Experimental and analytical investigation of high temperature fatigue crack growth at notches in a polycrystalline Nickel base superalloy

  • The scatter of fatigue crack growth data can become significant for coarse grained materials. By using a probabilistic description of crack propagation as the foundation of a lifetime prediction model, lifetime scatter of laboratory specimens can be reproduced. However, the lifetime of real components is subjected to additional scattering factors such as surface condition or uncertainty regarding direction and shape of emerging cracks. These factors need to be addressed in order to exploit the advantages of probabilistic description, i.e. the reduction of unnecessary conservatisms. High temperature LCF (Low-Cycle-Fatigue) tests were performed with center hole specimens of a coarse-grained Nickel base Superalloy. In addition, crack propagation tests with Double Edge Notch specimens were performed. A procedure to detect the shape of the starting crack that combines the potential drop method and induction thermography was developed. The geometry and the number of notches were varied.The scatter of fatigue crack growth data can become significant for coarse grained materials. By using a probabilistic description of crack propagation as the foundation of a lifetime prediction model, lifetime scatter of laboratory specimens can be reproduced. However, the lifetime of real components is subjected to additional scattering factors such as surface condition or uncertainty regarding direction and shape of emerging cracks. These factors need to be addressed in order to exploit the advantages of probabilistic description, i.e. the reduction of unnecessary conservatisms. High temperature LCF (Low-Cycle-Fatigue) tests were performed with center hole specimens of a coarse-grained Nickel base Superalloy. In addition, crack propagation tests with Double Edge Notch specimens were performed. A procedure to detect the shape of the starting crack that combines the potential drop method and induction thermography was developed. The geometry and the number of notches were varied. Moreover, specimen with different hole surface finishes were investigated, which showed a detrimental effect of the roughness of the hole surface. The results have been compared to predictions of a probabilistic tool for the estimation of lcf lifetime that has been calibrated beforehand on laboratory specimens with and without notches. In parallel, a fracture mechanics-based lifetime model was developed, which includes the initial crack size as a critical parameter. Thereby, the influence of the large grain size (>1mm), and the shape of the starting crack at the notch were considered. Acknowledgements The investigations are conducted as part of the joint research program COOREFLEX-Turbo in the frame of AG Turbo. The work is supported by Siemens AG and the Bundesministerium für Wirtschaft und Technologie (BMWi) as per resolution of the German Federal Parliament under grant number 03ET7071E.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • PresentationFedelich.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Bernard FedelichORCiD
Weitere Person:Adam Butz, Birgit RehmerORCiD, L. Mäde, S. Schmitz, M. Vöse
Dokumenttyp:Vortrag
Veröffentlichungsform:Präsentation
Sprache:Englisch
Jahr der Erstveröffentlichung:2022
Organisationseinheit der BAM:5 Werkstofftechnik
5 Werkstofftechnik / 5.2 Metallische Hochtemperaturwerkstoffe
5 Werkstofftechnik / 5.5 Materialmodellierung
DDC-Klassifikation:Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Ingenieurwissenschaften und zugeordnete Tätigkeiten
Freie Schlagwörter:LCF; Nickel-base superalloys; Notches
Themenfelder/Aktivitätsfelder der BAM:Material
Material / Degradation von Werkstoffen
Veranstaltung:Low Cycle Fatigue 9
Veranstaltungsort:Berlin, Germany
Beginndatum der Veranstaltung:21.06.2022
Enddatum der Veranstaltung:23.06.2022
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:21.07.2022
Referierte Publikation:Nein
Eingeladener Vortrag:Nein
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.