What reacts with what in bisphenol A polycarbonate/silicon rubber/bisphenol A bis(diphenyl phosphate) during pyrolysis and fire behavior?
- The pyrolysis and flame retardancy of a bisphenol A polycarbonate/silicon rubber/bisphenol A bis(diphenyl phosphate) (PC/SiR/BDP) blend were investigated and compared to those of PC/BDP and PC/SiR. The impact modifier SiR consists mainly of poly(dimethylsiloxane) (PDMS > 80 wt %). The pyrolysis of PC/SiR/BDP was studied by thermogravimetry (TG), TG–FTIR to analyze the evolved gases, and a Linkam hot stage cell within FTIR as well as 29Si NMR and 31P NMR to analyze the solid residue. The fire performance was determined by PCFC, LOI, UL 94, and a cone calorimeter under different external irradiations. The fire residues were studied by using ATR-FTIR as well as the additional binary systems PC + PDMS, PC + BDP, and BDP + PDMS, focusing on the specific chemical interactions. The decomposition pathways are revealed, focusing on the competing interaction between the components. Fire retardancy in PC/SiR/BDP is caused by both flame inhibition in the gas phase and inorganic-carbonaceousThe pyrolysis and flame retardancy of a bisphenol A polycarbonate/silicon rubber/bisphenol A bis(diphenyl phosphate) (PC/SiR/BDP) blend were investigated and compared to those of PC/BDP and PC/SiR. The impact modifier SiR consists mainly of poly(dimethylsiloxane) (PDMS > 80 wt %). The pyrolysis of PC/SiR/BDP was studied by thermogravimetry (TG), TG–FTIR to analyze the evolved gases, and a Linkam hot stage cell within FTIR as well as 29Si NMR and 31P NMR to analyze the solid residue. The fire performance was determined by PCFC, LOI, UL 94, and a cone calorimeter under different external irradiations. The fire residues were studied by using ATR-FTIR as well as the additional binary systems PC + PDMS, PC + BDP, and BDP + PDMS, focusing on the specific chemical interactions. The decomposition pathways are revealed, focusing on the competing interaction between the components. Fire retardancy in PC/SiR/BDP is caused by both flame inhibition in the gas phase and inorganic-carbonaceous residue formation in the condensed phase. The PC/SiR/BDP does not work as well superimposing the PC/SiR and PC/BDP performances. PDMS reacts with PC and BDP, decreasing BDP's mode of action. Nevertheless, the flammability (LOI > 37%, UL 94 V-0) of PC/SiR/BDP equals the high level of PC/BDP. Indeed, SiR in PC/SiR/BDP is underlined as a promising impact modifier in flame-retarded PC/impact modifier blends as an alternative to highly flammable impact modifiers such as acrylonitrile–butadiene–styrene (ABS), taking into account that the chosen SiR leads to PC blends with a similar mechanical performance.…
Autor*innen: | Eliza Wawrzyn, Bernhard SchartelORCiD, Henrik Seefeldt, Karrasch, Christian Jäger |
---|---|
Dokumenttyp: | Zeitschriftenartikel |
Veröffentlichungsform: | Verlagsliteratur |
Sprache: | Englisch |
Titel des übergeordneten Werkes (Englisch): | Industrial & engineering chemistry research |
Jahr der Erstveröffentlichung: | 2012 |
Verlag: | American Chemical Society |
Verlagsort: | Washington, DC |
Jahrgang/Band: | 51 |
Ausgabe/Heft: | 3 |
Erste Seite: | 1244 |
Letzte Seite: | 1255 |
Freie Schlagwörter: | BDP; Decomposition; Flame retardancy; Flammability; PC; PDMS; Pyrolysis |
DOI: | 10.1021/ie201908s |
ISSN: | 0888-5885 |
ISSN: | 1520-5045 |
Verfügbarkeit des Dokuments: | Physisches Exemplar in der Bibliothek der BAM vorhanden ("Hardcopy Access") |
Bibliotheksstandort: | Sonderstandort: Publica-Schrank |
Datum der Freischaltung: | 19.02.2016 |
Referierte Publikation: | Ja |
Datum der Eintragung als referierte Publikation: | 16.02.2012 |