Filtern
Erscheinungsjahr
Dokumenttyp
- Vortrag (78) (entfernen)
Referierte Publikation
- nein (78)
Schlagworte
- Welding (24)
- Hydrogen (22)
- Wasserstoff (11)
- Schweißen (8)
- Fügetechnik (7)
- Diffusion (6)
- High-entropy alloy (6)
- Mechanical properties (6)
- Forschung (5)
- Microstructure (5)
Organisationseinheit der BAM
- 9 Komponentensicherheit (53)
- 9.0 Abteilungsleitung und andere (41)
- 9.4 Integrität von Schweißverbindungen (37)
- 9.2 Versuchsanlagen und Prüftechnik (10)
- 6 Materialchemie (2)
- 6.2 Material- und Oberflächentechnologien (2)
- 8 Zerstörungsfreie Prüfung (2)
- 5 Werkstofftechnik (1)
- 5.1 Mikrostruktur Design und Degradation (1)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (1)
Microalloying elements such as Nb and Ti play a decisive function in achieving the desired mechanical strength of quenched and tempered, high-strength fine-grain structural steels with a nominal yield strength ≥ 690 MPa. The current specifications for the chemical composition only provide manufacturers with upper limits. However, even minor deviations in the alloy concept can have a significant impact on the mechanical properties. Consequently, accurate prediction of weldability and the integrity of welded joints becomes difficult or even impossible due to differences in composition and the resulting microstructures. Undesirable consequences include a possible softening of the heat-affected zone (HAZ) or, conversely, hardening effects. In view of these challenges, various microalloying strategies with different Ti and Nb contents are being systematically investigated for the first time using specially developed laboratory casting alloys. Each alloying route is based on the common S690QL, maintaining both the chemical composition and the heat treatment parameters. To analyse the weldability, three-layer welds were performed using gas metal arc welding (GMAW) and critical microstructures, such as areas of the heat-affected zone (HAZ) that exhibit significant softening or hardening, were identified. The effect of the softened HAZ region on failure was evaluated using transverse tensile specimens. Digital image correlation (DIC) is used to image changes in local strains in different HAZ regions in situ. Using a specially developed mirror system, the local strains of the microstructure zones on the top and bottom of the weld are recorded simultaneously. This makes it possible to analyse how the weld seam geometry (e.g., V-seam) influences the strain gradients. In addition, the analysis of the local deformation helps to understand the effects of the softened HAZ on the global strain, the fracture constriction, the fracture position, and the overall fracture behavior.
Offshore-Windenergieanlagen erfordern Gründungskonzepte aus unterpulver-(UP-)geschweißten Dickblechen (bspw. der Güte S420ML). Während der Schweißfertigung kann eine zeitverzögerte wasserstoffunterstützte Kaltrissbildung auftreten, deren Bewertung aufgrund der Bauteilgröße von Offshore-Strukturen sehr komplex ist. Deswegen wurde eine bauteilähnliche Geometrie (Mock-Up) entwickelt, um reale Steifigkeitsverhältnisse auf den Labormaßstab zu übertragen. Zusätzliche Versteifungen simulieren die Wirkung einer Einspannung bzw. Schrumpfbehinderung der Schweißnaht. Über die Verwendung von Schweißpulvern mit definierter Feuchte wurden zudem ein Extremszenario der Wasserstoffaufnahme simuliert. Entsprechend der vorgegebenen Mindestwartezeit für die ZfP von bis zu 48 h wurde die Schweißnaht zerstörungsfrei mit Phased-Array-Ultraschall-Prüfung (PAUT) geprüft und die Eigenspannungen über Röntgendiffraktometrie (XRD) bestimmt. Zusätzlich wurde die Wasserstoffverteilung in der Schweißverbindung numerisch simuliert. Außer zulässigen Defekten (wie Poren), wurde keine verzögerte Kaltrissbildung in den Mock-Ups festgestellt, was auf hohe Rissbeständigkeit hindeutet.
