Assessment of in-service welding conditions for pressurized hydrogen pipelines via component test
- Hydrogen is the energy carrier of tomorrow. This requires a reliable transport infrastructure with the ability to carry large amounts of hydrogen e.g. for steel industry or chemical industry. The conversion of existing natural gas (NG) grids is an essential part of the worldwide hydrogen strategies, in addition to the construction of new pipelines. In this context, the transportation of hydrogen is fundamental different from NG as hydrogen can be absorbed into the pipeline material. Given the well-known effects of hydrogen embrittlement, the compatibility of the materials for the intended pipelines must be investigated (typically low alloy steels in a wide range of strengths and thicknesses). However, pipelines require frequent maintenance, repair or the need for installation for further outlets. In some cases, it is necessary to perform welding on or onto the pipelines while they are still in service, i.e. with active gas flow under high pressure, e.g. such as the well-known “hotHydrogen is the energy carrier of tomorrow. This requires a reliable transport infrastructure with the ability to carry large amounts of hydrogen e.g. for steel industry or chemical industry. The conversion of existing natural gas (NG) grids is an essential part of the worldwide hydrogen strategies, in addition to the construction of new pipelines. In this context, the transportation of hydrogen is fundamental different from NG as hydrogen can be absorbed into the pipeline material. Given the well-known effects of hydrogen embrittlement, the compatibility of the materials for the intended pipelines must be investigated (typically low alloy steels in a wide range of strengths and thicknesses). However, pipelines require frequent maintenance, repair or the need for installation for further outlets. In some cases, it is necessary to perform welding on or onto the pipelines while they are still in service, i.e. with active gas flow under high pressure, e.g. such as the well-known “hot tapping”, see Fig. 1a. This in-service welding causes challenges for hydrogen operations in terms of additional hydrogen absorption during welding and the material compatibility. The challenge can be roughly divided into the possible austenitization of the inner pipe material exposed to hydrogen, which can lead to sufficient hydrogen absorption, and the welding itself, which causes an increased temperature range. Both lead to a significant increase in hydrogen solubility and diffusivity of the respective materials compared to room temperature. In this context, knowledge about hot tapping on hydrogen pipelines is scarce due to the lack of operating experience. Fundamental experimental investigations are required to investigate the transferability from NG to hydrogen pipeline grids. For this reason, the present study introduces a specially designed mock-up / demonstrator concept for the realistic assessment of the welding processing conditions, see Fig. 1b. The mock-up was designed to enable in-situ temperature measurement during welding as well as ex-post extraction of samples for the quantification of the absorbed hydrogen concentration, see Fig. 1c. For safety measures, the necessary pressurized hydrogen volume was limited by the insertion of a solid cylinder ensuring a 1 cm hydrogen gas layer. Welding experiments on the pressurized mock-ups with the diameters DN50 and DN200 have shown that the austenitization temperature can be reached on the inner surface of the pipeline, especially on thinner-walled pipelines, using current welding practices. This corresponds to an increased hydrogen uptake in the welded area of several ppm…


| Autor*innen: | Michael RhodeORCiD |
|---|---|
| Koautor*innen: | Kjell ErxlebenORCiD, Sebastian KaiserORCiD, C. Hadick, K. Schu, Thomas KannengießerORCiD |
| Dokumenttyp: | Vortrag |
| Veröffentlichungsform: | Präsentation |
| Sprache: | Englisch |
| Jahr der Erstveröffentlichung: | 2025 |
| Organisationseinheit der BAM: | 9 Komponentensicherheit |
| 9 Komponentensicherheit / 9.4 Integrität von Schweißverbindungen | |
| DDC-Klassifikation: | Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Ingenieurwissenschaften und zugeordnete Tätigkeiten |
| Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Angewandte Physik | |
| Freie Schlagwörter: | Component test; Hydrogen; In-service welding; Pipeline |
| Themenfelder/Aktivitätsfelder der BAM: | Energie |
| Energie / Wasserstoff | |
| Material | |
| Material / Degradationsmechanismen | |
| Veranstaltung: | 1st Conference on Hydrogen in Materials Science and Engineering (H2-MSE) |
| Veranstaltungsort: | Siegburg, Germany |
| Beginndatum der Veranstaltung: | 11.02.2025 |
| Enddatum der Veranstaltung: | 13.02.2025 |
| Verfügbarkeit des Dokuments: | Datei im Netzwerk der BAM verfügbar ("Closed Access") |
| Datum der Freischaltung: | 13.02.2025 |
| Referierte Publikation: | Nein |
| Eingeladener Vortrag (wissenschaftliche Konferenzen): | Nein |