. Consequently, a realistic implementation of the effect of laser radiation on the weld metal is crucial to obtain reliable and accurate simulation results. In this paper, we discuss manyfold different improvements on the laser-material interaction, namely, the ray tracing method, in the numerical simulation of the laser beam welding process. The first improvement relates to locating the exact reflection points in the ray tracing method using a so-called cosine condition in the determination algorithm for the intersection of reflected rays and the keyhole surface. A second correction refers to the numerical treatment of the Gaussian distribution of the laser beam, whose beam width is defined by a decay of the laser intensity by a factor of 1/e2, thus ignoring around 14% of the total laser beam energy. In the third step, the changes in the laser radiation distribution in the vertical direction were adapted by using different approximations for the converging and the diverging regions of the laser beam, thus mimicking the beam caustic. Finally, a virtual mesh refinement was adopted in the ray tracing routine. The obtained numerical results were validated with experimental measurements.
The amount of absorbed energy in the keyhole as well as its spatial and temporal distribution is essential to model the laser beam welding process. The recoil pressure, which develops because of the evaporation process induced by the absorbed laser energy at the keyhole wall, is a key determining factor for the macroscopic flow of the molten metal in the weld pool during high-power laser beam welding. Consequently, a realistic implementation of the effect of laser radiation on the weld metal is crucial to obtain reliable and accurate simulation results. In this paper, we discuss manyfold different improvements on the laser-material interaction, namely, the ray tracing method, in the numerical simulation of the laser beam welding process. The first improvement relates to locating the exact reflection points in the ray tracing method using a so-called cosine condition in the determination algorithm for the intersection of reflected rays and the keyhole surface. A second correction refers to the numerical treatment of the Gaussian distribution of the laser beam, whose beam width is defined by a decay of the laser intensity by a factor of 1/e2, thus ignoring around 14% of the total laser beam energy. In the third step, the changes in the laser radiation distribution in the vertical direction were adapted by using different approximations for the converging and the diverging regions of the laser beam, thus mimicking the beam caustic. Finally, a virtual mesh refinement was adopted in the ray tracing routine. The obtained numerical results were validated with experimental measurements.
The amount of absorbed energy in the keyhole as well as its spatial and temporal distribution is essential to model the laser beam welding process. The recoil pressure, which develops because of the evaporation process induced by the absorbed laser energy at the keyhole wall, is a key determining factor for the macroscopic flow of the molten metal in the weld pool during high-power laser beam welding. Consequently, a realistic implementation of the effect of the laser radiation on the weld metal is crucial to obtain reliable and accurate simulation results.
In this paper, we discuss manyfold different improvements on the laser-material interaction, namely the ray-tracing method, in the numerical simulation of the laser beam welding process. The first improvement relates to locating the exact reflection points in the ray tracing method using a so-called cosine condition in the determination algorithm for the intersection of the reflected rays and the keyhole surface. A second correction refers to the numerical treatment of the Gaussian distribution of the laser beam, whose beam width is defined by a decay of the laser intensity by a factor of 1/e2 thus ignoring around 14 % of the total laser beam energy. In a third step, the changes in the laser radiation distribution in the vertical direction were adapted by using different approximations for the converging and the diverging regions of the laser beam thus mimicking the beam caustic. Finally, a virtual mesh refinement was adopted in the ray tracing routine. The obtained numerical results were validated with experimental measurements.
A steel pipeline segment of 2.5 m length was subjected to quasi-static four-point bending load in three steps for studying the initial cracking and damage accumulation based on the Acoustic Emission (AE) technique and by the direct current potential drop (DCPD) technique. For the latter, a new post-test analysis method was established.
AE is found more sensitive to crack initiation than DCPD. Formation of mesoscopic and macroscopic cracks as well as their closure and the resulting friction generate weighted peak frequencies below 400 kHz, whereas microscopic cracking produces AE with broad band spectra identifiable by weighted peak frequencies above 400 kHz. Critical states alike the maximum load level and the leak opening were accompanied by peak amplitudes above 85 dBAE. This rather fundamental study provides a data base for possibly developing advanced strategies of detection and alarm systems based on acoustic monitoring of pipelines, or at least, steel structures.
Since there is a continuously growing demand for complex, frequently heavy-sectioned spheroidal graphite cast iron (SGI) castings it is worth paying attention to the chunky graphite (CHG) degeneration which may occur under certain technological circumstances. Although a reference line for preventive actions in terms of general metallurgical and process measures could be drawn to avoid CHG in heavy-sectioned ferritic SGI castings, a broad majority of experts claim the avoidance of CHG in heavy sections cannot yet be rated a hundred percent process safe. A major reason may be seen in the fact that a universal, generally accepted explanation of CHG formation and growth has not yet been established, although several theories have been proposed. Nevertheless, metallurgical aspects are not in the focus of this paper.
This paper is about the current state of methods to detect CHG in SGI on the laboratory and component scales. Capabilities and limits of different metallographic, fractographic and non-destructive computer tomographic methods to recognize and quantify CHG are discussed. With respect to the characteristic fili-gree three-dimensional string-like, multi-branched CHG structure, which is non-isometric and non-dispersed, serious implications on the possibility to quantitatively characterize the amount of CHG must be considered.
In contrary to the metallurgical aspects, the knowledge about the impact of CHG on the materials and com-ponents properties is still surprisingly limited. Therefore, special emphasis of this paper is on the impact of CHG degeneration on the properties of ferritic SGI. Experimental results are reviewed to illustrate the effect of CHG on mechanical strength and ductility properties as well as fracture mechanics properties in terms of crack resistance and fracture toughness.
The present situation is characterized by discussions and uncertainty about the acceptance or rejection of SGI components containing CHG. Addressing this, conclusions from the materials engineering point of view are drawn for quality control, a safe operational strategy in the foundry and component safety.
Since there is a continuously growing demand for complex, frequently heavy-sectioned spheroidal graphite cast iron (SGI) castings it is worth paying attention to the chunky graphite (CHG) degeneration which may occur under certain technological circumstances. Although a reference line for preventive actions in terms of general metallurgical and process measures could be drawn to avoid CHG in heavy-sectioned ferritic SGI castings, a broad majority of experts claim the avoidance of CHG in heavy sections cannot yet be rated a hundred percent process safe. A major reason may be seen in the fact that a universal, generally accepted explanation of CHG formation and growth has not yet been established, although several theories have been proposed. Nevertheless, metallurgical aspects are not in the focus of this paper.
This paper is about the current state of methods to detect CHG in SGI on the laboratory and component scales. Capabilities and limits of different metallographic, fractographic and non-destructive computer tomographic methods to recognize and quantify CHG are discussed. With respect to the characteristic fili-gree three-dimensional string-like, multi-branched CHG structure, which is non-isometric and non-dispersed, serious implications on the possibility to quantitatively characterize the amount of CHG must be considered.
In contrary to the metallurgical aspects, the knowledge about the impact of CHG on the materials and com-ponents properties is still surprisingly limited. Therefore, special emphasis of this paper is on the impact of CHG degeneration on the properties of ferritic SGI. Experimental results are reviewed to illustrate the effect of CHG on mechanical strength and ductility properties as well as fracture mechanics properties in terms of crack resistance and fracture toughness.
The present situation is characterized by discussions and uncertainty about the acceptance or rejection of SGI components containing CHG. Addressing this, conclusions from the materials engineering point of view are drawn for quality control, a safe operational strategy in the foundry and component safety.
Based on state-of-the-art research and regulations, the application of the fracture mechanics master curve (MC) concept to ferritic ductile cast iron (DCI) is being investigated in a recently started German joint research project between BAM Berlin and MPA Stuttgart. This paper outlines the research approach and the planned investigations and provides first results.
According to the IAEA guidelines SSG 26, the safety assessment of DCI containers for transport as well as interim and final storage of radioactive materials is based on the fracture mechanics criterion of general crack initiation exclusion. Within this context, the focus of the current research project is on the further development of brittle fracture safety assessment methods under dynamic loading conditions. Within fracture mechanics safety assessments for steels in nuclear technology, the probabilistic MC concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. The MC concept allows for an effective statistical consideration of the scatter of the material toughness in the transition regime. Furthermore, the MC can also be used for elevated loading rates as they occur in accident or crash scenarios. However, for DCI, a systematic review of potential modifications to the MC assumptions and procedure according to ASTM E1921 and an associated validation are still lacking. Therefore, a corresponding methodology shall be established to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using samples extracted from a component.
For the experimental program, a DCI material was produced as it is generally used for transport and storage containers. A basic mechanical-technological material characterization consisting of tensile, Charpy, and Pellini tests is planned. A comprehensive fracture mechanics test program was compiled covering dynamic testing of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25, and SE(B)140 specimens. Moreover, numerical analyses of different specimen geometries and test setups are planned to investigate the influences of stress triaxiality and loading rate. Throughout the experimental program, the microstructure-property relationship will be investigated based on quantitative metallographic and fractographic analyses. Finally, different MC assessment strategies will be considered, and modifications will be made if necessary.
Was Sie schon immer über Chunky-Graphit wissen w(s)ollten, aber bisher nicht zu fragen wagten
(2023)
Duktile Gusseisenwerkstoffe mit Kugelgraphit (GJS) haben ein erhebliches technisches Potenzial und sind von wirtschaftlicher Bedeutung. Nicht zuletzt daher ist es ökonomisch sinnvoll, gesellschaftlich nachhaltig und wissenschaftlich interessant, ihren Herstellungsprozess zu optimieren. Eine maßgebliche Rolle kommt hierbei der Vermeidung von Qualitätsabweichungen in Form von Gefügefehlern zu. Dieser Beitrag befasst sich mit der – leider vielfach nicht richtig oder zu wenig verstandenen, aber insbesondere bei kostenintensi-ven dickwandigen Gussteilen relevanten - Graphitentartung Chunky-Graphit (CG).
Die metallurgischen Ursachen von CG werden noch immer kontrovers diskutiert. Eine allgemein akzeptierte Theorie zur Bildung und dem Wachstumsmechanismus von CG existiert nicht, in der Gießereipraxis wird gleichwohl eine Fülle spezifischer technologischer Abhilfemaßnahmen praktiziert [1].
Der Schwerpunkt dieses Beitrages liegt jedoch nicht auf der metallurgischen Seite, sondern auf der Beschrei-bung der spezifischen Morphologie von CG (Bild 1), dessen Detektion im Werkstoff bzw. Bauteil sowie den Auswirkungen von CG auf die Werkstoffeigenschaften. Detailliert werden Möglichkeiten und Grenzen zer-störungsfreier und zerstörender Untersuchungsverfahren zur Identifikation und Quantifizierung von CG aufgezeigt. Ausgehend von der charakteristischen Morphologie von CG wird dessen Einfluss auf das Ver-formungs- und Bruchverhalten von GJS behandelt. Beispielhaft werden dabei die Eigenschaften Festigkeit, Verformbarkeit, das Risswachstumsverhalten und die Bruchzähigkeit diskutiert und Schlussfolgerungen für die Bewertung von mit CG behafteten GJS-Bauteilen abgeleitet.
Based on state-of-the-art research and regulations, the application of the fracture mechanics master curve (MC) concept to ferritic ductile cast iron (DCI) is being investigated in a recently started German joint research project between BAM Berlin and MPA Stuttgart. This paper outlines the research approach and the planned investigations and provides first results.
According to the IAEA guidelines SSG 26, the safety assessment of DCI containers for transport as well as interim and final storage of radioactive materials is based on the fracture mechanics criterion of general crack initiation exclusion. Within this context, the focus of the current research project is on the further development of brittle fracture safety assessment methods under dynamic loading conditions. Within fracture mechanics safety assessments for steels in nuclear technology, the probabilistic MC concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. The MC concept allows for an effective statistical consideration of the scatter of the material toughness in the transition regime. Furthermore, the MC can also be used for elevated loading rates as they occur in accident or crash scenarios. However, for DCI, a systematic review of potential modifications to the MC assumptions and procedure according to ASTM E1921 and an associated validation are still lacking. Therefore, a corresponding methodology shall be established to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using samples extracted from a component.
For the experimental program, a DCI material was produced as it is generally used for transport and storage containers. A basic mechanical-technological material characterization consisting of tensile, Charpy, and Pellini tests is planned. A comprehensive fracture mechanics test program was compiled covering dynamic testing of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25, and SE(B)140 specimens. Moreover, numerical analyses of different specimen geometries and test setups are planned to investigate the influences of stress triaxiality and loading rate. Throughout the experimental program, the microstructure-property relationship will be investigated based on quantitative metallographic and fractographic analyses. Finally, different MC assessment strategies will be considered, and modifications will be made if necessary.
