Material investigation and long-term sealing behavior of Helicoflex® metal seals used in containers for spent nuclear fuel

  • In Germany spent nuclear fuel is stored and transported in casks that possess bolted lid systems equipped with double jacket metal seals of Helicoflex® type in order to enable safe enclosure of the radioactive inventory. A dry interim storage period of 40 years was planned and the casks are licensed for that time span. However, due to political reasons and delayed disposal projects this time span is expected to increase significantly. It is therefore necessary to evaluate the long-term sealing behavior of the casks exceeding 40 years of operating time. In this paper, we discuss our approach to investigate the aging behavior of such metal seals, and to predict the long-term sealing behavior. Accelerated aging component tests with seals are performed at temperatures up to 150°C to investigate the course of seal force, useable resilience and leakage rate. Even though these tests have already shown a significant decrease in seal force and useable resilience after aging times of less thanIn Germany spent nuclear fuel is stored and transported in casks that possess bolted lid systems equipped with double jacket metal seals of Helicoflex® type in order to enable safe enclosure of the radioactive inventory. A dry interim storage period of 40 years was planned and the casks are licensed for that time span. However, due to political reasons and delayed disposal projects this time span is expected to increase significantly. It is therefore necessary to evaluate the long-term sealing behavior of the casks exceeding 40 years of operating time. In this paper, we discuss our approach to investigate the aging behavior of such metal seals, and to predict the long-term sealing behavior. Accelerated aging component tests with seals are performed at temperatures up to 150°C to investigate the course of seal force, useable resilience and leakage rate. Even though these tests have already shown a significant decrease in seal force and useable resilience after aging times of less than 1 year, for most seals the leakage rate stayed better than the specified value. However, observation of the leakage rate has to be continued to determine the aging effect on the seal properties. As a main influence on the seal long-term behavior the increasing permanent deformation of the outer jacket has been recognized. It is made of aluminum or silver which means that the temperatures that are relevant for the aforementioned application in casks lead to creep deformation. For further investigation of seal behavior a comprehensive research program concerning the material characteristics and aging behavior of the individual seal components, with an emphasis on the outer jacket material, has been launched. The aim is to get a better understanding of the time and temperature dependent creep mechanisms and deformation. The examinations are separated into tests on seal segments and tests on standardized specimen. In order to be able to study the aging process, seal segments are compressed in flanges and stored at temperatures ranging from room temperature to 150°C. After defined time intervals the segments are analyzed by using standardized tests including structure investigation and creep tests. The results are compared with the behavior of the specimen basic raw material. This is done to ensure comparability of the thin jacket material and additional sheet material used for standardized tests. Thus, the prediction of component changes after different aging times at different temperatures can be made. As a result forecasts on the long term seal behavior are intended.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • FinalPaper_17135_0114110259.pdf
    eng
  • Waste-Management-Symposia-2017.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Tobias Grelle, Dietmar Wolff, Ulrich Probst, Matthias JaunichORCiD, Holger Völzke
Dokumenttyp:Beitrag zu einem Tagungsband
Veröffentlichungsform:Graue Literatur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):Waste Management Symposia 2017 Proceedings
Jahr der Erstveröffentlichung:2017
Erste Seite:Article 17135, 1
Letzte Seite:8
DDC-Klassifikation:Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Angewandte Physik
Freie Schlagwörter:Creep; Long-term behavior; Metal seal
Veranstaltung:Waste Management Symposia
Veranstaltungsort:Phoenix, AZ, USA
Beginndatum der Veranstaltung:05.03.2017
ISBN:978-0-9828171-6-2
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:16.06.2017
Referierte Publikation:Nein
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.