Filtern
Erscheinungsjahr
Dokumenttyp
- Vortrag (106) (entfernen)
Sprache
- Englisch (106)
Referierte Publikation
- nein (106)
Schlagworte
- Hydrogen (106) (entfernen)
Organisationseinheit der BAM
- 9 Komponentensicherheit (49)
- 9.0 Abteilungsleitung und andere (27)
- 3 Gefahrgutumschließungen; Energiespeicher (26)
- 9.4 Integrität von Schweißverbindungen (22)
- 3.5 Sicherheit von Gasspeichern (21)
- 2 Prozess- und Anlagensicherheit (13)
- 2.1 Sicherheit von Energieträgern (13)
- 8 Zerstörungsfreie Prüfung (11)
- 9.5 Tribologie und Verschleißschutz (9)
- 1 Analytische Chemie; Referenzmaterialien (6)
Based on the initial call in March 2024, an update time-frame is introduced on the working plan for a comprehensive review paper series on joining and welding technologies for the manufacturing of components and parts used in sustainable energy generation, conversion, and transport with focus on hydrogen and wind energy.
Characterization of Hydrogen Diffusion in a Thick-walled Submerged Arc Multi-Layer Weld Joint
(2021)
The energy production of the future will be dominated by CO2-emission free techniques like wind turbines and become essential in scope of the planned hydrogen economy. As onshore installation capacity is limited, the in-crease of the number of offshore wind turbines (OWT) is a major goal. In that connection, the OWTs continuously increase in size and weight and demand adequate foundations concepts like monopiles or tripods. These compo-nents are typically manufactured from welded mild steel plates with thickness up to 200 mm. The predominant welding technique is submerged arc welding (SAW) with up to five wires. In accordance with the standards, the occurrence of delayed hydrogen assisted cracking is anticipated by either a hydrogen removal heat treatment (HRHT) or a so-called minimum waiting time (MWT) before non-destructive testing (NDT) of the respective weld joint is allowed. The reason for the MWT is the necessary time for the hydrogen diffusion at ambient temperature due the high plate thickness. Both the effectiveness of a HRHT at elevated temperatures or the MWT at ambient temperature can be estimated by calculation of the diffusion time. This time depends on reliable hydrogen diffu-sion coefficients and these are rare in literature. For that reason, this study presents the hydrogen diffusion coef-ficients obtained from a multi-layer SAW joint of an offshore steel grade. Two different experimental techniques were used to identify the respective diffusion behavior: (1) hydrogen desorption experiments with a carrier gas hot extraction analyzer at elevated temperatures for the characterization of a HRHT and (2) the electrochemical permeation technique at ambient temperature for the characterization of an MWT. From both experiments, the respective diffusion coefficients were calculated. The obtained DCs are different from those reported in literature, i.e., the duration or applicability of a HRHT or MWT must be critically discussed.
High-strength low-alloyed (HSLA) steels with yield strength ≥ 690 MPa are gaining popularity in civil engineering and construction of heavy vehicles. With increasing yield strength, the susceptibility for degradation of the mechanical properties in presence of diffusible hydrogen, i.e. hydrogen-assisted cracking (HAC) generally increases. HAC is a result of the critical interaction of local microstructure, mechanical load and hydrogen concentration. In existing standards for welding of HSLA steels, recommendations like working temperatures and dehydrogenation heat treatment (DHT) are given to limit the amount of introduced hydrogen during welding. The recommendations are based on investigations with conventional arc welding processes. In the past decade, modern weld technologies were developed to enable welding of narrower weld seams with V-grooves of 30°, e.g. the modified spray arc process. In that connection, a reduced number of weld runs and weld volume are important technical and, hence, economic benefits. In the present study, the hydrogen distribution in S960QL multi-layer welds with thickness of 20 mm was analyzed. The influence of different weld seam opening angles, heat input, working temperature and DHT was investigated. The results show that weldments with narrow groove contained increased diffusible hydrogen amount. Hydrogen concentration has been reduced by decreasing both the heat input and working temperature. Hydrogen free weldments were only achieved via subsequent DHT after welding. Furthermore, hydrogen distribution was experimentally determined across the weld seam thickness in HSLA GMA welded multi-layer welds for the first time.
