Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (20) (entfernen)
Schlagworte
- Fire (20) (entfernen)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (5)
- 3 Gefahrgutumschließungen; Energiespeicher (4)
- 3.2 Gefahrguttanks und Unfallmechanik (4)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (3)
- 7.1 Baustoffe (2)
- 2 Prozess- und Anlagensicherheit (1)
- 2.1 Sicherheit von Energieträgern (1)
- 8 Zerstörungsfreie Prüfung (1)
- 8.5 Röntgenbildgebung (1)
The number of vehicles using or transporting cryogenic fuels such as Liquefied Hydrogen (LH2) or Liquefied Natural Gas (LNG) increases fast in the land transportation sector. Does this also entail new risks? The storage of cryogenic fuels requires tanks with Thermal Super Insulations (TSI) to keep the fluid cold and limit the formation of boil-off gas. TSI has proven itself in some applications since the middle of the 20th century, but in the land transport sector they are still quite new, where accidents involving fires, collisions, and their combination are to be expected. This work focuses on investigating the behavior of different types of TSI while exposed to a heat source representing a fire. To this aim, a High-Temperature Thermal Vacuum Chamber (HTTVC) was applied, which allows the thermal loading of a thermal insulation material in a vacuum and measuring the heat flow transported through the TSI in parallel. In this study, the results of 6 samples are presented regarding 3 types of MLI, rock wool, perlites, and microspheres. The thermal exposure caused different effects on the samples. In practice, this can be connected to the rapid release of flammable gases as well as to a Boiling Liquid Expanding Vapour Explosion (BLEVE). These results are relevant for reducing the risks to people and infrastructures in the progressive establishment of tanks for cryogenic fluids in our industry and society. The data presented in the study can be used to improve the design of tanks and TSIs, the assessment of accident scenarios, and the development of measures for first responders.
Multilayer Insulation (MLI) is frequently used in vacuum conditions for the thermal insulation of cryogenic storage tanks. The severe consequences of the degradation of such materials in engulfing fire scenarios were recently evidenced by several large-scale experimental tests. In the present study, an innovative modelling approach was developed to assess the performance of heat transfer in polyester-based MLI materials for cryogenic applications under fire conditions. A specific layer-by-layer approach was integrated with an apparent kinetic thermal degradation model based on thermogravimetric analysis results. The modeling results provided a realistic simulation of the experimental data obtained by High-Temperature Thermal Vacuum Chamber tests reproducing fire exposure conditions. The model was then applied to assess the behavior of MLI systems for liquid hydrogen tanks in realistic fire scenarios. The results show that in intense fire scenarios degradation occurs rapidly, compromising the thermal insulation performances of the system within a few minutes.
The interest in hydrogen-based green energy is increasing worldwide, and the same is true for hydrogen-powered vehicles. Among the possible solutions to store hydrogen in such vehicles, cryogenic tanks equipped with multi-layer insulation (MLI) are the most promising to increase the amount of energy stored per unit volume. However, MLI is affected by severe deterioration when exposed to an external source of heat such as a fire following a car accident, leaving the tank unprotected and leading to failure in a relatively short time. In this work, a one-dimensional model to evaluate MLI thermal degradation when a liquid hydrogen tank is exposed to fire is presented. The relevance of taking MLI degradation into account when simulating the pressure increase due to external fire exposure is here demonstrated through the analysis of several case studies. The results show that MLI systems performance depletes within a few minutes of exposure to hydrocarbon poolfire.
This study provides an analysis on the fire safety of passengers and the fire protection of coaches and buses. A brief review of major bus fire incidents, an overview of current regulations in Europe, and their limitations are presented. The study finds that the current small-scale fire test methods described in UN ECE Reg No. 118 need to be replaced by test methods that can assess the reaction to fire of materials when exposed to ignition sources of varying sizes. To address these shortcomings, the study proposed an expert recommendation to update the material fire safety requirements and testing for buses. Additional measures are proposed, derived from objectives and strategies applied in other transport sectors, and can be tested through existing European and international standards, which are widely used by several industries. These measures aim to extend the time with tenable conditions for a safe evacuation in case of fire, reduce the degree of damage to buses, reduce the risk for fast and excessive thermal exposure on modern energy carriers needed for a more sustainable transport sector.
Acetylene pressure cylinders are widely used in the industrial sector for welding, flame cutting, or heating.