The role of defects in the fatigue strength of Wire Arc Additively Manufactured (WAAMed) Ti-6Al-4V is analysed by means of the IBESS model, a fracture mechanics short crack growth approach based on the cyclic R-curve. Pores and crack-like defects are analysed. Estimations of the role of pore shape and size agree well with published fatigue data of WAAM Ti-6Al-4V with pores. The model is also used to explain the effect of fabrication defects on the scatter of experimental data. This demonstrates that short crack growth models represent a suitable engineering tool for the fatigue assessment of defective AM materials.
Komponenten von Fahrrädern werden im Betrieb vorwiegend schwingend beansprucht. Typische Werkstoffe sind Stahl, Aluminiumlegierungen, Messing, CFK und thermoplastische Kunststoffe. Da es sich, unabhängig von der Preiskategorie, um konstruktiven Leichtbau handelt, werden einige Bauteile betriebsfest mehr oder weniger weit oberhalb der Dauerfestigkeit ausgelegt. Die im normalen Betrieb auftretenden Schäden sind daher weit überwiegend Schwingbrüche. Andere Schadensmechanismen wie z.B. Korrosion spielen quantitativ eine untergeordnete Rolle. Schwingbrüche treten nach einer Periode unbemerkten Risswachstums oft ohne Vorwarnung und ohne makroskopische Verformung auf. Im Falle von sicherheitsrelevanten Komponenten wie Rahmen, Gabeln, Lenkern, Sattelstützen, Kurbelarmen oder Pedalen kann dies zu erheblichen Personenschäden führen, die den Wert des ursächlichen Bauteilschadens weit überschreiten.
Über einen langjährigen Zeitraum wurden gebrochene Komponenten aus dem Alltag und aus Gerichtsverfahren analysiert. Das Hauptaugenmerk lag hierbei auf der fraktographischen Analyse, teilweise wurden die zu Grunde liegenden Schadensursachen ermittelt. Einflussfaktoren sind beispielsweise konstruktive Kerben an ungünstigen Stellen, aber auch Werkstoffwahl und Fertigungsqualität spielen eine Rolle. In den meisten Fällen wurde jedoch die konstruktive Lebensdauer überschritten. Diese wird praktisch nie mitgeteilt, und eine wiederkehrende Prüfung sicherheitsrelevanter Bauteile findet nicht statt.
Im Sinne der Vermeidung von Schäden und Unfällen könnte darauf hingewirkt werden, für sicherheitsrelevante Komponenten Lebensdauern besser abzuschätzen und von der Laufleistung abhängige Sichtprüfungen zu empfehlen.
This work explores the feasibility of producing bead-on-plate welds of a CrCoNi medium entropy alloy and a CrMnFeCoNi high entropy alloy using electron beam welding. The alloys were welded in two states: one in an as-cold-rolled condition and the other in an annealed condition. In addition, the materials are welded with two different parameters. The FCC microstructure of the welds is investigated using scanning electron microscopy assisted by energy-dispersive X-ray spectroscopy and electron-backscattered diffraction. The impact of the weld on the microstructure is discussed. The heat-affected zone is negligible for the annealed condition of both medium and high entropy alloys since there is no driving force for recrystallisation and the exposure time to high temperature is insufficient for grain coarsening. The texture formed in the fusion zone is also discussed and compared to the texture in the base metal and the heat-affected zone. Although the grain growth along the (100) crystallographic direction is preferential in all cases, the crystallographic texture type differs from each weld. Higher hardness values are measured in the medium entropy alloy’s base metal and fusion zone than in the high entropy alloy.
This work investigates the microstructure formed in friction stir welds of FCC alloys, focused on two multiprincipal alloys: a CoCrFeMnNi high-entropy alloy (HEA) and a CoCrNi medium-entropy alloy (MEA). A commercial stainless steel AISI 304 is used for comparison. The largest nugget was formed in the MEA, while the smallest was formed in the HEA. Grain refinement occurs in the stirred zone in all welds. Discontinuous dynamic recrystallisation is the predominant restoration mechanism during friction stir welding of the three investigated alloys. A sharp decrement in the Σ3 boundary fraction occurs in the stirred zone of the AISI 304 and HEA welds, while comparable values with the base metal are found for the MEA weld. The peak in the maximum index of crystallographic texture is observed on the advancing side of the stirred zone of the AISI 304 weld. A strong <001> θ-fibre texture is formed in the advancing side of the nugget in the AISI 304 from a well-established {123} <634> S-type texture in the base metal. Multiple crystallographic texture components without specific fibres are identified in most regions of the welds, indicating the complex shear path history during friction stir welding.
Die Wasserstoffinfrastruktur ist eine zentraler Bestandteil der erfolgreichen Umsetzung der wasserstoffbasierten Energiewende. Dabei bilden Ferngasleitungen quasi das "Rückgrat" der Transportinfrastruktur großer Gasmengen. Dabei müssen unter Umständen Reparaturen an den Pipelines durchgeführt werden. Dabei ist in der Erdgasinfrastruktur das Schweißen an in Betrieb befindlichen (d.h. von Gas durchflossenen) Pipelines Stand der Technik. Es ist jedoch vollkommen offen, inwieweit diese Technik auf die reine Wasserstoffpipelines übertragbar sind. Hierzu leistet das Projekt H2SuD wichtige Beiträge zur Aufklärung des Einfluss eines Reparaturschweißprozesses auf die Wasserstoffaufnahme und Degradation im Betrieb befindlicher H2 Gasleitungen.
Creep-resistant steels such as the 13CrMoV9-10, used in the construction of thick-walled pressure vessels, are most commonly submerged arc welded (SAW). These steels can develop stress relief cracks (SRC) if the mandatory post weld heat treatment (PWHT) is performed improperly. Current PWHT parameters, such as heating rate and holding time at a specific holding temperature, are based on both empirical experience and conventional free shrinking welding experiments to characterize the SRC-susceptibility of the weld. These cannot adequately depict the higher residual stresses caused by the structurally induced stiffness of the surrounding construction. This study discusses the development of a repeatable, precise, and time-efficient methodology to study the effects of different stress levels and heating rates on the SRC susceptibility of the coarse grain heat-affected zone (CGHAZ). For that purpose, samples were thermically treated to simulate a coarse grain heat-affected zone (CGHAZ) and subsequently exposed to representative levels of stress during the heating phase of a PWHT. The recorded stress and heating rate–dependent strains were mathematically analyzed via curve tracing/calculus to identify interdependent effects. This procedure facilitates the measurement of material characteristics such as carbide growth on grain boundaries at the µm-scale via an integrated value over the entire sample volume. The first and second derivatives show a slight, precipitate-dependent, increase in hardness of the sample, depending on the heating rate and applied stress. This new methodology generates an improved assessment of the SRC susceptibility of SAW microstructures of creep-resistant CrMoV steels.
Multi-Principal-Element or High-Entropy Alloys (MPEAs/HEAs) have gained increasing interest in the past two decades largely due to their outstanding properties such as superior mechanical strength and corrosion resistance. However, research studies on their processability are still scarce. This work assesses the effect of different machining conditions on the machinability of these novel alloys, with the objective of advancing the introduction of MPEA systems into industrial applications. The present study focuses on the experimental analysis of finish-milling conditions and their effects on the milling process and resulting surface finish of CoCrFeNi, Al0.3CoCrFeNi and Al0.3CoCrFeNiMo0.2 alloys fabricated via Spark Plasma Sintering. Ball-nose-end milling experiments have been carried out various milling parameters such as cutting speed, feed per cutting edge, and ultrasonic assistance. In situ measurements of cutting forces and temperature on the tool edge were performed during the experiments, and surface finish and tool wear were analyzed afterwards. The results exhibited decreasing cutting forces by means of low feed per cutting edge and reduced process temperatures at low cutting speed, with the use of ultrasonic-assisted milling. It was shown that the machinability of these modern alloys through conventional, as well as modern machining methods such as ultrasonic-assisted milling, is viable, and common theories in machining can be transferred to these novel MPEAs.
State-of-the-art laser powder bed fusion (PBF-LB/M) machines allow pre-heating of the substrate plate to reduce stress and improve part quality. However, two major issues have been shown in the past: First, with increasing build height the apparent pre-heat temperature at the surface can deviate drastically from the nominal pre-heat temperature in the substrate plate. Second, even within a single layer the local surface pre-heat temperature can show large gradients due to thermal bottlenecks in the part geometry underneath the top surface. Both lead to unwanted changes in microstructure or defects in the final parts. In this study, a first attempt is taken to show the feasibility of pre-heating the top surface with the onboard laser beam to overcome the mentioned issues. A single layer of a group of three parts built from IN718 to a height of 33.5 mm is pre-heated in a commercially available PBF-LB/M machine to an average steady state surface temperature of 200 °C using the onboard laser beam. The parts are continuously heated, omitting powder deposition and melting step. Temperatures are measured by thermocouples underneath the surface. The experiments are supported by a thermal finite element (FE) model that predicts the temperature field in the parts. When heating the parts uniformly with the laser beam, differences in surface temperatures as large as 170 K are observed. To overcome this inhomogeneity, the heat flux supplied by the laser beam is modulated. An optimized, spatial heat flow distribution is provided by the thermal FE model and translated into a scan pattern that reproduces the optimized heat distribution on the PBF-LB/M machine by locally modulating hatch distance and scan velocity. This successfully reduces the differences in surface temperature to 20 K. Thermographic imaging shows that a homogeneous surface temperature can be achieved despite the localized heat input by the beam. The potential for industrial application of the optimized laser-heating technique is discussed.
Effect of Tensile Loading and Temperature on the Hydrogen Solubility of Steels at High Gas Pressure
(2023)
The hydrogen solubility in ferritic and martensitic steels is affected by hydrostatic stress, pressure, and temperature. In general, compressive stresses decrease but tensile stresses increase the hydrogen solubility. This important aspect must be considered when qualifying materials for high‐pressure hydrogen applications (e.g., for pipelines or tanks) by using autoclave systems. In this work, a pressure equivalent for compensating the effect of compressive stresses on the hydrogen solubility inside of closed autoclaves is proposed to achieve solubilities that are equivalent to those in pipelines and tanks subjected to tensile stresses. Moreover, it is shown that the temperature effect becomes critical at low temperatures (e.g., under cryogenic conditions for storing liquid hydrogen). Trapping of hydrogen in the microstructure can increase the hydrogen solubility with decreasing temperature, having a solubility minimum at about room temperature. To demonstrate this effect, the generalized law of the hydrogen solubility is parameterized for different steels using measured contents of gaseous hydrogen. The constant parameter sets are verified and critically discussed with respect to the high‐pressure hydrogen experiments.
Fracture mechanics-based methods can be applied to the fatigue assessment of mechanical components containing defects or cracks subjected to cyclic loading. The knowledge of the crack growth behavior for short and long cracks enables the determination of both finite and infinite life regimes. Nevertheless, a first problem arises from the empirical determination of the fatigue data, which vary according to the test conditions, e.g., the test method, frequency and the stress ratio R. This is due to crack closure and further environmental phenomena affecting crack propagation behavior. A second issue regards the lack of standard experimental procedures for the determination of the fatigue crack propagation threshold ΔKth dependency on the crack size. This is problematic, since ΔKth increases with the build-up of the closure effects in the short crack regime and its inaccurate experimental determination leads to large deviations in the assessment and, even more critical, to non-conservative predictions. Aiming at providing more reliable and safer assessment procedures, the present work proposes a method based on effective crack growth data obtained at high stress ratios (R ≈ 0.8). A short-crack model based on the cyclic R-curve and CPLR data is employed for describing the development of the closure effects. The predictions are compared to established methods and validated by experimental tests.
