Filtern
Dokumenttyp
- Vortrag (31) (entfernen)
Referierte Publikation
- nein (31)
Schlagworte
- SEM (31) (entfernen)
Organisationseinheit der BAM
- 6 Materialchemie (18)
- 6.1 Oberflächen- und Dünnschichtanalyse (17)
- 5 Werkstofftechnik (3)
- 5.1 Mikrostruktur Design und Degradation (3)
- 8 Zerstörungsfreie Prüfung (2)
- 1 Analytische Chemie; Referenzmaterialien (1)
- 1.6 Anorganische Referenzmaterialien (1)
- 3 Gefahrgutumschließungen; Energiespeicher (1)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (1)
- 6.6 Physik und chemische Analytik der Polymere (1)
Eingeladener Vortrag
- nein (31)
Investigation of degradation of the aluminum current collector in lithium-ion batteries by GD-OES
(2022)
Lithium-ion batteries (LIBs) are one technology to overcome the challenges of climate and energy crisis. They are widely used in electric vehicles, consumer electronics, or as storage for renewable energy sources. However, despite innovations in batteries' components like cathode and anode materials, separators, and electrolytes, the aging mechanism related to metallic aluminum current collector degradation causes a significant drop in their performance and prevents the durable use of LIBs. Glow-discharge optical emission spectroscopy (GD-OES) is a powerful method for depth-profiling of batteries' electrode materials. This work investigates aging-induced aluminum deposition on commercial lithium cobalt oxide (LCO) batteries' cathodes. The results illustrate the depth-resolved elemental distribution from the cathode surface to the current collector. An accumulation of aluminum is found on the cathode surface by GD-OES, consistent with results from energy-dispersive X-ray spectroscopy (EDX) combined with focused ion beam (FIB) cutting. In comparison to FIB-EDX, GD-OES allows a fast and manageable depth-profiling. Results from different positions on an aged cathode indicate an inhomogeneous aluminum film growth on the surface. The conclusions from these experiments can lead to a better understanding of the degradation of the aluminum current collector, thus leading to higher lifetimes of LIBs.
The use of duplex stainless steels (DSS) in energy related applications is well known. Nowadays, DSS steels become more favorable than austenitic steels due to the outstanding mechanical properties, the good corrosion resistance and the lower nickel content. However, the use of the duplex grade in acidic environments such as seawater often leads to severe degradation of the structural integrity of the steel by hydrogen-induced/assisted cracking (HAC) phenomena, which can eventually result in premature failure. Hydrogen assisted degradation and cracking of steels are active fields of research even though this topic is intensively studied for more than a century. A bottleneck is the analytical validation of the theoretical models proposed ion the literature at the sub-micron scale.
Industrial and the research communities see a need for an accurate analytical method by which it is possible to image the distribution of hydrogen in the microstructure of a steels or and other alloys. Among the very few available methods hydrogen imaging methods, Time-of-Flight secondary ion mass spectrometry (ToF-SIMS) has the principal capability for mapping of hydrogen in a steel’s microstructure. The combination of ToF-SIMS with multivariate data analysis (MVA), electron microscopy (SEM) and electron-backscattered diffraction (EBSD) is a powerful approach for providing chemical and structural information. The use of data fusion techniques has been shown recently to enhance the better understanding of the hydrogen induced degradation processes in in a DSS steel.
PTFE/PS core-shell-nanoparticles were characterised by STXM, T-SEM, and ToF-SIMS. Shell-thicknesses were calculated and compared. Preliminary results from ToF-SIMS showed the capabilities of this method.
Investigation of core-shell nanoparticles using scanning transmission x-ray microscopy (STXM)
(2018)
A scanning transmission x-ray microscopy (STXM) based methodology is introduced for determining the dimensions (shell thickness, core and total diameter) of core-shell nanoparticles which exhibit a strong x-ray absorption contrast and a well-defined interface between core and shell material. A low radiation dosage during data acquisition and, therefore, less x-ray beam induced damage of the sample is achieved by recording STXM images only at two predetermined energies of maximum absorption contrast, instead of recording a stack of images across the whole absorption edge. A model core-shell nanoparticle, polytetrafluoroethylene (PTFE) cores with polystyrene (PS) shell, is used for demonstration. Near edge x-ray absorption fine structure (NEXAFS) spectroscopy confirms the significant difference in x-ray absorption behavior between PTFE and PS. Additionally, due to the insolubility of styrene in PTFE a well-defined interface between particle core and shell is expected. In order to validate the STXM results, both the naked PTFE cores as well as the complete core-shell nanoparticles are examined by scanning electron microscopy (SEM). The introduced STXM based methodology yields particle dimensions in good agreement with the SEM results (deviation equal or less than 10%) and provides additional information such as the position of the particle core which cannot be extracted from a SEM micrograph.
A scanning transmission x-ray microscopy (STXM) based methodology is introduced for determining the dimensions (shell thickness, core and total diameter) of core-shell nanoparticles which exhibit a strong x-ray absorption contrast and a well-defined interface between core and shell material. A low radiation dosage during data acquisition and, therefore, less x-ray beam induced damage of the sample is achieved by recording STXM images only at two predetermined energies of maximum absorption contrast, instead of recording a stack of images across the whole absorption edge. A model core-shell nanoparticle, polytetrafluoroethylene (PTFE) cores with polystyrene (PS) shell, is used for demonstration. Near edge x-ray absorption fine structure (NEXAFS) spectroscopy confirms the significant difference in x-ray absorption behavior between PTFE and PS. Additionally, due to the insolubility of styrene in PTFE a well-defined interface between particle core and shell is expected. In order to validate the STXM results, both the naked PTFE cores as well as the complete core-shell nanoparticles are examined by scanning electron microscopy (SEM). The introduced STXM based methodology yields particle dimensions in agreement with the SEM results and provides additional information such as the position of the particle core which cannot be extracted from a SEM micrograph.