The formation of magnesium fluoride sols and xerogels according to the fluorolytic sol–gel synthesis based on the reaction of Mg(OMe)2 with non-aqueous HF has been thoroughly investigated by X-ray scattering (WAXS/XRD), TEM, SAXS, DLS and 19F MAS NMR spectroscopy. Mechanistic insights were gained by following the reaction progress and formation of intermediate phases of the fluorination of magnesium alkoxides. For F:Mg ratios of 0.3 and 0.4 the formation of two crystalline phases was observed containing the recently obtained compound [Mg6F2(OCH3)10(CH3OH)14] hexanuclear dicubane units. The stoichiometric reaction yields magnesium fluoride nanoparticles with crystallite sizes below 5 nm, which show broad reflections in the X-ray diffraction pattern. Metal fluoride sols prepared by this way undergo tremendous changes over the first several weeks after synthesis. Immediately after the fluorination, particles of about 120 nm—probably agglomerates—are formed, which break apart in the course of about one month of ageing and low-viscous, transparent sols with particles of about 12 nm are obtained. At the same time structural re-organisation processes within the magnesium fluoride particles are observed by an increase of the (110) reflection in WAXS.
CTAB-stabilized gold nanoparticles were synthesized by applying the seeding-growth approach in order to gain information about the size dependence of the catalytic reduction of p-nitrophenol to p-aminophenol with sodium borohydride. Five different colloidal solutions of stabilized gold nanoparticles have been characterized by TEM, AFM, UV-Vis, SAXS, and DLS for their particle size distributions. Gold nanoparticles (mean sizes: 3.5, 10, 13, 28, 56 nm diameter) were tested for their catalytic efficiency. Kinetic data were acquired by UV-Vis spectroscopy at different temperatures between 25 and 45 °C. By studying the p-nitrophenol to p-aminophenol reaction kinetics we determined the nanoparticle size which is needed to gain the fastest conversion under ambient conditions in the liquid phase. Unexpectedly, CTAB-stabilized gold nanoparticles with a diameter of 13 nm are most efficient.