Die Anwendung bruchmechanischer Methoden zur schadenstoleranten Bauteilauslegung ist für zyklische Lasten im Bereich der Paris-Geraden Stand der Technik. Technisch relevant sind jedoch häufig geringere Lasten im Schwellenwertbereich der d𝑎/d𝑁-Δ𝐾-Kurve. Aufgrund des großen Einflusses von Rissschließeffekten ist dessen Bestimmung jedoch nicht nur aufwändig, sondern auch potenziell fehlerbehaftet. Die Bauteilauslegung erfolgt zweckmäßigerweise auf der Basis effektiver, d. h. rissschließkorrigierter Rissfortschrittsdaten. Von großer Bedeutung ist auch der intrinsische Schwellenwert, unterhalb dessen keine Risserweiterung mehr eintritt. In diesem Forschungsprojekt erfolgte eine Untersuchung des Einflusses verschiedener Prüfverfahren und Umgebungsbedingungen auf die Ermittlung des Schwellenwerts gegen Ermüdungsrissausbreitung Δ𝐾th. Es wurden statistisch abgesicherte Empfehlungen zur experimentellen Ermittlung des intrinsischen Schwellenwerts Δ𝐾th,eff abgeleitet. Dieser dient auch als Eingangsparameter einer weiterentwickelten Prozedur zur Bauteilauslegung auf der Basis bei einem Lastverhältnis von 𝑅 ≈ 0,8 ermittelter, effektiver, Rissfortschrittsdaten. Es zeigte sich, dass die bei einem Lastverhältnis von 𝑅 ≈ 0,8 in Laborluft bei höherer Prüffrequenzen (≥90 Hz) ermittelten Schwellenwerte eine konservative Abschätzung des intrinsischen Schwellenwerts erlaubten. Bei Lastverhältnissen 𝑅 ≪ 0,8 wurde ein teilweise stark ausgeprägter Einfluss extrinsischer Effekte auf das Rissfortschrittsverhalten festgestellt. Eine Untersuchung der Bruchflächen ergab Oxidschichtdicken in der Größenordnung mehrerer hundert Nanometer. Bei Reduktion der Prüffrequenz auf ≈55 Hz und Prüfung in feuchter Luft (60 % r.F. und 80 % r.F.) konnte auch bei 𝑅 = 0,8 Rissschließen beobachtet werden. Die weiterentwickelte Prozedur zur Bauteilauslegung auf Basis effektiver Rissfortschrittsdaten lieferte aber stets konservative Ergebnisse in einem tolerierbaren Fehlerbereich und ist deshalb zur Anwendung geeignet. Die im Projekt gewonnenen Erkenntnisse tragen zu einer robusten Bauteilauslegung auf bruchmechanischer Basis bei. Der stark reduzierte Versuchsumfang bei Nutzung effektiver Rissfortschrittsdaten gegenüber der Ermittlung von spannungsverhältnisabhängigen Rissfortschrittskurven beschleunigt und vereinfacht die Bauteilauslegung auf Basis bruchmechanischer Methoden.
Alloy 36 (1.3912), also known as “Invar,” is an alloy with 36% nickel. The alloy has a remarkably low thermal expansion coefficient in certain temperature ranges. This peculiarity is called the invar effect, which was discovered in 1896 by the Swiss physicist Charles Édouard Guillaume. Therefore, it is used in applications in which dimensional stability is critical, such as molding tools for composite materials in aerospace, automotive applications, or liquified natural gas (LNG) cargo tanks. Moreover, increasingly complex structures and the optimization of resource efficiency also require additive manufacturing steps for the production or repair of components. Additively manufactured components have a heterogeneous microstructure and anisotropic mechanical properties. In addition, the manufactured components require subsequent machining surface finishing, like finish milling, to achieve their final contour. Nickel iron alloys are difficult to machine. Additionally, inhomogeneous microstructure may lead to unstable cutting forces and conditions. In part I of this investigation, the initial alloy 36 is modified with the elements Ti, Zr, and Hf up to a maximum of 0.33 wt.-%. The influence of the modification elements on the microstructure as well as on the hardness of the AM components is examined. Furthermore, one modification is applied to metal arc welding process and investigated. Part II focuses on the effect of the alloy modifications on machinability as well as on the surface integrity of plasma-transferred-arc-welded (PTA) and finish milled invar components.
The application of anti-corrosion coated, high-strength steels in the automotive industry has increased in recent years. In combination with various zinc-based surface coatings, liquid metal embrittlement cracking can be observed in some of these materials. A high-quality, crack-free spot-welded joint is essential to realize the lightweight potential of the materials. In this work, the LME susceptibility of different coatings, which will be determined by the crack length and the occurrence rate, will be investigated using a welding under external load setup. The uncoated specimens did not show any LME. EG, GI and GA showed significantly less LME than ZM coatings. The latter coatings showed much larger crack lengths than the EG, GI and GA coatings. Furthermore, two mechanisms regarding the LME occurrence rate were observed: the occurrence of LME in zinc–magnesium coatings was theorized to be driven by the material properties of the coatings, whereas the occurrence of LME at EG, GI and GA samples was forced mainly by the application of the external tensile load.
In the experimental setup of this work, the materials were exposed to unusually high mechanical loads (up to 80% of their yield strength) to evoke LME cracks.
Eine typische Automobilkarosserie kann bis zu 5000 Widerstandspunktschweißverbindungen aufweisen, welche hohen Qualitätsanforderungen genügen müssen. Daher ist eine durchgehende Prozessüberwachung unerlässlich. Die Transformation zur E-Mobilität in der Automobilindustrie und die damit einhergehende Reichweitenproblematik treiben die Entwicklung und Einführung neuer hochfester Stähle an. Dies resultiert in einem gesteigerten Fertigungsaufwand hinsichtlich einer stabilen Prozess-führung in der Fügetechnik. Um diesen Anstieg an Komplexität zu bewältigen, sind die Methoden der künstlichen Intelligenz ein geeignetes Mittel. Mit ihnen kann, durch Auswertung der Prozessparameter und -signale, die individuelle Schweißpunktqualität sichergesellt werden. Die Vorhersagegenauigkeit von neuen Daten, also das extrapolieren, stellt für die meisten Algorithmen eine große Herausforderung dar.
In dieser Arbeit wird ein künstliches neuronales Netz zur Vorhersage des Punktdurchmessers von Widerstandspunktschweißungen anhand von Prozessparametern implementiert. Die Vorhersagegenauigkeit und Extrapolationsfähigkeit des Modells wird durch die Auswertung des dynamischen Widerstandssignals verbessert.
Um die Extrapolationsfähigkeit zu untersuchen, wird die Vorhersagegenauigkeit des Modells mit Daten getestet, die sich in Bezug auf den Werkstoff und der Beschichtungszusammensetzung deutlich von den Trainingsdaten unterscheiden. Dazu wurden mehrere Schweißexperimente mit Werkstoffen verschiedener Hersteller durchgeführt und nur ein Teil der Daten in das Training einbezogen. Die Ergebnisse dieser Arbeit verdeutlichen den positiven Einfluss der Prozesssignale auf die Robustheit des Modells und die Skalierbarkeit der Algorithmen
künstlicher neuronaler Netze auf Daten außerhalb des Trainingsraums.
Das DVS-Vorhaben 01.3211 „Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ ist ein Kooperationsprojekt der Bundesanstalt für Materialforschung und -prüfung (BAM) und dem Institut für Schweißtechnik und Trennende Fertigungsverfahren (ISAF) der Technischen Universität Clausthal. Das Übergeordnete Projektziel ist das Erlangen von Erkenntnissen für eine sichere und wirtschaftliche, kombinierte additive und abtragende Fertigung aus kostenintensiven Werkstoffen hochbelasteter Komponenten insbesondere für KMU. Dabei stehe die beiden Werkstoffe CoCr26Ni9Mo5W (2.4681) und FeNi36 (1.3912) im Fokus. Mittels Modifikation der Schweißzusätze sind homogen und isotrop ausgeprägte Werkstoffeigenschaften und eine Erhöhung der Prozessstabilität und Fertigungsfreiheitsgrade bei der additiven Fertigung erzielbar. Darüber hinaus wird der Einfluss nachfolgender abtragender Bearbeitungsschritte des ultraschallunterstützen und des konventionellen Fräsprozesses untersucht. Die mit dem Forschungsvorhaben verbundenen Nutzen für KMU sind die Stärkung der Innovationsfähigkeit und der Wirtschaftlichkeit sowie die Erhöhung der Wettbewerbsfähigkeit. In AP-3 wurden die Mikrostruktur der MSG-Schweißung der CoCr-Referenzlegierung untersucht. In AP-4 wurden Zerspanversuche an der MSG-Schweißung der CoCr-Referenzlegierung durchgeführt.
In vielen Anwendungen werden aufgrund zunehmender Anforderungen an den Widerstand gegenüber hohen, kombinierten mechanischen, tribologischen, thermischen und korrosiven Beanspruchungen Hochleistungsle¬gierungen eingesetzt. Den vielfach komplexen Bauteilstrukturen, herausfordernden Fertigungseigenschaften und der Erhöhung der Ressourceneffizienz lässt sich heute mit der additiven Fertigung (AM) begegnen, dem oftmals noch unzureichende Kenntnisse über die resultierende Homogenität und Anisotropie der speziellen Gefüge und den damit verbundenen Eigenschaften entgegensteht. Viele Anwendungen benötigen zudem definierte Oberflächen mit hohen Anforderungen an die Oberflächenintegrität, dem durch komplementären Einsatz von additiven und abtragenden Fertigungsschritten Rechnung getragen wird. Hochleistungslegierungen auf der Basis von Nickel oder Kobalt sind infolge der niedrigen Wärmeleitfähigkeit verbunden mit hoher Festigkeit und Zähigkeit äußerst herausfordernd mit Blick auf eine wirtschaftliche Zerspanung mit geometrisch bestimmter Schneide. Ein Vorhaben (IGF-Nr. 20.979 N/DVS-Nr. 1.3211) der BAM und TU Clausthal/ISAF befasst sich mit der Lösung dieser Problemstellung durch gezielte Beeinflussung des Gefüges mittels Modifikation der Schweißzusatzwerkstoffe und den Einsatz des ultraschallunterstützten Fräsens (US), bei gleichzeitiger Sicherstellung der geforderten Eigenschaften der untersuchten Werkstoffe. Es werden die Ergebnisse der Mikrostruktur und der Zerspanbarkeit der Modifikationen der MSG-Schweißung der FeNi36-Referenzlegierung mit 0,4 Gew.-% Zr und der Modifikationen der MSG-Schweißung der CoCr-Referenzlegierung mit 1 Gew.-% Zr sowie Hf vorgestellt. Abschließend werden aus den Ergebnissen Handlungsempfehlungen abgeleitet.
Nickel alloys are cost intensive materials and generally classified as difficult-to-cut material. However, machining of these materials is needed especially in case of alloy 36 (1.3912), which is commonly used in mould construction for the production of fibre-reinforced composites. With regard to repair, modification and manufacturing of such components, additive manufacturing offers significant economic advantages. Nevertheless, subsequent machining steps are needed to achieve the final component contour and defined surface conditions. Dependent on the material and machining process conditions, detrimental tensile residual stresses may be the result on the machined surface, having negative impact on the component performance and safety. In this investigation, machining experiments were carried out on wire arc additive manufactured components made of alloy 36, varying the cutting speed and the feed rate. In addition, the conventional milling process (CM) was compared with a modern, hybrid machining process, the ultrasonic-assisted milling (US). The cutting forces and the surface-near residual stresses were analysed using X-ray diffraction. A significant improvement of the machinability as well as the surface integrity by using the ultrasonic assistance was observed, especially at low cutting speeds. The CM induced mainly tensile residual stresses, the US mainly compressive residual stresses.
Die additive Fertigung (AM) durch schweißtechnische Verfahren eröffnet vielfach ökonomische Vorteile für eine ressour-ceneffiziente Bauteilherstellung. Gerade hinsichtlich der Homogenität und Anisotropie der resultierenden Schweißgefüge und den damit verbundenen Eigenschaften gibt es noch offene Fragestellungen. Die Einstellung der finalen Bauteilgeo-metrie und Oberflächengüte erfordert den komplementären Einsatz abtragender Fertigungsschritte. Hochleistungslegie-rungen auf der Basis von Nickel oder Kobalt sind aufgrund ihrer niedrigen Wärmeleitfähigkeit verbunden mit hoher Festigkeit und Zähigkeit schwer spanbar. Eine gezielte Gefügebeeinflussung mittels Modifikation der AM-Schweißzusatz-werkstoffe und der Einsatz des ultraschallunterstützten Fräsens (US) bietet das Potential insgesamt die Zerspanungssi-tuation zu verbessern. Dieser Lösungsansatz unter Gewährleistung des Erhalts der geforderten Werkstoff- bzw. Bauteileigenschaften ist Untersuchungsgegenstand eines Gemeinschaftsvorhabens (IGF-Nr. 20.979 N/DVS-Nr. 1.3211) der BAM und TU Clausthal/ISAF. Der vorliegende Beitrag stellt Ergebnisse für die beiden untersuchten FeNi- und CoCr-Legierungen sowie wesentliche Zusammenhänge zwischen Legierungsmodifikation, entstehender Gefügemorphologie und Zerspanungseigenschaften der mittels MAG additiv gefertigter Proben vor. Das größte Potential für die Modifikation zeigten Zr und Hf. Die Zulegierung in das Schweißgut erfolgte durch Beschichtung von Massivdrähten sowie durch Her-stellung von Fülldrähten.
Rapidly advancing technologies and progressive digitisation are posing challenges to the established quality infrastructure (QI). In response, the key stakeholders of the German QI established the initiative QI-Digital aimed at developing new solutions for modern quality assurance. One of the central use cases herein is quality assurance for additive manufacturing, in which a fully interlinked additive manufacturing process chain is established. The intention is to collect and process data from each production step, allowing for a comprehensive digital view of the physical material flow. Within this process chain, prototypes of digital QI tools like machine readable standards and digital quality certificates are being demonstrated, tested, and evolved. This is complemented by research on the process level, comprising the evaluation and refinement of methods for in-situ and ex-situ quality assurance, as well as algorithms for registration, reduction, and analysis of process data. This paper presents the status, goals, and vision for the QI-Digital use case additive manufacturing.
