Observation of the weld pool shape in partial penetration welding and its influence on solidification crack formation for high-power laser beam welding
- In this study, steel-glass experiments were conducted to observe the melt pool geometry using a high-speed camera. The high-speed recordings and optical flow analysis show that two main flows take place in form of vortices. The lower vortex drives the melt backwards from the front keyhole wall and thus causes an extension of the melt pool, which is called bulging. This bulging promotes solidification cracking by forming a closed area filled with melt and the accumulation of impurities in the final solidification phase, resulting in low-melting phases which are under tensile stress at the end of solidification.
Autor*innen: | Nasim BakirORCiD, Ömer Üstündag, Andrey GumenyukORCiD, Michael RethmeierORCiD |
---|---|
Dokumenttyp: | Beitrag zu einem Tagungsband |
Veröffentlichungsform: | Graue Literatur |
Sprache: | Englisch |
Titel des übergeordneten Werkes (Englisch): | Lasers in Manufacturing Conference 2021 |
Jahr der Erstveröffentlichung: | 2021 |
Organisationseinheit der BAM: | 9 Komponentensicherheit |
9 Komponentensicherheit / 9.3 Schweißtechnische Fertigungsverfahren | |
Erste Seite: | 1 |
Letzte Seite: | 5 |
DDC-Klassifikation: | Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Ingenieurwissenschaften und zugeordnete Tätigkeiten |
Freie Schlagwörter: | Laser beam welding; Partial penetration; Solidification craking; Weld pool shape |
Themenfelder/Aktivitätsfelder der BAM: | Material |
Veranstaltung: | Lasers in Manufacturing Conference 2021 |
Veranstaltungsort: | Online meeting |
Beginndatum der Veranstaltung: | 21.06.2021 |
Enddatum der Veranstaltung: | 21.06.2021 |
Verfügbarkeit des Dokuments: | Datei im Netzwerk der BAM verfügbar ("Closed Access") |
Datum der Freischaltung: | 25.10.2021 |
Referierte Publikation: | Nein |