Comparison of the material parameters of polyethalene grades with the test performance behaviour of packagings for the transport of dangerous goods in relation to the pre-storage time with 55% nitric acid

  • The material parameters melt flow rate (MFR), density (D), notched impact strength (NIS) at –30°C, stress crack resistance [determined with the Full Notch Creep Test (FNCT)] and resistance to oxidative degradation (Ox) have been selected for a comparison of polyethylene grades in the European standard EN 15507. These parameters have a relationship with design type tests of packagings for the transport of dangerous goods. This paper presents the results of additional investigations to determine the impact of the pre-storage time of jerricans with 55% nitric acid at 40°C and 23°C on the marginal drop heights in drop tests at –18°C, on the MFR and on the tensile properties. Jerricans made of different polyethylene grades were pre-stored with 55% nitric acid for 21, 42 and 84 days at 40°C and for six months at 23°C. The tests showed that the NIS values at –30°C of polyethylene grades were not comparable with marginal drop heights determined in drop tests at –18°C. Pre-damage withThe material parameters melt flow rate (MFR), density (D), notched impact strength (NIS) at –30°C, stress crack resistance [determined with the Full Notch Creep Test (FNCT)] and resistance to oxidative degradation (Ox) have been selected for a comparison of polyethylene grades in the European standard EN 15507. These parameters have a relationship with design type tests of packagings for the transport of dangerous goods. This paper presents the results of additional investigations to determine the impact of the pre-storage time of jerricans with 55% nitric acid at 40°C and 23°C on the marginal drop heights in drop tests at –18°C, on the MFR and on the tensile properties. Jerricans made of different polyethylene grades were pre-stored with 55% nitric acid for 21, 42 and 84 days at 40°C and for six months at 23°C. The tests showed that the NIS values at –30°C of polyethylene grades were not comparable with marginal drop heights determined in drop tests at –18°C. Pre-damage with 55% nitric acid for 21 days at 40°C led to an increase in the marginal drop heights of the jerricans. Altering the test regulations by increasing pre-storage time with 55% nitric acid to 42 days would be an alternative. The test results demonstrated clearly that pre-storage of the jerricans for six months at 23°C caused a higher increase in the MFR and lower marginal drop heights for the jerricans when compared with pre-stored jerricans for 21 days at 40°C.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • Weltschev_et_al-2014-Packaging_Technology_and_Science.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Margit Weltschev, Ute Niebergall, Jan Werner
Dokumenttyp:Zeitschriftenartikel
Veröffentlichungsform:Verlagsliteratur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):Packaging technology & science
Jahr der Erstveröffentlichung:2013
Verlag:Wiley
Verlagsort:Chichester, UK
Jahrgang/Band:27
Erste Seite:409
Letzte Seite:421
Freie Schlagwörter:Drop tests; Nitric acid; Packagings for the transport of dangerous goods; Polyethylene grades; Resistance to oxidative degradation; Tensile properties
DOI:10.1002/pts.2037
ISSN:0894-3214
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:20.02.2016
Referierte Publikation:Ja
Datum der Eintragung als referierte Publikation:27.06.2013
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.