Als Beispiel für moderne Produktion ist die additive Fertigung (ugs. „3D-Druck“) bei der Herstellung von hochkomplexen metallischen Bauteilen, bionisch inspiriertem Leichtbau oder Prototypen nicht mehr wegzudenken. Die Qualitätssicherung (QS) von Bauteilen für sicherheitskritische Anwendungen stellt jedoch noch eine Herausforderung dar. Die Additive Fertigung (AM) ist ein vergleichsweise junges und datenintensives Fertigungsverfahren. Daher ist es ideal geeignet, die neuen Werkzeuge einer digitalen Qualitätsinfrastruktur (QI) für die moderne Produktion zu erproben und weiterzuentwickeln.
Die Entwicklung einer digitalen QI ermöglicht die objektive Qualitätssicherung in der Additiven Fertigung und macht die Technologie gerade auch für kleine und mittelständische Unternehmen besser nutzbar. Sie wird vollwertig im Rahmen des Qualitätsanspruchs „Made in Germany“ einsetzbar – gerade auch beim Umbruch in Industriezweigen. Der Vortrag gibt Einblicke in aktuelle Arbeiten und die Ziele des Use Case Additive Fertigung.
Rapidly advancing technologies and progressive digitisation are posing challenges to the established quality infrastructure (QI). In response, the key stakeholders of the German QI established the initiative QI-Digital aimed at developing new solutions for modern quality assurance. One of the central use cases herein is quality assurance for additive manufacturing, in which a fully interlinked additive manufacturing process chain is established. The intention is to collect and process data from each production step, allowing for a comprehensive digital view of the physical material flow. Within this process chain, prototypes of digital QI tools like machine readable standards and digital quality certificates are being demonstrated, tested, and evolved. This is complemented by research on the process level, comprising the evaluation and refinement of methods for in-situ and ex-situ quality assurance, as well as algorithms for registration, reduction, and analysis of process data. This paper presents the status, goals, and vision for the QI-Digital use case additive manufacturing.
In the course of tomorrow's hydrogen-based energy transition, the construction of the corresponding infrastructure will play a central role. In that context, large diameter long-distance transmission pipelines for hydrogen will be the backbone in the European Union with service pressures from 70 to 90 bar (e.g., depending on national regulations). It is a major goal to rededicate the existing LNG infrastructure despite the necessity of new pipelines. From that point of view repairing of such transmissions pipelines via welding can be necessary. For the LNG infrastructure, it is state of the art that repair welding is conducted at pipelines under service, i.e., the LNG is still flowing as pressurized gas in the steel pipes. The reason is that a shut-down of large diameter pipelines is not so easy or sometimes impossible. In fact, as long no oxygen enters the pipeline, there would be any combustion or (in the worst case) explosion. At the moment, it is entirely open if current repair welding procedures for LNG pipelines can be transferred to pure hydrogen pipelines. In opposite to LNG, hydrogen can be way easier absorbed to the pipeline steels and diffuses through the material. If it accumulates in susceptible regions, i.e., in the welded joint, hydrogen assisted embrittlement could occur. The planned welding procedure requires a so-called preheating and maintenance of the weld joint of up to 300°C for several hours. This temperature is way higher compared to the typical service temperature of max. 40 to 50°C at operational pressures of 100 bar. In accordance to API 941, these low-alloyed pipeline steels are subjected to short-term service loads, which they are not designed for. For that reason, a collaborative project between BAM and DVGW (German Association for Gas and Water professions) was initiated in 2022 to answer the following questions by experiments and numerical simulation of: (1) How many hydrogen is additionally absorbed during the heating of the material to max. 300°C under remaining operational pressures? (2) Is the hydrogen concentration sufficient to reach a critical condition? (3) Which material and weld microstructure is the most susceptible? (4) Is there a significant difference in the repair welding behavior of LNG pipelines that had been already in use for long-term? (5) Which welding parameters and joint dimensions must be ensured for safe repair welding repair of typical pipelines? For that reason, the present study gives an overview on the current practice in repair welding of in-service pipelines, the industrial importance of this topic for the hydrogen-based energy transition and summarizes first results.
In the course of tomorrow's hydrogen-based energy transition, the construction of the corresponding infrastructure will play a central role. The majority of materials used to date are typically welded for component fabrication. In that context, steels are widely applied and can be prone to hydrogen embrittlement. For the evaluation of any hydrogen effect on, for example, the mechanical properties of a welded metallic material, the hydrogen content must be precisely determined. According to ISO 3690, carrier gas hot extraction (CGHE) can be used. In addition to the pure quantification of hydrogen, thermal desorption analysis (TDA) with varied heating rates can be used to determine and evaluate the bonding state at microstructural defects in the material. For both techniques, experimental and measurement influences have to be considered, which have a great effect on the result. For CGHE, for example, ISO 3690 suggests different sample geometries as well as minimum extraction times. The present study summarizes results and experiences of numerous investigations with different sample temperatures and geometries (ISO 3690 type B and cylindrical TDA samples) regarding: the influence of the sample surface (polished/welded), measurement accuracies depending on the sample volume. In particular, a deviating extraction temperature to the set temperature, can significantly falsify the measurement results. Based on the results, methods are shown to quickly reach the desired extraction temperature without having to physically interfere with the measurement equipment. This serves to substantially improve the reliability of hydrogen measurement through increased signal stability and accelerated hydrogen desorption. In general, an independent temperature measurement with dummy samples for the selected heating procedure is advisable to exclude possible unwanted temperature influences already before the measurement. In addition (and way more important), the methods described can be transferred directly to industrial applications.
Residual stresses Analysis in Additively Manufactured alloys using neutron diffraction (L-PBF)
(2023)
An overview of recent progress at BAM of residual stress analysis in additively manufactured, in particular Laser Powder Bed Fusion of metallics materials, using neutron diffraction will be presented. This will cover important topics of the stress-free reference, the diffraction elastic moduli and principal stress determination.
This presentation summarizes the latest research results of the influence of the post weld heat treatment (PWHT) rate and
the global mechanical stress conditions on the stress relief cracking (SRC) susceptibility of low-alloyed and creep-resistant CrMoV steel submerged arc weld joints. It was found that a certain effect of very low heating rates could be confirmed. In addition, the interlinking of SRC susceptibility increasing effects during the PWHT and the ex-post indentification in metallographic cross-section via microstructure characterization is very complex.
Multielement-Legierungen (MPEA - Multiple Principal Element Alloys, gemeinhin auch als Hochentropielegierungen bezeichnet) stellen eine neue Klasse von Werkstoffen dar, die aus mindestens drei Legierungselementen mit jeweils 5 bis 35 Atom-% bestehen. Somit unterscheidet sich diese Legierungskonzept fundamental von konventionellen Werkstoffen wie Stahl oder Nickellegierungen. Hierzu werden die Legierungselemente gezielt ausgewählt und die Mikrostrukturen ein- und zum Teil auch mehrphasig eingestellt. Das Ziel ist dabei, hochinnovative MPEA mit individuell einstellbaren Eigenschaften für die industrielle Anwendung zu identifizieren. Dabei werden insbesondere Zielkonflikte, wie bspw. der Trade-off zwischen Festigkeit und Duktilität bei konventionellen Stählen, überwunden. Insbesondere die hohe mechanische Festigkeit bei höchster Korrosionsbeständigkeit sind bei bestimmten Legierungssystemen von hohem Interesse. Hier kann u.a. die Substitution klassischer hochlegierter Stähle oder von Ni-Basislegierungen perspektivisch erfolgen. In den letzten 20 Jahren lag der Fokus jedoch auf der reinen Materialsynthese. Mit der Zunahme verfügbarer Werkstoffquantitäten, stehen Verarbeitungsfragen, wie werkstoff- und beanspruchungsgerechte Füge- bzw. Schweißverfahren jetzt im Mittelpunkt. Der Schweißeignung von MPEA wurde bis Ende 2022 nur äußert wenig Aufmerksamkeit zuteil. Erfahrungen zu Mischverbindungen (sogenannte DMWs - Dissimilar Metal Welds) fehlen dabei vollständig, sind jedoch essenziell für die Anwendung dieser Werkstoffe in Verbindung mit konventionellen Werkstoffen. Die vorliegende Studie präsentiert erstmals im deutschen Sprachraum, die umfassenden experimentellen Ergebnisse zur Schweißeignung von MPEA-Mischverbindungen und der resultierenden Mikrostruktur. Dazu wurden zwei äquiatomare MPEAs CoCrFeMnNi (Hochentropie-) und CoCrNi (Mittelentropielegierung) mittels WIG- und Rührreibschweißen mit einem konventionellen, hochlegierten und austenitischen Cr-Ni-Stahl (1.4301) gefügt. Die erstmals untersuchten DMWs resultierten dabei in sehr interessanten Mikrostrukturen, mechanisch-technologische Eigenschaften wurden durch instrumentierte Zugversuche gewonnen, die gleichzeitig der Ermittlung der lokalen Verformung im Schweißnahtbereich dienten (durch Verwendung der berührungslosen DIC-Digital Image Correlation-Technik). Dabei zeigt sich für beide Schweißverfahren eine Erweichung in der WEZ der MPEAs sowie eine geringfügig verminderte Zugfestigkeit. Durch die Experimente konnte der prinzipielle Nachweis der Schweißeignung der MPEAs für DMWs mit konventionellen Werkstoffen erbracht werden, die auch eine dementsprechende mechanische Beanspruchbarkeit ermöglichen. Dies ermöglicht zielgerichtete weitere Betrachtungen dieser höchst innovativen Werkstoffe.
Alloy Modification and ultrasonic assisted milling of wear resistant alloys with defined surfaces
(2023)
The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. There is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces.
A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process.
In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on machining for a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA) is investigated. Through metallurgical investigations and in-situ measurement of cutting forces and temperatures at the cutting edge during the milling process as well as the subsequent investigation of tool wear and surface integrity, a detailed analysis and correlation between microstructural properties and machinability is feasible. The findings allow recommendations for standards and processing guidelines, enabling safe and economical production of highly stressed steel components with non-critical, cost-reduced materials.
Alloy Modification and ultrasonic assisted milling of wear resistant alloys with defined surfaces
(2023)
The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. There is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces.
A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process.
In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on machining for a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA) is investigated. Through metallurgical investigations and in-situ measurement of cutting forces and temperatures at the cutting edge during the milling process as well as the subsequent investigation of tool wear and surface integrity, a detailed analysis and correlation between microstructural properties and machinability is feasible. The findings allow recommendations for standards and processing guidelines, enabling safe and economical production of highly stressed steel components with non-critical, cost-reduced materials.
The long-term global goals of achieving almost net zero carbon emissions in the next decades are closely linked to the development of highly efficient components in plant, process and energy engineering, and their sustainable and resource-saving production. Plant components must increasingly withstand tribological loads in addition to high thermal, mechanical, and corrosive stresses. Such combined stresses demand high-performance alloys economically tailored to the application for wear protection and components produced as semi-finished products, via additive manufacturing (AM) or claddings via deposition welding. For instance, the protection of special components made of less cost-intensive materials, e.g., steel in process engineering for screw machines or exhaust gas separation, is feasible applying cost-intensive Ni- or Co-based hard-phase claddings.
Today an increasing number of above-mentioned applications demand precise finishing machining of components to ensure defined compact surfaces with a high integrity and complex contours. Contour milling is standard process for finishing machining of metals. Especially, the desired properties of wear resistant materials (e.g., high strength, hard precipitations) imply significant challenges for milling processes and tools, leading frequently to uneconomic milling conditions due to intolerable high tool wear and surface defects. Inhomogeneous, anisotropic weld structures due to cladding or AM of wear resistance alloys lead to further deteriorations of milling processes due to unstable milling conditions and process forces during chip removal.
To tackle these challenges, already several approaches exist, (1) to enhance machinability of the claddings by alloy modifications to specifically influence solidification and hard phases morphology (precipitation shape, size, distribution) and (2) to achieve significant improvements of the machining situation (e.g., increase of tool life and surfaces integrity) by means of modern hybrid machining processes such as ultrasonic-assisted milling. This contribution shows a comprehensive overview of recent results with these promising approaches for additively welded Ni- CoCr-alloys.
Alloy modification and ultrasonic assisted milling of wear resistant alloys with defined surfaces
(2023)
The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. In addition to increasing demands to replace conventional cobalt alloys with nickel alloys as a result of price and supply risks, there is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces.
A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process.
In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on machining is investigated. The alloy used is a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA). Through metallurgical investigations and in-situ measurement of cutting forces and temperatures at the cutting edge during the milling process as well as the subsequent investigation of tool wear and surface integrity, a detailed analysis and correlation between microstructural properties and machinability is feasible. The findings allow recommendations for standards and processing guidelines, enabling safe and economical production of highly stressed steel components with non-critical, cost-reduced materials.