The hydrogen economy requires large-scale storage and transportation options like long-distance transmission pipelines. The applied materials (typically steels) must be carefully tested under different conditions (pressure, temperature, impact of impurities, etc.) for their suitability and service with hydrogen. In combination with mechanical load, as occurs in every gas network, hydrogen can induce degradation of the mechanical properties and promote finally resulting in embrittlement, i.e., the formation of cracks. The conventional testing procedures consist of autoclaves in which samples are strained under pressurized hydrogen. The test apparatus requires large amounts of hydrogen and thus a high level of safety and costs. In very specific cases, these tests might be replaced by simplified electrochemical charging. However, these test alternatives raise several questions regarding the equivalency of both testing scenarios. In the early 1980’s the idea of a so-called hollow tensile sample raised and was reinitiated 2021 in ISO TC 164 by T. Ogata (NIMS, Japan) and further developed (e.g. by Fraunhofer IWM, Germany). The idea was: the sample itself represents the autoclave instead of charging a sample from outside. For that reason, a hole is drilled through the sample and the inner surface is pressurized by hydrogen gas during the mechanical testing. Indeed, this represents the main advantage as no expensive pressure-resistant autoclave equipment for large H-volumes is necessary, which significantly reduces the safety-related issues and thus the high costs. In the following, we show recent activities at BAM Berlin on adaption of the hollow-specimen technique for slow strain rate testing (SSRT). The current research activities are focussed on macroscopic influences like the sample geometry, minimum necessary dimensions, and microscopic influences e.g., on the surface by the processing method (drill hole quality and geometric precision) as well as the gas pressure effect (mechanical deformation of surface in different media).
Microalloying elements, such as Nb and Ti, are essential for the targeted mechanical strength of quenched and tempered, high-strength fine-grained structural steels with a nominal yield strength ≥ 690 MPa. Current specifications for chemical composition only provide upper limits for manufacturers. But even small deviations in the alloying route can have a drastic effect on the mechanical properties. Thus, an adequate prediction of the weldability and the integrity of the welded joint becomes difficult or even impossible due to the varying composition and, hence, the microstructures. Undesirable side effects are the possible softening of the heat-affected zone (HAZ) as well as the opposite effect of hardening. Against this background, different microalloying routes with varying Ti and Nb contents are systematically investigated for the first time on specially designed lab-cast alloys. The basis of each alloy route was the common S690QL in terms of both the chemical composition as well as the heat treatment. To investigate the weldability, three-layer welds were performed using metal active gas welding (MAG) and critical microstructural areas with high softening/hardening were identified. The scope was here on the identification of phase transformations during cooling and on the respective metallurgical precipitation behavior. Isothermal and non-isothermal phase calculations were performed using Thermo-Calc® and showed that the prediction of the non-equilibrium precipitation characteristics during welding is not trivial, especially for this relatively complex chemical composition. The mechanical properties of the welded joints were identified by both Charpy tests (toughness) and tensile tests (strain and strength). During the test, the local straining behavior of the welded joints, was identified using a digital image correlation (DIC) system, see Figure 1. Despite the generally good weldability of the materials, the results show a significant influence of the microalloying route as well as the welding heat input on the different precipitation kinetics.
Dissimilar metal TIG weld joints of multiple principal element alloys (MPEA) to austenitic steel 304
(2023)
Multi-element alloys (MPEA - Multiple Principal Element Alloys) represent a new class of materials consisting of at least three alloying elements, each with 5 to 35 atomic %. This material class includes high-entropy alloys (HEA, with n ≥ 4 elements). The underlying alloying concept differs fundamentally from conventional materials such as the Fe-based steel. For this purpose, the alloying elements are specifically selected, and the microstructures are adjusted in a single-phase and, in some cases, multi-phase manner. The aim is to identify highly innovative MPEA with individually adjustable properties for industrial applications. In the last 20 years, however, the focus has been on pure material synthesis. With the increase in available material quantities, the focus is on processing issues such as joining and welding processes. In that connection, the weldability of MPEAs has received very little attention so far. Experience with dissimilar metal welds (DMWs) is completely lacking but is essential for the application of these materials if joint to conventional materials. This study presents selected experimental results on the weldability of MPEA-DMWs and the resulting microstructures. For this purpose, the equiatomic CoCrFeMnNi (HEA) was investigated in cold-rolled (CR) and heat-treated (HT) condition and joined by tungsten inert gas (TIG) welding to an austenitic stainless steel 304. The DMWs showed defect-free conditions (no lack of fusion, cracks and so on), whereas the cold-rolling increases the microhardness. The global mechanical properties were obtained by instrumented tensile tests of cross-weld samples and showed sufficient yield and tensile strength comparable to that of the individual base materials (BM). The local strain conditions were determined by digital image correlation and showed the highest local strains to occur in the intermixed weld metal. Indeed, the preferred fracture location of the cross-weld tensile samples was in the weld metal. Finally, the experiments proofed the weldability of the MPEAs to conventional 304. This enables targeted further considerations for example as structural materials.
