Impact of saline aquifer water on surface and shallow pit corrosion of martensitic stainless steels during exposure to CO2 environment (CCS)
- Pipe steels suitable for carbon capture and storage technology (CCS) require resistance against the corrosive environment of a potential CCS-site, e.g. heat, pressure, salinity of the aquifer, CO2-partial pressure. Samples of different mild and high alloyed stainless injection-pipe steels partially heat treated: 42CrMo4, X20Cr13, X46Cr13, X35CrMo4 as well as X5CrNiCuNb16-4 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CO2-saturated synthetic aquifer environment similar to possible geological on-shore CCS-sites in the northern German Basin. Main corrosion products are FeCO3 and FeOOH. Corrosion rates obtained at 100 bar are generally much lower than those measured at ambient pressure. Highest surface corrosion rates are 0.8 mm/year for 42CrMo4 and lowest 0.01 mm/year for X5CrNiCuNb16-4 in the vapour phase at ambient pressure. At 100 bar the highest corrosion rates are 0.01 mm/year for 42CrMo4, X20Cr13 (liquid phase), X46Cr13 and less than 0.01Pipe steels suitable for carbon capture and storage technology (CCS) require resistance against the corrosive environment of a potential CCS-site, e.g. heat, pressure, salinity of the aquifer, CO2-partial pressure. Samples of different mild and high alloyed stainless injection-pipe steels partially heat treated: 42CrMo4, X20Cr13, X46Cr13, X35CrMo4 as well as X5CrNiCuNb16-4 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CO2-saturated synthetic aquifer environment similar to possible geological on-shore CCS-sites in the northern German Basin. Main corrosion products are FeCO3 and FeOOH. Corrosion rates obtained at 100 bar are generally much lower than those measured at ambient pressure. Highest surface corrosion rates are 0.8 mm/year for 42CrMo4 and lowest 0.01 mm/year for X5CrNiCuNb16-4 in the vapour phase at ambient pressure. At 100 bar the highest corrosion rates are 0.01 mm/year for 42CrMo4, X20Cr13 (liquid phase), X46Cr13 and less than 0.01 mm/year for X35CrMo4 and X5CrNiCuNb16-4 after 8000 h of exposure with no regard to atmosphere. Martensitic microstructure offers good corrosion resistance.…
Autor*innen: | Anja Pfennig, Axel KranzmannORCiD |
---|---|
Dokumenttyp: | Beitrag zu einem Tagungsband |
Veröffentlichungsform: | Graue Literatur |
Sprache: | Englisch |
Titel des übergeordneten Werkes (Englisch): | IOP Conference Series: Earth and Environmental Science |
Jahr der Erstveröffentlichung: | 2018 |
Organisationseinheit der BAM: | 5 Werkstofftechnik |
5 Werkstofftechnik / 5.1 Mikrostruktur Design und Degradation | |
Veröffentlichende Institution: | Bundesanstalt für Materialforschung und -prüfung (BAM) |
Verlag: | IOP Publ. |
Jahrgang/Band: | 150 |
Erste Seite: | 81 |
Letzte Seite: | 90 |
DDC-Klassifikation: | Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Angewandte Physik |
Freie Schlagwörter: | CCS; CO2 corrosion; Pipeline |
Themenfelder/Aktivitätsfelder der BAM: | Energie |
Veranstaltung: | 8th International Conference on Future Environment and Energy (ICFEE 2018) |
Veranstaltungsort: | Phuket, Thailand |
Beginndatum der Veranstaltung: | 10.01.2018 |
DOI: | 10.1088/1755-1315/150/1/012012 |
URN: | urn:nbn:de:kobv:b43-465896 |
Verfügbarkeit des Dokuments: | Datei für die Öffentlichkeit verfügbar ("Open Access") |
Lizenz (Deutsch): | Creative Commons - Namensnennung |
Datum der Freischaltung: | 19.11.2018 |
Referierte Publikation: | Ja |
Datum der Eintragung als referierte Publikation: | 19.11.2018 |
Schriftenreihen ohne Nummerierung: | Wissenschaftliche Artikel der BAM |