Die Ziele zur Verringerung der CO2-Emissionen sind eng verknüpft mit der Entwicklung hocheffizienter und wirtschaftlicher Komponenten aus Stahl in der Anlagen-, Verfahrens- und Kraftwerktechnik, die für hohe kombinierte korrosive, tribologische, thermische und mechanische Beanspruchungen auf Anwendungsfall und Stahlwerkstoff abgestimmte Verschleißschutzschichten erfordern. Neben zunehmenden Forderungen infolge des Preis- und Lieferrisikos konventionelle Kobalt- durch Nickellegierungen zu ersetzen, wächst in der Industrie der Bedarf nach definierten Oberflächen hoher Güte bzw. Funktionsflächen für die Schutzschichten. Eine für Bauteile mit komplexer Geometrie erforderliche Fräsbearbeitung ist insbesondere für KMU aufgrund hohen Werkzeugverschleißes oftmals nicht wirtschaftlich realisierbar, jedoch für viele Einsatzfälle dringend notwendig.
In einem Gemeinschaftsvorhaben der BAM und des ISAF der TU Clausthal (Fosta P1550/IGF 21959 N) wird daher untersucht, wie mittels Legierungsmodifikationen der Schweißzusätze für nickelbasierte plasmaauftraggeschweißte Verschleißschutzschichten und durch Einsatz innovativer ultraschallunterstützter Fräsprozesse eine günstigere Zerspanbarkeit erreicht werden kann, ohne das Verschleißschutzpotential zu mindern.
Im vorliegenden Beitrag wird der Einfluss der mittels Legierungsmodifikation eingestellten Gefüge- und Ausscheidungsmorphologie auf die Zerspanung untersucht. Dies erfolgt anhand einer typischerweise für Schneckenmaschinen eingesetzte Verschließschutzlegierung zur Substitution entsprechender CoCr-Legierungen (Stellite), einer NiCrMoSiFeB-Legierung (Handelsname: Colmonoy 56 PTA). Durch metallurgische Untersuchungen und In-situ-Messung auftretender Prozesskräfte und Temperaturen an der Werkzeugschneide beim Fräsprozesses sowie der anschließenden Untersuchung von Werkzeugverschleiß und Oberflächenintegrität ist eine detaillierte Analyse und Korrelation zwischen den mikrostrukturellen Eigenschaften und der Zerspanbarkeit möglich. Die Vorgehensweise erlaubt einer Beurteilung des Einflusses der ultraschallunterstützten Fräsbearbeitung auf den Prozess sowie die resultierenden Oberflächenintegrität. Unter systematischer Anwendung dieser Methodik sowie der Berücksichtigung der Anbindung zum Stahlsubstratwerkstoff und der Wirksamkeit des Verschleißschutzes lässt sich letztlich eine gezielte Optimierung der Zerspanungssituation und des Verschleißschutzes erreichen. Die Erkenntnisse erlauben Handlungsanweisungen und Empfehlungen für Normen und Verarbeitungsrichtlinien, die besonders KMU eine sichere und wirtschaftliche Fertigung hochbelasteter Stahlkomponenten mit unkritischen, kostenreduzierten Werkstoffen ermöglichen sollen.
Alloy Modification and ultrasonic assisted milling of wear resistant alloys with defined surfaces
(2023)
The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. In addition to increasing demands to replace conventional cobalt alloys with nickel alloys as a result of price and supply risks, there is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces.
A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process.
In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on machining is investigated. The alloy used is a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA). Through metallurgical investigations and in-situ measurement of cutting forces and temperatures at the cutting edge during the milling process as well as the subsequent investigation of tool wear and surface integrity, a detailed analysis and correlation between microstructural properties and machinability is feasible. The findings allow recommendations for standards and processing guidelines, enabling safe and economical production of highly stressed steel components with non-critical, cost-reduced materials.
Die Verringerung der CO2-Emissionen ist eng mit der Entwicklung hocheffizienter und wirtschaftlicher Komponenten aus Stahl in der Anlagen- und Verfahrenstechnik verknüpft. Um den hohen kombinier-ten korrosiven, tribologischen, thermischen und mechanischen Beanspruchungen stand zu halten, werden auf Anwendungsfall und Stahlwerkstoff abgestimmte Verschleißschutzschichten eingesetzt. Neben der zunehmenden Forderung konventionelle Kobalt- durch Nickellegierungen zu ersetzen, wächst auch der Bedarf nach definierten Ober- bzw. Funktionsflächen hoher Güte. Aufgrund hohen Werkzeugverschleißes ist die erforderliche Fräsbearbeitung zu Herstellung der komplexen Geomet-rien der Bauteile für KMU oftmals wirtschaftlich nicht möglich. Mittels Legierungsmodifikation der Schweißzusätze für nickelbasierte plasmaauftraggeschweißte Verschleißschutzschichten und durch den Einsatz innovativer ultraschallunterstützter Fräsprozesse soll eine günstigere Zerspanbarkeit er-reicht werden, ohne das Verschleißschutzpotential zu mindern. Im vorliegenden Beitrag wird der Ein-fluss der mittels Legierungsmodifikation eingestellten Gefüge- und Ausscheidungsmorphologie auf die Zerspanbarkeit untersucht. Dies erfolgt anhand einer typischerweise für Schneckenmaschinen einge-setzten Verschleißschutzlegierung NiCrMoSiFeB-Legierung („Colmonoy 56 PTA“), die konventionelle CoCr-Legierungen (Stellite) substituiert. Metallurgische Untersuchungen und In-situ-Messungen auf-tretender Prozesskräfte an der Werkzeugschneide beim Fräsen sowie anschließende Untersuchungen von Werkzeugverschleiß und Oberflächenintegrität ermöglichen eine detaillierte Analyse und Korrela-tion zwischen mikrostrukturellen Eigenschaften und Zerspanbarkeit.
Hybrid laser-arc welding (HLAW) was applied for butt welding of 14.5 mm thick plates of ferritic cryogenic steel X8Ni9 containing 9% Ni, which is used for manufacturing storage and transport facilities of liquefied natural gas (LNG). The weld seam formation and the achievable metallurgical and mechanical properties of the hybrid welds were investigated experimentally for two types of filler wire, an austenitic wire dissimilar to the base metal (BM) and an experimentally produced matching ferritic wire. Safe penetration and uniform distribution of the austenitic filler metal in the narrow hybrid weld could only be achieved in the upper, arcdominated part of the weld. The pronounced heterogeneous distribution of the austenitic filler metal in the middle part and in the root area of the weld could not ensure sufficient notched impact toughness of the weld metal (WM). As a result, a decrease in the impact energy down to 17±3 J was observed, which is below the acceptance level of ≥34 J for cryogenic applications. In contrast, the use of a matching ferritic filler wire resulted in satisfactory impact energy of the hybrid welds of up to 134±52 J at the concerned cryogenic temperature of -196 °C. The obtained results contribute to an important and remarkable conversion in automated manufacturing of LNG facilities. In other words, the results will help to develop a new laser-based welding technology, where both quality and productivity are considered.The efficiency of the developed welding process has been demonstrated by manufacturing a prototype where a segment of the inner wall of large size LNG storage tank was constructed. In this concern, hybrid laser arc welding was conducted in both horizontal (2G) and vertical (3G) positions as a simulation to the actual onsite manufacturing. The prototype was fabricated twice where its quality was confirmed based on non-destructive and destructive examinations.
In Neutron-Bragg-Edge Imaging (NBEI) experiments, we studied the phase transition during butt-welding of supermartensitic steel plates. Gas tungsten arc welding (GTAW) was used with a motorized torch allowing for automated weldments. The austenitization in the heat affected zone (HAZ) underneath the welding head could be clearly visualized at λ = 0.39 nm, a wavelength smaller than the Bragg edge wavelengths of both austenite and martensite. Also, the re-transformation into the martensitic phase upon cooling was detected. However, we observed an unexpected additional change in transmission at λ = 0.44 nm that is a wavelength larger than the wavelength of the Bragg edges of both the martensitic and austenitic phases. We attribute this change to the Deybe-Waller-Factor that describes the temperature dependence of coherent scattering at a crystal lattice. The observed two-dimensional attenuation map corresponds well with a temperature distribution modelling by software macros in ANSYS. Here, the absolute temperature values could be achieved by calibrating the modelled attenuation with help of a thermocouple placed at the steel plate. This allows in return for a direct two-dimensional temperature reading based on the Debye-Waller-relation between neutron attenuation and sample temperature.
The poster starts by presenting the current limitations of the methods used to assess hydrogen effects on materials. Next, an alternative technique called the Hollow Specimen Technique is presented, which aims to overcome the limitations of the current standardised techniques, followed by its advantages. Finally, the H2HohlZug project, its work packages and objectives are presented.
As the world shifts to a decarbonized economy, the demand for hydrogen-based technologies is rapidly increasing. In order to make optimal use of hydrogen as an energy carrier, the infrastructure for hydrogen storage and transport in particular, must meet high technical safety standards. The indispensable basis for such safety assessments are the material properties, which must be evaluated under operating conditions that are as real as possible.
The conventional method for the assessment of the material properties in gaseous hydrogen is conducted by testing materials in high-pressure hydrogen gas in a pressure vessel (autoclave). It is an established method that allows to perform common standardized tests such as tensile, fatigue and crack growth tests under varying hydrogen conditions. However, this method is complex and entails high costs due to extensive safety regulations.
The hollow specimen technique is a more efficient test method, which can be used to assess the mechanical properties of materials under high-pressure hydrogen gas. The procedure is conducted by enclosing high-pressure gas into a hole along the axis of the tensile test specimen. Recently, this method has been successfully performed at pressures up to 1000 bar and over a wide range of temperatures. Due to the low hydrogen volume needed, this method requires minimal safety regulation; therefore, the costs are reduced when compared to the conventional autoclave technique. This method is now in a standardization process, which has been initiated by Japan as a new working package in ISO (TC 164/SC 1/WG 9).
The following contribution presents preliminary results obtained testing common grades of metastable austenitic stainless steel. For this purpose, the mechanical properties and fracture surface of solid and tubular specimens were assessed and compared using slow strain rate tensile (SSRT) test as part of the preliminary work at the Fraunhofer IWM. In a similar way, pipeline steels evaluated under hydrogen atmospheres using the geometry adapted by BAM will be presented. Within the framework of the TransHyDE flagship project, more results with the goal of supporting the standardization of the hollow specimen technique are expected to be obtained.
Reducing CO2 emissions to 62 percent up to 2030 and achieving greenhouse neutrality up to 2050 are the key goals of the EU's climate protection legislation. The expansion of technologies for climate-neutral energy generation is not the only important contribution to reducing greenhouse gases, the efficient use of material systems is also a key factor. In the area of plant engineering, steel components are provided with a wear-protection coating for efficient use to protect them against corrosive, tribological, thermal and mechanical stresses. The wear-protection coatings are primarily made of Co alloys, which are to be replaced by alternative materials, such as nickel alloys, because of the poor working conditions regarding the extraction of the cobalt and because of the health risks. In terms of corrosion behavior, many applications require a crack-free wear protection layer and additional machining. Machining by milling is not economical for wear materials, especially for SME because of the high tool wear, but it is essential to produce defined surfaces with high quality.
Alloy modifications of the filler metals for nickel-based plasma deposition welded wear protection coatings and the use of innovative ultrasonic-assisted milling processes are examined to determine how more favorable machinability can be achieved without reducing the wear protection potential. The focus is on the NiCrSiFeB alloy, which is intended to replace CoCr alloys in the area of screw machines. The modification of hard facing layers in terms of microstructure and precipitation morphology as well as suitability for machining is investigated and compared with the CoCr alloy. In this aspect, the alloy modifications are generated by a PTA process by systematically adjusting the preheating and interpass temperatures, a crack-free wear-resistant layer can be generated, which is subsequently machined by a milling process. In addition to the crack-free properties,
the microstructure, the bonding as well as the mixing between the NiCrFeB alloy and a 1.8550 as well as between the CoCr alloy and a 1.4828 are analyzed and compared in the joining areas. In addition, heating and cooling rates are determined and a chemical analysis of the weld metals is performed. This study provides important knowledge about the differences between NiCrFeB alloy and CoCr alloys in terms of microstructure morphology, bonding and mixing behavior in the joining zones to the basic material.
Design and construction of a rainfall simulator to test metal runoff at atmospheric conditions
(2023)
A rainfall simulator was presented as an environmental assessment tool to quantify wash-off concentrations from metallic materials. It is part of the RUNOFF-project, which studies and re-assesses the durability of roofing and facade materials under current atmospheric conditions in Germany.
