Filtern
Dokumenttyp
Sprache
- Deutsch (8)
- Englisch (8)
- Mehrsprachig (1)
Schlagworte
- Thermal shock (3)
- Ceramics (2)
- Weibull statistics (2)
- Acoustic emission (1)
- Active thermography (1)
- Advanced ceramic (1)
- Copper substrate (1)
- Different media (1)
- Differential scanning calorimetry (1)
- Elastische Energie (1)
- Emission coefficient (1)
- Environmental media (1)
- Fraktographie (1)
- Hochtemperaturanwendungen (1)
- Hydrogen storage materials (1)
- Laser (1)
- Laser irradiation (1)
- Laser-thermal shock (1)
- Local thermal excitation (1)
- Mechanical milling (1)
- Nanocomposite hydrides (1)
- Oxidation protection (1)
- Radiation thermometry (1)
- Rocket engine (1)
- Rule-of-mixtures (1)
- SSiC (1)
- Schichtherstellung (1)
- Schichttestung (1)
- Stress distribution (1)
- Temperature measurement (1)
- Thermal barrier coating (1)
- Thermal barrier coating (TBC) (1)
- Thermal shock stress (1)
- Thermal transport (1)
- Thermography (1)
- Thermoschock (1)
- Water transport (1)
- Wood preservatives (1)
- X-ray diffraction (1)
- Yttria stabilized zirconia (1)
Eingeladener Vortrag
- nein (4)
In rocket engine combustion chambers, the cooling channels experience extremly high temperatures and environmental attack. Thermal protection can be provided by Thermal Barrier Coatings. Due to the need of good heat conduction, the inner combustion liner is made of copper. The performance of a standard coating system for nickel based substrates is investigated on copper substrates.
Thermal cycling experiments are performed on the coated samples. Due to temperature limitations of the copper substrate material, no thermally grown oxide forms at the interface of the thermal barrier coating and the bond coat. Delamination of the coatings occurs at the interface between the substrate and the bond coat due to oxide formation of the copper at uncoated edges. In real service a totally dense coating can probably not be assured which is the reason why this failure mode is of importance. Different parameters are used for thermal cycling to understand the underlying mechanisms of delamination. Furthermore, laser heating experiments account for the high thermal gradient in real service. Pilot tests which led to a delamination of the coating at the substrate interface were performed successfully.
Der vorliegende Beitrag beschreibt typische Bruchmuster, die an SSiC Proben nach Thermoschockexperimenten beobachtet wurden und korreliert diese qualitativ mit der aufgebrachten Belastung. Der Thermoschock wird durch eine schnelle, in der Probenmitte beginnende spiralförmige Aufheizung dünner Scheiben mit Laserstrahlung realisiert. Durch diese Versuchsführung wandert ein zunehmender Temperaturgradient von der Mitte beginnend in radialer Richtung durch die Probe. Dieser Temperaturgradient ist für die Ausbildung von Druckspannungen im Probeninneren und Zugspannungen im kalten Randbereich der Probe verantwortlich. Beim Erreichen einer kritischen, versagensrelevanten Spannung tritt Probenbruch auf. Dabei wird die bis zu diesem Zeitpunkt in der Probe gespeicherte elastische Energie teilweise in die Schaffung von Rissoberflächen umgewandelt. Der Zusammenhang zwischen gespeicherter elastischer Energie und Bruchmuster wird dargestellt.
The determination of critical failure parameters during thermal shock requires a time and space resolved temperature measurement of the sample. High frequency pyrometry is a suitable technique for such a measurement task, which usually requires the knowledge of the optical properties of the investigated material. Another challenge is the infrared transparency of materials to be checked in the wavelength range of the pyrometer. The thermal shock disks are very thin, due to the need of homogeneous temperature distribution and to maintain a two-dimensional problem. To allow a pyrometric temperature measurement a universal calibration method for high frequency infrared cameras has been developed. Pyrometry in various media was demanded, as well as the estimation of optical properties (reflection, transmittance and emission) for the selected ceramics to be tested.
The thermal shock behavior of three commercial-advanced ceramics (SSiC, MgO–PSZ, Al2O3) is characterized in air and vacuum applying a laser thermal shock. The available testing system permits the reproducible setting of defined temperature profiles in thin disks and allows a heating-up thermal shock in various media. Due to the accurate determination of the time- and space-resolved temperature distribution, the local stress state can be calculated as a function of time. It is shown that the thermal shock strength is highest for SSiC and lowest in Al2O3 with MgO–PSZ in between. The approach presented in this work allows quantifying the stress state at failure in terms of tangential tensile stress. The investigated environment does not affect the thermal shock resistance under the studied experimental conditions.
Laser thermal shock experiments - performance and evaluation on the basis of advanced ceramics
(2011)
The thermal shock behaviour in air and vacuum of three different advanced ceramics is investigated by introducing a new testing method. This thermal shock testing system permits the reproducible setting of defined temperature profiles in thin disks. In order to perform heating - up thermal shock experiments under reproducible conditions and to measure the transient temperature fields, a laser beam is directed spirally across the surface of the specimen. In this process, the specimen is heated up faster than the temperature gradient is compensated by thermal conductivity. Resulting temperature fields were recorded space and time resolved. Based on the knowledge of the local temperature distribution at the moment of failure, the critical fracture stress can be calculated. The scatter of thermal shock strength is quantitatively determined for the tested ceramics by using a improved statistical method.