Effect of weld penetration depth on hydrogen-assisted cracking of high-strength structural steels
(2019)
The need for steels with highest mechanical properties is a result of the increasing demands for energy and resource efficiency. In this context, high-strength structural (HSS) steels are used in machine, steel and crane construction with yield strength up to 960 MPa. However, welding of HSS steels requires profound knowledge of three factors in terms of avoidance of hydrogen-assisted cracking (HAC): the interaction of (1) microstructure, (2) local stress/strain and (3) local hydrogen concentration. In addition to the three main factors, the used weld-arc process is also important for the performance of the welded joint, especially when using modern arc variants. In the past, the conventional transitional arc process (Conv. A) was mainly used for welding of HSS grades. In the past decade, the so-called modified spray arc process (Mod. SA) has been used increasingly for welding production. This modified process enables reduced seam opening angles with increased deposition rates compared to the conventional process. Economic benefits of using this arc type are: a reduced number of necessary weld beads and a lower weld seam volume, which result in decreased total welding time and costs. Nonetheless, investigations on a high-strength S960QL showed significantly higher hydrogen concentrations in the weld metal at a reduced seam opening angle with Mod. SA. This indicates an increased susceptibility of the welded component to HAC. Hence, existing recommendations on HAC-avoidance cannot be transferred directly to the Mod. SA-process. In the present study, the susceptibility to HAC of the HSS steel S960QL with same type of filler material was investigated. For that purpose, both Conv. A and Mod. SA were used with same heat input at different deposition rates. For assessment of the HAC susceptibility, the externally loaded implant test was used. Both conducted test series with Conv. A and Mod. SA showed similar crack critical stress of about 280 MPa. Below this value, no delayed fracture appeared. The welds with Mod. SA showed higher hydrogen concentrations. The fracture occurred in the heat-affected zone (HAZ) or in the weld metal (WM). However, the test series with Mod. SA showed a significant extension of the time to failure of several hours compared to tests carried out with Conv. A.
Metallic organic frameworks are the materials stirring great interest by their large variety of structure types and chemical composition as well as low density and very high surface area, which are desirable properties for gas storage such as for hydrogen, methane or carbon dioxide. Using different so called secondary building units offer an opportunity to form tunable structures with channels of various geometry and allow in this way to study the absorption of the molecular hydrogen, methane or carbon dioxid in the systematic way.
The subject of permeation of hoses according to ISO 3821 for
hydrogen was discussed for a long time in ISO/TC 44/SC 8. The reason
is a considerable leakage of hydrogen diffused into the hose material
over the end face of the hose. Because of this unsolved, safety-related
problem of hoses sold on the market, measurements should be carried
out in order to be able to better assess the problem. BAM has declared
its attendance to provide a required fast solution to this issue.
A conclusion on the WIPANO research project "Safety of Prestressing Steel" was presented in the final committee meeting at the end of the project. The project's exciting findings and recommendations for a new method were discussed with the audience of national and international stakeholders of the prestressing steel industry and representatives of inspection bodies and standardization.
This talk reports the findings of the WIPANO "Knowledge and Technology Transfer via Patents and Standards" research project "Safety of Prestressing Steels," founded by the German Ministry of Economic Affairs and Climate Action (BMWK). A new test method for assessing the susceptibility of prestressing steels to hydrogen-induced stress corrosion cracking (SCC) is presented, which serves the demands of a lower scattering compared with the present standard. Moreover, the ability to differentiate between high susceptible and low susceptible prestressed wires is possible, modifying the method by hydrogen charging and surface preparation.
Hydrogen plasma treatment of iron ores or iron oxide containing wastes can be an efficient option to produce green iron e.g. for steel production. This way iron oxide is reduced to metallic iron in the liquid form by the highly reactive species that are formed in a hydrogen plasma. Hydrogen plasma can be used at the same time to remove undesired gangue elements. The presentation shows the experimental setup, shows first results of iron ore reduction by hydrogen plasma and gives an outlook for industrial application of the technology.
The polymer chemical structure of the polyimide has a major influence on the tribological behaviour. The addition of graphite in PI2 has a beneficial effect in hydrogen on the friction and wear. The low friction of graphite is associated with a lubricant film in hydrogen. The influence of hydrogen on graphite is more effective than humidity. CNTs have a similar effect to that of graphite in PEEK composites. TiO2 particles improve significantly the wear rate both in vacuum and hydrogen environment. In LH2 friction and wear decrease for unfilled polymers. Friction of graphite filled composites increases slightly and wear rate is stable.