Studying building materials is important as they have a significant impact on achieving a variety of goals and targets within the sustainable developments goals (SDGs). The durability of materials is essential to reach sustainability. However, the durability of metallic materials is strongly depended on climate conditions, which have changed as a result of technical measures in industry, climate change and increasing urbanisation. In Germany at least, the data base is not up-to-date leading to prediction models regarding corrosion resistance and durability of metallic materials which can no longer be trusted and therefore need to be re-assessed and updated. Also, not only the demand for sustainable but also environmentally friendly building materials has increased dramatically. A number of construction materials produce chemical hazards, and therefore have negative impacts on water quality, soils health and ecosystems. To limit these impacts, environmental assessment methods and tools are needed to measure and quantify the inputs and outputs of building materials throughout their lifetime.
In 2015, the University of Manchester hosted a workshop (‘Mind the Gap’) aimed at identifying gaps in a number of structural integrity fitness-for-service procedures, including R5, R6, BS 7910 and API/ASME. The findings were subsequently summarised in a journal paper and shared with the relevant stakeholders. A second workshop, this time hosted by the University of Bristol in 2017, was intended to build on the findings of the earlier event, identifying which gaps had been filled, which remain and whether new ones have been identified in the meantime. ‘Mind the Gap 2’ was wide-ranging, including consideration of failure by fracture, fatigue crack growth, hightemperature creep and environmentally assisted crack growth, along with the use of innovative techniques to follow the progress of crack growth from the atomic to the macroscopic scale. A summary of the whole event is thus outside the scope of a single paper, so here we concentrate mainly on advances in fracture assessment, on the interface between inspection and ECA, and on how developments are being incorporated into structural integrity procedures. There is a particular emphasis on the energy transition in the UK, where the planned energy mix will include both nuclear power and offshore wind.
Fatigue tests were performed on the forged aluminum alloy EN AW-2618A in the T61 state. Different stress ratios (R = -1, R = 0.1) were selected to study the influence of mean stress on fatigue life. Two overaged states (10 h/230 ◦C, 1000 h/230 ◦C) were also tested to investigate the influence of overaging on fatigue life. Transmission electron microscopy (TEM) was used to characterize the precipitates (S-phase), which are mainly responsible for the strength of the alloy. A fractographic analysis was also performed to determine the failure mode. Overaging reduces the fatigue life compared to the T61 state. The longer the aging time, the lower the fatigue resistance. The reason is the decrease in (yield) strength, which correlates with the radius of the S-phase: the precipitate radius increases by a factor of approximately two for the overaged states compared to the initial state. The analysis of the fracture surfaces showed crack initiation occurs predominantly on the outer surface and is
associated with the primary phases.
Soft polymers such as the investigated polyurethane, characterized by low Young’s moduli and prone to high shear deflection, are frequently applied in pneumatic cylinders. Their performance and lifetime without external lubrication are highly determined by the friction between seal and shaft and the wear rate. FEM simulation has established itself as a tool in seal design processes but requires input values for friction and wear depending on material, load, and velocity. This paper presents a tribological test configuration for long stroke, reciprocating movement, allowing the generation of data which meet the requirements of input parameters for FEM simulations without the geometrical influences of specific seal profiles. A numerical parameter study, performed with an FEM model, revealed the most eligible sample geometry as a flat, disc-shaped sample of the polymer glued on a stiff sample holder. At the same time, the study illustrates that the sensitivity of the contact pressure distribution to Poisson’s ratio and CoF can be minimized by the developed and verified setup. It ensures robust, reliable, and repeatable experimental results with uniform contact pressures and constant contact areas to be used in databases and FEM simulations of seals, enabling upscaling from generically shaped samples to complex seal profiles.
Überblick über die derzeitig wichtigsten additiven Fertigungsverfahren für metallische Werkstoffe in der Industrie (PBF, DED, BJT) und Berücksichtigung der wesentlichen Prozessmerkmale und Nachbearbeitungsschritte. Vorstellung der wichtigsten Defektphänomene und Nennung von Ursachen und Abhilfemaßnahmen.
Das Master Curve (MC) Konzept nach ASTM E1921 wird momentan u.a. in der Kerntechnik für die bruchmechanische Sicherheitsbewertung ferritischer Stähle eingesetzt. Für ferritisches Gusseisen mit Kugelgraphit (GJS) fehlt jedoch eine Validierung dieser Methode und ggf. eine systematische Überprüfung möglicher Modifikationen grundlegender Ansätze des MC-Konzepts. Aus diesem Grund soll in einem kürzlich gestarteten BMUV-Verbundprojekt zwischen der MPA Stuttgart und der BAM Berlin die Anwendbarkeit des MC-Konzepts auf GJS bei dynamischer Beanspruchung untersucht werden. Ziel ist es, eine effektive und effiziente Methodik bereitzustellen, mit der mittels einer vergleichsweise kleinen Stichprobe bruchmechanischer Kleinproben eine Referenztemperatur T0 zur werkstoffspezifischen Temperaturjustierung der MC ermittelt werden kann.
Das Master Curve (MC) Konzept nach ASTM E1921 wird momentan u.a. in der Kerntechnik für die bruchmechanische Sicherheitsbewertung ferritischer Stähle eingesetzt.
Für ferritisches Gusseisen mit Kugelgraphit (GJS) fehlt jedoch eine Validierung dieser Methode und ggf. eine systematische Überprüfung möglicher Modifikationen grundlegender Ansätze des MC-Konzepts. Aus diesem Grund soll in einem kürzlich gestarteten BMUV-Verbundprojekt zwischen der MPA Stuttgart und der BAM Berlin die Anwendbarkeit des MC-Konzepts auf GJS bei dynamischer Beanspruchung untersucht werden. Ziel ist es, eine effektive und effiziente Methodik bereitzustellen, mit der mittels einer vergleichsweise kleinen Stichprobe bruchmechanischer Kleinproben eine Referenztemperatur T0 zur werkstoffspezifischen Temperaturjustierung der MC ermittelt werden kann.
Within fracture mechanics safety assessment for steels in nuclear technology, the probabilistic master curve (MC) concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. However, for ductile cast iron (DCI), a systematic review of potential modifications to the assumptions and the procedure according to ASTM E1921 and an associated validation are still lacking. For this reason, the application of the fracture mechanics MC concept to ferritic ductile cast iron is being investigated in a recently started joint research project between MPA Stuttgart and BAM Berlin. According to the IAEA guidelines SSG 26, the safety assessment of DCI containers for transport as well as storage of radioactive materials is based on the fracture mechanics criterion of general crack initiation exclusion. Within this context, the focus of the current research project is on the further development of brittle fracture safety assessment methods. Therefore, a methodology shall be established to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using samples extracted from a component. For the experimental program, a DCI material will be produced as it is generally used for transport and storage containers. A basic mechanical-technological material characterization consisting of tensile, Charpy and Pellini tests is planned and a comprehensive fracture mechanics test program was compiled covering dynamic testing of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25, and SE(B)140 specimens. Numerical analyses of different specimen geometries and test setups are planned to investigate the influences of stress triaxiality and loading rate. Throughout the experimental program, the microstructure-property relationship will be investigated based on quantitative metallographic and fractographic analyses. Finally, different MC assessment strategies will be considered and modifications will be made if necessary.
Within fracture mechanics safety assessment for steels in nuclear technology, the probabilistic master curve (MC) concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. However, for ductile cast iron (DCI), a systematic review of potential modifications to the assumptions and the procedure according to ASTM E1921 and an associated validation are still lacking. For this reason, the application of the fracture mechanics MC concept to ferritic ductile cast iron is being investigated in a recently started joint research project between MPA Stuttgart and BAM Berlin. According to the IAEA guidelines SSG 26, the safety assessment of DCI containers for transport as well as storage of radioactive materials is based on the fracture mechanics criterion of general crack initiation exclusion. Within this context, the focus of the current research project is on the further development of brittle fracture safety assessment methods. Therefore, a methodology shall be established to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using samples extracted from a component. For the experimental program, a DCI material will be produced as it is generally used for transport and storage containers. A basic mechanical-technological material characterization consisting of tensile, Charpy and Pellini tests is planned and a comprehensive fracture mechanics test program was compiled covering dynamic testing of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25, and SE(B)140 specimens. Numerical analyses of different specimen geometries and test setups are planned to investigate the influences of stress triaxiality and loading rate. Throughout the experimental program, the microstructure-property relationship will be investigated based on quantitative metallographic and fractographic analyses. Finally, different MC assessment strategies will be considered and modifications will be made if necessary.
The strain field can reflect the initiation time of solidification cracks during the welding process. The traditional strain measurement is to first obtain the displacement field through digital image correlation (DIC) or optical flow and then calculate the strain field. The main disadvantage is that the calculation takes a long time, limiting its suitability to real-time applications. Recently, convolutional neural networks (CNNs) have made impressive achievements in computer vision.
To build a good prediction model, the network structure and dataset are two key factors. In this paper, we first create the training and test sets containing welding cracks using the controlled tensile weldability (CTW) test and obtain the real strain fields through the Lucas–Kanade algorithm. Then, two new networks using ResNet and DenseNet as encoders are developed for strain prediction, called StrainNetR and StrainNetD. The results show that the average endpoint error (AEE) of the two networks on our test set is about 0.04, close to the real strain value. The computation time could be reduced to the millisecond level, which would greatly improve efficiency.
AbstractLaser beam welding has become widely applied in many industrial fields in recent years. Solidification cracks remain one of the most common welding faults that can prevent a safe welded joint. In civil engineering, convolutional neural networks (CNNs) have been successfully used to detect cracks in roads and buildings by analysing images of the constructed objects. These cracks are found in static objects, whereas the generation of a welding crack is a dynamic process. Detecting the formation of cracks as early as possible is greatly important to ensure high welding quality. In this study, two end-to-end models based on long short-term memory and three-dimensional convolutional networks (3D-CNN) are proposed for automatic crack formation detection. To achieve maximum accuracy with minimal computational complexity, we progressively modify the model to find the optimal structure. The controlled tensile weldability test is conducted to generate long videos used for training and testing. The performance of the proposed models is compared with the classical neural network ResNet-18, which has been proven to be a good transfer learning model for crack detection. The results show that our models can detect the start time of crack formation earlier, while ResNet-18 only detects cracks during the propagation stage.
LTT (Low Transformation Temperature) - Schweißzusätze stellen eine Alternative zur Verfügung, um die Schwingfestigkeit in Schweißnähten zu erhöhen. Ziel dieses Vortages ist es zum einem die Thematik der LTT - Schweißzusätze, insbesondere in hybrider Ausführung zu erläutern, Zum anderen werden die Ergebnisse der Vorversuche präsentiert.
Through a hybrid use of Low Transforamtion Temperature welding filler, fatigue strength of welds should be increased. Through the hybrid use of LTT welding filler the Integrity of a weld will be less affected. By creating several variants of LTT weld geometries an idea of the optimum residual stress reduction is given.
This study was carried out to investigate the neutron transmission signal as a function of sample temperature during a welding process. A theoretical description that includes the Debye-Waller factor was used to describe the temperature influence on the neutron crosssections. Neutron imaging using a monochromatic beam helps to observe transmission variations related to the material temperature. In-situ neutron imaging of welding experiments show the distribution of the temperature in bulk steel samples. The performed finite element modelling of expected temperature distributions shows good agreement with the obtained experimental data.
The essence of dynamic failure is closely linked to the formation of adiabatic shear bands (ASB), which result from the localization of shear strain under high deformation speeds accompanied by a rapid temperature increase. Understanding this phenomenon is crucial in view of safety issues when impacts of fast rotating machine components (i.e. aircraft turbine blades) may occur. Our contribution addresses both the experimental evidence and characterization of ASBs due to high-speed impact tests at the Split HOPKINSON pressure bar (SHPB) setup and the finite element analysis to determine the parameters of the underlying constitutive model, which is closely related to JOHNSON-COOK (JC) material model.
Experimental investigations were performed on notched shear specimens made of the fine -grained structural steel S690QL and the displacements in the regions affected by shear localization were measured with subset-based local Digital Image Correlation (DIC). The displacement fields, obtained in the SHPB tests, were considered as an objective to validate and to identify the constitutive parameters with. The JC model could reasonably reproduce the displacement distribution. In order to overcome the issues with mesh dependency we provide a nonlocal extension based on the implicit gradient model approach.
Im Additive Manufacturing Verfahren Directed Energy Deposition (DED) wird bei der Verarbeitung von Werkzeugstahl in der Regel reines Argon als Schutzgas verwendet. Dabei kann die Verwendung von speziellen Schutzgasgemischen, auch bei geringen Anteilen zugemischter Gase, durchaus die Bauteilqualität positiv beeinflussen.
