Mechanical Strength and Corrosion Rate of Aluminium Composites (Al/SiO2): Nanoparticle Silica (NPS) as Reinforcement

  • The fabrication and characteristics of amorphous silica reinforced Al matrix composites are studied in this paper. The major starting materials were commercial Al powder and extracted nanoparticle SiO2 (NPS) powder from Indonesian silica sands. Two different active solutions,namely N-butanol and tetramethylammonium hydroxide (TMAH), were introduced during synthesis. Characterisations in terms of physical, mechanical, microstructural and corrosion rate examinations were also employed. Introducing the SiO2 nanoparticles into the Al matrix has decreased the density and increased the porosity of the composites. The addition of N-butanol into Al/SiO2(Al/SiO2(B)) led to broader and lower X-ray diffraction profiles than the addition of TMAH (Al/SiO2(T)). From the microstructural analysis, we found that the SiO2 particles enter and agglomerate into the opening gap of the Al sheets. Furthermore, yield strength, ultimate compression strength and modulus of elasticity tended toThe fabrication and characteristics of amorphous silica reinforced Al matrix composites are studied in this paper. The major starting materials were commercial Al powder and extracted nanoparticle SiO2 (NPS) powder from Indonesian silica sands. Two different active solutions,namely N-butanol and tetramethylammonium hydroxide (TMAH), were introduced during synthesis. Characterisations in terms of physical, mechanical, microstructural and corrosion rate examinations were also employed. Introducing the SiO2 nanoparticles into the Al matrix has decreased the density and increased the porosity of the composites. The addition of N-butanol into Al/SiO2(Al/SiO2(B)) led to broader and lower X-ray diffraction profiles than the addition of TMAH (Al/SiO2(T)). From the microstructural analysis, we found that the SiO2 particles enter and agglomerate into the opening gap of the Al sheets. Furthermore, yield strength, ultimate compression strength and modulus of elasticity tended to reduce the addition of SiO2. The corrosion rate of Al/SiO2(T) was lower than that of Al/SiO2(B) composites.zeige mehrzeige weniger

Volltext Dateien herunterladen

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen: Munasir, Triwikantoro, M. Zainuri, Ralph BäßlerORCiD, Darminto
Dokumenttyp:Zeitschriftenartikel
Veröffentlichungsform:Verlagsliteratur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):Journal of Physical Science
Jahr der Erstveröffentlichung:2019
Organisationseinheit der BAM:7 Bauwerkssicherheit
7 Bauwerkssicherheit / 7.6 Korrosion und Korrosionsschutz
Veröffentlichende Institution:Bundesanstalt für Materialforschung und -prüfung (BAM)
Verlag:USM Press
Verlagsort:Pulau Pinang, Malaysia
Jahrgang/Band:30
Ausgabe/Heft:1
Erste Seite:81
Letzte Seite:97
DDC-Klassifikation:Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Ingenieurwissenschaften und zugeordnete Tätigkeiten
Freie Schlagwörter:Al/SiO2 composite; Aluminium; Corrosion rate; Mechanical strength; Silica
Themenfelder/Aktivitätsfelder der BAM:Material
DOI:10.21315/jps2019.30.1.7
URN:urn:nbn:de:kobv:b43-487185
ISSN:1675-3402
ISSN:2180-4230
Verfügbarkeit des Dokuments:Datei für die Öffentlichkeit verfügbar ("Open Access")
Lizenz (Deutsch):License LogoCreative Commons - CC BY - Namensnennung 4.0 International
Datum der Freischaltung:21.08.2019
Referierte Publikation:Nein
Schriftenreihen ohne Nummerierung:Wissenschaftliche Artikel der BAM
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.