Sometimes during work, not only with acetylene cylinders, fires occur and in this case the risk of destruction increases and the behavior of such an exposed cylinder is unpredictable. The purpose of this study is to identify those critical conditions when acetylene cylinders burst and explode in fires. In the present study, acetylene cylinders were exposed to fire conditions. For this purpose, a woodpile as a source of fire was chosen, tested, and evaluated. In addition to the fire condition, this option guaranteed reproducibility and similar conditions for all tests. The individual cylinders were equipped with thermocouples measuring the shell temperature, and half of them were prepared in order to measure the temperatures inside the cylinder. An important factor was the measurement of the amount of pressure that was achieved during the destruction of the cylinder. For this purpose, a pressure transducer was attached to the outlet of the cylinder valve. Exposed to direct fire, they can explode in 10 min, which was confirmed. The critical pressure of 40 bar has been reached in 6 min, followed by destruction after 7 min in fire. Cylinders with internal thermocouples were destroyed when lower pressure was achieved. This confirms the fact that any change of the pressure cylinder affects the original properties. After the tests, the fragments of the selected cylinders were subjected to material tests. The results obtained in these tests are the main source of information for understanding the behavior of acetylene cylinders in fire and the possibility of increasing the safety of intervening rescue services in an emergency.
An overview of test standards and regulations relevant to the fire testing of pressure vessels
(2021)
Fire exposure of storage and transportation vessels of hazardous materials (including pressure liquefied gases) can result in BLEVEs and other high-consequence incidents with large societal and economic impacts. To reduce risk most countries have numerous regulations, codes of practice and guidance notes covering the design, operation and maintenance of vessels and thermal protection systems. Yet despite such regulations there remains no internationally accepted fire test procedure for pressure vessel and accompanying thermal protection systems that is capable of meeting a range of regulatory requirements. This paper considers some of the regulations in place in the western world and considers the origin of these based on large and medium-scale testing conducted to date. It examines conditions found in these tests to propose a set of recommendations on which to base a standard method of test. These recommendations are proposed as being representative of a credible large pool fire scenario that may occur.
Water migration in one-side heated concrete: 4D in-situ CT monitoring of the moisture-clog-effect
(2019)
Explosive spalling due to fire exposure in concrete structures can lead severe damage and, in the worst case, to premature component failure. For this reason, an in situ investigation of water Migration in concrete due to surface heating was undertaken.
During these experiments, a miniaturized concrete specimen within a confining and insulating double-hull was subjected to surface heating during simultaneous X-ray computed tomography (CT) scanning. Through the use of subtraction-based Image analysis techniques, it was possible to observe and quantify not only drying within areas of the concrete matrix close to the heated surface, but also the migration of moisture to both pore and matrix regions deeper within the specimen. It was also discovered that the correction of CT images for specimen deformation using DVC and variable detector performance using calibrated image filters significantly improved the quality of the results. This clearly demonstrates the potential of X-ray CT for evaluation of other rapid-density-change phenomena in concrete and other building materials.
Editorial façade fire safety
(2018)
This Special Issue of Fire and Materials brings together a collection of papers that were presented at the 2016 Interflam conference in the Fire & Facades session along with recent submissions to the Fire and Materials Journal that are very relevant to the Fire and Facades subject. Having attended the Interflam conference, all Fire and Materials Journal editors who attended realised the importance of this topic. We felt it important that this session content would both be reviewed and made available to a wider audience and that it was timely that we featured this increasing important topic in our journal. Accordingly, authors of selected papers were invited to update and extend their papers for journal submission, and other appropriate peer review papers subsequently submitted to the Journal were included in the collection.
As part of energy‐efficient renovations or for the construction of new buildings often external thermal insulation composite (ETIC) are used. In 2015, in Germany almost 37 million square meters were installed. But several fires involving ETIC systems with polystyrene foam (EPS) insulation in Germany led to an extensive discussion about fire safety of such systems. A collection initiated by the Frankfurt fire service of façade fires which include polystyrene insulation foam1 shows that more than two thirds of all reported fires started in front of buildings. In half of these fires burning waste containers were the first burning objects. Consequently, German building authorities called for tests of existing approved ETIC systems with EPS insulation in a fire Scenario representing a burning waste container. As these tests revealed weaknesses in the existing ETIC systems measures were introduced to enhance the systems. However, the recently introduced German test standard DIN 4102‐20 does not take These changes into account. The DIN test represents a fire where flames emerge an opening but is downscaled regarding the size of the fire load and therefore does not represent a fully developed fire in a room. In ETIC systems with EPS insulation, the render is an important factor for the fire performance of these systems as collapse of the render usually leads to very rapid fire development. Intermediate scale tests with ETICs specimens indicate that mechanical damages of the render weaken the System significantly. Challenges and possible measures to enhance fire safety of ETIC systems are discussed.
Severe fires at the Friedrichshain flak bunker in May 1945 destroyed or severely damaged an important part of the collection of the Kaiser-Friedrich-Museum, Berlin, today’s Bode Museum. Fragments of two marble sculptures by Tullio Lombardo, sculptor of the Italian renaissance, have survived and are now stored in the Bode Museum. In preparation for restoration, the condition of the sculptures has been documented in detail in 2010. The study revealed that the fragments are not stable enough to exhibit them in a horizontal nor in an upright position. The intention of a further study in 2012 was to find a correlation between ultrasonic velocity and mechanical properties of burned Carrara marble as a basis for stabilization measures. The results and numerous supplementary experiments show that the current condition of the sculptural fragments can not only be explained by the exposure to fire.