In Vorarbeiten der Messer SE & Co. KGaA zeigte ein gewisser Sauerstoffanteil im Schutzgas die Tendenz, den Flankenwinkel von Schweißspuren beim DED zu verbessern. In der vorliegenden Studie wurde daher detailliert untersucht in wie weit unterschiedliche Schutzgasgemische einen Einfluss auf die Qualität sowie die geometrischen Eigenschaften der additiv gefertigten Strukturen des Werkzeugstahls 1.2709 beim Laser-DED ausüben. Es erfolgten zunächst Testschweißungen in Form von Einzelspuren mit unterschiedlichen Gemischen aus dem Basisschutzgas Argon mit geringen Anteilen verschiedener Gase. Dabei wurde der Einfluss der Zusätze auf die Spurgeometrie und Aufbauqualität untersucht. Auf Basis dieser Vorversuche wurde eine Auswahl vielversprechender Gasgemische getroffen und Detailuntersuchungen in Form von Spuren, Flächen und Quadern unter Zugabe verschiedener Mengen an Zusätzen durchgeführt. Zur Bewertung des Einflusses der Schutzgasbeimengungen wurden der Flankenwinkel, die Porosität und das Gefüge der Proben anhand metallografischer Schliffe untersucht. Es zeigte sich, dass eine Zugabe von geringen Anteilen an Zusätzen zunächst zu einer Vergrößerung des Flankenwinkels im Vergleich zu reinem Argon führt. Mit steigendem Anteil der Gase nimmt dieser Winkel jedoch ab. So kann je nach Menge des zugesetzten Gases eine individuelle Benetzung des aufgetragenen Materials an der Oberfläche erreicht werden. Auch die Porosität ließ sich durch Schutzgasgemische beeinflussen und zeigt ein abweichendes Verhalten im Vergleich zu reinem Argon.
It is proposed to model the experimentally observed weld pool boundary with superellipses (Lamé curves) and to find the unknown parameters of the curves using optimization methods. It has been shown experimentally that during laser welding of austenitic stainless steel with a thickness of 2 mm at a speed of 20 mm/s, the rear weld pool part has a shape close to triangular which can be accurately approximated by a superellipse. Analytical dependences of the trajectory and growth rate of the crystal and its cross-sectional area on the geometry of the rear weld pool part are obtained.
Der Vortrag stellt die Arbeiten der BAM in der Initiative QI-Digital vor, in deren Rahmen Lösungen für eine moderne und digitale Qualitätsinfrastruktur entwickelt werden. Schwerpunkt liegt auf dem zentralen Werkzeug Quality-X sowie dem Pilotprojekt "Moderne Qualitätssicherung in der Additiven Fertigung".
Bei dem Vortrag werden die potentiellen mikrobiologischen Einflüsse im Falle der Lagerung von Wasserstofflagerung in unterirdischen geologischen Formationen vorgestellt, die Zusammenarbeit mit internen und auch externen Partnern. Der Fokus liegt dabei auf UGF; anaerobe Umgebungen, Sulfate reduzierenden Bakterien, methanogenen Archaea, weiterleitenden Systeme und die Kombination der Untersuchung abiotisch/biotische
Hydrogen has great potential into the decarbonization process of the energy and transport sectors, thus helping to mitigate the urgent issue of global warming. It can be sustainably produced through water electrolysis with potentially zero emissions, and efficiently used in fuel cell systems. Despite its environmental advantages, hydrogen is an extremely flammable substance and its interaction with most metallic materials could result in their mechanical properties degradation to an extent that could make them inherently unsafe.
Extensive material testing under realistic operating conditions is required to determine the criteria under which hydrogen-induced damage is to be expected. In-situ slow strain rate tensile (SSRT) test is an option that allow the quantification of the behavior of metals in hydrogenated environments. The standardized procedure for testing in-situ the pressurized gaseous hydrogen
effect on metals consists of the utilization of an autoclave as a containment volume. Testing inside an autoclave is difficult, expensive, and time-consuming, and requires specialized equipment and trained personnel. A relatively recent method to circumvent these issues and provide affordable and reliable test results consists in using hollow specimens as the gas containment volume, thus applying the hydrogen pressure inside rather than outside the
specimen. This experimental setup allows us to minimize the volume of hydrogen and perform the tests safely and effectively. This study focuses on the evaluation of tensile properties of X65 pipeline steel, which was in vervice for natural gas transport, tested in a high-pressure hydrogen environment using hollow specimens. A constant nominal strain rate of 1ꞏ10-6 s-1 is applied. Tests are performed with different manufacturing techniques for the drilling process, which results in difeerent surface conditions. The effect of the roughness on the HE was investigated. For the evaluation the effect on the reduced area at fracture (RA) and the elongation loss were determined. Further fractographic analysis were performed. In this way, this study provides insights on the applicability of novel, reliable, and safer testing method which can be used to assess HE, particularly in relation with hydrogen-induced loss of ductility in metallic material.
Large scale hydrogen assisted cracking test for thick walled SAW joints for offshore applications
(2023)
Offshore wind turbines continuously increase in size and weight and demand adequate offshore foundations concepts like monopiles, tripods or jackets. These components are typically submerged arc welded (SAW) high-strength thick steel plates like the S420ML. During welding, the occurrence of delayed hydrogen assisted cracking (HAC) must be anticipated. HAC is a critical combination of the local hydrogen concentration within a susceptible microstructure under certain mechanical load, i.e., the occurring (welding) residual stresses. The welding sequence of the thick-walled plates complicate the residual stress distribution due to the necessary repeated thermal cycling, i.e., welding seam / layer deposition to fill the joint. For that purpose, SAW with two-wire-technique was used to weld a specially designed and prototype-like mock-up of a real component with a thickness of 50 mm, filled more than 20 passes and a seam length of 1,000 mm. Additional welded stiffeners simulated the effect of a high restraint, to stimulate critical HAC conditions. The necessity of a minimum waiting time (MWT) before the NDT can be conducted (to exclude HAC) was critically verified by the application of ultrasonic testing of the welded joint at different time-steps of the NDT of 48 h after welding. The residual stresses were determined by a robot XRD goniometer. Tensile residual stresses up to the yield limit are found both in the weld metal and in the heat-affected zone. Numerical modelling allowed the qualitative estimation of the hydrogen diffusion in the weld. A remarkable HAC occurrence was not identified and proves both, a certain resistance of the weld joint to HAC and the (questionable) duration of the MWT.
Die schädigende Wirkung von Wasserstoff auf die mechanischen Eigenschaften von Stählen ist zwar bekannt, aber noch immer nicht ausreichend erforscht. Die schnelle und sichere Markteinführung von Wasserstofftechnologien macht es erforderlich, dieses Thema genauer zu untersuchen. Im Allgemeinen wird dies oft als Wasserstoffversprödung bezeichnet. Daher ist es wünschenswert, eine Prüfmethode zu entwickeln, die auf einfache Weise die Materialeigenschaften unter Wasserstoffatmosphäre ermitteln kann. Derzeit werden mechanische Prüfungen unter Wasserstoffatmosphäre in Autoklaven durchgeführt. Für diese Technik ist eine aufwendige Hardware erforderlich, daher sind die Prüfungen teuer und die Prüfkapazitäten nur in geringem Umfang verfügbar. Die hier vorgestellte Prüfmethode verspricht einen zukunftsweisenden Ansatz zur Reduzierung von Kosten und Bearbeitungszeiten durch die Verwendung von Hohlkörpern, d.h. die Probe selbst stellt den Autoklav dar.
Die Wasserstoffinfrastruktur ist eine zentraler Bestandteil der erfolgreichen Umsetzung der wasserstoffbasierten Energiewende. Dabei bilden Ferngasleitungen quasi das "Rückgrat" der Transportinfrastruktur großer Gasmengen. Dabei müssen unter Umständen Reparaturen an den Pipelines durchgeführt werden. Dabei ist in der Erdgasinfrastruktur das Schweißen an in Betrieb befindlichen (d.h. von Gas durchflossenen) Pipelines Stand der Technik. Es ist jedoch vollkommen offen, inwieweit diese Technik auf die reine Wasserstoffpipelines übertragbar sind. Hierzu leistet das Projekt H2SuD wichtige Beiträge zur Aufklärung des Einfluss eines Reparaturschweißprozesses auf die Wasserstoffaufnahme und Degradation im Betrieb befindlicher H2 Gasleitungen.
Einfluss der Schweiß- und Prüfparameter bei der Heißrissbewertung hochfester Schweißzusatzwerkstoffe
(2023)
Die Heißrissneigung beim Schweißen kann mittels einer ganzen Reihe von Prüfverfahren ermittelt werden. Eine etablierte Methode ist die sogenannte Varestraint-Prüfung, welche auch an der Bundesanstalt für Materialforschung und -prüfung (BAM) als modifizierter Varestraint/Transvarestraint-Test (MVT) zum Einsatz kommt. Die Ergebnisse von Varestraint-Prüfungen hängen jedoch stets in unterschiedlichem Maße von der individuellen Prüfmaschinenauslegung und den verwendeten Prüfparametern ab. Dies kann zu einer uneinheitlichen Bewertung des Rissverhaltens führen, wenn die Risslänge konventionell als Kriterium für die Rissneigung herangezogen wird. Scheinbare Abhängigkeiten von Prozessparametern erschweren dann die Interpretation der Ergebnisse. Eine neuartige Bewertungsmethodik entkoppelt den Maschineneinfluss vom Materialverhalten und verwendet die Dehnrate als Risskriterium in Analogie zu Prokhorovs Heißrissmodell. Die neue Auswertung wird anhand einer Studie hochfester Schweißzusatzwerkstoffe vorgestellt, deren Rissverhalten in Abhängigkeit der chemischen Zusammensetzung und der Schweißparameter bewertet wird.
It was found that there is a systematic dependence of the crack growth on the welding parameters as well as on the load. Decreasing welding speeds with simultaneously higher heat input promote crack formation with increasing strain rate.
Based on the results, a new crack criterion was finally selected which allows an extended assessment of the material behavior during the MVT-test. The threshold introduced can quantify the dependencies of the crack formation on the welding and testing parameters, which could not be comprehensively described with the conventional evaluation. In principle, the evaluation routine can also be transferred to other Varestraint or externally loaded hot cracking tests.
The use of Low Transformation Temperature (LTT) filler materials is an innovative way to reduce welding residual stresses. The generation of compressive residual stresses in the weld and heat-affected zone can lead to an improvement of the fatigue life of high-strength welds. However, high-alloy filler metals can be prone to solidification cracking. Two important LTT alloys were evaluated under variable welding and loading parameters using the Modified Varestraint/Transvarestraint (MVT) test. Initially conflicting results were interpreted using a newly developed image-based crack detection routine [1]. Based on the melt pool dimensions, the shape of the isotherms is reconstructed, and the theoretical crack growth along numerically determined crystallization paths is considered in relation to the cracks observed. Decreasing welding speeds with simultaneously higher heat input promote crack formation with increasing strain rate.
Influence of Residual Stresses on Stress Relief Cracking of Thick-Walled Creep-Resistant Steel Welds
(2023)
Controlling the residual stress level during welding of creep-resistant Cr-Mo-V steels is crucial to avoid so called stress relief cracking (SRC) during post weld heat treatment (PWHT) of large-scale components. In the present study, a laboratory scale test specimen (400 mm x 400 mm x 25 mm) was used to simulate thick-walled component welds made of 13CrMoV9-10. The aim was to identify the level and distribution of residual stresses to evaluate the suitability of the specimen for laboratory based SRC testing. High restraint was ensured by the specimen geometry with a narrow welding gap in the center. This gap was filled by submerged arc welding in a multi-layer technique. Two specimens were welded with identical parameters and compared in the as-welded state and after PWHT (705 °C for 10 h). Neutron diffraction was used to determine the residual stresses in the weld metal, the heat-affected zone (HAZ) and the base material at different depths longitudinal, transverse, and normal to the welding direction. The experiments were performed on the instrument E3 of the research reactor BERII of HZB Berlin, Germany. Complementarily, laboratory X-ray diffraction was applied to characterize the surface residual stresses. In the welded state, especially in the weld metal and the adjacent HAZ, the residual stress can reach the yield strength of the untreated material. The highest levels occur in the longitudinal direction. The transverse and normal directions are characterized by residual stress of lower magnitude. As expected, the residual stress is almost completely relieved after PWHT.
Additive manufacturing (AM) processes enable the efficient production of advanced constructions. Direct energy deposition processes such as wire and arc-based additive manufacturing (DED-arc) are important methods. The wire filler metals enable a wide range of materials. In addition, the arc process provides a high deposition rate compared to laser and powder-based processes. Furthermore, components can be manufactured near-net-shape, offering significant savings in cost, time, and resources. Combined with the use of high-strength steels to reduce wall or component thicknesses in the context of lightweight design, great opportunities for saving energy and resources can be achieved. In a joint project of BAM and Chemnitz University of Technology, the main influences and complex interactions of material, production process, design and processing steps on the residual stress level are investigated. The aim is to develop processing recommendations and a cold cracking test for economical processing and stress-related design of high-strength steels with DED-arc. This study focuses on residual stress analysis by neutron diffraction (ND) and X-ray diffraction (XRD) on defined test specimens. The ND analysis were performed at the Paul Scherrer Institute (PSI) and the XRD analysis at BAM. The study shows a quantitative and qualitative comparison of the residual stress magnitudes and distribution between the component bulk (ND) and surface (XRD) analyses. The ND analysis reveals that in DED-arc AM walls the residual stresses dominate in the direction of welding and are negligibly small in each case transverse to the direction of welding. The topology of the analyzed residual stresses shows almost identical residual stress maps. In addition, the residual stresses are significantly influenced by the solid phase transformation of the material due to low cooling times in the area of the top layer.
