Thermal extraction combined with thermal desorption: A powerful tool to investigate the thermo-oxidative degradation of polyamide 66 materials

  • Using thermogravimetric analysis (TGA) with a solid-phase adsorber for thermal extraction, followed by subsequently analysing the adsorber with thermo-desorption gas chromatography mass spectrometry (TDS-GC–MS) enables measurement of polymer degradation under oxidizing atmosphere, and the identification of certain complex hydrocarbon degradation products by chromatographic separation and defined mass patterns. This technique, thermal-extraction desorption gas chromatography mass spectrometry (TED-GC–MS) was used to investigate the thermo-oxidative degradation of PA 66 and PA 66 doped with 2 wt% of metal oxide particles. In TGA pure PA 66 formed more residue under an oxidizing atmosphere than an inert one. In contrast to the measurements under inert atmosphere, several condensed aromatic species containing nitrogen could be identified in thermo-oxidative measurements. These degradation products were formed through condensation reactions of primary amides originating from imideUsing thermogravimetric analysis (TGA) with a solid-phase adsorber for thermal extraction, followed by subsequently analysing the adsorber with thermo-desorption gas chromatography mass spectrometry (TDS-GC–MS) enables measurement of polymer degradation under oxidizing atmosphere, and the identification of certain complex hydrocarbon degradation products by chromatographic separation and defined mass patterns. This technique, thermal-extraction desorption gas chromatography mass spectrometry (TED-GC–MS) was used to investigate the thermo-oxidative degradation of PA 66 and PA 66 doped with 2 wt% of metal oxide particles. In TGA pure PA 66 formed more residue under an oxidizing atmosphere than an inert one. In contrast to the measurements under inert atmosphere, several condensed aromatic species containing nitrogen could be identified in thermo-oxidative measurements. These degradation products were formed through condensation reactions of primary amides originating from imide hydrolysis. The formation of such highly condensed species also causes higher char formation. Four metal oxides have shown an impact on the thermo-oxidative degradation of PA 66: Fe2O3 on η-Al2O3 < pure Fe2O3 = Fe2O3 on γ-Al2O3 < pure ZnO. For ZnO even a char-stabilizing effect could be observed. A catalytic effect of these metal oxides causes more condensed cyclopentanone and pyridine derivates. Thus, more water is formed and released, resulting in increased hydrolysis of the imides and degradation at lower temperatures.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • 1-s2.0-S0165237015301157-main.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Erik Dümichen, Ulrike BraunORCiD, R. Kraemer, P. Deglmann, R. Senz
Dokumenttyp:Zeitschriftenartikel
Veröffentlichungsform:Verlagsliteratur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):Journal of analytical and applied pyrolysis
Jahr der Erstveröffentlichung:2015
Verlag:Elsevier B.V.
Verlagsort:Amsterdam
Jahrgang/Band:115
Erste Seite:288
Letzte Seite:298
Freie Schlagwörter:Metal oxide particles; PA 66; Solid-phase extraction; Thermo-oxidation; Thermogravimetry
DOI:10.1016/j.jaap.2015.08.006
ISSN:0165-2370
ISSN:1873-250X
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:20.02.2016
Referierte Publikation:Ja
Datum der Eintragung als referierte Publikation:05.10.2015
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.