Die Wasserstoffinfrastruktur ist eine zentraler Bestandteil der erfolgreichen Umsetzung der wasserstoffbasierten Energiewende. Dabei bilden Ferngasleitungen quasi das "Rückgrat" der Transportinfrastruktur großer Gasmengen. Dabei müssen unter Umständen Reparaturen an den Pipelines durchgeführt werden. Dabei ist in der Erdgasinfrastruktur das Schweißen an in Betrieb befindlichen (d.h. von Gas durchflossenen) Pipelines Stand der Technik. Es ist jedoch vollkommen offen, inwieweit diese Technik auf die reine Wasserstoffpipelines übertragbar sind. Hierzu leistet das Projekt H2SuD wichtige Beiträge zur Aufklärung des Einfluss eines Reparaturschweißprozesses auf die Wasserstoffaufnahme und Degradation im Betrieb befindlicher H2 Gasleitungen.
Der Vortrag gibt einen kurzen Überblick über die Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige Herausforderungen. Fügetechnologien, insbesondere die Schweißtechnik, haben dabei wesentliche Bedeutung für die Umsetzung von technischen Komponenten der Wasserstofftechnologien. Forschungsschwerpunkte ergeben sich insbesondere für die Erzeugung und den Transport des Wasserstoffs.
This study gives an overview on the important field of joining processes for component fabrication in hydrogen technologies. The current main issues and future perspectives are highlighted for the different technological field of hydrogen generation, storage, transport and use. In addition, the emerging field of additive manufacturing is included. Some remarks are given for standardization and regulations.
Large scale hydrogen assisted cracking test for thick walled SAW joints for offshore applications
(2023)
Offshore wind turbines continuously increase in size and weight and demand adequate offshore foundations concepts like monopiles, tripods or jackets. These components are typically submerged arc welded (SAW) high-strength thick steel plates like the S420ML. During welding, the occurrence of delayed hydrogen assisted cracking (HAC) must be anticipated. HAC is a critical combination of the local hydrogen concentration within a susceptible microstructure under certain mechanical load, i.e., the occurring (welding) residual stresses. The welding sequence of the thick-walled plates complicate the residual stress distribution due to the necessary repeated thermal cycling, i.e., welding seam / layer deposition to fill the joint. For that purpose, SAW with two-wire-technique was used to weld a specially designed and prototype-like mock-up of a real component with a thickness of 50 mm, filled with 22 passes and a seam length of 1,000 mm. Additional welded stiffeners simu-lated the effect of a high restraint, to stimulate critical HAC conditions. The necessity of a minimum waiting time (MWT) before the NDT can be conducted (to exclude HAC) was critically verified by the application of ultrasonic testing of the welded joint at different time-steps of the NDT of 48 h after welding. The residual stresses were determined by a robot XRD goniometer. Tensile residual stresses up to the yield limit are found both in the weld metal and in the heat-affected zone. Numerical modelling allowed the qualitative estimation of the hydrogen diffusion in the weld. A remarkable HAC occurrence was not identified and proves both, a certain resistance of the weld joint to HAC and the (questionable) duration of the MWT.
Die Umstellung der Wirtschaft auf wasserstoffbasierte Energieversorgung soll in Deutschland vor allem auf Basis der Umstellung des bestehenden Erdgasnetzes erfolgen. Dabei sollen ca. 90 % dieser Fernleitungsnetze auf dem bestehenden Erdgasnetz basieren. Die Beimischung von Wasserstoff zum Erdgas als auch der reine Wasserstofftransport werfen jedoch die Frage auf, ob und wie kompatibel die eingesetzten Materialien sind. Die Reparatur- und Erweiterungsfähigkeit von Erdgas-Bestandspipelines ist zu klären, wenn diese auf Wasserstoff umgestellt werden. Denn gerade Gashochdruckleitungen müssen regelmäßig gewartet und erweitert werden, um einen ordnungsgemäßen Betrieb sicherzustellen. Insbesondere das Schweißen unter Betriebsdruck bzw. an in Betrieb befindlichen Gasleitungen ist eine der wichtigsten Instandhaltungstechnologien, unabhängig von der Zusammensetzung des geförderten Mediums. Es ist daher dringend notwendig, eine geeignete Teststrategie zu erarbeiten, welche die nötigen Vorrausetzungen für sicheres Schweißen an in Betrieb befindlichen Druckwasserstoffleitungen schafft und entsprechende Kriterien für die Praxis liefert. Im Projekt H2-SuD - Einfluss des Schweißens auf die Wasserstoffaufnahme und Degradation im Betrieb befindlicher H2-Ferngasleitungen - soll geklärt werden, ob und wie stark mit einer Eigenschaftsdegradation geschweißter Rohrstähle in Gasnetzen in Folge einer Wasserstoffaufnahme zu rechnen ist. Die Präsentation gibt dazu einen kurzen Überblick über den aktuellen Status des Projektes. Die Förderung erfolgt im Rahmen der DVGW-Innovationsprogammes Wasserstoff (Nr. G 202131).