The contribution describes a newly developed software tool for crack identification and selection in Modified Varestraint Transvarestraint (MVT) testing. From the digital crack information, in addition to the classical results, such as Total Crack Length (TCL) and Maximum Crack Length (MCL), advanced evaluations can be applied, taking into account the loading and welding parameters. A numerical parameter study is conducted to demonstrate how the isolated variation of individual welding and loading parameters, affects the crack lengths that can potentially be expected based on the machine specifics. An alternative crack criterion is presented that evaluates the crack formation in relation to the machine behavior. Some examples demonstrate the possibilities and limitations of the approach. The criterion can be used to compare and transfer the results of different varestraint test variants.
Einfluss der Schweiß- und Prüfparameter bei der Heißrissbewertung hochfester Schweißzusatzwerkstoffe
(2023)
Die Heißrissneigung beim Schweißen kann mittels einer ganzen Reihe von Prüfverfahren ermittelt werden. Eine etablierte Methode ist die sogenannte Varestraint-Prüfung, welche auch an der Bundesanstalt für Materialforschung und -prüfung (BAM) als modifizierter Varestraint/Transvarestraint-Test (MVT) zum Einsatz kommt. Die Ergebnisse von Varestraint-Prüfungen hängen jedoch stets in unter-schiedlichem Maße von der individuellen Prüfmaschinenauslegung und den verwendeten Prüfparametern ab. Dies kann zu einer uneinheitlichen Bewertung des Rissverhaltens führen, wenn die Risslänge konventionell als Kriterium für die Rissneigung herangezogen wird. Scheinbare Abhängigkeiten von Prozessparametern erschweren dann die Interpretation der Ergebnisse. Eine neuartige Bewertungsmethodik entkoppelt den Maschineneinfluss vom Materialverhalten und verwendet die Dehnrate als Risskriterium.
Enhanced crack detection method using Convolutional Neural Networks for Varestraint type tests
(2023)
Varstraint type tests are globally established in the measurement of hot cracking susceptibility of welds. Evaluation of such tests is done under a light microscope and can be heavily influenced by human subjectivity. To reduce the human error source in evaluation, a concept based on Convolutional Neural Networks (CNNs) is proposed. An AI was constructed and trained on self-produced data to detect and segment cracks in microscope images. The advantages, besides a faster evaluation, include higher precision and the availability of data that was not available before.
Der MVT-Test ist die an der BAM entwickelte und genutzte Version des Varestraint-Tests der weltweit für die Charakterisierung der Erstarrungsrissanfälligkeit von Schweißzusätzen und Legierungen eingesetzt wird. Die Auswertung solcher Tests erfolgt klassisch unter dem Lichtmikroskop. Durch Automatisierung des Auswerteprozesses mit KI kann der Informationsgehalt des Tests besser ausgeschöpft und eine höhere Vergleichbarkeit zwischen Testergebnissen gewährleistet werden.
Der Modifizierte Varestraint-Transvarestraint-Test wird an der Bundesanstalt für Materialforschung und -prüfung als Variante des Varestraint-Tests verwendet. Die Auswertung dieser Tests findet klassisch durch Abmessungen der entstandenen Risse unter dem Lichtmikroskop statt. Eine solche Auswertung ist aufwendig und fehleranfällig. Convolutional Neural Networks können trainiert werden, um die Risse auf digitalen Bildern zu segmentieren, wodurch der menschliche Fehler in der Auswertung eliminiert werden kann. Die Ergebnisse können durch Overlay mit den Originalbildern verglichen werden.
Der modifizierte Varestraint-Transvarestraint-Test (MVT-Test) ist die an der BAM vorherrschende Version des Varestraint-Tests der weltweit Anwendung findet. Die Auswertung des Tests erfolgt durch Messen von Risslängen unter dem Lichtmikroskop. Der Vortrag beleuchtet Theorien über die Aussagekraft der Messung, stellt neue Herangehensweisen vor und vergleicht diese anhand von Beispielen.
Structural alloys are largely employed in key industrial sectors and their demand is predicted to rise rapidly for the next decades. Most of these materials require a large amount of energy for extraction and manufacturing, which causes the emission of greenhouse gases and other pollutants. Therefore, strategies for improving the sustainability of structural metallic alloys are urgently needed.
Additive Manufacturing (AM), in particular Laser Powder Bed Fusion (PBF-LB/M), aims to be a sustainable manufacturing process, as it allows the build-up of complex geometry in near net-shape from 3D models, while minimizing material waste and the energy required for the process and post-process treatments.
Nevertheless, the application of additively manufactured parts in structural safety-relevant applications is still hindered by the poor fatigue performance. The cause of this has been mainly attributed to the presence of manufacturing defects and surface roughness. Therefore, a huge effort has been made to optimize the process parameters and to introduce post-process treatments to minimize the defect content. However, material flaws cannot be fully eliminated, but these can be considered in a damage tolerance framework for the prediction of the fatigue performance of additively manufactured metallic materials, which is essential for part design and qualification.
This work aims at presenting different modelling strategies for the prediction of the fatigue limit of AM metals. Simple empirical models and more complex models based on fatigue short crack propagation are proposed. The investigated material is an AlSi10Mg alloy fabricated by PBF-LB/M and subjected to two different low-temperature heat-treatments (265°C for 1 h and 300°C for 2h). The results show that the models can provide good approximation of the fatigue limits and help in the interpretation of the scatter of fatigue data.
The Kitagawa-Takahashi (KT) diagram is a well-established tool in the fatigue community for the prediction of the fatigue limit of metallic materials in presence of defects. Nevertheless, its determination is associated with a large number of fatigue tests carried out on specimens with artificial defects (notches) to describe the fatigue limit-defect size relationship in the short crack regime. The preparation of the specimens and the execution of the tests is time expensive. Therefore, few phenomenological models have been introduced in the past to provide a first approximation of the KT diagram based solely on the fatigue limit for smooth specimen and the fatigue crack propagation threshold for long cracks. Despite the use of such models is widely spread, these suffer from problems related to the uncertainties of the material parameters. Furthermore, the mechanics of short cracks, which is the physical mechanism behind the concept of the fatigue limit, is not considered. This work discusses the advantages and drawbacks of using short fatigue crack propagation models for predicting the fatigue limit of flawed metallic materials. The KT diagrams for a EA4T railway axle steel in as-received and full-hardened condition are approximated by means of the cyclic R-curve method.
The fatigue assessment of welded joints requires several input data, which can be subdivided into three categories: geometry, material and loading. The number of input data depends essentially on the complexity of the models employed and on the level of accuracy of the analysis. It is common practice to use safety factors in design to account for the scatter of the input parameters. Nevertheless, overly-conservative factors lead often to unrealistic estimations of fatigue life. This work presents a fracture mechanics-based model for the structural integrity assessment of welded joints under constant amplitude fatigue loading, in which the local geometry at the weld toe and the fatigue crack growth properties are considered statistically distributed. The approach is validated against a large number of experimental data.
Fraucture mechanics-based probablistic structural integrity assessment for aero-engine turbine disk
(2023)
Aero-engine turbine disks are safety-relevant components which are operated under high thermal and mechanical stress conditions. The aim of this work is to present part of a fracture mechanics-based probabilistic assessment procedure under development which aims at calculating the critical rotational speed of the turbine disk based on the numerical-analytical solutions and regulations for the failure probability. In particular, the rim-peeling failure mode is considered as case study. A semi-circular surface crack is modelled at the most stressed region at the diaphragm of a turbine disk. In order to design a lab representative specimen, beside the crack driving force, expressed in terms of J-integral, also the constraint to plastic deformation e.g., stress triaxiality, at the crack-tip must be similar for the same crack in the specimen and in the disk. The analytical solutions to calculate the crack driving force for the lab representative specimen are used for the Monte Carlo simulations, the result of which has been assessed in the form of a Failure Assessment Diagram (FAD). The results of the probabilistic structural integrity assessment show good agreement between Monte Carlo simulations and certification values for the disk in terms of expected failure mode and value of the critical speed.
The process-structure-property-performance relationship is a fundamental paradigm in metal additive manufacturing (AM). The knowledge of how process parameters and post-process treatments influence the material properties and therefore the structural integrity of additively manufactured metallic components is of paramount importance. With respect to this, one of the unsolved problems related to the unique AM process is the reliability of witness samples for part qualification. Focusing on the Laser Powder Bed Fusion (PBF-LB/M) process, the microstructure and therefore the mechanical performance of test coupons are not representative of parts of the same material in every case. This work summarizes part of the results of an ongoing cooperation between BAM and BASF, which aims at addressing this issue by designing dedicated specimens, representative of the fatigue properties of the real component. The considered case study consisted in the fabrication and characterization of the fatigue properties of a pressure vessel made of AISI 316L. The first phase of the project was devoted to the process monitoring to understand the relationship between process parameters and temperature distribution during the fabrication of the component. Finite element models were tuned on the experimental data from the process monitoring and simulations of the temperature field in the component were conducted. The numerical results were in good agreement with the temperature profiles measured during the fabrication of the component. The second phase dealt with the evaluation of the fatigue and fatigue crack propagation properties on specimens extracted from different regions of the pressure vessel. The experimental investigations showed significant differences in hoop and longitudinal direction. A clear dependence of the fatigue properties on heat accumulation (temperature distribution) and defect size was pointed out. The third phase encompassed the fabrication and testing of the representative specimens. Numerical simulations were used to design specimens displaying the same temperature profile as in the most critical region of the component. The fatigue testing of the representative specimens is subject of ongoing work.
Die neue Generation von bainitischen Schmiedestählen bietet auf der einen Seite ein erhebliches Festigkeitspotenzial, das es im Sinne des Leichtbaus auch für zyklisch belastete Sicherheitsbauteile zu heben gilt. Auf der anderen Seite geht mit dieser Festigkeitssteigerung im Vergleich zu Vergütungsstählen ein Verlust an Duktilität und Zähigkeit einher. Am Beispiel des Demonstratorbauteils Achsschenkel ging das Forschungsvorhaben der Frage nach, wie ein Freigabeprozess zu gestalten ist, damit das Festigkeitspotenzial der neuen Stähle zuverlässig ausgenutzt werden kann. Als Ergebnis wird eine Vorgehensweise dargestellt, die den Eigenschaften der neuen Generation von Schmiedestählen Rechnung trägt, um den sicheren Betrieb der Komponenten zu gewährleisten.
High entropy alloys (HEA) are a new class of materials that have been investigated since the early 2000s and offer great potential to replace conventional alloys. However, since they sometimes have significant contents of expensive alloying elements such as Co or Ni, their use is only conceivable in highly stressed areas of components. For this purpose, the weldability with conventional alloys such as high-alloy austenitic steels must be investigated. In addition to the resulting microstructure, the mechanical properties are also fundamental for the usability of HEAs in DMWs. For this purpose, TIG welds of CoCrFeMnNi HEA (cold rolled and recrystallized state) with AISI 304 austenitic steel are investigated. These mechanical properties are analyzed in this work by means of tensile tests and local hardness measurement. The local strain behavior of the welded joints is also characterized by means of Digital Image Correlation (DIC). The results of the local hardness measurement show a clear influence of the initial condition of the HEA on the HAZ. Thus, the HEA in the cold-rolled condition shows a clear softening because of recrystallization processes in the HAZ. On the other hand, there is no influence on the hardness of the weld metal, which is approx. 200 HV0.1 in both cases. The tensile tests show a consistent failure of the weld in the weld metal. However, regardless of the HEA condition, strengths in the range of the recrystallized HEA (RM ~ 550–600 MPa) are achieved, although with significantly reduced fracture elongations.
Um Bauteile vor Verschleiß und Korrosion zu schützen werden Beschichtungen aus resistenteren Materialien aufgetragen. Hierzu zählen unter anderen die Legierungen auf Cobalt-Chrom Basis. Der diskrete Materialsprung ist jedoch unter thermischen und mechanischen Belastungen häufig Ursache für das Versagen der Beschichtung. In dieser Arbeit werden daher Materialgradierungen von verschiedenen Stahllegierungen zu einer Cobalt-Chrom Basislegierung untersucht. Die Ergebnissen werden dafür auch mit Resultaten zu vorangegangenen Untersuchungen verglichen. Kern der Arbeit bilden geätzte Schliffbilder der Materialpaarungen und Auswertungen mittels Farbeindringprüfung sowie die metallografische Bestimmung der Porosität. Ziel der Arbeit ist ein defektfreier Aufbau der funktional gradierten Materialpaarungen.